• 제목/요약/키워드: 1Cr-1Mo Steel

검색결과 354건 처리시간 0.027초

Sp-Creep 시험에 의한 고온 크리프 특성 평가 기술 개발(ll) - 보일러 헤더 - (Development of Evaluation Technique of High Temperature Creep Characteristics by Small Punch-Creep Test Method (ll) - Boiler Header -)

  • 백승세;이동환;하정수;유효선
    • 대한기계학회논문집A
    • /
    • 제26권1호
    • /
    • pp.55-60
    • /
    • 2002
  • For the development of a new creep test technique, the availability of SP-Creep test is discussed for 1Cr-0.5Mo boiler header material. And some results are also compared with those of 2.25Cr- 1Mo steel which widely uses as boiler superheater tube. The results can be summarized as follows. The load exponents(n) obtained by SP-Creep test for 1Cr-0.5Mo steel are decreased with increasing creep temperature and the values are 15.67, 13.89, and 17.13 at 550$^{circ}C$ ,575$^{circ}C$ and 600$^{circ}C$, respectively. The temperature dependence of the load exponent is given by n = 107.19 - 0.1108T. This reason that load exponents show the extensive range of 10∼16 is attributed to the fine carbide such as M$_{23}$C$_{6}$ in lath tempered martensitic structures. At the same creep condition, the secondary creep rate of 1Cr-0.5Mo steel is lower than the 2.25Cr-1Mo steel1 due to the strengthening microstructure composed by normalizing and tempering treatments. Through a SEM observation, it can be summarized that the primary, secondary, and tertiary creep regions of SP-Creep specimen are corresponding to plastic bending, plastic membrane stretching, and plastic instability regions among the deformation behavior of four steps in SP test, respectively.y.

Fe-16Cr-6Ni-6Mn-1.7Mo 스테인리스 합금의 700~900℃에서의 대기중 산화 (Atmospheric Oxidation of Fe-16Cr-6Ni-6Mn-1.7Mo Stainless Steel between 700 and 900℃)

  • 이동복
    • 대한금속재료학회지
    • /
    • 제49권2호
    • /
    • pp.153-160
    • /
    • 2011
  • The AISI 216L stainless steel with a composition of Fe-16Cr-6Ni-6Mn-1.7Mo (wt.%) was oxidized at $700{\sim}900^{\circ}C$ in air for 100 h. At $700^{\circ}C$, a thin $Mn_{1.5}Cr_{1.5}O_4$ oxide layer with a thickness of $0.4{\mu}m$ formed. At $800^{\circ}C$, an outer thin $Fe_2O_3$ oxide layer and a thick inner $FeCr_2O_4$ oxide layer with a total thickness of $30{\mu}m$ formed. The non-adherent scale formed at $800^{\circ}C$ was susceptible to cracking. At $900^{\circ}C$, an outer thin $Fe_2O_3$ oxide layer and a thick inner $Mn_{1.5}Cr_{1.5}O_4$ oxide layer formed, whose total thickness was $10{\sim}15{\mu}m$. The scales formed at $900^{\circ}C$ were non-adherent and susceptible to cracking. 216 L stainless steel oxidized faster than 316 L stainless steel, owing to the increment of the Mn content and the decrement of Ni content.

시효열화시킨 1Cr-1Mo-0.25V 강의 고온에서의 J$_lc$ 및 T$_mat$ 의 평가 (Evaluation of J$_lc$ and T$_mat$ of aged 1Cr-1Mo-0.25V steel at elevated temperature)

  • 윤기봉;윤석호;서창민;남승훈
    • 대한기계학회논문집
    • /
    • 제18권11호
    • /
    • pp.2860-2870
    • /
    • 1994
  • When crack are detected in aged turbine rotors of power plants, information on fracture resistance of the aged material at operating temperature is needed for determination of critical loading condition and residual life of the turbine. In this study, fracture toughness (J$_lc$) and tearing modulus(T$_mat$) of virgin and thermally degraded 1Cr-1Mo-0.25V steel, which is one of the most widely used rotor steels, were measured at 538.deg. C according to ASTM E813 and ASTM E1152, respectively. Five kinds of specimen with different degradation levels were prepared by isothermal aging heat treatment at $630^{\circ}C.$ It was observed that J$_lc$ and T$_mat$ value decreased as the degradation level increased. Analysis of microstructures using a scanning electron microscope showed that the decrement of J$_lc$ is related to segregation of impurities at grain boundaries. It was also verified that the DC electric potential drop method is accurate and reliable for crack length monitoring at elevated temperature.

