Active belite cement clinkers were synthsized by using natural raw materials with borax and calcium phosphate ({{{{ {Ca }_{3 }( {PO}_{4}) }}2) In both case {{{{alpha ^、 {C }_{2 }S }} were formed but borax was more efficient. The cement syn-thesized with the addition of borax was hydrated with the addition of anhydrite(5 wt%) and slag(30wt%, 40wt% 50wt%) The addition of 50wt% slag with anhydrite was good for strength development in 7days and the compressive strength was developed to twice than no addition of slag at 28 days strength.
The purpose of this study is to develope of alternative adimixture for manufacture of PHC pile(compressive strength above 800kg/$\textrm{cm}^2$). For the investigation, properties of alternative admixture admixed with II-anhydrite and pozollanic fine powders(e.q., Fly-ash, Silica-Fume), the fluidity and viscosity in the cement pastes, the fluidity and compressive strength in mortars at steam curing condition, were respectively examined. Also, properties of compressive strength of concretes with exiting admixture(specimen name SM) and alterantive admixture(specimen name AP) for PHC pile, at steam and standard curing condition, were compared each other. As a result of this experimental study, it was found that specimens admixed with II-anhydrite and pozollanic fine powders had an increase on the fluidity of cement paste and mortar, and compressive strength of mortar and concrete was as good as concrete with SM.
II형 무수석고의 평균 입경과 치환율이 시멘트페이스트의 유동성에 미치는 영향에 대해 비교하였다. 나프탈렌계(NSF)와 폴리카르본산계(NT-2) 등 2가지 고유동화제의 첨가량을 0~2.0wt%으로 변화시켰을 때 3종으로 구분한 II형 무수석고의 평균입경(4, 14, $35{\mu}m$)과 치환율(3, 5, 10, 15wt%)의 변화에 따른 영향을 측정하였다. 이들 변수들에 따른 영향을 측정하기 위하여 시멘트페이스트의 초기 유동성 및 경과시간별로 겉보기 점도를 관찰하였다. 시멘페이스트의 초기유동성은 II형 무수석고의 평균입경에 의한 영향보다는 II형 무수석고의 치환율 증가에 의한 영향이 더욱 큰 것으로 나타났다. II형 무수석고의 치환율을 10wt%로 고정시 NT-2, 1.0wt% 첨가로 시멘트페이스트의 유동성은 동일 첨가량의 NSF보다 크게 향상되었다. 이는 측정된 변수들의 범위 중에서 가장 우수한 시멘트 페이스트의 유동성을 보여주는 경우이다. NT-2, 1.0wt% 첨가에서 II형 무수석고의 치환율 증가에 따라 시멘트 페이스트의 겉보기 점도가 현저하게 감소되었다. 이로부터 시멘트 페이스트의 유동성 향상을 위해서는 NT-2의 첨가와 더불어 시멘트를 II형 무수석고로 일정비율 치환하는 것이 더욱 효과적임을 알 수 있었다.
In this study, the influence of specific surface area of cement, substitution ratio of gypsum anhydrite on the physical properties of concrete were investigated by measurements of slump, air content and compressive strength. The results showed that reducing the specific surface area of cement under 3200$\textrm{cm}^2$/g and using 20% of gypsum anhydrite were desirable to prevent the decrease in workability and strength of concrete in summer season.
In an effort to improve the mechanical properties of the belite cement active belite cement clinker was synthesized. Properties of the clinker were characterized by a XRD, FT-IE optical microscopy and SEM. The additive effects of slag on the hydration properties were investigated by the measurement of compressive strength heat evolution and SEM. The experimental results exhibited that the 3wt% borax was effective in stabilizing $\alpha$'-C2S and the addition of 5wt% anhydrite and 40wt% slag wee effective in the hydration.
II-anhydrite, slag, and fly ash produced as industrial by-product were reutilized for the manufacture of high strength admixtures for cement and concrete. The effects of these admixtures on the compressive strength of cement mortar and concrete were examined with those of domestic admixture. At the condition mortar and concrete. Especially, adding of II-anhydrite was very effective for the increasing of compressive strength. Therefore it is possible that these admixture as a high strength admixture apply to cement and concrete.
