The Characteristics of Cr-Free Coating Hot Dip Galvanized Sheet Steel

  • Kim, Jong-Gi;Moon, Man-Been;Yun, Jeong-Mo
    • Corrosion Science and Technology
    • /
    • 제10권1호
    • /
    • pp.24-29
    • /
    • 2011
  • The greatest purpose of chromate treatment is to improve anti-corrosion by stabilizing a metal surface. Because metal surface forms a compound by absorbing oxygen or water in the air by being generally unstable, it is necessary to improve anti-corrosion of the metal by forming the metal surface with a stable film. When considering the economical efficiency and requirements together because the film of the metal surface treated with chromate has good anti-corrosion and the stability also in the air by being compact and strong, Chromate treatment has been used most up to the electronics industry from the auto industry. However, these days, because hexavalent chromium is both a toxic agent to be able to cause cancers and deadly poisonous environmental pollutant, the strong legal controls on its use is being imposed all over the world. Because of this reason, a new anti-corrosion method is being required. Also, by users' various demands, the passivations that have recently been developed require various characteristics such as conductivity, chemical resistance, alkali cleaning resistance as well as anti-corrosion. We could confirm the results such as excellent anti-corrosion compared to chromate, conductivity, chemical resistance and detergent resistance as the result of analysis of various characteristics of the galvannealed sheet steels coated with Cr-Free solution developed in this research.

차체구조물의 부식이 충돌안전도에 미치는 영향에 관한 연구 (The Study on Effect of Collision Safety by Corrosion of Body Structure)

  • 박인송;정태용
    • 한국자동차공학회논문집
    • /
    • 제10권4호
    • /
    • pp.141-148
    • /
    • 2002
  • Repair were made for front pillar, center pillar and side-step panel for lightweight vehicles with head-on and 40% off-set collision of 15 km/h in a RCAR standard. The salt dilution was sprayed and the compression tests were performed for vehicles with and without anti-corrosional treatment after repair. After 764 hours of salt-dilt sprayed test without using anti-corrosion, the mean penetration depth fur corrosion was shown to be 58% of the thickness. The resulyed decrease in bending stiffness by 10∼20% can cause reduction of the residual life and crash-absorption capability for damaged vehicles. The corrosoin safety tests showed that the anti-corrosional treatment should be made to improve the safety characteristics for a or damaged car.

역수압 작용을 고려한 방수·방식재의 부착강도 시험방법에 관한 연구 (A Study on the Test Methods of Bond Strength in Waterproofing and Anti-corrosion Materials by Reversed Pressure)

  • 김명지;최수영;최성민;오상근
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.232-233
    • /
    • 2014
  • Recently, water treatment facility is usually eastablished in underground, and waterproofing and anti-corrosion materials for concrete structures applied water treatment tank is developing in various ways. However, as the limit of research focused on durability improvement of top coating material, it is insufficient to study on the adhesion strength between the concrete surface and primer. Therefore, there is to confirm the adhesion of between concrete surface and the three primers used as anti-corrosion waterproofing materials, and to investigate the properties of adhesion strength according to the condition such as wet codition and water pressure condition of the concrete surface in this study.

  • PDF

열처리를 통한 3가 크롬도금층의 마모 및 부식특성 개선 (Improvement of the Wear Resistance and Anti-Corrosion of the Trivalent Cr Platings Using Heat Treatments)

  • 남기석;박율민;나종주;권식철
    • 열처리공학회지
    • /
    • 제16권6호
    • /
    • pp.335-340
    • /
    • 2003
  • To improve properties of wear resistance and anti-corrosion of the trivalent chromium platings, oxinitrocarbunsing and steam oxidation were conducted. Armophous trivalent Cr platings could be transformed to chromium carbides of high hardness, that showed low friction and wear rate. Even though micro-cracks were within as platings, superior anti-corrosion property was obtained by these treatments due to healing of cracks at the interface between the trivalent chromium platings and substrate.

