전자 교반과 결정립 미세화에 의한 반용융 A356 재료의 결정립 크기 비교 (A Comparison of the Grain Size of Semisolid A356 Aluminum Alloy Obtained by EMS Stirring and Grain Refinement)

  • 양자오;서판기;고재홍;정용식;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 추계학술대회논문집
    • /
    • pp.148-151
    • /
    • 2004
  • Different kinds of feedstock of semisolid a356 aluminum alloy manufactured by EMS stirring only, inoculation of Al-5Ti-B only and combination of inoculation and EMS stirring were investigated. It is found that the grain size of these feedstock are $350{\mu}m$ for EMS casting only, $320{\mu}m$ for inoculation by Al-5Ti-B, and $100{\mu}m$ for the combination of EMS stirring and inoculation of Al-5Ti-B master alloys. The microstructure of the sample obtain by combination of inoculation and EMS system show the best homogeneousness and finest grains.

  • PDF

6극 전자석 전자교반 레오캐스팅에 따른 A356의 조직적 / 기계적 영향분석 (Microstructure and Mechanical Property of A356 for Rheocasting Using 6-Pole Electromagnetic Stirring Casting Process)

  • 김백규;노중석;방희재;허민;박진하;전충환
    • 한국주조공학회지
    • /
    • 제40권3호
    • /
    • pp.61-65
    • /
    • 2020
  • Rheo-diecasting with stirring has been used in many material industries. As the 4th Industrial Revolution approaches the world, eco-friendly high-strength and light-weight materials become more important. Casting methods have been studied and used for aluminum-alloy automobile parts. This study carried out the effect analysis of the micro-structure and mechanical properties, such as yield/ultimate tensile strength, elongation, and hardness, of A356 using the 6-pole EMS (electro-magnetic stirring) casting process with a high electromagnetic force. As a result, the hardness and elongation of the A356 after T6 heat-treatment show a significant improvement, respectively, by 20% and 50%.

A356 알루미늄 합금의 파단 충격에너지에 대한 수축공결함의 영향 (Effect of Shrinkage Defect on Fracture Impact Energy of A356 Cast Aluminum Alloy)

  • 황성철;곽시영
    • 한국주조공학회지
    • /
    • 제34권1호
    • /
    • pp.22-26
    • /
    • 2014
  • Internal defects, such as shrinkage during casting, cause stress concentrations and initiate cracking. Therefore, it is important to understand the effects of internal defects on the mechanical properties including the impact behavior. This study evaluates the effects of internal casting defects on the impact performance of A356 Al-alloy castings. The internal shrinkage defects in the casting impact specimen are scanned using an industrial Computed Tomography (CT) scanner, and drop impact tests are performed with varing impact velocities on the A356 casting aluminium specimen ($10mm{\times}10mm$ section area) in order to locate the fracture energy under an impact load. The specimens with defects with a diameter less than 0.35 mm exhibit equivalent fracture impact energies of approximately 32 J and those with a 1.7 mm diameter defect reduced the fracture impact energy by 35%.

용융금속 교반공정을 통한 고Fe 함유 A356 합금의 미세조직 개질 (Microstructural Modification of High-Fe Containing A356 Alloy by Liquid Metal Shearing Process)

  • 김봉환;이상목
    • 한국주조공학회지
    • /
    • 제31권6호
    • /
    • pp.354-361
    • /
    • 2011
  • The liquid metal shearing device was constructed and assembled with a commercial high-pressure die-caster in order to induce intensive turbulent shearing force on molten aluminum alloys. The effect of the liquid metal shearing on the microstructure and tensile properties of A356 alloys was investigated with the variation of iron content. The experimental results show that dendritic primary ${\alpha}$-Al phase was effectively modified into a equiaxed form by the liquid metal shearing. It was also found that the needle-like ${\beta}$-AlFeSi phase in a Fe containing A356 alloy was changed into a blocky shape resulting in the improved mechanical properties. Based on the mechanical properties, it was suggested that the iron content in A356 alloy could be more widely tolerated by utilizing the liquid metal shearing HPDC process.

A356 합금의 중력 주조/단조와 Rheo-diecasting/단조의 미세조직 및 기계적 특성 비교 (Comparison of the Microstructure and Mechanical Property between Gravity Casting Forging and Rheo-diecasting Forging using A356 Alloy)

  • 이준영;임재용;이승용;문성원;홍준표
    • 한국주조공학회지
    • /
    • 제33권5호
    • /
    • pp.210-214
    • /
    • 2013
  • Recently, the automotive industry has replaced cast iron to lightweight materials like aluminum for engine efficiency of automobiles and an emission control by government. In this paper we studied two auto parts manufacturing methods using an alloy of A356. That is gravity casting and H-NCM Rheo-diecasting forging. We analyzed the microstructure and mechanical properties for this method. In Microstructure analysis results, H-NCM Rheo-diecasting forging has more finer microstrucre and better forging effect. Resulting in better mechanical properties than gravity forging.

