• Title/Summary/Keyword: Ag-solder

Search Result 396, Processing Time 0.028 seconds

An experimental study on the cytotoxicity of orthodontic wires (교정용 호선의 세포독성에 관한 실험적 연구)

  • Lim, Yong-Kyu;Yang, Won-Sik
    • The korean journal of orthodontics
    • /
    • v.26 no.5 s.58
    • /
    • pp.591-599
    • /
    • 1996
  • This study was undertaken to investigate the cytotoxicity of orthodontic wires after doing various treatments to the wires. 018x025 inch Stainless steel(A) and Co-Cr(B) wires were used and each of them were divided into 4 groups. A-1 and B-1 groups were as received state, and A-2 and B-2 groups were heat treated. A-3 and B-3 groups were electropolished after heat treatment, and A-4 and B-4 groups were soldered with Ag-solder. Each group had 3 wires and these were sterilized with Ethylene Oxide gas. We used human gingival fibroblast cell culture and agar overlay technique to investigate the cytotoxicity of each group of wires. The cytotoxicity of wire was assessed using reaction index (zone index/lysis index). The findings of this study were as follows. 1. Both of the stainless steel wire and Co-Cr wire showed no cytotoxicity in as received state. 2. Heat treatment or electropolishing of the wires had no effect on the cytotoxicity of the wires 3. Soldered stainless steel wires showed a little wider zone of discoloration than soldered Co-Cr wires, but the zone index and cytotoxicity(reaction index) was not different. 4. Soldered wires showed moderate cytotoxicity in both of the wires.

  • PDF

Drop reliability evaluation of Sn-3.0Ag-0.5Cu solder joint with OSP and ENIG surface finishes (OSP.ENIG 표면 처리된 기판과 Sn-3.0Ag-0.5Cu 솔더 접합부의 낙하충격 신뢰성 평가)

  • Ha, Sang-Ok;Ha, Sang-Su;Lee, Jong-Bum;Yoon, Jeong-Won;Park, Jai-Hyun;Chu, Yong-Chul;Lee, Jun-Hee;Kim, Sung-Jin;Jung, Seung-Boo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.16 no.1
    • /
    • pp.33-38
    • /
    • 2009
  • The use of portable devices has created the need for new reliability criterion of drop impact tests because of the tendency to accidentally drop in the use of these devices. The effects of different PCB surface finishes (organic solderability preservative (OSP) and electroless nickel immersion gold (ENIG)) and high temperature storage (HTS) test on the drop reliability were studied. Various drop test conditions were used to evaluate a drop reliability of assemblies to endure such impact and shock load. In the case of the as-reflowed samples (no HTS test), the SAC/OSP boards exhibited a better drop impact reliability than that of SAC/ENIG. However, the reverse was true if HTS test is performed. In addition, significant decrease of drop reliability was observed for both SAC/ENIG and SAC/OSP assemblies after HTS test. It was also observed that the thickness of intermetallic compound layer do play an important role in the brittle fracture of drop test.

  • PDF

Retarding Effect of Transferred Graphene Layers on Intermetallic Compound Growth at The Interface between A Substrate and Pb-free Solder (기판과 무연솔더 계면에 전사된 그래핀 층의 금속간화합물 성장 지연 효과)

  • Yong-Ho Ko;Dong-Yurl Yu
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.30 no.3
    • /
    • pp.64-72
    • /
    • 2023
  • In this study, after transferring graphene on a Cu substrate and printing a Sn-3.0Ag-0.5Cu Pb-free solder paste on the Cu substrate, effects of the transferred graphene on formations and growths of intermetallic compound (IMC) at the interface between the Cu substrate and the solder were reported during processes of reflow soldering and isothermal aging for 1000 h with various temperatures (125, 150, and 175 ℃). Thicknesses of Cu6Sn5 and Cu3Sn IMCs at the interfaces with graphene were decreased during the reflow soldering and isothermal aging processes compared to those without graphene. The transferred graphene layers also showed that the growth rate constant and square of growth rate constant which related to the growth mechanisms of Cu6Sn5 and Cu3Sn IMCs with t he t emperature a nd t ime of t he i sothermal aging c ould dramatically decreased.

