A method to determine the fracture energy of concrete is investigated. The fracture energy may be calculated from the area under the complete load-deflection curve which can be obtained from a stable three-point bend test. Several series of concrete beams have been tested. The Present experimental study indicates that the fracture energy decreases as the initial notch-to-beam depth ratio increases Some problems to be observed to employ the three-point bend method are discussed. The appropriate ratio of initial notch-to-beam depth to determine the fracture energy of concrete is found to be 0.5. It is also found that the influence of the self-weight of a beam to the fracture energy is very small A simple and accurate formula to predict the fracture energy of concrete is proposed.
Hot-wire measurements are reported on the developing turbulent flows subject to plane rate of strain in a rotating $90^{\circ}$ dog bend. The cross-section of the bend varies from $100mm{\times}50mm$ rectangular shape at the bend inlet gradually to the $50mm{\times}100mm$ shape at the bend outlet with remaining a constant area. Data signals from the rotating test section are transmitted through a slip ring to the personal computer which is located at the outside of the rotating disc. 3-dimensional velocity and 6 Reynolds stress components were calculated from the equations which correlate the fluctuating and mean voltage values measured with rotating a slant type hot-wire into 6 orientations. The effects of Coriolis and centrifugal forces on the mean motions and turbulence structures are investigated with respect to rotational speed.
Shemirani, Alireza Bagher;Haeri, Hadi;Sarfarazi, Vahab;Akbarpour, Abbas;Babanouri, Nima
Structural Engineering and Mechanics
/
제66권3호
/
pp.379-386
/
2018
The present study addresses the direct and indirect methods of determining the mode-I fracture toughness of concrete using experimental tests and particle flow code. The direct method used is compaction tensile test and the indirect methods are notched Brazilian disc test, semi-circular bend specimen test, and hollow center cracked disc. The experiments were carried out to determine which indirect method yields the fracture toughness closer to the one obtained by the direct method. In the numerical analysis, the PFC model was first calibrated with respect to the data obtained from the Brazilian laboratory test. The crack paths observed in the simulated tests were in reasonable accordance with experimental results. The discrete element simulations demonstrated that the macro fractures in the models are caused by microscopic tensile breakages on large numbers of bonded particles. The mode-I fracture toughness in the direct tensile test was smaller than the indirect testing results. The fracture toughness obtained from the SCB test was closer to the direct test results. Hence, the semi-circular bend test is recommended as a proper experiment for determination of mode-I fracture toughness of concrete in the absence of direct tests.
본 논문에서는 산업안전 공학의 중요부분의 하나인 산업안전모와 화재진압시 소방관들이 쓰는 방수모의 안전도가 어느 정도인가를 각종 실험장치를 50cm. 100cm, 120cm, 높이의 변화를 주어 가면서 같은 중량으로 낙하시켜 물체에 의한 낙하시 충격에 견디는 힘의 상태. 주파수 분석기에 의한 강도 및 bend의 응답신호 등을 연구하였다. 그 결과 안전모와 스프링상수와 관계, 두뇌부분과 지면사이에서의 충격흡수력. 탄성력 등이 어느 정도인가를 수식 및 실험을 통해 알아봤을 때 산업현장에서 사용하는 안전모보다는 방수모의 탄성력과 강도력이 컸으며 또한 충격흡수력도 양호하다는 것을 알 수 있었다. 그러나 Goldsmith, W.의 “Response of a realistic human head-neck model to impact” Vol.100. 1978. pp.25-52의 실험연구결과 기준치를 보면 인간두뇌에 충격물체로 부터 전달되는 충격파의 흡수력은 뇌파의 신경을 파손시키지 않으려면 최소한도의 주파수범위가 400Hz, 증폭화 0.00310 이하 이여야 된다고 역설하였다. 그러나 우리나라의 방수모 강도의 안전성 및 bend의 충격흡수력은 410-810Hz의 주파수치가 나타났다. 고층에서 일정중량의 물체로 충격을 받았을 때 어느 정도로 흡수력을 방수모 bend에서 받아들어야만 두뇌신경에 충격적인 영향을 끼치지 않나 하는 우리 실정에 맞는 기준치가 설정되어야만 할 것으로 안다. Goldsmith ,W. 박사의 연구결과에 의한다면 국내에서 생산되는 산업안전모보다는 강도 및 충격흡수력이 양호하나 국제수준에는 못미치고 있었다. 이제 우리 방수모도 강도뿐만 아니라 방수모 내부의 bend 즉, 방수모와 두부 사이에 충격흡수력 장치를 좀더 과학적인 실험방법으로 개선되어 화재 진압시 물체낙하로 인한 두부보호에 좀더 노력을 기울일 필요가 있어야 될 것이다. 한편 방열복을 입은 상태에서 불길에 뛰어 들었을시 내부의 온도변화, 인체에 미치는 영향 등은 실험장치 불족으로 많은 문제점이 발생, 보다 심층의 연구가 필요할 것을 인식하였으나 뒤로 미룬채 마무리 지었다.