Magnetic Barkhausen Noise를 이용한 1Cr-1Mo-0.25V강의 열화도 평가 (Evaluation of 1Cr-1Mo-0.25V Steel Degradation Using Magnetic Barkhausen Noise)

  • 이종민;안봉영;남영현;남승훈;이승석;이억섭
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.250-255
    • /
    • 2001
  • It is inevitable to evaluate the life of turbine rotor because the operating periods of power plants need to be extended. The magnetic methods utilizing Magnetic Barkhausen noise curve were applied to detect the degradation caused by thermal aging. The Magnetic property of material depends on the domain dynamics and it is affected by the microstructure of material. Therefore the magnetic property is very sensitive to the microstructure change of the material. It is, thus, very useful to detect the state of degradation of varying materials. The test specimen made of 1Cr-1Mo-0.25V steel was used widely for turbine rotor material, and seven kinds of specimens with different degradation levels were prepared by the isothermal heat treatment at $630^{\circ}C$. With the increase of degradation, BHN was decreased. The result was compared with coercive force and vickers hardness.

  • PDF

수치해석에 의한 $2\frac{1}{4}Cr-1Mo$$CO_2$ 레이저 용접부의 잔류응력 분포 특성에 관한 연구 (A Study on the Distribution of Welding Residual Stresses in $2\frac{1}{4}Cr-1Mo$ Steel by $CO_2$ Laser Welding)

  • 방한서;김영표;김형;유석민
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2003년도 춘계학술대회 논문집
    • /
    • pp.274-278
    • /
    • 2003
  • In recent, an application of high energy density beam we/ding is increasing to obtain the high quality in weldments. Laser welding, especially, has been recognized as an useful method and its beam power has also increased according to the development of relevant technology. However, welding method in the fields of power plant is conservative because their structures have required to endure high temperature and pressure. So, authors conduct the numerical simulation in order to consider the possibility of laser welding on the material of the pressure vessels ($2\frac{1}{4}Cr-1Mo$ steel). As a result of this study, we can confirm the advantages of laser welding and obtain useful information for the experiments of weldability.

  • PDF

650 ℃의 10%O2+10%CO2 가스 환경에서 2.25Cr-1Mo강의 산화특성에 미치는 KCl(s)과 K2SO4(s)의 영향 (Effect of KCl(s) and K2SO4(s) on Oxidation Characteristics of the 2.25Cr-1Mo Steel in 10%O2+10%CO2 Gas Environment at 650 ℃)

  • 정광후;김성종
    • Corrosion Science and Technology
    • /
    • 제19권1호
    • /
    • pp.43-50
    • /
    • 2020
  • In this study, the effects of KCl(s) and K2SO4(s) on the oxidation characteristics of 2.25Cr-1Mo steel were investigated for 500 h in 10O2 + 10CO2 (vol%) gas environmen at 650 ℃. Oxidation kinetics were characterized by weight gain, oxide layer thickness, and fitted models for the experiment data were proposed. The fitted models presented considerable agreement with the experimental data. The oxide layer was analyzed using the scanning electron microscope, optical microscope, and energy dispersive X-ray spectroscopy. The oxidation kinetics of 2.25Cr-1Mo steel with KCl and K2SO4 coatings showed significantly different oxidation kinetics. KCl accelerated the oxidation rate very much and had linear oxidation behavior. In contrast, K2SO4 had no significant effect, which had parabolic kinetics. The oxide layer was commonly composed of Fe2O3, Fe3O4, and FeCr2O4 spinel. KCl strongly accelerated the oxidation rates of 2.25Cr-1Mo steel in the high-temperature oxidation environment. Conversely, K2SO4 had little effect on the oxidation rates.

