• 제목/요약/키워드: Average Grain Diameter

검색결과 71건 처리시간 0.021초

초음파법에 의한 저탄소강의 페라이트 결정립 크기 측정 (Measurement of Ferrite Grain Size by Ultrasonic Method in Low Carbon Steel)

  • 홍순택;권숙인;주웅용
    • 열처리공학회지
    • /
    • 제12권2호
    • /
    • pp.157-165
    • /
    • 1999
  • Grain size of steels is one of the most important parameters which influence yield strength and fracture toughness. Ultrasonic wave propagating in polycrystalline materials is mostly attenuated by scattering at grain boundary. Effect of ultrasonic attenuation on average ferrite grain size of carbon steels with tensile strength $40{\sim}60kgf/mm^2$ consisting of multi phases such as ferrite + pearlite and ferrite + pearlite + bainite was evaluated. The attenuation of these steels rapidly increased with average ferrite grain diameter. Average ferrite grain diameter ($D_{av}$, ${\mu}m$) could be expressed as $1.79+22.97*a^{1/2.03}$, where a is attenuation with unit of nepers/cm. From this study, it was confirmed that nondestructive ultrasonic method could be used in measuring average ferrite grain size indirectly.

  • PDF

국내산 낙엽송집성재의 지압특성 (Bearing Properties of Domestic Larix Glulam)

  • 김건호;홍순일
    • Journal of the Korean Wood Science and Technology
    • /
    • 제36권4호
    • /
    • pp.93-101
    • /
    • 2008
  • 하중방향(섬유평행방향, 섬유직각방향)과 접합구(볼트, 드리프트 핀) 적층면방향(평행, 수직)에 따른 국내산 낙엽송집성재의 지압강도시험을 실시하였다. 지압시편은 5 ply의 집성재를 사용하였고, 접합구의 직경은 12, 16, 20 mm를 사용하였다. 시험결과는 다음과 같다. 1) 볼트와 드리프트 핀의 각 직경에 따른 평균최대지압강도는 섬유평행하중방향의 경우 비슷한 경향을 보였으며, 섬유평행하중방향의 평균최대지압강도가 섬유직교방향보다 1.50~2.31배 높게 나타났다. 평균지압강도의 경우 섬유평행하중방향시편은 직경 16 mm에서 20 mm로 증가할 때 20% 감소하였으며, 섬유직교방향은 뚜렷한 경향이 없었다. 2) 평균지압초기강성의 경우 섬유평행하중방향은 직경 16 mm일 때 가장 크게 나타났다. 드리프트 핀 접합부의 전단강도실험 시 초기강성과 평균지압초기강성은 직경이 증가할수록 비슷한 경향을 보였다. 3) 지압강도시험 시 섬유평행방향시편의 파괴형상은 직경이 작을수록 할렬파단을 보였다. 섬유직교방향의 시편은 대부분이 섬유평행방향으로 할렬파단이 일어났으며 볼트가 드리프트 핀 시편보다 더 많이 나타났다. 4) 지압강도예측식을 통해 구한 예측지압강도와 실제 5% 유사항복지압강도를 비교하였을 경우 섬유평행방향은 KBCS, NDS의 예측지압강도와 비슷하게 나타났으나, 섬유직교방향은 NDS에서 제안한 예측식이 잘 적용되는 것을 알 수 있었다.

현장공기분사공정법(IAS)을 이용한 공기 영향반경과 흐름 양상 연구

  • 이준호;박갑성
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 2004년도 총회 및 춘계학술발표회
    • /
    • pp.213-217
    • /
    • 2004
  • Laboratory scale study for an area of influence and flowing aspect of groundwater saturated zone was conducted for three sediment grains. On the AMG(Average Modal diameter Grains) 0.34, 1.38, 3.89mm diameter samples, the affected area of the aquifer were 15.2, 37.0, 30.0%/m2 each. Air flow for AMG 0.34mm diameter grain size provides indication of pattern of channelized air flow in saturated zone and expansion state in above saturated zone. For AMG of 1.38, 3.89mm diameter grains, air flow are pervasive air flow, forming a symmetrical cone of influence around the injection point. And also AMG 1.38, 3.89mm diameter samples show onset of collapse and approach to steady state in above saturated zone, respectively. In this study, optimal sites for in situ air sparging, may be grain diameters between about AMC 1.5~2.5mm diameter.

