• Title/Summary/Keyword: Amalgam process

Search Result 30, Processing Time 0.026 seconds

Surface Treatments of Bronze Mirrors Excavated from Korean Peninsula (한반도 출토 청동거울의 표면처리 기법에 관한 연구)

  • Jeon, Ik-Hwan;Lee, Jae-Sung;Baek, Ji-Hye;Park, Jang-Sik
    • Journal of Conservation Science
    • /
    • v.22
    • /
    • pp.87-98
    • /
    • 2008
  • Microstructures and chemical compositions of 24 bronze mirrors recovered from the Korean peninsula were examined using the scanning electron microscope equipped with the energy dispersive spectrometer in an effort to characterize the treatments applied on their surface. Their provenance and chronology are mostly unspecified except for two objects from a Koryo burial site. In antiquity the surface of bronze mirrors was frequently finished by mere polishing when their tin content was high enough to guarantee the required reflectivity. In many cases, however, their surface was given a special treatment. The most typical treatment was to coat the surface with tin in two different processes referred to as wipe-tinning and amalgam-tinning. In wipe-tinning only tin was used, but in amalgam-tinning tin and mercury were used together. The surface was often coated with mercury in a process known as mercury-polishing. The present mirrors showed that all these techniques were in fact practiced, not only on the reflective surface but, in some cases, on the decorative surface. The detection of mercury played a crucial role in the assessment of a specific technique applied in each mirror. Mercury often remained in the substrate in the form of sulfide and thereby allowed the method of surface treatment to be estimated even when the coated layer was completely lost. The future study is expected to uncover the regional and temporal variation of the surface treatments to the better understanding of bronze mirrors with respect to provenance and chronology.

  • PDF

AN EXPERIMENTAL STUDY ON THE INFLUENCE OF FORMOCRESOL TO THE HEALING PROCESS OF AMPUTATED PULP (Formocresol이 손상치수조직(損傷齒髓組織) 치유(治癒)에 미치는 영향(影響)에 관(關)한 실험적(實驗的) 연구(硏究))

  • Kwon, Hyuk-Choon
    • Restorative Dentistry and Endodontics
    • /
    • v.12 no.2
    • /
    • pp.27-32
    • /
    • 1987
  • After a vital pulpotomy in human permanent teeth, the responses of the remaining pulp tissue under formocresol was studied histologically. The class I cavity was prepared on the teeth and the pulp was amputated. Formocresol was placed over the amputated tissue and the cavity was sealed with zinc phosphate cement and amalgam. The teeth were extracted after 1, and 3 weeks following the operation and were decalcified, sectioned and stained with hematoxylin and losin. Microscopic examination reveals as follows; I. Healing of the pulp at the amputated site did not occur in the pulps treated with formocresol. 2. At one week the pulps were normal except only slight inflammatory reaction. 3. At three weeks, the pulps showed the most serious inflammation, bleeding and necrotic state.

  • PDF

A Study of Conservation treatment and Scientific Analysis for Gilt-bronze ornament Excavated from DeokCheon-Ri, Gyeong Ju (경주 덕천리 유적 출토 금동장식의 보존처리 및 과학적 분석 연구)

  • Seo, Jung-eun;Han, Min-su;Ham, Chul-hee
    • 보존과학연구
    • /
    • s.27
    • /
    • pp.23-42
    • /
    • 2006
  • This study is about gilt bronze ornament, that is from Deok Cheon-Ri in Gyeong Ju, of conservation treatment process and of scientific analysis. This relic gathered with soil around the relic by Polyurethane foam. While the relic got rid of soil, Took X-rays. As the result, we decided to process reconstruction as condition that the relic was dug up. After the conservation treatment processed, we made a frame to display the relic. Investigated manufacture techniques of the relic after the conservation treatment processed, and thenexecuted scientific analysis of the relic for a chemical experiment. A analysis of the results of components for composition layers using the SEM-EDS can be briefly summarized as below; Firstly, the average contents of outer, inner and body corrosion layer have a Cu-60.9~39.3wt% and analyzed a little impurities material which is Fe-0.5wt%.Secondly, the average contents of body have a Cu-99.7wt% which was using manufactured by pure copper. Thirdly, gold layer have a mercury of 9.5wt% which indicate that layer was manufactured by mercury amalgam gilding technique.

