마그네슘 주조성형기술의 개발동향 (Development Trend of Magnesium Casting Technology)

  • 김현식;예대희;강민철
    • 한국주조공학회지
    • /
    • 제31권5호
    • /
    • pp.243-248
    • /
    • 2011
  • Magnesium alloys have many advantages such as light-weight, high machinability, damping capacity, etc. So magnesium alloy parts have been used in transportation, mobile phone, military industries. Because of HCP atomic structure, Magnesium is very difficult in plastic deformation process, so most of magnesium products are fabricated by casting process. Magnesium alloys have low heat-capacity, high fluidity and low Fe solubility. For these reasons it is more suitable than aluminum in mass-production by casting. And various casting technologies have been developed. So casting technologies for magnesium developed recently is discussed in this paper.

쌍롤 주조법에 의해 제조한 알루미늄 합금의 미세조직 (Microstructures of Twin Roll Cast Aluminum Alloys)

  • 박종우;김희수;백남익
    • 한국주조공학회지
    • /
    • 제16권2호
    • /
    • pp.149-157
    • /
    • 1996
  • Several aluminum based alloys were fabricated by a twin roll strip casting mill. As-cast microstructures and microsegregations of these aluminum alloys were investigated by means of optical microscope, scanning electron microscope and electron probe micro analysis. Clear distinction on microsegregation among the alloy systems was observed, that is, A1235 and A8011 alloys showed diffused segregation in the middle of the strip, while A3003 and A5086 alloys revealed a centerline segregation consisted of lamellar structure. Above center line segregation was resulted from enrichment of the alloying elements such as Mn, Fe, Cu, Si and eutictic reaction in central region of the alloy strip.

  • PDF

알루미늄 소재의 레오로지 직접단조공정에서 가압력이 액상 편석에 미치는 영향 (The Effect of Pressure on Liquid Segregation in Direct Rheo-Forging Process of Aluminum Alloys)

  • 오세웅;배정운;강충길
    • 소성∙가공
    • /
    • 제16권3호
    • /
    • pp.178-186
    • /
    • 2007
  • Rheo-forging process of aluminum alloy is suitable for large parts of net shape without defects and excellent mechanical properties in comparison with conventional die casting and forging process. To control the microstructure of the product with high mechanical properties in rheo-forming, solid fraction is required to prevent porosity and liquid segregation. Therefore, in rheo-forging process, die shape, pressure type and solid fraction are very important parameters. The defects such as porosity, liquid segregation and unfitting phenomena occur during rheo-forging process. To prevent these defects, mechanical properties and microstructure analysis of samples versus the change of pressure are carried out and the problem and its solutions are proposed. Also, the mechanical properties versus various pressures were compared with and without heat treatment. The alloys used for rheo-forming are A356 and 2024 aluminum alloy. The rheology material is fabricated by electromagnetic process with controlling current and stirring time.

Mg-Al계 합금의 기계적 성질에 미치는 Al의 영향 (The effects of aluminium contents on the mechanical properties of magnesium-aluminium alloy)

  • 맹완영;백정하;오인상;남태운
    • 열처리공학회지
    • /
    • 제7권2호
    • /
    • pp.139-146
    • /
    • 1994
  • In the molten state, magnesium alloys vigousey react with oxygen in the air, is protected from oxidation and burning by the addition of $SF_6$ to $CO_2$ atmosphere over the melt. The mechanical properties and metallographic examinatin have made of Mg-Al alloys containing 3, 6, 9% in the solution treated state and precipitated state, comparing mechanical properties obtained during unidirectional solidification with me chanical properties obtained during conventional casting. For a given solution treatment, a higher aluminum contents produce more or less fine grains in conventional casting. For a given artifical aging treatment, a higher aluminum contents produces much precitates at the grain boundary as well as within the grain in unidirectional solidification. As a result of this experiment, for a given heat treatment, the higher is aluminum contents the higher is the ultimate tensile strength, yield strength, hardness while the lower the elongation. Also the mechanical properties of unidirectional solidification is larger than that of conventional casting.

  • PDF

AC4A 알루미늄 합금의 주조특성에 미치는 미량 첨가원소의 영향 (Effect of Minor Additives on Casting Properties of AC4A Aluminum Casting Alloys)

  • 오승환;김헌주
    • 한국주조공학회지
    • /
    • 제37권5호
    • /
    • pp.148-156
    • /
    • 2017
  • The effects of minor additives on the casting properties of AC4A aluminum alloys were investigated. Measurements of the cooling curve and microstructure observations were conducted to analyze the effects of Ti-B and Sr minor elements during the solidification process. A fine grain size and an increase in the crystallization temperature for the ${\alpha}-Al$ solution were evident after the addition of 0.1wt% Al-5%Ti-1%B additive. The modification effect of the eutectic $Mg_2Si$ phase with the addition of 0.05% Al-10%Sr additive was prominent. A fine eutectic $Mg_2Si$ phase and a decrease in the growth temperature of the eutectic $Mg_2Si$ phase were evident. Fluidity, shrinkage and solidification-cracking tests were conducted to evaluate the castability of the alloy. The combined addition of Al-5%Ti-1%B and Al-10%Sr additives showed the maximum filling length owing to the effect of the fine ${\alpha}-Al$ grains. The macro-shrinkage ratio increased, while the micro-shrinkage ratio decreased with the combined addition of Al-5%Ti-1%B and Al-10%Sr additives. The macro-shrinkage ratio was nearly identical, while the micro-shrinkage ratio increased with the addition of the Al-10%Sr additive. The tendency of the occurrence of solidification cracking decreased owing to the effect of the fine ${\alpha}-Al$ grains and the modification of the $Mg_2Si$ phase with the combined addition of Al-5%Ti-1%B and Al-10%Sr additives.

