슬리브 시공유형별 기계적 및 열적 가속열화특성 분석 연구

  • 안상현;김병걸;김상수;손홍관;박인표
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 추계학술대회 논문집
    • /
    • pp.286-286
    • /
    • 2009
  • According to previous report, aged sleeves for old transmission lines have various defect such as biased installation or corrosion of steel sleeve. These defects can cause serious accidents such as rapid increasing of sag or falling out of overhead conductor from sleeves. Moreover, the defects have been limited power capacity of transmission line. This paper study on mechanical and thermal behavior of ACSR $410mm^2$ conductor and sleeve with various defect model. The conductor has been aged artificially for 50 years. The detailed results were presented in the text.

  • PDF

장력과 풍속이 ACSR 가공송전선의 온도에 미치는 영향 (Effect of Tension and Wind Velocity on Temperature of ACSR Overhead Conductor)

  • 김상수;김병걸;이동일;민병욱
    • 한국전기전자재료학회논문지
    • /
    • 제19권5호
    • /
    • pp.480-485
    • /
    • 2006
  • A research was undertaken on the thermal properties and behavior of the conductors in a controlled chamber, which was designed to implement the outdoor air temperature, heat and wind conditions With ACSR $410mm^2$ overhead conductors, we measured the maximum temperature of the conductors and the temperature gradient from the core to the surface regions as a function of current, tension, wind velocity and outdoor air temperature. This test also provided a comparative analysis between the measured temperature values of conductors in the controlled chamber and the theoretical calculations of ANSI/IEEE at normal condition. There was not much influence of tension on the conductor temperature. However, the compactness of conductor wires increased with an increase in tension, which eventually increased the coefficient of effective thermal conductivity and, accordingly the conductor temperature was reduced more or less.

산불에 노출된 강심알루미늄연선 송전선 알루미늄 선재의 기계적 및 전기적 특성 거동 (Mechanical and Electrical Properties of Aluminum Wires of ACSR Conductors due to Forest Fire)

  • 이원교;이정원;김병걸
    • 한국전기전자재료학회논문지
    • /
    • 제23권9호
    • /
    • pp.730-735
    • /
    • 2010
  • Forest fire can cause a serious damage to overhead conductors. Therefore, detailed investigation on the changes of mechanical and electrical properties of damaged conductors should be carried out to understand the effect of forest fires on conductors. This is of critical importance in maintaining transmission line safely. This paper examines the changes of mechanical and electrical properties of flame exposed conductor. Tensile strength (TS) decreased according to increase of forest fire temperature and conductivity changed according to forest fire temperature. Specimens were aluminum conductors of aluminium conductor steel reinforced (ACSR) 410, 240, 480 $mm^2$. In this paper, the electrical and mechanical characteristics of forest fires exposed overhead conductors depending on the diameter of aluminum conductors are presented. It was possible to estimate the degree of deterioration caused by forest fires. The detailed results are given in the paper.

환경적 요인에 의한 노후 가공송전선의 특성변화 (Change of Properties by Environment Conditions in Aged ACSR Overhead Conductor)

  • 김상수;김병걸;장태인;강지원;이동일;민병욱
    • 한국전기전자재료학회논문지
    • /
    • 제19권3호
    • /
    • pp.287-291
    • /
    • 2006
  • This paper describes mechanical and electric properties of ACSR $410\;mm^2$ conductor from many of older overhead conductor. Samples of conductors itemized two division according to operation sector, green area, salt and pollution area. Samples of conductors operated various environment conditions have undergone laboratory metallurigical investigation and tensile strength torsional ductility and electrical performance. The steel core were found to have retained their original properties to a large degree in both tensile strength and the number of turns to failure. On the other hand the aluminum conductor showed reductions in tensile strength. To determine the remaining useful life of aged conductor, an unacceptable deterioration level has to established for each diagnostic procedure.