주조/단조 기술을 이용한 알루미늄 Lower Control Arm 제조에 관한 연구 (A Study on the Manufacture of Lower Control Arm by Casting/Forging Process)

  • 유민수;권오혁;배원병
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 춘계학술대회논문집
    • /
    • pp.139-142
    • /
    • 2003
  • In this study, casting/forging process was used to produce an aluminum lower control arm for automobiles. Firstly, casting experiments were carried out to get an enhanced preform for forging the lower control arm. In the casting experiment, the effect of an additive, Sr, on the mechanical properties such as tensile strength and elongation and the microstructure of a cast preform were investigated. And a finite element analysis was peformed to determine an optimal configuration of the cast preform. Lastly, a forging experiment was carried out to make the final product of aluminum lower control arm by using the above cast preform. In the casting experiments, when 0.025% Sr was added into molten A356, the maximum values of tensile strength and elongation of the cast preform were obtained. In the forging experiment, It was confirmed that the optimal configuration of a cast preform predicted by FE analysis was very useful. The cast/forged product using designed preform was made without any defects.

  • PDF

Numerical and Experimental Study of Semi-solid A356 Aluminum Alloy in Rheo-Forging process

  • 김현호;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.371-374
    • /
    • 2009
  • Die casting process has been used widely for complex automotive products such as the knuckle, arm and etc. Generally, a part fabricated by casting has limited strength due to manufacturing defects by origin such as the dendrite structure and segregation. As an attempt to offer a solution to these problems, forging has been used as an alternative process. However, the forging process provides limited formability for complex shape products. Rheo-forging of metal offers not only superior mechanical strength but also requires significantly lower machine loads than solid forming processes. This paper presents the results of an A356 aluminum alloy sample, which were obtained by experiment and by simulation using DEFORM 3D. Samples of metal parts were subsequently fabricated by using hydraulic press machinery.

  • PDF

A356 중공 주조 샤시 부품에서의 국부적인 인장 변형 특성에 미치는 미세 조직 분석 (Microstructural Analysis of Local Tensile Deformation Characteristics in A356 Hollow Sand Cast Chassis Part)

  • 김재중;고영진;임종대
    • 한국자동차공학회논문집
    • /
    • 제18권6호
    • /
    • pp.1-6
    • /
    • 2010
  • Aluminum rear lower arm is designed for luxury sedan and manufactured by hollow sand casting in the present study. Here we present the relationship between local microstructure and coupon tensile test in the rear lower arm. The characteristics of the local tensile deformation are supposed to be dependent upon Si distribution and DAS (dendrite arm spacing). Si distribution affects the yield strength and DAS affects the elongation of local area in the part, respectively.

레오로지 박판의 전자교반을 응용한 진공 저압주조 제조공정 (Fabrication Process of Rheology Material Thin Plate Using Vacuum Low Pressure Die-casting Process with Electromagnetic Stirring)

  • 장신규;배정운;진철규;강충길
    • 한국주조공학회지
    • /
    • 제32권1호
    • /
    • pp.16-23
    • /
    • 2012
  • In this study, we develop the lower pressure die casting with rheo-forming process of A356 aluminum alloy and vacuum system which can control the crystal size and obtain the high strengthened-light material. Using this process, we fabricate the thin plate for bipolar plate through the low pressure die casting with electromagnetic stirring and vacuum-evacuation which can control the crystal grain by electromagnetic stirring. Thin plate ($110mm{\times}130mm{\times}1mm$) is fabricated by this process. The average Vickers hardness of thin plate is about 77 HV.

A356 합금 미세조직변화에 따른 기계적 특성에 관한 연구 (Mechanical Behavior of A356 depending on the Variation of Microstructure)

  • 김국주;권용남;이영선;이정환;이신호;이재현
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.273-276
    • /
    • 2004
  • A356 alloy is one of the most popular casting aluminum alloys due to its good castability. It is well known that the mechanical properties of A356 alloy strongly depend on its characteristic microstructure, such as the size of eutectic Si, primary $\alpha$ dendrite and so on. These microstructural features are determined during the casting and solidification process, which implies the strong relationship with mechanical properties with solidification methods. In the present study, the mechanical characteristics of A356 alloy was investigated by using squeeze cast control arm in terms of the microstructural features, such as the size of eutectic Si, primary a dendrite. By doing so, the most favorable microstructure of A356 could be determined for Al control arm that should be one of the most reliable parts in automobile.