Analysis of Air Void Systems in Latex-Modified Concretes with Cement Types (시멘트 종류에 따른 라텍스개질 콘크리트의 미세공극 구조 분석)

  • Yun, Kyong-Ku;Jeong, Won-Kyong;Kim, Ki-Heun;Kim, Kyong-Jin
    • International Journal of Highway Engineering
    • /
    • v.7 no.1 s.23
    • /
    • pp.73-82
    • /
    • 2005
  • Linear traverse method and point count method described at ASTM have been widely used to estimate the air void system in hardened concrete. These methods, however, are rarely used at present, because they require many efforts and time consuming works. Also these results depend on each person's decision, and are not repeatable. Thus, new image analysis method using microscope and computer processes has been approached for analyzing air void system in hardened concrete. The purpose of this study was to analysis the air void systems in latex-modified concretes using a reasonable and objective image analysis method with main experimental variables such as cement types(ordinary portland cement, rapid setting cement) and latex contents(0%,15%). In the results of this study, the use of polymer latex showed that it could be attributed to its air void systems, due to the fact that the latex emulsion acts as an air-entraining agent, which thus generally guarantees an adequate air-void system.

  • PDF

The Recycling of Inorganic Industrial Waste in Cement Industry (시멘트산업에서 무기질 산업 폐·부산물의 재활용)

  • Kang, S.K.;Nam, K.U.;Seo, H.N.;Kim, N.J.;Min, K.S.;Chung, H.S.;Oh, H.K.
    • Clean Technology
    • /
    • v.6 no.1
    • /
    • pp.61-69
    • /
    • 2000
  • In this study, generation process and properties of inorganic industrial waste which can be used in cement industry were investigated. The scheme of recycling to use the selected waste as raw materials, mineralizer and flux, admixture and raw materials for special cement was decided and then various experiments were carried out. The experimental results were as follows ; In the use of industrial waste as raw materials, ferrous materials could be substituted by Cu-slag, Zn-slag, electric arc furnace or convertor furnace slag etc., and a siliceous material could be substituted by sand from cast-iron industry. By-products from sugar or fertilizer industry, which has $CaF_2$ as the main component, and jarosite from Zn refinery enabled clinker phases to be formed at lower temperature by $100{\sim}150^{\circ}C$. Adding Cu slag and STS sludge in proper proportion to cement improved properties of cement. Fly ash and limestone powder as admixture had the same effect on cement. As a raw material for special cement, aluminium waste sludge could be used in making ultra early strength cement, which had the compressive strength of $300kg/cm^2$ within 2hours. And two different ashes from municipal incinerator could be raw materials of the cement which was mainly composed of $C_3S$ and $C_{11}A_7{\cdot}CaCl_2$ as clinker phases.

  • PDF

An Evaluation of Flexural Behavior of Fume Pipe Repaired by Hybrid Concrete Repair Materials (하이브리드 콘크리트 보수재료로 보수된 흄관의 휨 거동 평가)

  • Yoo, Sung Won;Choi, Young Cheol
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.6
    • /
    • pp.92-98
    • /
    • 2019
  • In this study, we developed a repair material incorporating PVA powder resin and nylon fiber into cemented carbide used in the existing field to improve adhesion performance and water tightness with existing concrete. Flexural behavior evaluation was performed. The main experimental variables were PVA powder resin, nylon fiber mixing rate and damage type, and performance tests were conducted to evaluate compressive strength and flexural behavior after repairing materials. It was found that all formulations fully satisfied the required performance of the repair material. The flexural strength test results of the repaired tube specimens showed that the performance of the repaired materials was maximized when the nylon fiber was added and the PVA powder was added in an appropriate amount. The flexural behavior of all the specimens showed the flexural behavior of the structural members with a low rebar ratio, suggesting that the amount of iron wire in the domestic fume pipe was somewhat insufficient. That is, it was confirmed that the amount of reinforcement of the steel wire was somewhat small, so that the concrete was cracked before the behavior of the concrete and the steel wire reached the extreme state, and the concrete was immediately destroyed beyond the tensile strength of the concrete.