  • PDF

Nail Withdrawal Behavior for Domestic Small Diameter Logs

  • Cha, Jae-Kyung
    • Journal of the Korean Wood Science and Technology
    • /
    • 제30권3호
    • /
    • pp.104-108
    • /
    • 2002
  • Nail withdrawal tests were conducted on clear wood of domestic small diameter logs. Nails were driven into the cross and longitudinal sections of each specimen, then nail withdrawal tests were performed. Nail withdrawal loads are strongly dependent on the direction of nail positions. The average load values for the nail withdrawal both in cross section and longitudinal section are higher in high specific gravity (SG) wood of sawtooth oak (Quercus acutissima Carr.) than those in low SG wood of Korean red pine (Pinus densiflora Sieb. et Zucc.) and pitch pine (Pinus rigida Mill.). The average ratio of the nail withdrawal loads for side-grain and end-grain are higher in the low SG wood than that in the high SG of wood. Both linear and non-linear regression analyses were conducted on nail withdrawal load with SG, good correlations were obtained between nail withdrawal load and SG.

Evaluation of Bearing Strength of Self-Tapping Screws according to the Grain Direction of Domestic Pinus densiflora

  • LEE, In-Hwan;KIM, Keonho;SHIM, Kug-bo
    • Journal of the Korean Wood Science and Technology
    • /
    • 제50권1호
    • /
    • pp.1-11
    • /
    • 2022
  • To evaluate the bearing strength of red pine cross-laminated timber (CLT) with self-tapping screw (STS), which is widely used as a fastener for connection in CLT building, the bearing test was conducted. Accoring to the STS's diameters (8, 10, 12 mm), the bearing test specimens with half hole were manufactured. Bearing strength was compared and reviewed in consideration of the configuration in STS and the loading direction to the grain of red pine. As a result of the bearing test on the STS's diameter, the yield bearing load increases as the larger diameter of the STS in all directions of the red pine. The bearing strength of the thread part (thread + tip) was higher than the shank part (shank + shank cutter). In compared with the directions to the grain of red pine, the bearing strength of the cross section parallel to the loading direction was the highest, and the tangent section was the lowest bearing strength. The average bearing strength of the loading direction in parallel to the grain was 23.43 MPa, which was about 45% higher than the average 16.16 MPa in perpendicular to the grain. The predicted bearing strength calculated by Eurocode (EN) and Korean Building Code (KBC)'s equation was lower than the experimental value. It is nessesary to propose the new equations of bearing strength reflected the configuration information of STS.

대수층 토양입자크기에 따른 공기분사 흐름 양상 (Effect of Sediment Size On Air Injection and Flowing Aspect of Groundwater Saturated Zone)

  • 이준호;박갑성
    • 한국지하수토양환경학회지:지하수토양환경
    • /
    • 제8권3호
    • /
    • pp.13-22
    • /
    • 2003
  • 현장공기분사공정의 복원효율에 있어서 중요한 인자로 작용 할 수 있는 것은 공기가 지하 포화대수층을 통과하면서 생기는 공기분사에 따른 흐름 양상과 토양입자크기에 따른 공기의 영향반경이다. 토양입자크기별 AMG 0.34, 1.38, 3.89 mm diameter 3가지 입자크기로 실험한 결과 AMG 0.34 mm diameter의 포화 대수층에서는 공기가 처음 결정된 방향으로만 흐르는 채널링 현상(channelized air flow)과 포화 대수층 가장 윗면에서는 확장모양(expansion state)을 가졌으며, 공기영향반경은 단위 면적당 15.2%/$\textrm{m}^2$이었다. AMG 1.38, 3.89 mm diameter의 포화 대수층에서는 공기가 퍼지는 현상(pervasive air flow)과 포화 대수층 가장 윗면에서는 각각 붕괴의 조짐(onset of collapse), 안정한 상태로 퍼짐모양(approach to steady state)을 가졌으며, 단위면적당 각각 37.0%/$\textrm{m}^2$, 30.0%/$\textrm{m}^2$영향반경이 계산되었다. 이 실험을 통해서 현장공기분사공정에 있어서 토양입자 크기에 따른 최대 영향반경효율을 얻을 수 있는 토양입자의 크기는 AMG 1.5-2.5 mm diameter로 사료된다.

