RESEARCH ON THE IMPROVEMENT OF FORGEABILITY OF SNCM STEEL

  • Park I.W.;Jung D.J.;Je J.S.;Joun M.S.;Kang S.S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2003.10b
    • /
    • pp.80-85
    • /
    • 2003
  • This research represents enhancement of forgeability of SNCM522H steel. Output Shaft (OP Shaft) has been used as a subject for the study. OP Shaft is used as component of power train for automobiles. To develop I pass cold forging process instead of existing 2 pass process for OP Shaft, studies in terms of process design and heat treatment were performed. To verify the new process, CAE simulations were performed. And hardness test, microstructural analysis and tensile tests after heat treatment were carried out to evaluate the validity of proposed heat treatment cycle. The 2 pass forging process could be reduced as 1 pass process through improvement of process and heat treatment cycle.

  • PDF

Mechanical Properties of Ti-Zr-Nb-Pd Based Alloys for Biomedical Applications (생체용 Ti-Zr-Nb-Pd계 합금의 기계적 성질)

  • Jung, Jong-Hyun
    • Journal of Technologic Dentistry
    • /
    • v.24 no.1
    • /
    • pp.95-104
    • /
    • 2002
  • For biomedical applications, Ti-X%Zr-Y%Nb-0.2%Pd(X:10$\sim$20, Y:2$\sim$8) alloys not containing harmful Al and V were newly designed, and the effect of alloy composition and heat treatment on the microstructure and mechanical properties was investigated. From the results, it was shown that the mechanical properties were enhanced with the addition of Zr or Nb. The effect of heat treating on room temperature strength was investigated by aging treatment after solution treatment. The mechanical properties of Ti-20%Zr-4%Nb-0.2%Pd alloy aged at 400$^{\circ}C$ for 10hrs was found to be superior to those of the pure Ti and Ti-6%Al-4%V ELI alloy.

  • PDF

Application of Pulsed Electric Fields with Square Wave Pulse to Milk Inoculated with E. coli, P. fluorescens, and B. stearothermophilus

  • Shin, Jung-Kue;Jung, Kwan-Jae;Pyun, Yu-Ryang;Chun, Myong-Soo
    • Food Science and Biotechnology
    • /
    • v.16 no.6
    • /
    • pp.1082-1084
    • /
    • 2007
  • Ultra-high temperature (UHT) processed full fat milk inoculated with Escherichia coli, Pseudomonas fluorescens, and Bacillus stearothermophilus was exposed to 30-60 kV/cm square wave pulsed electric field (PEF) with $1\;{\mu}sec$ pulse width, and $26-210\;{\mu}sec$ treatment time in a continuous PEF treatment system. Eight log reduction was obtained for E. coli and P. fluorescens and 3 logs reduced for B. stearothermophilus under PEF treatment conditions of $210\;{\mu}sec$ treatment time, 60 kV/cm pulse intensity at $50^{\circ}$. There was no significant change in pH and titration acidity of milk after PEF treatment. The electrical energy required to achieve 8 log reduction for E. coli and P. fluorescens was estimated to be about 0.74 kJ/L.

Effects of Hot-Air Heat Treatment on the Surface Color of Phyllostachys bambusoides Bamboo

  • LEE, Hyoung-Woo;LEE, Eun-Ju
    • Journal of the Korean Wood Science and Technology
    • /
    • v.49 no.6
    • /
    • pp.566-573
    • /
    • 2021
  • We investigated color changes on the outer surfaces of Phyllostachys bambusoides bam-boo by heat treatment under three different temperatures (180℃, 200℃, and 220℃) for three different durations (60 min, 90 min, and 120 min). A method of predicting the bam-boo surface color change after heat treatment was developed to provide valuable information and increase the added value of domestic bamboo products. The three average color parameters L*, a*, and b* decreased, and the overall color changes increased as the severity factor increased. The values of L* × a* × b* were highly related to the severity factor, and the optimal duration time for the desired bamboo surface color with a certain heat-treatment temperature could be estimated.

