Microstructural evolution and the intermetallic compound (IMC) growth kinetics in an Au stud bump were studied via isothermal aging at 120, 150, and $180^{\circ}C$ for 300hrs. The $AlAu_4$ phase was observed in an Al pad/Au stud interface, and its thickness was kept constant during the aging treatment. AuSn, $AuSn_2,\;and\;AuSn_4$ phases formed at interface between the Au stud and Sn. $AuSn_2,\;AuSn_2/AuSn_4$, and AuSn phases dominantly grew as the aging time increased at $120^{\circ}C,\;150^{\circ}C,\;and\;180^{\circ}C$, respectively, while $(Au,Cu)_6Sn_5/Cu_3Sn$ phases formed at Sn/Cu interface with a negligible growth rate. Kirkendall voids formed at $AlAu_4/Au$, Au/Au-Sn IMC, and $Cu_3Sn/Cu$ interfaces and propagated continuously as the time increased. The apparent activation energy for the overall growth of the Au-Sn IMC was estimated to be 1.04 eV.
The effect of flip chip bonding parameters on formation of intermetallic compounds (IMCs) between Au stud bumps and Sn-3.5Ag solder was investigated. In this study, flip chip bonding temperature was performed at $260^{\circ}C$ and $300^{\circ}C$ with various bonding times of 5, 10, and 20 sec. AuSn, $AuSn_2$ and $AuSn_4$ IMCs were formed at the interface of joints and (Au, Cu)$_6Sn_5$ IMC was observed near Cu pad side in the joint. At bonding temperature of $260^{\circ}C$, $AuSn_4$ IMC was dominant in the joint compared to other Au-Sn IMCs as bonding time increased. At bonding temperature of $300^{\circ}C$, $AuSn_2$ IMC clusters, which were surrounded by $AuSn_4$ IMC, were observed in the solder joint due to fast diffusivity of Au to molten solder with increased bonding temperature. Bond strength of Au stud bump joined with Sn-3.5Ag solder was about 23 gf/bump and fracture mode of the joint was intergranular fracture between $AuSn_2$ and $AuSn_4$ IMCs regardless bonding conditions.
In this study, failure mechanisms of Au stud bumps/ACF flip chip joints were investigated underhigh current stressing condition. For the determination of allowable currents, I-V tests were performed on flip chip joints, and applied currents were measured as high as almost 4.2Amps $(4.42\times10^4\;Amp/cm^2)$. Degradation of flip chip joints was observed by in-situ monitoring of Au stud bumps-Al pads contact resistance. All failures, defined at infinite resistance, occurred at upward electron flow (from PCB pads to chip pads) applied bumps (UEB). However, failure did not occur at downward electron flow applied bumps (DEB). Only several $m\Omega$ contact resistance increased because of Au-Al intermetallic compound (IMC) growth. This polarity effect of Au stud bumps was different from that of solder bumps, and the mechanism was investigated by the calculation of chemical and electrical atomic flux. According to SEM and EDS results, major IMC phase was $Au_5Al_2$, and crack propagated along the interface between Au stud bump and IMC resulting in electrical failures at UEB. Therefore. failure mechanisms at Au stud bump/ACF flip chip Joint undo high current density condition are: 1) crack propagation, accompanied with Au-Al IMC growth. reduces contact area resulting in contact resistance increase; and 2) the polarity effect, depending on the direction of electrons. induces and accelerates the interfacial failure at UEBs.
탄탈륨실리사이드 히터가 내장된 소자를 Ag 페이스트와 Au SBB(Stud Bump Bonding)를 이용하여 Au가 코팅 된 기판에 각각 접합 하였다. 전단 테스트와 전류를 흐르면서 열 성능을 측정하였다. Au 스터드 범프 본딩의 최적 플립칩 접합조건은 전단 후 파괴면 관찰하여 설정하였으며, 기판 온도를 $350^{\circ}C$, 소자 온도를 $250^{\circ}C$에서 하중을 300 g/bump 로 하여 접합하는 경우가 최적 조건이였다. 히터에 5 W 인가시 소자의 온도는 Ag 페이스트를 이용한 접합의 경우 최대 온도는 약 $50^{\circ}C$이었으며, Au 금속층을 갖고 있는 실리콘 기판에 Au 스터드 본딩으로 접합된 인 경우 약 $64^{\circ}C$를 나타내었다. 기판과의 접촉면적이 와이어본딩과 Au 스터드 범프 본딩 가 약 300배가 차이가 나는 경우 약 $14^{\circ}C$ 차이를 나타내었고, 전사모사를 통하여 접합면의 접촉저항이 중요한 이유임을 알 수 있었다.