건축물 에너지 사용량과 온실가스 배출량 감소를 목적으로, 열적 물성 등이 향상된 새로운 단열소재가 개발 사용되는 추세이다. 이중 기존 단열소재의 문제점 (가연성, 처짐, 수분 취약성, 단열성능 저하 등)을 보완한 미네랄 하이드레이트 소재가 새롭게 사용되고 있다. 미네랄 하이드레이트는 건축물 구조체로 사용되는 ALC의 제조방법과 유사하나, 구조체가 아닌 단열소재만으로 사용된다는 특징을 갖는다. 미네랄 하이드레이트 제조를 위해서는 시멘트, 생석회 및 무수석고 등이 사용되며, 무수석고는 전량 수입에 의존하고 있다. 따라서 본 연구에서는 수입대체효과 뿐만 아니라, 폐기물 재활용 측면에서 무수석고를 대체하여 석유제조 공정 부산 탈황석고를 사용하고자 하였다. 탈황석고를 미네랄 하이드레이트 원료로 사용할 경우, 무수석고 전량과 생석회 일부를 대체할 수 있었다. 더불어 탈황석고를 사용한 미네랄 하이드레이트는 기존 무수석고 사용시와 유사한 열적, 물리적 특성도 발현되었다.
이 연구에서는 산업부산물을 재활용하는 차원에서 화학비료공장의 인산제조과정 중 부산물로 발생되는 인산부산석고($CaSO_4/H_2O$)를 이수석고 형태인 건조석고, 반수석고, III형 무수석고, II형 무수석고로 실험용시료를 제조하여 화학분석을 통해 그 석고의 품질특성을 분석하고 조건별로 제조된 석고를 각각 3.0%씩 고로슬래그 시멘트에 첨가하여 시멘트 품질에 미치는 영향을 연구하였다. 그 결과 석고의 제조 조건에서 온도가 높아질수록 석고의 품질이 향상되는 결과가 확인 되었으며 $700^{\circ}C$ 소성조건인 II형 무수석고에서 시멘트 품질에 영향을 미칠 수 있는 수용성인산($S-P_2O_5$)이 현저히 낮아지는 경향이 나타났다. 또한 고로슬래그 시멘트 적용 실험 결과 II형 무수석고에서 재령 3일 압축강도와 건조수축 길이변화가 양호한 것으로 나타났고 재령 56일에서 압축강도는 반수석고, III형 무수석고, 건조석고, II형 무수석고 순으로 높게 나타나는 경향을 보였다.
미량성분 첨가에 의한 클링커내 고온형의 C2S상의 합성과 혼합재에 의한 수화 활성도의 증진을 시도하였다. 미량성분으로 첨가한 borax와 Ca3(PO4)2의 경우 모두 고온형을 합성하였으나, borax의 경우가 더 효과적이었다. 즉 borax의 경우 1.5~3 wt%의 첨가로 고온형의 α-C2S의 합성을 용이하게 하였다. borax를 첨가하여 합성한 클링커를 분쇄하고, 무수 석고 (5wt%) 와 슬래그 (30 wt%, 40 wt%, 50 wt%)를 첨가하여 수화시켰다. 무수 석고와 50%슬래그 첨가시 수화활성도 증진은 수화 1일에는 별 효과를 보이지 않았으나, 7일 이후 강도 발현이 좋았으며, 압축강도는 슬래그를 첨가하지 않은 경우보다 28일 강도에서 약 2배의 증진을 나타내었다.
In this study, thermal-hydrological-chemical modeling for the alteration of a bentonite buffer is carried out using a simulation code TOUGHREACT. The modeling results show that the water saturation of bentonite steadily increases and finally the bentonite is fully saturated after 10 years. In addition, the temperature rapidly increases and stabilizes after 0.5 year, exhibiting a constant thermal gradient as a function of distance from the copper tube. The change of thermal-hydrological conditions mainly results in the alteration of anhydrite and calcite. Anhydrite and calcite are dissolved along with the inflow of groundwater. They then tend to precipitate in the vicinity of the copper tube due to its high temperature. This behavior induces a slight decrease in porosity and permeability of bentonite near the copper tube. Furthermore, this study finds that the diffusion coefficient can significantly affect the alteration of anhydrite and calcite, which causes changes in the hydrological properties of bentonite such as porosity and permeability. This study may facilitate the safety assessment of high-level radioactive waste repositories.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.