Evaluation on Enhanced Biodegradability in Landfill Leachate by Fenton Oxidation (Fenton 산화법에 의한 매립장 침출수의 생물 분해성 증진에 관한 평가)

  • Lee, Byung-Dae
    • Journal of the Korean Applied Science and Technology
    • /
    • v.22 no.3
    • /
    • pp.250-256
    • /
    • 2005
  • This study was aimed to investigate treatment feasibility of leachate from D landfill that is located in gyr대ungbuk. From the analytical results of leachate, organic and nonbiodegradable matters were contained in high concentration. Thus chemical treatment was introduced to degrade nonbiodegradable matters in pre or post biological process. Two types of Fenton oxidation were adapted in this study. The first one is pre treatment process before biological treatment. The second one is post treatment process after biological treatment. The optimal conditions of both treatment methods were investigated as follows. In case of pre treatment process, the optimal conditions appeared in $Fe^{+2}/H_2O_2$(mmol/mmol): 0.1, $H_2O_2/CODcr$(mg/mg): 27.0, pH: 3 and reaction time: 2hrs. On the other hand, in case of post treatment process, the optimal conditions appeared in $Fe^{2+}$(mmol/mmol): 0.14, $H_2O_2/COD_{cr}$(mg/mg): 57.4, pH: 3 and reaction time: 1.25hrs. In the above optimal conditions, high COD removal was obtained in pre and post treatment process. Also it can expect that Fenton oxidation converted nonbiodegradable matters into biodegradable matters.

THE EFFECTS OF SEALING ON THE PLASMA-SPRAYED OXIDE-BASED COATINGS

  • Kim, Hyung-Jun;Sidoine Odoul;Kweon, Young-Gak
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.53-58
    • /
    • 2002
  • Electrical insulation and mechanical properties of the plasma sprayed oxide ceramic coatings were studied before and after the sealing treatment of the ceramic coatings. Plasma sprayed A1$_2$O$_3$-TiO$_2$ coating as the reference coating was sealed using three commercial sealants based on polymer. Penetration depth of the sealants to the ceramic coating was evaluated directly from the optical microscope using a fluorescent dye. It is estimated that the penetration depth of the sealants to the ceramic coating is from 0.2 to 0.5 mm depending on the sealants used. The preliminary test results with a DC puncture tester imply that the dielectric breakdown voltage mechanism of plasma sprayed ceramic coatings has been determined to be a corona mechanism. Dielectric breakdown voltage of the as-sprayed and as-ground samples have shown a linear trend with regard to the thickness showing an average dielectric strength of 20 kV/mm for the thickness scale studied. It is also shown that grinding the coating before sealing and adding fluorescent dye do not agent the penetration depth of sealants. All of the microhardness, two-body abrasive wear resistance, bond strength, and surface roughness of the ceramic coating after the sealing treatment are improved. The extent of improvement is different from the sealants used. However, three-point bending stress of the ceramic coating after the sealing treatment is decreased. This is attributed to the reduced micro-crack toughening effect since the cracks propagate easily through the lamellar of the coating without crack deflection and/or branching after the sealing treatment.

  • PDF

Texture of Asymmetrically Rolled AA 3003 Aluminum alloy (비대칭 압연한 AA 3003 합금의 조직 변화)

  • Akramov, S.;Kim, I.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.10a
    • /
    • pp.332-333
    • /
    • 2007
  • The effect of asymmetric rolling on the recrystallization texture of an AA 3003 Aluminum alloy was investigated by X-ray diffraction. It was found that the texture of asymmetrically rolled sheets prior to subsequent heat treatment promoted the formation of the <111>//ND textures, and remained after heat treatment at $275^{\circ}C$ during 20 min in salt bath condition.

