The effects of binder content and PA content on the flexural, compressive and impact strengths, water absorption and frezzing and thawing of polymer concrete using mixed waste plastics are examined. As a result the flexural, compressive and impact strengths of the polymer concretes using mixed waste plastics tend to increase with increasing binder content and filler content, regardless of the PA content. The flexural, compressive and impact strengths of the polymer concretes using mixed waste plastics decrease with increasing PA content. The water absorption of the polymer concretes using mixed waste Plastics tend to decreased with increasing binder content, regardless of the PA content. The durability factor of the polymer concretes using mixed waste plastics tend to increased with increasing binder content. However, the durability factor of the polymer concretes using mixed waste plastics tend to decreased with increasing PA content.
With several different dosages of multi-walled CNTs which was 0.1, 0.3, and 0.5% of the weight of binder, the fluidity in fresh CNT cement composites, as well as the strength and strength development with age of the hardened composites were investigated in this experimental study. The experimental results from flow test indicated that the increase in the dosage of CNTs badly impacted on the workability of fresh composites, and the results from rheological measurements presented the decrease in plastic viscosity and the increase in yield stress according to the amount of CNTs. In addition, the thixotrophy in the flow curve obtained from the rheology test was observed more noticeably in the composites with higher dosage of CNTs. With the experiments on the strength properties, the improvement of both compressive and tensile strengths with the increase of CNTs dosage could be obtained. Moreover, early strength development by adding CNTs was found when it was compared with plain cementious matrix without CNT.
재생콘크리트의 압축강도와 휨강도는 재생골재의 혼입량이 증가할수록 감소하였으며 플라이애쉬를 혼화재로 사용할 때 그 양이 증가할수록 재생콘크리트의 조기 압축강도는 떨어졌다. 골재원에 따른 압축강도는 재생골재의 혼입량이 적을수록, 양생기간이 길어질수록 증가하엿으나, 전반적으로 비슷한 강도변화의 경향을 보여주고 있다. 재생콘크리트의 휨강도 발현은 보통 콘크리트와 비슷하나, 휨강도에 대한 압축강도비는 보통 콘크리트에 비하여 낮았다. 재생콘크리트의 건조수축은 재생골재의 혼입량이 증가할수록 증가하였으며 , 특히 재령2주와3주사이에 건조수축량이 보통 콘크리트에 비해 월등히 높았다.
The effects of binder and alumina content on the setting time, drying shrinkage, strength, freezing and thawing resistance and water absorption of polymer-modified pastes with alumina powder were examined. As a result the setting time of the polymer-modified pastes with alumina powder tended to delay with increasing binder content. Irrespective of the type of polymer, the drying shrinkage of the polymer-modified pastes with alumina powder tended to decrease with increasing binder content and alumina powder content. Regardless of the type of polymer, the tensile and adhesion strengths of the polymer-modified pastes with alumina powder tended to increase with increasing binder content and alumina powder content. Irrespective of the type of polymer, the durability factors of the polymer-modified pastes with alumina powder tended to increase with increasing alumina content. Irrespective of the type of polymer, the water absorptions of the polymer-modified pastes with alumina powder tended to decrease with increasing binder content and alumina content.
The effects of binder content and recycling mixed waste plastics(PA) content on the workability, work life and hardening shrinkage of fresh polymer concrete using mixed waste plastics are examined. As a result, the workability of the polymer concretes using mixed waste plastics tend to improve with increasing binder content, PA content and filler content. The work life of the polymer concretes using mixed waste plastics is shortened with an increase in the initiator content and curing temperature. The length change of the polymer concretes using mixed waste plastics tend to increased with Increasing binder content and PA content. The result of the present research is expected to make a contribution to the recycling of final mixed waste plastics and the continuing efforts for the development of use of the recycled products are thought to expand the horizon for the recycling of the final mixed waste plastics.
To evaluate the bind rate and behavior of two types chloride ion-one is the chloride ion added in mixture when un-washed sea sand is used as fine aggregate, one is the chloride ion admitted in the new version of concrete standard specification, pore solution extracted in cement paste were analyzed. The results are follow. 1 As passing the time, the chloride concentration in the pore solution decreases with the Increase in the chloride content absorbed by the hydrate products. As compared with chloride contents in mixing water, the bound ratio of chloride at 49 days is 64∼90%. 2. The bound ratio of chloride in cement paste considering evaporable water as pore solution is obtained. In case of Pl∼P3(added chloride content wt of cement 0.046∼0.16 %), the bound ratio of chloride is 91.8∼93.5 %. P4(added chloride wt of cement 0.3%) is 89.1%, but P5(added chloride wt of cement 0.617%) bound is only 77%. 3. The bound ratio of chloride to wt of cement is 0.015∼0.475% with adding chloride. In case chloride added over 0.091 % wt of cement, the bound chloride content increases 1.7∼1.8 times in spite of added chloride increase twice. The bound ratio of chloride to wt of cement decreased with the increase in the chloride content. 4. The more increase added chloride content, the more increase the bound ration of chloride. But the absolute value of chloride content in pore solution increased.