Interfacial and Mechanical Properties of Sn-57Bi-1Ag Solder Joint with Various Conditions of a Laser Bonding Process (다양한 레이저 접합 공정 조건에 따른 Sn-57Bi-1Ag 솔더 접합부의 계면 및 기계적 특성)

  • Ahn, Byeongjin;Cheon, Gyeong-Yeong;Kim, Jahyeon;Kim, Jungsoo;Kim, Min-Su;Yoo, Sehoon;Park, Young-Bae;Ko, Yong-Ho
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.28 no.2
    • /
    • pp.65-70
    • /
    • 2021
  • In this study, interfacial properties and mechanical properties of joints were reported after Cu pads finished with organic solderability preservative (OSP) on flame retardant-4 (FR-4) printed circuit board (PCB) and electronic components were joined with a Sn-57Bi-1Ag solder paste by using a laser bonding process. The laser bonding process was performed under various bonding conditions with changing a laser power and a bonding time and effects of bonding conditions on interfacial and mechanical properties of joints were analyzed. In order to apply for industry, properties of bonding joints using a reflow bonding process which are widely used were compared. When the laser bonding process were performed, we observed that Cu6Sn5 intermetallic compounds (IMCs) were fully formed at the interface although the bonding times were very short about 2 and 3 s. Furthermore, void formations of the joints by using the laser bonding process were suppressed at the joints with comparing to the reflow bonding process and shear strengths of bonding joints were higher than that by using the reflow bonding process. Therefore, in spite of a very short bonding time, it is expected that joints will be stably formed and have a high mechanical strength by using the laser bonding process.

Creep Deformation Behaviors of Tin Pest Resistant Solder Alloys (Tin Pest 방지 솔더합금의 크리프 특성)

  • Kim S. B.;Yu Jin;Sohn Y. C.
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.12 no.1 s.34
    • /
    • pp.47-52
    • /
    • 2005
  • Worldwide movement for prohibition of Pb usage drives imminent implementation of Pb-free solders in microelectronic packaging industry. Reliability information of Pb-free solders has not been completely constructed yet. One of the potential reliability concerns of Pb-free solders is allotropic transformation of Sn known as tin pest. Volume increase during the formation of tin pest could deteriorate the reliability of solder joints. It was also reported that the addition of soluble elements (i.e. Pb, Bi, and Sb) into Sn can effectively suppress the tin pest. However, the mechanical properties of the tin pest resistant alloys have not been studied in detail. In this study, lap shear creep test was conducted with Sn and Sn-0.7Cu based solder alloys doped with minor amount of Bi or Sb. Shear strain rates of the alloy were generally higher than those of Sn-3.5Ag based alloys. Rupture strains and corresponding Monkman- Grant products were largest for Sn-0.5Bi alloy and smallest for Sn-0.7Cu-0.5Sb alloy. Rupture surface Sn-0.5Bi alloy showed highly elongated $\beta$-Sn globules necked to rupture by shear stresses, while elongation of $\beta$-Sn globules of Sn-0.7Cu-0.5Sb alloy was relatively smaller.

  • PDF

Retardation of Massive Spalling by Palladium Layer Addition to Surface Finish (팔라듐 표면처리를 통한 Massive Spalling 현상의 억제)

  • Lee, Dae-Hyun;Chung, Bo-Mook;Huh, Joo-Youl
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.11
    • /
    • pp.1041-1046
    • /
    • 2010
  • The reactions between a Sn-3.0Ag-0.5Cu solder alloy and electroless Ni/electroless Pd/immersion Au (ENEPIG) surface finishes with various Pd layer thicknesses (0, 0.05, 0.1, 0.2, $0.4{\mu}m$) were examined for the effect of the Pd layer on the massive spalling of the $(Cu,Ni)_6Sn_5$ layer during reflow at $235^{\circ}C$. The thin layer deposition of an electroless Pd (EP) between the electroless Ni ($7{\mu}m$) and immersion Au ($0.06{\mu}m$) plating on the Cu substrate significantly retarded the massive spalling of the $(Cu,Ni)_6Sn_5$ layer during reflow. Its retarding effect increased with an increasing EP layer thickness. When the EP layer was thin (${\leq}0.1{\mu}m$), the retardation of the massive spalling was attributed to a reduced growth rate of the $(Cu,Ni)_6Sn_5$ layer and thus to a lowered consumption rate of Cu in the bulk solder during reflow. However, when the EP layer was thick (${\geq}0.2{\mu}m$), the initially dissolved Pd atoms in the molten solder resettled as $(Pd,Ni)Sn_4$ precipitates near the solder/$(Cu,Ni)_6Sn_5$ interface with an increasing reflow time. Since the Pd resettlement requires a continuous Ni supply across the $(Cu,Ni)_6Sn_5$ layer from the Ni(P) substrate, it suppressed the formation of $(Ni,Cu)_3Sn_4$ at the $(Cu,Ni)_6Sn_5/Ni(P)$ interface and retarded the massive spalling of the $(Cu,Ni)_6Sn_5$ layer.

