• 제목/요약/키워드: Adhesion in Tension

검색결과 107건 처리시간 0.023초

양생조건에 따른 폴리머 시멘트 모르타르의 인장접착강도 (Adhesion in Tension of Polymer-Modified Mortars according to Curing Conditions)

  • 조영국
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2018년도 춘계 학술논문 발표대회
    • /
    • pp.200-201
    • /
    • 2018
  • The purpose of this study is to evaluate the adhesion in tension of polymer-modified mortars according to curing conditions. From the test results, the adhesion in tension is seriously affected by type of curing conditions compared with type of polymer dispersions or polymer-cement ratios. The maximum adhesion in tension of EVA-modified mortar with polymer-cement ratio of 20% cured by standard condition is about 1.81 times, the cement mortar cured in water. It is apparent that the adhesion in tension of polymer-modified mortars according to raising of polymer-cement ratio is also much more improved irrespective of type of polymer dispersions and curing conditions.

  • PDF

고로슬래그 및 플라이애쉬를 혼입한 폴리머 시멘트 모르타르의 인장접착강도 (Adhesion in Tension of Polymer-Modified Mortars with Blast-Furnace Slag and Fly ash)

  • 조영국
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2017년도 춘계 학술논문 발표대회
    • /
    • pp.232-233
    • /
    • 2017
  • The purpose of this study is to evaluate the Adhesion in tension of cement mortar according to adding admixtures such as polymer dispersions, blast-furnace slag and fly ash. From the test results, the adhesion in tension is seriously affected by type of polymer compared with polymer-binder ratios and types of admixture. The maximum adhesion in tension of EVA- modified mortar is about 1.46 times, the cement mortar. It is apparent that the adhesion in tension of polymer-modified mortars according to adding two admixtures is much more improved irrespective of polymer-binder ratio.

  • PDF

시험방법에 따른 폴리머 시멘트 모르타르의 인장 및 휨접착강도 개선에 관한 연구 (A Study on the Improvement of Adhesion in Tension and Flexure of Polymer Cement Mortar Depending on Various Test Methods)

  • 조영국
    • 한국건축시공학회지
    • /
    • 제19권1호
    • /
    • pp.47-57
    • /
    • 2019
  • 폴리머 종류에 상관없이 폴리머 시멘트비의 증가에 따라 접착성능은 크게 개선되었으며, A타입 인장접착강도는 1.90배, B 타입 인장(접착)강도는 2.17배, 휨(접착)강도는 1.83배 보통 시멘트 모르타르 보다 높게 나타났으며, 보통 시멘트 모르타르의 B 타입 인장(접착)강도에 대한 인장강도비와 휨(접착)강도에 대한 휨강도비인 상대강도비가 각각 46.9%, 72.6%를 나타냈으며, 폴리머 시멘트 모르타르의 경우에는 각각 50.1%~101.7%, 73.8%~132.9% 범위를 나타내, 폴리머 시멘트 모르타르가 높은 강도회복율을 보였다. 폴리머 종류에 따라서는 EVA를 사용하고, 폴리머 시멘트비로서는 접착성능과 경제성을 고려하면, P/C 10%~15% 범위를 제안할 수 있다.

양생존건이 폴리머 시멘트 모르터의 접착강도에 미치는 영향 (The Effect of Curing condition on Adhesion in Tension of Polymer-Modified Mortars)

  • 전우성;조영국;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 봄 학술발표회 논문집
    • /
    • pp.349-356
    • /
    • 1997
  • The purpose of this study is to evaluate the effect of curing conditions on adhesion in tension of polymer-modified mortar to cement mortar substrate in comparision with ordinary cement mortar. The polymer-modifies mortars using two polymer dispersions and a redispersible polymer power are prepared with various polymer-cement ratios, and tested for the adhesion in tension of the specimens subjected to five curing conditions. From the test results, the adhesion in tension of polymer-modified mortars tends to increase with increasing polymer-cement ratio irrespective of the polymer types and curing conditions. It is apparent that adhesion in tension of polymer-modified mortars is considerably influenced by curing conditions.

  • PDF

보수재료로서 고로슬래그 미분말 및 플라이애쉬를 혼입한 SAE 에멀젼 기반 폴리머 시멘트 모르타르의 휨접착 및 인장접착 특성 (Properties of Adhesion in Flexure and Tension of Polymer Cement Mortar Using SAE Emulsion with Blast-Furnace and Fly Ash as a Repair Material)

  • 조영국
    • 한국건축시공학회지
    • /
    • 제19권6호
    • /
    • pp.485-494
    • /
    • 2019
  • 본 연구는 고로슬래그 미분말 및 플라이애쉬를 혼입한 SAE 에멀젼 기반 폴리머 시멘트 모르타르의 휨과 인장특성에 대하여 실험하여 혼화재의 혼입효과를 평가하고자 하였다. PCM은 폴리머 시멘트비와 혼화재의 혼입율을 변화시켜 시험편을 제작하였으며, 휨강도, 휨접착강도, 인장강도 및 인장접착강도 시험을 실시하였다. 연구결과, 혼화재의 혼입에 따른 휨강도 및 휨접착강도 개선은 거의 발현되지 않았으나, 인장강도 및 인장접착강도에서는 혼화재의 혼입에 따른 강도개선 효과를 얻을 수 있었다. 특히 PCM의 인장 접착강도는 P/C 20%, 고로슬래그 미분말 혼입율 10%에서 최대 3.35MPa로 보통시멘트 모르타르의 약 2.36배, 혼화재를 혼입하지 않은 PCM의 약 1.32배의 높은 강도를 나타냈으며 인장접착강도/인장강도비는 평균 48.7%를 나타냈다. 본 연구를 통하여 PCM의 인장 및 인장접착강도 개선을 위해서는 혼화재 혼입율 5% 또는 10%를 제안할 수 있었다.