최근들어 성능이 우수하고 품질이 높은 새로운 건설소재를 개발하려는 노력이 계속되고 있다. 본 논문에서는 고강도화 및 연성확보를 위하여 폴리머 콘크리트에 섬유를 혼입한 섬유보강 폴리머 콘크리트를 제조하여 강도 및 역학적 특성을 규명하고자 하였다. 이를 위하여 포괄적인 실험연구를 수행하였으며 주요실험변수로는 강섬유의 혼입량과 채움재(filler)의 혼입량, 그리고 양생온도를 주요변수로 선정하였다. 강섬유의 혼입량은 체적비로 0%, 1%, 2%로 변화시켰으며, 채움재와 수지의 비는 1.0과 1.5로 하였다. 본 연구결과 섬유의 혼입으로 인하여 압축강도, 휨강도, 인장강도 모두 증가하였으며, 특히 인장강도의 증가가 더 크게 나타났다. 양생온도가 증가한 경우 폴리머의 중합반응이 좋아져 강도가 증가하였다. 또한 본 논문에서는 섬유보강 폴리머 콘크리트의 응력-변형도 관계곡선을 도축하였으며, 이것은 구조설계시 중요한 기초가 될 것으로 사료된다.
Journal of the Korea institute for structural maintenance and inspection
/
v.8
no.4
/
pp.265-273
/
2004
As a result of compressive strength experiment, rupture compressive strength showed more increases in specimens of 15% and 20% of Cockle shells in those of non-mixture. The specimen which was used general aggregate showed the highest value and ductility capacity was getting decreased as the amount of cockle shell was getting increased in the ductility capacity of specimen. We might conclude that the reason of the yield strength's decline was the lack of the bond strength which was caused by the amount of cockle shell.
Journal of the Korea Institute of Building Construction
/
v.16
no.3
/
pp.201-209
/
2016
This study is to examine experimentally on the engineering properties of fiber reinforced concrete using kenaf(KN) fiber and another organic fibers for comparing test, and propose the usable method of KN fiber as an natural fiber in the concrete industry. It is to select 4 contents(0, 0.3, 0.6 and $0.9kg/m^3$) of KN fiber and 4 organic fibers (Jute, Cellulose, Polypropylene and Nylon). For this study, it is to perform various tests including slump, air content, plastic and drying shrinkage, flexural and tensile strength, carbonation depth for the fiber reinforced concrete according to contents of KN fiber and 4 organic fibers. The results of this study are as follows : In case of KN fiber contents $0.6kg/m^3$, it shows the effective results from increasing concrete strength including flexural and tensile, from decreasing plastic and drying shrinkage, carbonation depth. Also KN fiber is confirmed having excellent performances by comparing with test results of another organic fibers as same contents $0.6kg/m^3$. Therefore, considering concrete test results, cost and environment, KN fiber is proposed as the optimum contents in the range of $0.6kg/m^3$ and an effective fiber materials, and needs to keep up these study on the site application.
Journal of the Korean Recycled Construction Resources Institute
/
v.2
no.1
/
pp.19-25
/
2014
The purpose of this study is to establish experimentally the mechanical properties of fiber reinforced concrete using kenaf dosages and propose the usable method of kenaf fiber in the concrete industry as natural fiber materials. Kenaf fiber help make the concrete strength including tensile and flexural stronger, more resistant to plastic and drying shrinkage, less amount of carbon dioxide because of having a rough surface and excellent tensile strength of fiber and improving the concrete's corrosion resistance. It is to select the kenaf dosages of 4 cases (0, 0.3, 0.6 and $0.9kg/m^3$ and perform various tests including slump, air content, plastic and drying shrinkage, flexural and tensile strength for fiber reinforced concrete. The results of this study are as follows : In case of increasing kenaf fiber dosages, show the slump decrease and air content increase, also take effect results for increasing concrete strength including flexural and tensile, decreasing plastic and drying shrinkage. therefore, considered test results and cost, the optimum dosages of kenaf fiber is proposed about $0.6kg/m^3$ and need to study on the site application considering concrete quality and another compared tests.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.