Cu-Xwt%Sn 합금 위에 선택적 산화막 SnO2 형성 유·무에 따른 내변색 및 내부식특성 평가 (Evaluation of Anti-tarnishing and Corrosion Resistance of Cu-Xwt%Sn Alloy before and After Selective SnO2 Oxide Film according to Potentiostatic Electrolysis Treatment)

  • 최지웅;김혜성
    • 열처리공학회지
    • /
    • 제34권6호
    • /
    • pp.265-271
    • /
    • 2021
  • In this study, anti-tarnishing and corrosion characteristics of a single 𝛽1' and Bangjja Yugi alloy in the Cl- ion environment before and after potentiostatic electrolysis treatment were compared. Stable and uniform SnO2 oxide film with several nanometer thickness is formed after potentiostatic electrolysis treatment. In the case of Bangjja Yugi prior to potentiostatic electrolysis (PE) treatment for exposure in Cl- environment, tarnishing occurs rapidly within 0.5hr, whereas PE treated Bangjja Yugi indicates stable surface without tarnishing up to 3hr. Especially, it is noticeable that anti-tarnishing and corrosion characteristic of PE treated single 𝛽1', which were significantly improved by 3 times and 15 times, respectively, compared to conventional Bangja Yugi.

Burn Damage에 따른 도막의 방청성 평가 (Evaluation of the Corrosion Protection Coating in Accordance with Burn Damage)

  • 서창호;박진환
    • Corrosion Science and Technology
    • /
    • 제15권6호
    • /
    • pp.290-296
    • /
    • 2016
  • This study was conducted in order to examine the effect of burn damage and the resultant anti-corrosion performance. The breakdown and defect of the paint film caused by burn damage are considered to affect not only the macroscopic appearance but also the adhesive force and the anti-corrosion performance of the paint film. The material of the paint film was epoxy paint that is used most widely for heavy-duty coating, and in order to induce burn damage, heat treatment with a torch was applied to the other side of the paint film. Surface and chemical structure changes according to aging were analyzed using FE-SEM and infrared absorption spectroscopy, and variation in the anti-corrosion performance was analyzed through the AC impedance test.

니켈기 자융성 합금 코팅의 방식특성에 미치는 후열처리의 영향 (Effect of Fusing Treatment on Anti-Corrosion Characteristics of Ni-based Self-flux Alloy Coating)

  • 김태용;김재동;김영식
    • 동력기계공학회지
    • /
    • 제17권4호
    • /
    • pp.79-85
    • /
    • 2013
  • This study aims at investigating the effect of a fusing treatments on anti-corrosion characteristics of Ni-based self-flux alloy coating. Ni-based coatings were fabricated by flame spray process on steel substrates, and fusing treatments were performed using a vacuum furnace at $800^{\circ}C$ $900^{\circ}C$, $1000^{\circ}C$ and $1100^{\circ}C$. After fusing treatments, corrosion tests were carried out using potentiostat/galvanostat at solution with pH 2 and pH 6. Corrosion potential(Ecorr) and corrosion current density(Icorr) could be analyzed from polarization curve. Fusing-treated coating at $1100^{\circ}C$ showed more favorable anti-corrosion characteristics than as-sprayed coating. Anticorrosive effect of fusing-treated coating at solution with pH 2 was relatively greater than at solution with pH 6. Fusing-treated coating at $1100^{\circ}C$ showed the most excellent anti-corrosion characteristics.

