In this study, the adhesion performance of the adhesive between the concrete base and the fiber panel was verified through experiments. Attachment to all three types by applying adhesive to panel and attaching to CRC board surface, method of applying adhesive to CRC board surface by panel, method of applying adhesive on panel and CRC board surface respectively, As a result of the performance test, the adhesive strength of the panel attached to the panel on the CRC board after the application of the adhesive was highest on both the back surface of the panel and the surface of the CRC board.
International Journal of Aerospace System Engineering
/
제1권1호
/
pp.44-47
/
2014
This study proposes a development for the nano silver adhesive, which is applicable to high efficiency LED(light-emitting diode) light. The important issue of LED light is heat exhaust from LED. Generally, the middle area of LED light is increased up to 380K. Therefore, the bottleneck between LED chip and heat sink are caused by high temperature. In this work, the adhesive material between LED Chip and heat sink was newly developed for improvement of bottleneck. The nano silver was adopted to solve heat problem of chip on board package for LED light. In order to evaluate the performance of the nano silver adhesive, the thermal analysis was performed. Moreover both adhesive performance and heat exhaust were verified through the prototype test. From the experimental test results, it is found that the developed nano silver adhesive has the high performance.
Because Self-Adhesive Waterproofing sheet has good constructability, it has been widely used. Also Self-Adhesive Waterproofing sheet is researched based on variety of materials and various of forms. However, producers have recognized about only pass KS quality standard. So, Self-Adhesive waterproofing sheet has been limited about improvement of performance. Therefore, in this research, proposed guideline of Self-Adhesive Waterproofing sheet for disinterested performance grade using probability theory and quality management theory.
To investigate the influence of manufacturing environment on bonding performance of mixed cross laminated wood (CLT) using polyurethane (PUR) adhesive, a boiling water soak delamination test according to the temperature and relative humidity was conducted. The 5-ply mixed CLT consisted of Japanese Larch for external and middle layer and yellow poplar for internal layer. The PUR adhesives with different opening times of 10 and 30 minutes were used. The mixed CLT was manufactured according to pressing times of PUR and manufacturing environments of summer and winter. In case of summer environment, the delamination rate of the mixed CLT with pressing time of 4 hours using a PUR adhesive with open time of 10 minutes met the requirements of KS F 2081. In case of winter environment, the delamination rate of the mixed CLT didn't meet the requirements of KS standard. However, it was possible to confirm the effect of improving the adhesive performance by adjusting the pressing time according to the open time of the adhesive under the manufacturing conditions. The delamination rate of CLT with open time 30 minutes PUR, manufactured by indirect moisture supply methods was 11.2% better than direct moisture supply methods. As a result of delamination test in the same condition of relative humidity and adhesive, it was found that the temperature of manufacturing environment influences the adhesive performance.
The tile construction methods for existing have been used materials within limit which adhesion by wet method in masonry wall and concrete structure. These existing adhesive tech can caused many problems in construction of large and reform tile, after that it can be happened loose scale, peel off, falling off tile by heat and vibration or impact. In according to, this study is to test tile for bond stability, adhesive property by impact, vibration. low property by heat and then, we have the results as below; (1) The tile adhesive stability can be effected as adhesive area between bond agent and tile, adhesive area can more wide and press enough to ensure property. (2) Existing adhesive strength and standard relative tile construction is limited to adjust performance tile on the concrete and masonry wall. In summary, It is necessary to establish standard of performance and test method to ensure tile adhesive salability in dry wall.
Adhesive joining technique is considered as one of hot issues in developing advanced composite structures. The designer should be familiar with important guidelines of fundamental principles and ideas underlying the design and application of adhesive joints for a correct joint design. This study deals with the following characteristics of adhesive joining techniques: (1) design parameters the affect the performance of joining, (2) fundamental principles and design methods of joining, (3) adhesive selection, (4) surface pre-treatment of the adherand, and (6) test methods. The results would be used to predict the performance of adhesive joints subjected to a thermal aging.
In this study, flexural strength and tile adhesion strength were evaluated by using a mortar, dry mortar and an epoxy resin reinforced mortar to examine the adhesion performance by reinforcing the epoxy resin adhesive. As a result, it was clearly confirmed that the effect of improving the adhesion strength by reinforcing the epoxy resin adhesive regardless of the type of tile, and in particular, when applying the epoxy resin adhesive to the porcelain and polishing tiles, it is judged that sufficient adhesion performance can be secured.
The adhesive performance of marine mussel extract was compared with that of the commercial medical adhesives for fastening biotissue (SIS) bandages. Joints bonded with mussel extract showed stronger strength than those bonded with other commercial adhesives. The bonding strength was much improved when the moisture in the Joint was reduced using superporous hydrogel regardless of curing time under humid condition ($37^{\circ}C$ and 91% relative humidity). Water inflow into the SIS joint seemed to degrade the performance of mussel extracts adhesive especially for the joints of short period of curing time. The strength of SIS joints coated with surgical sealant was well maintained after being exposed to water inflow.
PURPOSES : The purpose of this study is to select the proper sealing method and to see the performance of the saw and seal method for concrete rehabilitation based on accelerated pavement testings and lab tests. METHODS : Two accelerated pavement testings were conducted. One is to select proper sealing method of the asphalt joints and the other is to see the performance of the saw and seal method. Lab tests were conducted to select proper sealing method and a test section was constructed to see the field performance. RESULTS : The result of the first accelerated pavement testing indicated that the adhesive preformed sealants showed good performance when asphalt layer was rutted and in terms preventing from water infiltration. The second acceleration test indicated that the saw and seal method using the adhesive preformed sealant showed much better performance than the control. In the lab test bitumen, rubber and epoxy showed good performance as the adhesive. CONCLUSIONS : Saw and Seal method using the adhesive preformed sealant would markedly reduce the joint damage on the asphalt overlay.
This study suggest the improvement of the CFRP adhesive mixing ratio about acoustic window to enhance SONAR performance. The CFRP of submarine is produced by allocation an acoustic window zone by the beam width of SONAR sensors. During the sea trial, SONAR system's bearing and range accuracy data is not in tolerance due to debonding phenomenon on CFRP. The inappropriate mixing ratio of adhesives caused that peeling phenomenon occurred in the acoustic window part, which is the reason for the deterioration of SONAR sensors performance. The report includes explanation of test procedure of SONAR, root cause analysis, CFRP manufacturing procedure, laboratory tests results, and proof of the performance at the sea trial.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.