폴리머 첨가율에 따른 CLC의 강도 특성 (Strength Properties of CLC According to Additional Ratio of Polymer)

  • 이정택;이창우;황우준;이상수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.83-84
    • /
    • 2022
  • Zero-energy construction is being emphasized due to environmental pollution. However, in the case of external insulation using organic insulation with good insulation performance, there are many studies on inorganic insulation as it shows limitations on fire stability. In addition, as the demand for stone for exterior walls increases, Cellular Light -weight Concrete(CLC) with polymer is used to supplement fire stability and insulation performance, and the construction of stone is complemented by combining organic insulation, inorganic insulation, and stone. In this study, the compressive strength and adhesion in tension of CLC are studied. As a result of the experiment, the compressive strength of 28 days according to the polymer addition rate did not change. The adhesion in tension according to the polymer addition rate tends to increase as the addition rate increases. The target adhesion in tension is 0.8 MPa, but the maximum value of the experiment did not reach the target value, and further research was needed to combine to maintain the density and improve the adhesion in tension.

  • PDF

보수재료로서 EVA 에멀젼과 고로슬래그 미분말 및 플라이애쉬를 혼입한 폴리머 시멘트 모르타르의 인장·접착특성 (Tensile and Adhesive Properties of Polymer Cement Mortar with EVA Emulsion, Blast-Furnace Slag and Fly Ash as a Repair Material)

  • 조영국
    • 대한건축학회논문집:구조계
    • /
    • 제35권11호
    • /
    • pp.147-154
    • /
    • 2019
  • The purpose of this study is to evaluate the effect of admixtures as blast-furnace slag(BF) and fly ash(FA) on tensile and adhesive properties of polymer cement mortar(PCM) with EVA emulsion. The test specimens are prepared with five polymer-cement ratio(P/C) and five admixture contents, and tested for tensile strength and adhesion in tension. From the test results, the tensile strength and adhesion in tension could be improved by an appropriate combination of P/C and admixture contents. In particular, the maximum of tensile strength of PCM with P/C 10% and BF content of 10% is 4.70MPa which is about 1.55 times higher than that of plain mortar, and about 1.22 times that of PCM that does not contain any mixture. The ratio of adhesion in tension to tensile strength of PCM with admixtures averaged 55.8%. It is also apparent that admixture contents of 5% or 10% could be proposed for improvement of tensile strength and adhesion in tension of PCM.

벽면흡착에 의해 야기되는 유동 수치해석 (NUMERICAL SIMULATION OF FLOWS INDUCED BY WALL ADHESION)

  • 명현국
    • 한국전산유체공학회:학술대회논문집
    • /
    • 한국전산유체공학회 2011년 춘계학술대회논문집
    • /
    • pp.2-5
    • /
    • 2011
  • This paper presents a numerical study on multiphase flows induced by wall adhesion The CSF(Continuum Surface Force} model is used for the calculation of the surface tension force and implemented in an in-house solution code(PowerCFD). The present method(code) employs an unstructured cell-centered method based on a conservative pressure-based finite-volume method with volume capturing method(CICSAM) in a volume of fluid(VOF) scheme for phase interface capturing As an application of the present method, the effects of wall adhesion are numerically simulated with the CSF model for a shallow pool of water located at the bottom of a cylindrical tank. Two different cases are computed, one in which the water wets the wall and one in which the water does not wet the wall. It is found that the present method simulates efficiently and accurately surface tension-dominant multiphase flows induced by wall adhesion.

  • PDF

콘크리트 보수용 폴리머 복합재료의 접착강도 특성 (Adhesion Properties of Polymer Composite Materials for Concrete Repair)

  • 지경용;연규석;이윤수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표논문집(II)
    • /
    • pp.330-335
    • /
    • 1998
  • This research was conducted to evaluate the adhesion in tension of the polymer mortars for cement concrete repair. Various polymer types, binder ratios, and wet/dry conditions of the surface were considered in this study. Styrene-butadiene rubber (SBR) and ethylen vinyl acetate (EVA) used for polymer cement mortars. Epoxy resin (EP), and unsaturated polyester resin (UP) were used for polymer mertars. Adhesion in tension for the dry condition of the substrate surface was higher than that for the wet condition of the substrate surface under the same binder ratio. Therefore, in repairing concrete, the dry surface condition was effective on adhesion.

  • PDF

복합화약 원료들간의 표면특성 해석 (Analysis of surface interaction between filler and binder of PBXs)

  • 심정섭
    • 한국군사과학기술학회지
    • /
    • 제4권1호
    • /
    • pp.207-215
    • /
    • 2001
  • Plastic bonded explosive(PBX) is mainly composed of the nitramine-ploymer compositions. PBX is characterized by high velocity and pressure of detonation, low vulnerability and good thermal stability. Many important applications of PBX require the good adhesion between nitramine crystals and the binder. For PBXs as well as propellants, where good mechanical properties are of great importance, dewetting therefore must be prevented by strong adhesion between filler-binder. Adhesion depends on surface characteristics of filler and binder. In order to design for better adhesion, an understanding of the surface properties of explosive and binder is required. The surface free energies are calculated from contact angle values by the method of Kaelble. Critical surface tension of solids are calculated by Zisman plot. Critical surface tension is a useful parameter for characterizing the wettability of solid surface. In this study, HMX and 3 kinds of copolymers are selected, since they are widely used in many plastic bonded explosives. The technical objective of this investigation is to predict the interaction between filler and binder from their surface free energies.

  • PDF