Localized Corrosion Resistance and Microstructural Changes in UNS N07718 Alloy After Solution Heat Treatment

  • Yoon-Hwa Lee;Jun-Seob Lee;Soon il Kwon;Jungho Shin;Je-Hyun Lee
    • Corrosion Science and Technology
    • /
    • 제23권2호
    • /
    • pp.166-178
    • /
    • 2024
  • The localized corrosion resistance of UNS N07718 alloy was investigated after solution heat treatment. When the alloy was heat-treated at 1050 ℃ for 2.5 hours, it experienced an increase in average grain diameter, a reduction in grain boundary area, and the dissolution of delta phases along grain boundaries. Additionally, primary metallic nitrides (MN) and metallic carbides (MC), enriched with either Ti or Nb, were identified and exhibited a random distribution within the microstructures. Despite the solution heat treatment, the composition, diameter, and abundance of MNs and MCs remained relatively consistent. The critical pitting temperature (CPT), as determined by the ASTM G48-C immersion test, revealed similar values of 45 ℃ for both treated and untreated alloys. However, a decrease in maximum pit depth and corrosion rate was observed after the solution heat treatment. The microstructural changes that occurred during the heat treatment and their potential implications were discussed to understand the influence of the solution heat treatment.

High-Temperature Deformation Behavior of Ti3Al Prepared by Mechanical Alloying and Hot Pressing

  • Han, Chang-Suk;Jin, Sung-Yooun;Kwon, Hyuk-Ku
    • 한국재료학회지
    • /
    • 제30권2호
    • /
    • pp.57-60
    • /
    • 2020
  • Titanium aluminides have attracted special interest as light-weight/high-temperature materials for structural applications. The major problem limiting practical use of these compounds is their poor ductility and formability. The powder metallurgy processing route has been an attractive alternative for such materials. A mixture of Ti and Al elemental powders was fabricated to a mechanical alloying process. The processed powder was hot pressed in a vacuum, and a fully densified compact with ultra-fine grain structure consisting of Ti3Al intermetallic compound was obtained. During the compressive deformation of the compact at 1173 K, typical dynamic recrystallization (DR), which introduces a certain extent of grain refinement, was observed. The compact had high density and consisted of an ultra-fine equiaxial grain structure. Average grain diameter was 1.5 ㎛. Typical TEM micrographs depicting the internal structure of the specimen deformed to 0.09 true strain are provided, in which it can be seen that many small recrystallized grains having no apparent dislocation structure are generated at grain boundaries where well-developed dislocations with high density are observed in the neighboring grains. The compact showed a large m-value such as 0.44 at 1173 K. Moreover, the grain structure remained equiaxed during deformation at this temperature. Therefore, the compressive deformation of the compact was presumed to progress by superplastic flow, primarily controlled by DR.

