• Title/Summary/Keyword: 제강

Search Result 389, Processing Time 0.029 seconds

Triboelectrostatic Recovery of High Zinc-Containing Particulate contents from Steel-Making Process Dust (전기로 제강분진 중 고아연함량입자 성분의 마찰대전분리 회수)

  • Chang Hyun-Joo;Kim Dong-Su;Kim Hang-Goo;Cho Min-Yaung;Namkung Won
    • Resources Recycling
    • /
    • v.13 no.2
    • /
    • pp.39-46
    • /
    • 2004
  • The amount of electric furnace dust has been steadily increasing due to the increase of iron scraps which are usually recycled by electric furnace melting process. To date, this electric furnace dust has usually been treated by landfilling, however, because of shortage of landfill sites and heavy metal leaching more desirable treatment schemes are urgently needed. Among several possible schemes for the proper treatment of electric furnace dust, its recycling can be said to be most desirable. In present study, the triboelectrostatic separation of zinc and zinc-containing components from electric furnace dust was attempted based on its physicochemical properties such as particle shape, size distribution, and chemical assay. The dust was found to be mixed with spherical and non-spherical shaped particles and its major component materials were $ZnFe_2$$O_4$, ZnO, Fe, Zn, and FeO. The content of zinc-containing components in the entire dust was observed to be in the range of 15~30 wt%, which reasonably justified that zinc is recyclable. The triboelectrostatic characteristic of each component material was found to be different each other since their work functions were different, and based on this characteristic zinc and zinc-containing component could be flirty separated from the dust. After selecting a proper tribo-elec-trification material, the separation features of zinc and zinc-containing component were examined by taking the distance of electrodes, electric field strength, and scavenging as the experimental variables. The highest zinc-content obtained under the optimal separating condition was found to be up to 50wt%.

Residual Effects of Basic Oxygen Furnace Slag as Soil Conditioner in the Rice Paddy Field (논토양 벼 재배에서 제강슬래그의 토양개량제로서의 시용효과)

  • Lim, June-Taeg;Kim, Young-Sin;Park, Jn-Jin;Lee, Choong-Il;Hyun, Kyu-Hawn;Kwon, Byung-Sun;Kim, Hak-Jin
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.33 no.3
    • /
    • pp.205-211
    • /
    • 2000
  • This study was conducted to evaluate the residual effects of basic oxygen furnace (BOF) slag applied in rice paddy fields as soil conditioner one year before. The experimental fields of Lim et al. (2000) located in Youjung and Nampyung were used for this purpose. Both variety (Oryza sativa L. cv. Dongjinbyeo) and cultural practices were the same as those in Lim et al. (2000). Soil chemical properties, plant height, number of tillers per plant, yield and yield components were observed. The temporal variation of treatment mean value in soil chemical properties appeared to be similar trends in both Youjung and Nampyung experimental fields. Soil pH and Ca content were still significantly higher than those in control treatment up to July of the second season, but decreased progressively as time passed. However, the effects lasted longer as slag rate became higher. BOF slag seems to have residual effects as a soil conditioner or Ca fertilizer in soil for two years. BOF slag rate of $4Mg\;ha^{-1}$ raised soil pH almost the same as lime rate of $2Mg\;ha^{-1}$. Content of $SiO_2$ in soil applied slag appeared to be higher compared with control. Fe and Mg content in soil with slag treatment was significantly higher than that of control in 1997, but it was almost the same level as that of control in 1998. In YouJung experimental field, rough rice yield of slag teatment became higher as slage rate incresed. Slag rate of $12Mg\;ha^{-1}$ showed the highest rough rice yield of $5,400kg\;ha^{-1}$ among treatment, which was 14% higher than that of control with $4,720kg\;ha^{-1}$. Slag rate of $12Mg\;ha^{-1}$ showed relatively higher plant height and higher number of tillers at the early growth stage compared with other treatments. In NamPyung experimental field, rough rice yield was the highest at the plot of lime rate $2Mg\;ha^{-1}$ and became higher as slag rate increased. There were no significant differences in rough rice yield between lime treatment and slag treatments. Slag rate of $12Mg\;ha^{-1}$ showed the highest rough rice yield of $7,170kg\;ha^{-1}$ among slag treatment, which was 8% significantly higher than that of control with $6,670kg\;ha^{-1}$. Slag rate of $12Mg\;ha^{-1}$ showed relatively slower growth in plant height at the early growth stage, but superior growth at the later growth stage, and significantly higher number of spiklets per panicle and 1000-grain weight than that of control.