  • PDF

A Study on Elemental Diffusion in Gilded Artifacts (도금 유물에서 확인되는 확산 현상에 관한 연구)

  • Jeon, Ik-Hwan;Lee, Jae-Sung;Park, Jang-Sik
    • Journal of Conservation Science
    • /
    • v.26 no.2
    • /
    • pp.109-120
    • /
    • 2010
  • Four gilded bronze objects and a gilded silver object were examined for elemental diffusion between the gilding layer and the mating matrix. The gilded bronzes consist of three objects from three different historical periods, the Korean Three Kingdoms period, the Koryo and the Choseon periods and one from an unknown period. The gilded silver was from the Koryo period. The amalgam process seems to have been the major technique employed for all of them in gilding. The occurrence of substantial diffusion was observed in all but the anonymous object, particularly in the Choseon artifact where evidence was found that the diffusion phenomenon was intentionally utilized in gilding. The gold content in the gilded bronzes decreases gradually from surface to interior while the copper content increases to the interior, making it difficult to locate the boundary between the gilding layer and the matrix. This gradual change in composition must have resulted from elemental diffusion at elevated temperatures. The oxygen content negligible in the gilding layer precludes the possibility of corrosion being responsible for the varying composition. It is observed that non-uniform diffusion caused variation of colors in the surface of gilded bronzes. The change of colors induced by diffusion, which is always accompanied by the unique surface morphology and chemical compositions, is distinguished from the color change by corrosion. In the gilded silver object, diffusion of mercury was observed along with that of gold and silver.

HISTOPATHOLOGIC STUDY ON THE HEALING PROCESS OF APICAL WOUND IN APPLYING SEVERAL MATERIALS (치근단 손상부의 치유에 영향을 미치는 제재에 관한 병리조직학적 연구)

  • Cho, Young-Gon
    • Restorative Dentistry and Endodontics
    • /
    • v.14 no.2
    • /
    • pp.49-64
    • /
    • 1989
  • The purpose of this study was to evaluate the effect of several materials on the healing process of apical wound. Sixteen mandibular premolars obtained from 4 healthy dogs were used for this study. Under general anesthesia, the pulpal chamber of each tooth was opened and the pulps were extirpated. The root canals were then instrumented with H-file and irrigated with physiologic saline solution ; the apices were purposely perforated and enlarged with the engine K-reamer. In the experimental groups, apical wounds were filled with one of calcium hydroxide, hydroxylapatite, and tricalcium phosphate materials, mixture of each materials and physiologic saline solution, with a lentulo spiral. In the control group, apical wounds were not filled with any material. All the root canals were filled by the lateral condensation technique with gutta-percha cone and ZOE sealer. The access opening of all the teeth were closed with amalgam. On the 10, 20, 40 and 60th day after experiment, experimental animals were sacrificed. Segments of jaws, each containing one tooth, were fixed in 10% formalin solution and decalcified in Plank-Rychlo solution. The specimens were embedded in paraffin and serially sectioned to an average thickness of $6{\mu}m$. The sections were stained by hematoxylin-eosin and Masson's trichrome stain method and examined under light microscope. The results were as follows : 1. In the experimental groups, the new bone formations were observed in apical wounds. 2. Fourty days later, apical wounds were healed by granulation tissue in the experimental groups, but were not healed by granulation tissue in the control group, and the healing process of experimental groups were more rapid than that of control group. 3. Sixty days later, chronic inflammation disappeared in the experimental groups, and the materials used showed biologic affinity to the periapical tissue. 4. In all the groups, the resorption of cementum appeared on the 10th and 20th day after experiment, and the deposition of cementum appeared on the 40th and 60th day after experiment, especially showing narrowness of apical foramen due to newly formed cementum in calcium hydroxide group. 5. Calcum hydroxide and tricalcium phosphate particles were gradually resolved, but hydroxylapatite particles were not resolved through the experimental period.