탄탈륨 판재의 어닐링 집합조직과 결정립 크기 (Annealing Textures and Grain Size of Tantalum Sheet)

  • 강전연;박성원;박준영;박성준;송이화;박성택;김광련;오경원
    • 소성∙가공
    • /
    • 제28권5호
    • /
    • pp.247-256
    • /
    • 2019
  • In this study, the development of annealing textures in cold rolled and annealed tantalum sheets was analyzed using electron backscatter diffraction. At $900^{\circ}C$, the textures of the recrystallized grains in the partially and completely recrystallized microstructures displayed significant similarities. The average diameter of the recrystallized grains with ${\gamma}-fiber$ orientations exceeded that of grains with different orientations, and the average growth rates were unrelated to the orientations after an initial stage of recrystallization. Additional cold rolling and annealing was done for controlled initial microstructures and textures inherited from various processes of prior cold rolling and annealing. This second cycle of the process resulted in stronger textures with major ${\gamma}-fiber$ orientations as a result of the enhanced ${\gamma}-fiber$ orientations in the preceding textures. A coarse-grained prior microstructure resulted in a weaker annealing texture than a fine grained one regardless of the stronger previous texture, which was occasioned by the sub-structures of the minor orientations at local deformation inhomogeneities such as sharp in-grain shear bands.

곡물건조저장법 개선을 위한 농가용 Grain Bin에 관한 연구 (Study on the Small Grain Bin for the Improvement of Grain Drying and Storage)

  • 김성래
    • 한국농공학회지
    • /
    • 제16권1호
    • /
    • pp.3263-3291
    • /
    • 1974
  • Experimental work of grain bin was carried out to develop the methods of natural air in-bin drying and storage. The method is considered to be more economical, labour saving, and an effective countermeasure to grain loss. To examine the possibility of farm use of the grain bin and to analyze the related factors concerned with in-bin grain drying and storage, ambient air conditions (especially the change of air temperature and relative humidity) and grain quality during drying and storage periods were investigated. A laboratory model bin was constructed to investigate the effect of different forced air conditions on the drying characteristics of rice. In addition, a grain bin with 2.2m diameter and 1.8m height, considered to be the optimum size for the average Korean farm, was constructed and tested to examine the drying and storing characteristics of rice. The weather data analyzed in this study was the nine-year (from 1964 to 1972) record of air temperature and relative humidity in the Suweon area, and the thirty-year (from 1931 to 1960) record of pentad normal relative humidity and air temperature in the Seoul area. From the results of the weather data analyses, the adequate air delivery hours (which was arbitrary defined as the condition to give less than 75% relative humidity) to dry the rice during October were about nine hours (from approximately 10 A.M. to 7 P.M, ) a day, in which the average air temperature was about 15.9$^{\circ}C$ and average relative humidity was 66%. The occurence of days having three hours of such conditions was 1, 2, and 1-day within the 1st, 2nd add last 10-day periods for the month of October, respectively. Therefore, it may be considered that the weather condition in October was satisfactory for the forced natural air drying. The results of the laboratory model bin test were analyzed to obtain the drying curve and drying rate for different drying stages and grain layers in the bin corresponding to various conditions of forced natural air. A drying experiment with a prototype grain bin showed that an approximate 5 percent grain moisture gradient through a 1.6 meter grain deposit was observed after 80 hours of intermittent drying, giving an over dried zone in the lower grain layers and an extremely high grain moisture zone in the upper layers. This indicates that an effective measure should be taken to reduce this high moisture gradient. In order to investigate the drying characteristics of bulk grain in a layerturning operation a grain bin test was performed. This showed a significant improvement of uniform drying. In this test, approximate 107 hours were required to dry a depth of 1.6 meter of grain from an initial moisture content of 22.2 percent to a moisture content of 16.7 percent using an air delivery rate of 2.8 cubic meter per a minute per every cubic meter of grain. This resulted in a 2 percent moisture gradient from the top to the bottom of the bin. During storage period, till the end of June the average temperature of grain was 2~3$^{\circ}C$ higher than ambient air temperature. But during July when the grain moisture content went up slightly (less than 1 percent), the average temperature of the grain also increased to 3~5$^{\circ}C$ higher than ambient air temperature. It is therefore recommended that for safe grain storage, grain should not be stored in sheet metal bins after mid May. From the above results, in-bin rice drying and storage can be used effectively on Korean farms. It is strongly recommended that the use of grain-bin system should be implemented for farm use to improve farm drying and storage of rice.

  • PDF