동결, 고온-열탕 및 고온-고압처리된 토끼 장관골의 자가이식후 신생골 형성능의 비교 (Comparison of Osteogenic Potentials of Deep Freezed, Boiled and Autoclaved Autogenous Long Bone Graft in Rabbits)

  • 장한;김용식;이남기;김승기;이기행;고해석;조형래;이승구
    • 대한골관절종양학회지
    • /
    • 제2권1호
    • /
    • pp.18-26
    • /
    • 1996
  • We investigated the effect of deep-freezed, boiled and autoclaved autogenous long bone graft on the incorporation of the radial diaphyseal reconstruction in 30 rabbits by radiogram and histology for 8 weeks. Immediate histologic changes of 1cm of resected long bone treated by deep freezing, boiling and autoclaving in each 2 rabbits were also observed as control. Resected, boiled ($95^{\circ}C$ for 5 min.) and reimplanted bone was compared with resected, autoclaved ($131^{\circ}C$ for 5 min.) and reimplanted bone, and resected, deep freezed with liquid nitrogen for 5 minutes and thawing in saline and reimplanted bone in the reconstruction of bilateral radial defects in each of 8, and in total 24 adult rabbits. The results were as follows : 1. Immediate histologic changes showed that intracortical osteocytes in lacunae were partially necrotized and the cortex were faintly stained with they Masson trichrome stain in both boiled and deep freezed groups, while they completely necrotized and their cortex stained more weakly with Masson trichrome stain in autoclaved group which means less amount of collagen and protein in cortex of long bone. 2. Radiographies at 8 weeks showed complete union with more marked incorporation and external callus formation in all boiled and freezed groups, whereas there was delayed union in four of sixteen (25%) in autoclaved group. Histologically, at 8 weeks after boiled and freezed, more intense incorporation with new bone formation and neovascularization were observed, whereas transverse clefts consisted with delayed union in 4 cases of autoclaved group (25%) were observed at osteotomy site. Through these studies, the boilod and deeply freezed bones acted as an osteoinductive material as well as osteoconductive, but the autoclaved bone only as osteoconductive. Though boilod and deeply freezed bone showed higher osteogenic potentials than autoclaved bone, the necrotizing effect on cortical and boiled bone was inferior to that of autoclaved. Thus the deeply freezed bone can be used for the treatment of aggressive benign or less malignant bone tumor not involving cortical bone, but the autoclaved bone supplemented with bone graft for the treatment of malignant bone tumor involving cortex of long bone.

  • PDF

Bone Healing Properties of Autoclaved Autogenous Bone Grafts Incorporating Recombinant Human Bone Morphogenetic Protein-2 and Comparison of Two Delivery Systems in a Segmental Rabbit Radius Defect

  • Choi, Eun Joo;Kang, Sang-Hoon;Kwon, Hyun-Jin;Cho, Sung-Won;Kim, Hyung Jun
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • 제36권3호
    • /
    • pp.94-102
    • /
    • 2014
  • Purpose: This study aims to validate the effect of autoclaved autogenous bone (AAB), incorporating Escherichia coli-derived recombinant human bone morphogenetic protein-2 (ErhBMP-2), on critical-sized, segmental radius defects in rabbits. Delivery systems using absorbable collagen sponge (ACS) and fibrin glue (FG) were also evaluated. Methods: Radius defects were made in 12 New Zealand white rabbits. After autoclaving, the resected bone was reinserted and fixed. The animals were classified into three groups: only AAB reinserted (group 1, control), and AAB and ErhBMP-2 inserted using an ACS (group 2) or FG (group 3) as a carrier. Animals were sacrificed six or 12 weeks after surgery. Specimens were evaluated using radiology and histology. Results: Micro-computed tomography images showed the best bony union in group 2 at six and 12 weeks after operation. Quantitative analysis showed all indices except trabecular thickness were the highest in group 2 and the lowest in group 1 at twelve weeks. Histologic results showed the greatest bony union between AAB and radial bone at twelve weeks, indicating the highest degree of engraftment. Conclusion: ErhBMP-2 increases bony healing when applied on AAB graft sites. In addition, the ACS was reconfirmed as a useful delivery system for ErhBMP-2.

Stepwise verification of bone regeneration using recombinant human bone morphogenetic protein-2 in rat fibula model

  • Nam, Jung-Woo;Kim, Hyung-Jun
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • 제43권6호
    • /
    • pp.373-387
    • /
    • 2017
  • Objectives: The purpose of this study was to introduce our three experiments on bone morphogenetic protein (BMP) and its carriers performed using the critical sized segmental defect (CSD) model in rat fibula and to investigate development of animal models and carriers for more effective bone regeneration. Materials and Methods: For the experiments, 14, 16, and 24 rats with CSDs on both fibulae were used in Experiments 1, 2, and 3, respectively. BMP-2 with absorbable collagen sponge (ACS) (Experiments 1 and 2), autoclaved autogenous bone (AAB) and fibrin glue (FG) (Experiment 3), and xenogenic bone (Experiment 2) were used in the experimental groups. Radiographic and histomorphological evaluations were performed during the follow-up period of each experiment. Results: Significant new bone formation was commonly observed in all experimental groups using BMP-2 compared to control and xenograft (porcine bone) groups. Although there was some difference based on BMP carrier, regenerated bone volume was typically reduced by remodeling after initially forming excessive bone. Conclusion: BMP-2 demonstrates excellent ability for bone regeneration because of its osteoinductivity, but efficacy can be significantly different depending on its delivery system. ACS and FG showed relatively good bone regeneration capacity, satisfying the essential conditions of localization and release-control when used as BMP carriers. AAB could not provide release-control as a BMP carrier, but its space-maintenance role was remarkable. Carriers and scaffolds that can provide sufficient support to the BMP/carrier complex are necessary for large bone defects, and AAB is thought to be able to act as an effective scaffold. The CSD model of rat fibula is simple and useful for initial estimate of bone regeneration by agents including BMPs.