  • PDF

Electrochemical Behaviors of Copper-1-(2-Thiazolylazo)-2-naphthol Complex in Acetonitrile (아세토니트릴 용매 중에서 Copper-1-(2-Thiazolylazo)-2-naphthol 착물의 전기화학적 거동)

  • Bae Zun Ung;Lee Heung Lark;Park Tae Myung;Seo Moo Lyong
    • Journal of the Korean Chemical Society
    • /
    • v.35 no.4
    • /
    • pp.405-409
    • /
    • 1991
  • The electrochemical behaviors of copper-1-(2-thiazolylazo)-2-naphthol [Cu(II)-TAN] complex in acetonitrile (AN) solution have been investigated by the use of polarography, controlled potential coulometry and UV-Vis spectroscopy. Cu(II)-TAN complex exhibit three reduction waves at -0.91 V, -1.34 V and -1.65 V vs. S.C.E. in acetonitrile solution containing 5.0 ${\times}\;10^{-3}$M tetraethylammonium perchlorate. Every reduction wave is diffusion controlled. The first reduction wave is considerably reversible and this process is attributed to the formation of anion radical. The second reduction process to the dianion is followed by a chemical reaction producing a complex of hydrazo complex. The third reduction process produce Cu(Hg) amalgam and amine compound.

  • PDF

Case report: Full mouth rehabilitation for patient with heavy occlusal force and excessive abrasion (강한 교합력과 과도한 마모를 보이는 환자의 전악수복 증례)

  • Park, Ji-Hee;Vang, Mong-Sook;Yang, Hong-So;Park, Sang-Won;Yun, Kwi-Dug;Lim, Hyun-Pil
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.51 no.2
    • /
    • pp.119-124
    • /
    • 2013
  • Many of the patients with extensive abrasion need comprehensive restorative treatment. The abrasion is usually caused by attrition, besides of it, there are many reasons for it. The plan of treatment should be started on assessment of the type of attrition and the etiologic analysis. Patient with well-developed masticatory muscle, alveolar process, and high occlusal force and also with little muscle length difference between the stable and the contracted state should be carefully assessed for the vertical dimensional loss and the restoration should be carefully designed. Decrease of tooth length can be compensated by the growth of the alveolar bone height; therefore, consistency of the occlusal vertical dimension is maintained. Accordingly, a careless increase of the vertical dimension can produce muscle fatigue, depressed tooth and pain, and fracture of the restoration. In this case, the patient with multiple tooth abrasion and clenching habit, the edentulous maxillary area is restored with amalgam inserted RPD, and the dentulous area of the maxilla and mandible are treated with fixed restoration accompanying with the increase of vertical dimension. Consequently, we are going to report about the satisfying result in both functional and esthetic aspects.

The Gilt Bronze Saddle Accessory Excavated from Tomb No. 89 of Kyodong in Changnyong 75 - Reports on Conservation Treatment and Manufacturing Technique - (창녕(昌寧) 교동(校洞) 제 89호분 출토 금동제 안교장식 - 보존처리와 제작기법 조사 -)

  • Kim, Kyung-hee;Han, Man-sung;Ahn, Byong-chan
    • Conservation Science in Museum
    • /
    • v.1
    • /
    • pp.75-86
    • /
    • 1999
  • Conservation treatments were done for the gilt bronze saddle accessory excavated from Tomb No. 89 in Kyo-dong, Changnyong in Japanese rule period. The saddle accessory, broken into numerous pieces, was mixed with other remains. Principal aims of conservation treatments were to recover original shape of object and stabilize its material. In the process of treatments manufacturing technique of the remain was examined minutely. Thick layers of corrosion substances were peeled off and numerous pieces were pasted together to restore the original shape. And then the saddle accessory was mounted on an acrylic board to be handled and exhibited safely. In this process, it was confirmed that various ancient techniques of metalic crafts such as amalgam gilding, riveting, piercing, line engraving, stamping, chasing etc. had been used to make the saddle accessory.