  • PDF

Effects of Supercritical Carbon Dioxide Treatment on Meat Quality and Sensory Evaluation in Soy Sauce and Hot-pepper Paste Marinated Pork

  • Choi, Young Min;Lee, Sang Hoon;Choe, Jee Hwan;Kim, Kyoung Heon;Rhee, Min Suk;Kim, Byoung Chul
    • Food Science of Animal Resources
    • /
    • v.33 no.5
    • /
    • pp.581-586
    • /
    • 2013
  • The objective of this study was to investigate the effects of supercritical carbon dioxide (SC-$CO_2$) treatment on meat quality and sensory evaluation of marinated pork. Meat marinated in two traditional Korean marinades, soy sauce and hot-pepper paste, and raw marinated meat were then treated with 7.4, 12.2, or 15.2 MPa $CO_2$ at $31.1^{\circ}C$for 10 min. The SC-$CO_2$ treatments had no effect on the meat pH (p>0.05) or Warner-Bratzler shear force (p>0.05). There was no significant difference (p>0.05) in the total loss (sum of treatment loss and cooking loss) between the control and SC-$CO_2$ treated samples at 15.2 MPa (soy sauce marinated pork: 21.78 vs. 18.97%; hot-pepper marinated pork: 21.61 vs. 18.01%). After the SC-$CO_2$ treatment, lighter surface colors were observed in the treatment samples compared to those of the control samples (p< 0.001). However, tasting panelists were unable to distinguish a difference in color or in overall acceptability of the control and treatment (p>0.05). In the case of soy sauce marinated pork, when SC-$CO_2$ applied at 15.2 MPa and $31.1^{\circ}C$for 10 min, treatment samples showed a tenderer meat than the control samples. Therefore, the SC-$CO_2$ treatment conditions had no adverse effects on the sensory quality characteristics of the marinated meat products.

Complex heat-treatment effects on as-built CoCrMo alloy (적층공정법으로 제작된 CoCrMo 합금의 복합열처리 효과)

  • Lee, Jung-Il;Kim, Hung Giun;Jung, Kyung-Hwan;Kim, Kang Min;Son, Yong;Ryu, Jeong Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.28 no.6
    • /
    • pp.250-255
    • /
    • 2018
  • The CoCrMo as-built alloys prepared by 3D-printing process are studied on tensile strength, wear resistance, crystal structure and microstructure after complex heat-treatment including HIP. In this study, HIP treatment for removing micropores, ambient heat-treatment for formation of metal carbides, and solution heat-treatment for homogenization of the created metal carbides were tried and characterized for applying to artificial joint. The complex heat-treatment effects of the CoCrMo as-built alloys prepared by 3D-printing process were owing to the densification during HIP, formation of metal carbides and homogenization of the created metal carbides. The effects of the complex heat-treatment were confirmed by XRD, FE-SEM and EDS.

Effect of Different Conditions of Sodium Chloride Treatment on the Characteristics of Kenaf Fiber Bundles

  • Tamaryska, SETYAYUNITA;Ragil, WIDYORINI;Sri Nugroho, MARSOEM;Denny, IRAWATI
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.6
    • /
    • pp.392-403
    • /
    • 2022
  • Currently, composite board manufacturing using natural fibers has the potential to expand owing to environmental awareness. To produce a composite board, treatment is required to improve the mechanical and physical properties of the natural fibers. In this study, sodium chloride (NaCl) was used for the chemical treatment. However, studies on chemical treatments using NaCl are limited. This study aimed to investigate the characteristics of kenaf fibers after NaCl treatment. The NaCl treatment concentrations were 1, 3, and 5 wt.% at room temperature, with soaking durations of 1, 2, and 3 h. The tensile strength, strain, and Young's modulus were measured to evaluate the mechanical properties of the fibers. The fiber bundle diameter, weight change owing to treatment, and contact angle were determined to analyze the effect of NaCl treatment. The kenaf fiber bundle treated with 5 wt.% NaCl for 3 h exhibited the highest tensile strength, Young's modulus, reduction in fiber bundle diameter, weight change, and decrease in contact angle compared to those of untreated fiber bundles. The tensile properties of the fiber bundle exhibited a tendency to decrease with increasing fiber bundle diameter. Increasing the soaking duration from 1 to 2 h did not result in a significant decrease in the fiber bundle diameter or an increase in tensile strength. However, a further increase in the soaking duration from 2 to 3 h resulted in a considerable decrease in the fiber bundle diameter and an increase in the tensile strength.