골연부 종양에서 저온 열처리한 자가골을 이용한 재건술 (Autogenous Low Heat Treated Bone Graft for Bone Reconstruction in Bone and Soft Tissue Tumors)

  • 전대근;이종석;김석준;조완형;곽봉준;이수용
    • 대한골관절종양학회지
    • /
    • 제4권2호
    • /
    • pp.81-87
    • /
    • 1998
  • Although autoclaved autogenous bone reconstruction is one of the established procedures, it may have some problems in bone regeneration and mechanical property. The purpose of this study is to evaluate the efficacy of more biologic and anatomical reconstruction where allograft is not readily available. From Aug.1991 to Feb. 1996 the authors analyzed 32 cases of reconstruction with autogenous low heat treated bone. Autogenous graft sites were humerus 4, tibia 4, pelvis 9, and 15 femur. Average follow-up period was 23(range;12-51) months. There were 49 graft-host junctional sites. Diaphysis was 22, metaphysis 10, and flat bone 17. Average duration of healing for the 38 united sites was 7 months. Average union time for each anatomical area 8 months in 19 diaphysis, 12 months in 7 metaphysis, and 12.7 months in 12 flat bone(pelvis). Eleven nonunion sites consisted of 3 diaphysis(3/22), 3 metaphysis(3/10), and 5 flat bone(5/17). Complications other than nonunion were local recurrence(4), bone resorption(3), graft fracture(2), osteomyelitis(1), metal failure(2), and wound infection(1). Initial bone quality and stable fixation technique was important for union rate. Plate and screw is a good method for diaphyseal lesion. Metaphyseal and flat bone are weak area for rigid fixation and one stage augmentation with iliac bone graft can be a salvage procedure.

  • PDF

생체골의 열전도성 및 열처리된 골의 염전력 변화에 대한 실험적 연구 (Experimental Studies on Heat Conductivity of Human Bone and Torsional Strength of Pasteurized Porcine Tibia)

  • 박일형;김신근;신동규;인주철
    • 대한골관절종양학회지
    • /
    • 제1권1호
    • /
    • pp.7-16
    • /
    • 1995
  • 인체골 4 시편(specimen)과 돼지 경골 25쌍을 이용하여, 생체골의 열전도성 측정과 열처리후 열처리온도와 시간에 따른 골의 염전력을 실험한 결과를 요약하면 다음과 같다. 인체골에 있어서 골수강을 제거하지 않고 $60^{\circ}C$의 항온식염수에서 열처리하면, 골심부의 온도가 $20^{\circ}C$에서 $58^{\circ}C$에 도달하는데 소요된 시간은 경골근위부가 32분 50초, 대퇴골 원위부가 30.분, $80^{\circ}C$ 항온조에서는 경골근위부가 12분 50초, 대퇴골 원위부가 11분 10초 소요되었다. 돼지 경골간부의 피질골내부(endosteum)에 열전대를 부착하고 뼈 양끝을 밀봉하여 같은 실험을 행한 결과 $50^{\circ}C$까지는 시간에 비례해서 일정한 비율로 온도상승이 이루어 졌으며, $20^{\circ}C$에서 $58^{\circ}C$에 이르는 시간이 $60^{\circ}C$ 항온조에서는 7분, $70^{\circ}C$에서는 3분 30초, $80^{\circ}C$에서는 2분이었다. 따라서 임상에서 골수강을 제거 후 장골의 간부(shaft) 만을 항온조에 달굴때는 골구강내에도 데워진 심염수로 가득차게 되므로 상기 시간의 절반이 못되는 짧은 시간내에 피질골의 내부가 $58^{\circ}C$에 이르리라고 판단되었다. 골수강을 소파하지 않은 돼지 경골을 각각 4쌍씩 우측만을 $60^{\circ}C$ 35분, $80^{\circ}C$ 15분 열처리한 후 실험군의 최대염전력은 대조군과 비교할 때 +7.0%, -5.1%, -3.2%, -4.2%의 변화가 있었고, $80^{\circ}C$ 15분 열처리후는 -4.3%, -3.8%, -1.4%(1예는 실험 오류로 제외됨)의 변화가 있었다. 골수강을 완전 제거한 되재 경골을 각각 4쌍씩 우측만을 $60^{\circ}C$, $70^{\circ}C$, $80^{\circ}C$에서 15분 열처리 후 실험군의 최대염전력은 대조군과 비교할 때 -3.4%, -4.2%, -0.7%, +2.7%의 변화가 있었고, $70^{\circ}C$ 15분 열처리후는 -2.8%, -3.9%, -2.1%(1예는 실험 오류로 제외됨)의 변화가 있었으며, $80^{\circ}C$ 15분 열처리후는 +5.2%, -4.4%, -2.9%, -0.3%의 염전력 변화가 있었다. 그러므로 골수강을 제거하지 않고 $80^{\circ}C$ 35분, $60^{\circ}C$ 15분 열처리 하거나, 골수강을 완전소파 후 $60^{\circ}C$ 15분, $70^{\circ}C$ 15분, $80^{\circ}C$ 15분 열처리해서는 각군사이에 염전력의 유의한 차이는없었다. 이상의 결과로 돼지 경골의 경우 $60^{\circ}C$ 항온에서는 35분까지, $80^{\circ}C$이하의 항온에서는 15분까지 열처리하여도 골강도에는 거의 영향이 없는 것으로 나타났다.

  • PDF