Morphology, Mineralogy and Genetic Implication of Placer Gold from the Huongkhe Area, Vietnam (베트남 홍케 지역 사금의 산상과 생성연구)

  • Choi, Sang-Hoon;Choi, Seon-Gyu;Han, Jin-Kyun
    • Economic and Environmental Geology
    • /
    • v.29 no.3
    • /
    • pp.235-246
    • /
    • 1996
  • Placer gold in collected heavy minerals from several localities in Huongkhe area, is consistently very finegrained (${\leq}100$ to $400{\mu}m$). The size and size distribution show somewhat differences at Dongdo and Hoahai : at Dongdo, predominant relatively larger and wide distribution; at Hoahai, characteristic relatively finer and narrow distribution range. The morphology of gold grains is divided into the four groups assumed by the dimension ratio : spherical, subprismoidal, prismoidal, and irregular. The gold grains at Dongdo show wide morphological distribution, whereas, at Hoahai, spherical form is predominant (${\approx}75%$). Three main types of gold are classified based on their chemical composition and mode of occurrence: type I (electrum; fineness=568~931), type II (amalgam; fineness=671~927), and type III (native gold; fineness=923~999). Type I gold contains, relatively high and variable silver contents (${\approx}11$ to 58 atomic % Ag), and has been classified into two subtypes based on their silver contents (type IA, ${\approx}11{\sim}39$ atomic % Ag; type IB, ${\approx}40{\sim}58$ atomic % Ag). However, type I gold would have been generally original compositions of electrum which originated at the provenance deposits. Mercury reacts with gold and silver to form amalgam (type II gold) which has variable Hg contents (1.2~30.5 atomic % Hg). The mercury contents in gold grains at Hoahai (10.9~30.5 atomic % Hg) are higher than those at Dongdo (5.8~21.1 atomic % Hg). The gold grains from the area generally exhibit a high-purity gold (type III) rim. The individual rims on the various grains range from <1 to $80{\mu}m$ in thickness and have silver contents of <10 atomic percent Ag, even though the core compositions range from ${\approx}11$ to 58 atomic percent Ag. The rim of gold most likely is responsible for the commonly cited cases of gold from placer deposits assaying at higher values of fineness than the gold in the corresponding source lode. The gold-rich rim in the Huongkhe area apparently forms by a combination of self-electrorefining and preferential dissolution of silver under oxidizing nature during the weathering and transport process. All data of gold grains in the Huongkhe area suggest that the transport distances and/or time of placer gold at Hoahai are generally farther than those at Dongdo. The mercurian gold bearing provenance deposits at Dongdo and Hoahai would be suggest nearest epithermal gold-silver vein-type.

  • PDF

Conservation and Analysis of Gilding Silver Buddhas and Relics Discovered Inside Buddha of Joseon Period (조선시대 은제금도금불상과 그 복장품의 보존처리 및 재질연구)

  • Kwon, Yoonmi;Park, Seungwon;Yu, Heisun;Choi, Heeyoon;Yun, Eunyeong
    • Conservation Science in Museum
    • /
    • v.9
    • /
    • pp.31-49
    • /
    • 2008
  • We have investigated and conserved three small Buddha statues dating from Joseon period that were purchased by the National Museum of Korea. Chemical analysis and investigation of internal structures were enabled us to identify its compositions and hollow spaces which have various materials just like fabrics, silver ornaments, beads and wood fragments. The fabrics date from the early years of the Joseon dynasty to the middle one. The compositions of matrix of the Buddha statues vary 80-90 wt% Ag and 7-15 wt% Cu. And its surface layers were gilt with amalgam. Mechanical and chemical cleaning with EDTA-2Na were applied together during the cleaning process.