고합금강과 오스테나이트 스테인레스 강의 저사이클 피로 특성 연구 (Study on Characteristics of Low Cycle Fatigue for High Alloy and Austenite Stainless Steel)

  • 김용찬;백세현
    • 동력기계공학회지
    • /
    • 제14권6호
    • /
    • pp.29-34
    • /
    • 2010
  • As the steam temperature of fossil power plant boiler is increasing, the use of 9Cr-1Mo high alloy material is prevalent and it is needed to investigate the characteristics of low cycle fatigue for high alloy and austenite stainless steel that has used up to recently. As a result of test, in 9Cr-1Mo high alloy steel, the relation of strain and fatigue life is non-linear and the crack mode of low cycle fatigue is brittle but in the austenite stainless steel, that of strain and fatigue life is linear and the crack mode of low cycle fatigue is ductile. Comparing the fatigue life between high alloy and austenite stainless steel, there is no consistent characteristics as to strains. But the fatigue life of 9Cr-1Mo steel is longer by 25% than that of STS304 stainless steel in the relatively low, 0.3% strain. In the other strain, the fatigue life of two materials is similar.

X20CrMoV 12 1 강의 용접부에서의 균열진전 특성연구 (Time-dependent Crack Growth in X20CrMoV 12 1 Steel Weld joint)

  • 이남우;김광수;정용근;박종근
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.322-327
    • /
    • 2000
  • This paper investigates the time-dependent crack growth in X20CrMoV 12 1 steel weld joints. Crack growth test are carried out $545^{\circ}C$ on side-grooved 1/2T CT specimens under static loads. A simulated material is produced for the intercritical HAZ, where fracture normally occurs. Constitutive properties are obtained for the simulated HAZ material as well as for the base metal and weld metal. Finite element analyses of crack growth are performed on the models with and without a HAZ layer, using the experimental crack length-time history. The inclusion of HAZ layer increase the load line velocities significantly. The crack growth rates are correlated reasonably well with $C^*$. The smallest crack size for the validity of $C^*$ is found much smaller than the ASTM crack initiation size for 1T CT specimen of creep ductile materials.

  • PDF

전기비저항을 이용한 2.25Cr-1Mo 강 열화재의 미세조직 및 연성-취성천이온도 평가 (Evaluation of Microstructure and Ductile-Brittle Transition Temperature in Thermally aged 2.25Cr-1Mo Steel by Electrical Resistivity Measurement)

  • 박재원;권숙인
    • 비파괴검사학회지
    • /
    • 제22권3호
    • /
    • pp.284-291
    • /
    • 2002
  • 전기비저항법을 이용하여 2.25Cr-1Mo 강의 경년열화도를 평가하고자 하였다. 2.25Cr-1Mo 강이 $540^{\circ}C$에서 장시간 노출되었을 때 일어나는 미세조직 변화를 모사하기 위해 인공 열화를 실시하였으며 열화에 따른 미세조직 인자 (고용원소의 함량), 기계적 성질 (연성-취성 천이온도 ), 전기비저항을 측정하여 이들간의 상호관계를 구하고자 하였다. 열화재에서는 기지내의 고용 원소 (Mo 와 Cr)의 고갈이 나타났다. 연성-취성 천이온도는 열화 초반부에 급격히 증가 후 포화되는 경향을 보인 반면 전기비저항은 열화 초반부에 급격히 감소 후 포화되는 경향을 보였다. 즉, 열화 시간에 따른 연성-취성 천이온도의 변화 경향과 전기비저항의 변화는 서로 반대적으로 변화하는 관계를 나타내었다.

구형압입시험에 의한 1Cr-1Mo-O.25V강의 기계적 물성 평가 (Spherical Indentation Testing to Evaluate Mechanical Properties in 1Cr-1Mo-0.25V Steel)

  • 이종민;이승석;이억섭;남영현
    • 비파괴검사학회지
    • /
    • 제22권5호
    • /
    • pp.516-522
    • /
    • 2002
  • 발전소의 터빈 로터강의 수명을 평가하기 위하여 $630^{\circ}C$에서 등온 열처리된 7가지의 서로 다른 시편을 준비하였다. 탄소강, 스테인레스강 등의 금속재료의 유동특성을 평가하기 위하여 개발된 구형압입 시험을 통하여 서로 다르게 열화된 1Cr-1Mo-0.25V강의 기계적 물성을 측정하고 이를 인장시험에서의 결과와 비교하였다. 유동특성을 결정짓는 요소로 재료항복기울기와 구속인자지수를 사용하였다. 이는 가공경화지수의 변화가 매우 작고 불규칙적으로 나타났기 때문이다. 또한 재료항복기울기의 영향을 고려하였을 때 구속인자지수의 영향은 적은 것으로 나타났다.