Wettability Analysis of Liquid Phase in Partial Melted Solders Using Wetting Balance

  • Park, J.Y.;Ha, J.S.;Kang, C.S.;Kim, M.I.;Shin, K.S.;Jung, J.P.
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2000.04a
    • /
    • pp.81-86
    • /
    • 2000
  • To evaluate the possibility of the partial melting soldering. wettability of partial melted solders was measured using wetting balance. Off eutectic Sn-Pb allows are wettable in their partial melting zone. Especially, Pb rich alloys showed excellent wettability while wettability of Sn rich alloys were adequate or poor. It is found that wettability increases over $200^{\circ}C$ regardless of composition liquid fraction and phases of the original alloy Sn-7Ag alloy showed good wettability in their partial melting zone, while Sn-65Bi alloy was non-wettable under their melting points.

  • PDF

The interfacial reaction between Sn-based lead-free solders and Pt (Sn-base 무연솔더와 Pt층의 계면반응에 대한 연구)

  • 김태현;김영호
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2003.11a
    • /
    • pp.76-79
    • /
    • 2003
  • 본 실험에서는 $S0.7wt\%Cu,\;Sn3.8wt\%Ag0.7wt\%Cu$ solder와 금속층으로서의 좋은 특성을 가지고 있지만 아직 연구 보고 된 적 없는 Pt층과의 리플로 반응에 의해 형성되는 계면금속간화합물의 상 분석을 시도 하였다 또한 솔더내 Cu함량에 따른 계면금속간화합물의 변화에 대하여 연구하기 위해 $Sn1.7wt\%Cu$솔더와 Pt층의 계면반응 현상에 대한 연구도 수행하였다. $Sn0.7(1.7)wt\%Cu$솔더는 순수한 Sn과 Cu를 이용하여 중량비로 제조하였고, $Sn3.8wt\%Ag0.7wt\%Cu$솔더는 솔더페이스트를 사용하였다. 분석은 SEM, EDS, XRD를 이용하였다. 분석 결과 세 가지 무연솔더 모두에서 $PtSn_4$가 계면 금속간화합물로 존재함을 발견하였으며 $1.7wt\%Cu$를 포함한 솔더와 Pt와의 반응에서는 고용도 이상으로 첨가된 Cu에 의해 솔더 내부에 조대한 형상의 $Cu_6Sn_5$가 존재함을 SEM 및 EDS분석을 통하여 발견 하였다.

  • PDF

Reliability Evaluation of Silver Patterns Using Ink-jet Printing Technology (잉크젯 기술을 이용하여 인쇄된 실버 패턴의 신뢰성 분석)

  • Shin, Kwon-Yong;Kim, Myong-Ki;Lee, Sang-Ho;Hwang, Jun-Young;Kang, Heui-Seok;Kang, Kyung-Tae
    • Proceedings of the KIEE Conference
    • /
    • 2008.07a
    • /
    • pp.1450-1451
    • /
    • 2008
  • To investigate the reliability of the conductive lines patterned by ink-jet printing, we evaluated the reliability of the ink-jet printed silver (Ag) patterns according to the guide lines built up as assessments methods in the production of conventional rigid printed circuit boards. The assessment methods include the uniformity of line width and space, adhesive strength, dielectric withstand, solder float, thermal shock test and pressure cooker test (PCT). To prepare assesment vehicles, different regular test patterns were created by Ag ink-jet printing on the same polyimide substrate for each of assessment methods.

  • PDF