An Experimental Study on Rapid Repairing Mortar for Road with Steel Slag (철강 슬래그를 사용한 도로용 긴급보수 모르타르에 관한 실험적 연구)

  • Jung, Ui-In;Kim, Bong-Joo;im, Jin-Man;Kwak, Eun-Gu
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.5
    • /
    • pp.419-427
    • /
    • 2018
  • The purpose of this study is to recycle steel slag generated from the iron producing process and to use steel slag as a construction material which is currently landfilled Steel slag is subjected to aging treatment due to the problem of expansion and collapse when it reacts with water. The Slag Atomizing Technology (SAT) method developed to solve these problems of expanding collapse of steel slag. In this study, experimental study on the emergency repair mortar using the reducing slag, electric arc furnace slag and silicon manganese slag manufactured by the SAT method is Reduced slag was shown an accelerated hydration when it was replaced with rapidly-setting cement, and the rate of substitution was equivalent to 15%. It is shown that the electric furnace oxide slag is equivalent to 100% of the natural aggregate, and it can be replaced by 15-30% when the silicon manganic slag is substituted for the electric furnace oxide slag. With the above formulation, it was possible to design the rapidly repair mortar for road use. These recycling slags can contribute on achieving sustainability of construction industry by reducing the use of cement and natural aggregates and by reducing the generation of carbon dioxide and recycling waste slag.

Autogenous Shrinkage of Very-Early Strength Latex-Modified Concrete with Latex Contents (라텍스함량 변화에 따른 VES-LMC의 자기수축)

  • Park, Won-Il;Choi, Pan-Gil;Yun, Kyong-Ku;Lee, Bong-Hak
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.11 no.3
    • /
    • pp.1059-1065
    • /
    • 2010
  • Very-early strength latex-modified concrete (VES-LMC) was developed for the purpose of fast-track overlay of a concrete bridge deck under heavy traffic, concentrated on the workability, durability, and strength gain so that it can be opened to the traffic only three hours after its placement. The mixture of VES-LMC might accompany very high heat of hydration at early-age because of its inherent rapid hardening property and could have susceptibility to autogenous shrinkage because of its relatively low water-cement ratio. This study evaluated the effect of the latex-cement ratio(L/C) both of the constant and variable slumps on the autogenous shrinkage of VES-LMC by carrying out simple temperature rise test and early-age shrinkage experiment. Test results are as follows: The latex contributes on the enhancement of the concrete durability but has little effect on its hydration and the accompanied heat of hydration in VES-LMC. Autogenous shrinkage increased with the increase in latex-cement ratio at variable slumps and its pattern followed regularly a logarithmic increase. However, the influence of water-cement ratio and latex-cement ratios for the test specimens at constant slump on early-age autogenous shrinkage property was found to be minor due to the simultaneous effect of the two experimental variables.

Early-Age Deformation of Very-Early Strength Latex- Modified Concrete with Ultra-Fine Fly Ash Contents (울트라파인 플라이 애시 혼입률에 따른 VES-LMC의 초기거동 특성)

  • Choi, Pan-Gil;Park, Won-Il;Yun, Kyong-Ku;Lee, Bong-Hak
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.11 no.3
    • /
    • pp.1040-1046
    • /
    • 2010
  • The main disadvantage of rapid setting concrete is the occurrence of cracking because of fast hydration reaction due to high thermal expansion and shrinkage. However, if the fly ash is used in concrete, it is possible to prevent cracking since the hydration heat can be decreased. Although Very-Early Strength-Latex Modified Concrete(VES-LMC) is an excellent material, occurrence of cracking has been reported because of high hydration heat. In the present study, new method which can apply the fly ash to the VES-LMC was developed. Research for the new method to improve the safety for the cracking was conducted. Safety was confirmed by reducing the shrinkage and hydration heat in the condition of overcoming the low early-age strength. Detailed conclusions are follows. Early-age compressive strength was decreased a little with increase of UFFA content. However, 28-d compressive strength was statistically insignificant regardless of UFFA contents. If the UFFA is replaced 15% to 20% of unit cement weight in concrete, maximum shrinkage can be reduced up to 43% to 47%. Usage of UFFA in VES-LMC guarantees the safety for cracking since it is very effective to control of early-age shrinkage.