본 연구의 목적은 OSP, 전해 Au과 무전해 Ni/Au로써 표면처리를 달리한 연성회로기판 상에 Au 스터드 플립칩 범프의 초음파 접합 가능성을 연구하는 것이었다. Au 스터드 범프는 표면처리 방법에 상관없이 성공적으로 연성회로기판의 패드 상에 초음파 접합되었다 접합 강도는 접합 시간에 민감하게 영향을 받았다. 접합 시간이 길어짐에 따라 접합 강도는 증가하였으나, 2초 이상의 접합 시간에서는 이웃 범프끼리 단락되는 bridge 현상이 발생하였다. 최적 접합조건은 OSP 처리된 가판상에 0.5초간 초음파 접합하는 것이었다.
통신분야에서 사용주파수대역의 증가, 제품의 소형화 및 가격경쟁력등의 요구에 따라 RF 소자의 패키징 기술도 플라스틱 패키지 대신에 flip chip interconnection, MCM(multichip module)등과 같은 고밀도 실장기술이 발전해가고 있다. 따라서, 본 논문은 최근 수년간 보고된 응용사례를 중심으로 RF flip chip의 기술적인 개발방향과 장점들을 분석하였고, RF 소자 및 시스템의 개발단계에 따른 적합한 적용기술을 제시하였다. RF flip chip의 기술동향을 요약하면, 1) RF chip배선은 microstrip 대신에 CPW 구조을 선택하며, 2) wafer back-side grinding을 하지 않아서 제조공정이 단순하고 wafer 파손이 적어 제조비용을 낮출 수 있고, 3) wire bonding 패키징에 비해 전기적인 특성이 우수하고 고집적의 송수신 모듈개발에 적합하다는 것이다. 그러나, CPW 배선구조의 RF flip chip 특성에 대한 충분한 연구가 필요하며 RF flip chip의 초기 개발 단계에서 flip chip interconnection 방법으로는 Au stud bump bonding이 적합할 것으로 제안한다.
Interconnect - Wire bonding-> Flip chip interconnect ; At research step, Au stud bump bonding seems to be more proper .Package -Plastic package-> $Z_{0}$ controlled land grid package -Flip Chip will be used for RF ICs and CSP for digital ICs -RF MCM comprised of bare active devices and integrated passive components -Electrical design skills are much more required in RF packaging .Passive Component -discrete-> integrated -Both of size and numbers of passive components must be reduced
Microwave model and high-frequency measurement of the ACF flip-chip interconnection was investigated using a microwave network analysis. S-parameters of on-chip and substrate were separately measured in the frequency range of 200 MHz to 20 GHz using a microwave network analyzer HP8510 and cascade probe. And the cascade transmission matrix conversion was performed. The same measurements and conversion techniques were conducted on the assembled test chip and substrate at the same frequency range. Then impedance values in ACF flip-chip interconnection were extracted from cascade transmission matrix. ACF flip chip interconnection has only below 0.1nH, and very stable up to 13 GHz. Over the 13 GHz, there was significant loss because of epoxy capacitance of ACF. However, the addition of SiO$_2$filler to the ACF lowered the dielectric constant of the ACF materials resulting in an increase of resonance frequency up to 15 GHz. High frequency behavior of metal Au stud bumps was investigated. The resonance frequency of the metal stud bump interconnects is higher than that of ACF flip-chip interconnects and is not observed at the microwave frequency band. The extracted model parameters of adhesive flip chip interconnects were analyzed with the considerations of the characteristics of material and the design guideline of ACA flip chip for high frequency applications was provided.
This paper presents the development of new anisotropic conductive adhesives with enhanced thermal conductivity for the wide use of adhesive flip chip technology with improved reliability under high current density condition. The continuing downscaling of structural profiles and increase in inter-connection density in flip chip packaging using ACAs has given rise to reliability problem under high current density. In detail, as the bump size is reduced, the current density through bump is also increased. This increased current density also causes new failure mechanism such as interface degradation due to inter-metallic compound formation and adhesive swelling due to high current stressing, especially in high current density interconnection, in which high junction temperature enhances such failure mechanism. Therefore, it is necessary for the ACA to become thermal transfer medium to improve the lifetime of ACA flip chip joint under high current stressing condition. We developed thermally conductive ACA of 0.63 W/m$\cdot$K thermal conductivity using the formulation incorporating $5 {\mu}m$ Ni and $0.2{\mu}m$ SiC-filled epoxy-bated binder system to achieve acceptable viscosity, curing property, and other thermo-mechanical properties such as low CTE and high modulus. The current carrying capability of ACA flip chip joints was improved up to 6.7 A by use of thermally conductive ACA compared to conventional ACA. Electrical reliability of thermally conductive ACA flip chip joint under current stressing condition was also improved showing stable electrical conductivity of flip chip joints. The high current carrying capability and improved electrical reliability of thermally conductive ACA flip chip joint under current stressing test is mainly due to the effective heat dissipation by thermally conductive adhesive around Au stud bumps/ACA/PCB pads structure.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.