본 연구에서는 굽힘-비틀림 커플링(bend-twist coupled, BTC) 설계개념을 적용한 10 MW급 복합재 풍력 블레이드의 구조 최적 설계를 수행하였다. BTC 설계개념은 동적 하중 상황에서 블레이드의 굽힘과 비틀림 거동 사이의 연동을 유도하여, 단면 받음각 변화에 의한 수동적인 적응 하중저감이 가능하다. 인자연구를 통해 최적의 BTC 설계인자를 추출하여 블레이드 구조설계에 적용하였다. BTC 개념이 동적 하중 감소에 미치는 영향을 가늠하기 위해 블레이드 루트 부에서의 피로등가하중을 계산한 결과, BTC 개념이 적용된 블레이드를 적용한 경우 피로등가하중이 2-3% 정도 감소하는 것을 확인할 수 있었다. BTC 효과를 시험적으로 검증하기 위해 1:29 비율의 블레이드 stiffener 축소모델을 제작하였으며, 정하중 시험을 통해 처짐 거동 시 끝단에서의 비틀림을 측정하였다.
불균형 모멘트가 작용하는 무량판 슬래브 내부접합부를 대상으로 폐쇄형 전단보강근으로 보강한 1개 실험체와 밴드형 전단보강근으로 전단보강한 2개의 실험체를 제작하여 구조성능을 평가하였다. 구조성능평가 결과, 구조설계기준(KBC 2009)으로 평가한 불균형모멘트는 실험결과의 95%로 매우 잘 일치하나, 개정 구조설계기준(KCI 2012)으로 산정한 불균형모멘트는 실험결과의 약 60%에 불과하여, 내부접합부의 불균형모멘트를 과대평가하는 것으로 나타났다. 밴드형 전단보강근은 기존 전단보강근과 비교하여 유사한 구조성능을 가지며, 시공성이 우수한 것으로 나타나 중진지역의 무량판구조물 설계 시 적용할 수 있는 것으로 평가되었다.
원자로 압력용기 재료인 SA 533 Grade B Class 1강의 파괴인성에 대하여 -4$0^{\circ}C$~288$^{\circ}C$의 온도 구간에서 Charpy 충격시편을 이용하여 연구하였다. 동적 파괴인성은 계장화 충격시험으로, 정적 파괴인성은 unloading compliance 방법에 따라 3-point bend test로 수행되었으며, 결과는 큰 시편에 의한 자료와 비교하였다. 온도에 대한 재료의 적절한 파괴인성치(하한값)는 천이온도 이상에서는 정직 파괴인성을, 그 이하의 온도에서는 동적 파괴인성을 택함으로써 유추할 수 있음을 알게 되었으며 side-groove가 14%이상일 때 시험은 ASTM E 813의 조건을 만족함을 보였다.
대한치과보존학회 2003년도 제120회 추계학술대회 제 5차 한ㆍ일 치과보존학회 공동학술대회
/
pp.575-575
/
2003
The majority of studies comparing the mechanical properties of brittle dental restorative materials now include use of the Weibull Modulus (m). This modulus is determined from analysis of the statistical distribution of strength measurements, which can be determined using a variety of methods, including biaxial flexure, 3pt bend and 4pt bend. In comparing materials it is usually implicitly assumed that the modulus (m) is independent of test method although it is recognised to be highly dependent on flaw distributions. However, in some cases flaw distributions can be modified by sample preparation and test method may modify stressing patterns. This study investigated the pattern of strength and m in two light setting materials.
Diagnosing and improving adhesion of advanced packaging and thin films is an essential part of the research and development in microelectronics. In this paper, the four-point bend test and the double cantilever beam test among various adhesion measurement methods are reviewed.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.