Durability Properties of Ultra Rapid Hardening Mortar Produced with Alumina-based Binder for Repairing Sewage Treatment Pipes (하수관거 보수용 알루미나계 결합재 초속경 모르타르의 내구 특성)

  • Eun-Ho, Kim;Byung-Jae, Lee;Sun-Mok, Lee;Yun-Yong, Kim
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.4
    • /
    • pp.482-488
    • /
    • 2022
  • In this study, the durability of ultra rapid hardening mortar for sewage pipe was evaluated by type of mortar binder. As a result of analyzing the internal structure for each type of mortar, it was confirmed that Al2(OH)3 was generated in the internal structure of the CAC-based mortar, and its corrosion resistance was superior to that of other types of mortar. As a result of the compressive strength test, OPC had the tsmallest strength, followed by CAC100 > CAC100P > CAC80. This trend was similar to the previous study results. Chloride ion penetration resistance and freeze-thaw test showed similar trends. That is, CAC and C12A7 were better than OPC, and CSA was worse than OPC. This is mostly beacuse of cracks caused by expansion of CSA-based mortar. CAC100P mix showed the best chemical resistance. It is thought that this is because the alumina gel formed inside the mortar and the polymer combine to make the internal structure more dense.

A Experimental Study on the Seawater Attack Resistance of Grouting Mixtures (내해수성 주입재 배합에 관한 실험적 연구)

  • Chun, Byungsik;Choi, Dongchan;Kim, Younghun;Kim, Jinchun
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.1
    • /
    • pp.53-59
    • /
    • 2010
  • In seawater deposition condition, the corrosion and chemical attack of grouts are similar to those of concrete structure. Used in domestic MSG (Micro Silica Grouting) mixtured large amounts of silicate materials containing as cement powder is $8,000cm^2/g$ of the specific surface area or more due to the high hydration activity and high-strength, high durability, and features, $C_3A$ content of less than 5% to meet the standards chemical attack of seawater was evaluated as a cement material. Therefore, in this paper, with excellent seawater attack resistant MSG in combination with rapid hardening mineral was used, those of seawater characteristics were evaluated experimentally. Typically, sodium-silicate minerals or rapid hardening cements are used in domestic. About the homogel specimens with combination of MSG and rapid hardening agents for compressive strength, weight and length change characteristics were evaluated experimentally, and so we could present the excellent seawater resistant grouts combination.

Strength Properties of Mortar According to Types of Binders for Reducing Curing Process of Concrete Secondary Products for Reduction CO2 (CO2 절감을 위한 콘크리트 2차제품 양생단계저감용 결합재 종류에 따른 모르타르 강도특성)

  • Kim, Ha-Seog;Baek, Dae-Hyun;Lee, Sea-Hyun
    • Resources Recycling
    • /
    • v.23 no.4
    • /
    • pp.37-46
    • /
    • 2014
  • Carbon dioxide generated from construction materials and construction material industry among the fields of construction is approximately 67 million tons. It is about 30% of the carbon dioxide generated in the fields of construction. In order to reduce carbon dioxide in the fields of construction, it is necessary to control the use of fossil fuel consumed and decrease carbon emission by reducing the secondary and tertiary curing generating carbon dioxide in construction material industry. Therefore, this study manufactured mortar by having cement as the Plain and substituting three binding materials up to 50% and then adopted different curing methods to analyze congelation and strength characteristics. Test results for strength property by changing binding materials showed that specimens with blast furnace slag, CSA 15% and CAMC 5% resulted in positive effect for strength.

Estimation of Air Void System and Permeability of Latex-Modified Concretes by Image Analysis Method (화상분석법을 이용한 라텍스개질 콘크리트의 공극 구조와 투수성의 상관성 분석)

  • Jeong Won-Kyong;Yun Kyong-Ku;Hong Seung-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.5 s.89
    • /
    • pp.695-702
    • /
    • 2005
  • It is known that latex-modified concretes were increased their durability and permeability by added latex. The purpose of this study was to analysis the air void systems in latex-modified concretes using a reasonable and objective image analysis method with main experimental variables such as water-cement ratios, latex contents(0%, 15%) and cement types(ordinary portland cement, high-early strength cement and very-early strength cement). The results are analyzed spacing factor, air volume after hardened, air distribution and structure. Also, air void systems and permeability of latex-modified concretes were compared with correlation. The results are as follows; The same w/c ratio LMC showed better air entraining effect than OPC with AE water reducer. The VES-LMC showed that the number of entrained air below $100{\mu}m$ increased more than four times. In the HES-LMC, micro entraining air having range from 50 to $500{\mu}m$ increased above 7 times without antifoamer. Though spacing factor was measured low, latex-modified concretes were showed that permeability was good. It is considered that air void system does not have an effect on the property of latex-modified concretes but latex film is more influenced in the their durability.