가공송전선의 열적거동과 전류 및 외기온도의 영향 (Effect of Ambient Temperature and Current on Overhead Conductor)

  • 김상수;김병걸;현석규;이동일;민병욱
    • 한국전기전자재료학회논문지
    • /
    • 제19권5호
    • /
    • pp.486-491
    • /
    • 2006
  • A research was undertaken on the thermal properties and behavior of the conductors in a controlled chamber, which was designed to implement the outdoor air temperature, heat and wind conditions. With ACSR $410mm^2$ overhead conductors, we measured the maximum temperature of the conductors and the temperature gradient from the core to the surface regions as a function of current, tension, wind velocity and outdoor air temperature. This test also provided a comparative analysis between the measured temperature values of conductors in the controlled chamber and the theoretical calculations of ANSI/IEEE at normal condition.

산불에 노출된 가공송전선의 열화특성연구

  • 장용호;김병걸;김상수;한세원;이원교
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 추계학술대회 논문집
    • /
    • pp.282-282
    • /
    • 2009
  • Forest Fire can cause a serious damage to overhead conductors. Therefore, the detailed investigation for the changes of mechanical and electrical properties of damaged conductors should be carried out to understand the effect of forest fires on conductors. This is very important to maintain transmission line safely. Specimenes for this study were Al conductores of ACSR $410mm^2$, ACSR 480 R and ACSR $240mm^2$. This paper describes the changes of mechanical and electrical properties of same flame exposed Al conductor. The detailed will be given in the text.

  • PDF

통전 중 산불에 노출된 가공송전선의 온도 및 장력 변화 거동 (Temperature and Load Change behavior of Overhead Conductor under loading current due to Forest Fire)

  • 김병걸;장용호;김상수;한세원
    • 한국전기전자재료학회논문지
    • /
    • 제22권4호
    • /
    • pp.366-371
    • /
    • 2009
  • The authors have published several technical reports on the deterioration of conductor due to forest fire in series so far. This is because even we have been experiencing hundreds of forest fires every year, no systematic research on conductor which is very vulnerable to fire have been fulfilled. This paper describes the sag-tension behavior of conductor under loading current normally when only partial area of a long conductor is exposed to fire. Temperatures of Overhead Conductor were different with measurement position. When the partial area of conductor was heated up to $500^{\circ}C$, 20 % of permanent tension loss was observed. This results in the increase of sag of 1.5 m when span is 300 m. The other results will be presented in the text.

소화약제 및 산불에 노출된 가공송전선의 전기적, 기계적 거동 변화 (The Mechanical and Electrical behavior Changes of Overhead Conductor due to Forest Fire and Agents)

  • 장용호;김병걸;김상수;한세원;김진한
    • 전기학회논문지
    • /
    • 제58권2호
    • /
    • pp.242-247
    • /
    • 2009
  • Forest Fire can cause a serious damage to overhead conductors. Therefore, the detailed investigation for the changes of mechanical and electrical properties of damaged conductors should be carried out to understand the effect of forest fires on conductors. This is very much important to maintain transmission line safely. Oxidation of overhead conductor was increased with temperature and time(maximum time : 30min). Conductivity of Al conductor was decreased by Agents. The detailed will be given in the text.

산불과 소화약제에 노출된 가공송전선의 기계적 및 전기적 특성 변화 (The Mechanical and Electrical property changes of Overhead Conductor due to Forest Fire and Agents)

  • 장용호;김병걸;김상수;한세원;김진한
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.459-460
    • /
    • 2008
  • Forest Fire can cause a serious damage to overhead conductors. Therefore, the detailed investigation for the changes of mechanical and electrical properties of damaged conductors should be carried out to understand the effect of forest fires on conductors. This is very much important to maintain transmission line safely. Oxidation of overhead conductor was increased with temperature and time(maximum time : 30min). Conductivity of Al conductor was decreased by Agents. The detailed will be given in the text.

  • PDF

산불에 노출된 가공송전선의 기계적 및 전기적 특성 거동 연구 (Mechanical and Electrical Properties Behavior Study of Overhead Conductor due to Forest Fire)

  • 장용호;김병걸;김상수;한세원;김진한
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.108-109
    • /
    • 2008
  • Forest Fire can cause a serious damage to overhead conductors. Therefore, the detailed investigation for the changes of mechanical and electrical properties of damaged conductors should be carried out to understand the effect of forest fires on conductors. This is very much important to maintain transmission line safely. Especially, this paper describes the changes of mechanical and electrical properties of flame exposed conductor. The detailed will be given in the text.