미술작품의 보존을 위한 기화성 방청제 및 방청필름의 적용성 연구 (Applicability of Volatile Corrosion Inhibitor and VCI Films for Conservation of Artworks)

  • 범대건;한예빈
    • 보존과학회지
    • /
    • 제36권2호
    • /
    • pp.82-92
    • /
    • 2020
  • 현대 미술작품은 재료와 제작기법, 종류가 매우 다양하게 사용되고 있으며 특히 조각작품 중 많은 비율을 차지하는 금속의 경우 형태가 다양하고 여러 재질과 혼합된 작품이 다수 존재한다. 이러한 구조적, 재료적 특성은 보존처리 시 기존의 처리 방법을 적용하기 어려운 경우가 많아 보다 다양한 처리 재료 및 방법이 요구된다. 본 연구에서는 금속 작품의 효과적인 보존처리를 위해 방청제(Rust inhibitor, 防錆劑)를 작품에 직접적으로 도포하는 방법이 아닌 기화성 방청제를 적용하였으며, 기화성 방청제 및 이를 함유한 방청필름의 방청효과를 평가하였다. 금속 시편을 대상으로 기화성 방청제를 적용한 방청처리 결과, 시편의 색도 변화는 미미하였으며, 부식 속도는 방청 미처리 시편과 비교하였을 때 절반 정도 감소하는 것을 확인하였다. 방청필름 적용 실험 결과, 방청필름 사용 시 미처리 및 폴리에틸렌 필름을 사용한 시편보다 부식화합물의 발생이 감소하였다. 접촉각 및 표면에너지, 표면전기저항 측정을 통해 표면의 물성을 측정하였으며 방청피막이 형성됨을 확인하였다. 또한 기화성 방청제 및 방청필름을 실제 조각작품에 적용하여 방청효과를 확인하였다.

440A 강의 균일부식에 미치는 합금원소와 열처리의 영향(I) (The Effect of Alloying Elements and Heat Treatment on the Uniform Corrosion of 440A Martensitic Stainless Steel(I))

  • 김영철;강창룡;정병호
    • 동력기계공학회지
    • /
    • 제15권2호
    • /
    • pp.42-48
    • /
    • 2011
  • 440A martensitic stainless steels which were modified with reduced carbon content(~0.5%) and addition of small amount of nickel, vanadium, tungsten and molybdenum were manufactured. Effects of alloying elements and tempering temperatures on the uniform corrosion in the solution of lN H2S04 were investigated through the electrochemical polarization test. When tempering temperature is constant, corrosion current density in active-passive transition point, Icorr, decreased a little with an increase of austenitizing temperature. In addition to this, when austenitizing temperature is constant, longer holding time showed a little lower Icorr and Ipass, passive current density. And when austenitized at $1050^{\circ}C$ and tempered in a range of $350{\sim}750^{\circ}C$, best anti-corrosion properties were obtained at $350^{\circ}C$ tempering temperature while worst at $450^{\circ}C$ or $550^{\circ}C$. The specimens tempered at below $450^{\circ}C$ and above $550^{\circ}C$, similar and good anti-corrosion characteristics were obtained regardless of alloying elements added, showing anti-corrosion characteristics are influenced more by tempering temperature than by alloying elements.

Silane계 유무기 하이브리드 적용 합금도금강판 내식성 향상 코팅 기술 개발 (Development of anti-corrosive coating technique for alloy plated steel sheet using silane based organic-inorganic hybrid materials)

  • 박종원;이경황;박병규;홍신협
    • Corrosion Science and Technology
    • /
    • 제12권6호
    • /
    • pp.295-303
    • /
    • 2013
  • Silane surface treatments have been developed as an alternative for toxic and carcinogenic chromate-based treatments for years. It is consistently observed that ultra-thin films offer excellent corrosion protection as well as paint adhesion to metals. The silane performance is comparable to, or in some cases better than, that of chromate layers. Based on the tetra-ethylorthosilicate(TEOS) and methlyl trieethoxysilane(MTES), inorganic sol was synthesized and formed hybrid networks with $SiO_2$ nano particle and polypropylene glycol(PPG) on Zn alloyed steel surface. According to SST results, addition of 10nm and 50nm $SiO_2$ nanoparticle in synthesized solution improved anti-corrosion property by its shear stress relaxation effect during curing process. Also, SST results were shown that anti-corrosive property was affected by the amounts of organic compounds.