용융금속 교반공정을 통한 고Fe 함유 A356 합금의 미세조직 개질 (Microstructural Modification of High-Fe Containing A356 Alloy by Liquid Metal Shearing Process)

  • 김봉환;이상목
    • 한국주조공학회지
    • /
    • 제31권6호
    • /
    • pp.354-361
    • /
    • 2011
  • The liquid metal shearing device was constructed and assembled with a commercial high-pressure die-caster in order to induce intensive turbulent shearing force on molten aluminum alloys. The effect of the liquid metal shearing on the microstructure and tensile properties of A356 alloys was investigated with the variation of iron content. The experimental results show that dendritic primary ${\alpha}$-Al phase was effectively modified into a equiaxed form by the liquid metal shearing. It was also found that the needle-like ${\beta}$-AlFeSi phase in a Fe containing A356 alloy was changed into a blocky shape resulting in the improved mechanical properties. Based on the mechanical properties, it was suggested that the iron content in A356 alloy could be more widely tolerated by utilizing the liquid metal shearing HPDC process.

알루미늄 합금 주물의 냉각 속도에 따른 기계적 성질 예측 (Effect of Cooling Rate on the Prediction of Mechanical Properties of Al Alloys)

  • 동권식;조인성;황호영
    • 한국주조공학회지
    • /
    • 제32권5호
    • /
    • pp.225-230
    • /
    • 2012
  • In this study, a more practical and simulation approach which can predict the mechanical properties of aluminum alloys is proposed. First, cooling rate, micro-structure, and mechanical properties of casting product were measured through casting experiment. The relation between cooling rate and SDAS decrease exponentially and the linearly decreasing relation exist between SDAS and mechanical properties. Then, the cooling rate was calculated by casting process simulation and the mechanical properties were predicted by using the relations that were derived through experiment. Experimentally measured mechanical properties and predicted values by simulation were in the range of relatively small difference. The mechanical properties of various Al alloys are expected to be predicted by the casting process simulation before actual casting.

급속응고한 Al-Be합금의 미세조직 및 인장특성 (Microstructure and Tensile Property of Rapidly Solidified Al-Be alloy)

  • 이인우;박현호;김명호
    • 한국주조공학회지
    • /
    • 제15권5호
    • /
    • pp.459-468
    • /
    • 1995
  • For high performance aerospace structures, the properties of highest priority are low density, high strength, and high stiffness(modulus of elasticity). Addition of beryllium decrease the density of the aluminum alloy and increase the strength and the stiffness of the alloy. However it is very difficult to produce the Al-Be alloy having useful engineering properties by conventional ingot casting, because of the extremely limited solid solubility of beryllium in aluminum. So, rapid solidification processing is necessary to obtain extended solid solubility. In this study, rapidly solidified Al-6 at% Be alloy were prepared by twin roll melt spinning process and single roll melt spinning process. Twin roll melt spun ribbons were extruded at $450^{\circ}C$ with reduction in area of 25 : 1 after vacuum hot pressing at $550^{\circ}C and 375^{\circ}C$. The microstructure of melt spun ribbon exhibited a refined cellular microstructure with dispersed Be particles. As advance velocity of liquid/solid interface increase, the morphology of Be particle vary from rod-like type to spherical type and the crystal structure of Be particle from HCP to BCC. These microstructural characteristics of rapidly solidified Al-6at.%Be alloy were described on the basis of metastable phase diagram proposed by Perepezko and Boettinger. The extruded ribbon consisted of recrystallized grains dispersed with Be particles and exhibited improved tensile property compared with that of extruded ingot.

  • PDF

자동차 부품용 내열 알루미늄 합금의 고온 피로 변형 거동 (High Temperature Fatigue Deformation Behavior of Automotive Heat Resistant Aluminum Alloys)

  • 박종수;성시영;한범석;정창렬;이기안
    • 대한금속재료학회지
    • /
    • 제48권1호
    • /
    • pp.28-38
    • /
    • 2010
  • High temperature high cycle and low cycle fatigue deformation behavior of automotive heat resistant aluminum alloys (A356 and A319 based) were investigated in this study. The microstructures of both alloys were composed of primary Al-Si dendrite and eutectic Si phase. However, the size and distribution for eutectic Si phase varied: a coarse and inhomogeneous distributed was observed in alloy B (A319 based). A brittle intermethallic phase of ${\alpha}-Fe\;Al_{12}(Fe,Mn)_3Si_2$ was detected only in B alloy. Alloy B exhibited high fatigue life only under a high stress amplitued condition in the high cycle fatigue results, whereas alloy A showed high fatigue life when stress was lowered. With regard to the low-cycle fatigue result ($250^{\circ}C$) showing higher fatigue life as ductility increased, alloy A demonstrated higher fatigue life under all of the strain amplitude conditions. Fractographic observations showed that large porosities and pores near the outside surface could be the main factor in the formation of fatigue cracks. In alloy B. micro-cracks were formed in both the brittle intermetallic and coarse Si phasese. These micro-cracks then coalesced together and provided a path for fatigue crack propagation. From the observation of the differences in microstructure and fractography of these two automotive alloys, the authors attempt to explain the high-temperature fatigue deformation behavior of heat resistant aluminum alloys.