  • PDF

Evaluation of Basic Oxygen Furnace Slag as Soil Conditioner in the Soybean Upland Field (밭토양 콩재배에서 제강슬래그의 토양개량제로서의 시용 효과)

  • Lim, June-Taeg;Kim, Hee-Kwon;Park, In-Jin;Lee, Choong-Il;Hyun, Kyu-Hawn;Kwon, Byung-Sun;Kim, Hak-Jin
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.33 no.6
    • /
    • pp.493-497
    • /
    • 2000
  • An experiment was conducted to evaluate the possibility of using basic oxygen furnace (BOF) slag as soil conditioner in soybean upland field. In 1997, soybean (Glycine max L. cv. Eunha) crop was cultivated under different application rates of BOF slag at an experimental field of Chonnam Rural Development Administration in Nampyung, Najoo city. Five treatments, four application rates of BOF slag (0, 4, 8, $12Mg\;ha^{-1}$) and one application rate of lime ($2Mg\;ha^{-1}$) were tried with three replications. Plant height and shoot dry weight per plant were measured five times during the growth period. Chemical contents of soybean plant tissues and soil were also measured at the same sampling date. Yield were estimated by harvesting $6.6m^2$ per experimental unit and yield components were measured by sampling 10 plants per experimental unit at the harvest date. In upland soil, application of BOF slag rarely affected contents of total nitrogen, organic matter, available phosphate and potassium in soil. Soil pH, and contents of Ca and Fe in soil became higher as BOF slag rate increased. Enhancement of soil pH by application of BOF slag appeared to be closely related with increase in soil Ca content. Application rate of $2Mg\;ha^{-1}$ of lime showed almost the same effect in increase of soil Ca content as application rate of $4{\sim}8Mg\;ha^{-1}$ of BOF slag. Slag treatment hardly affected the contents of total nitrogen, $P_2O_5$, CaO, $K_2O$ and MgO in the shoot of soybean plants. Soybean plants under treatments of BOF salg showed better growth from the earlier growth stage compared with those of control treatment, and at the later growth stage, their growth was even superior to that of lime treatment. BOF slag rate of $8Mg\;ha^{-1}$ showed the highest soybean yield with $1,232kg\;ha^{-1}$. which was $330kg\;ha^{-1}$ or 37% higher than the yield of control with $902kg\;ha^{-1}$, As a result, BOF slag appeared to be useful material as a soil conditioner as well as nurient source for Ca and Fe in upland soybean fields, and its optimal rate for higher yield seemed to be around $8Mg\;ha^{-1}$.

  • PDF

A Chemical Study of the Periodic Precipitation Reaction in Natural Rocks (자연 암석에서 나타나는 주기적침전반응의 화학적 연구)

  • Jun, Sang-Ho;Han, Mi-Ae
    • Economic and Environmental Geology
    • /
    • v.40 no.4
    • /
    • pp.491-496
    • /
    • 2007
  • This study conducted a chemical experiment on the Leisegang phenomenon, which is known to be the principle of rhyolite formation, and analyzed the results. Even if the same chemical elements precipitated, the shape of Leisegang rings was different according to the condition of medium and depending on inner electrolyte and outer electrolyte. The experiment used agar, gelatin and mung-bean jelly as media. We prepared 0.01M inner electrolyte containing agar 1%, gelatin 2% and mung-bean jelly 5% and curdled the solution at room temperature for 12 hours and, as a result, we obtained viscosity optimal for experimenting on the diffusion of outer electrolyte, and Leisegang rings appeared clearly according to the characteristic of each chemical element. In $PbI_2$ with solubility product($K_{sp}$) of $7.9{\times}10^{-9}$ the intervals of Leisegang rings caused by the reaction of inner electrolyte 0.01M KI and outer electrolyte 25% $Pb(NO_3){_2}$ were narrow between 0.01cm and 0.12cmm but increased gradually, but in with of $8.3{\times}10^{-17}$ the intervals of Leisegang rings caused by the reaction of inner electrolyte 0.01M KI and outer electrolyte 25% $AgNO_3$ were between 0.7cm and 0.45cm and decreased gradually. This suggests that, in the chemical formation of Leisegang rings, the interval and size of the rings are correlated with the solubility product of the precipitates.

제강분진을 반응촉매로 이용한 침출수의 연속산화처리공정

  • 강정우;장윤석;지원현;김성용;배범한;장윤영
    • Proceedings of the Korean Society of Soil and Groundwater Environment Conference
    • /
    • 2001.09a
    • /
    • pp.164-167
    • /
    • 2001
  • 본 연구에서는 포항제철소에서 제철부산물로 발생되는 제강분진을 전처리 없이 산화촉매로 사용하여 김포 수도권 매립지의 침출수 처리공정에서 펜톤산화조에 유입되는 원수를 대상으 로 과산화수소를 이용한 연속식 산화처리 실험을 수행하였다. 먼저 회분식 실험결과를 바탕 으로 최적 반응조건에서 lab-scale 연속식 기초반응실험과 자체 설계.제작한 연속산화공정에서의 처리실험을 수행하였다. 또한 기존의 펜톤산화공정에서 Fe 공급원으로 사용되고 있는 FeSO$_4$.7($H_2O$)와의 반응성 비교실험도 수행하였다. 반응기간동안 일정 pH를 유지하기 위해 pH controller를 사용하였으며 침출수 수질은 CODcr로 나타내었다. 반응 pH 3.5, 체류시간 1 hr, 과산화수소 주입량 1,500mg/1에서 제강분진과 FeSO$_4$.7($H_2O$)를 각각 주입하여 수행한 연속처리 기초실험에서는 제강분진을 산화반응촉매로 사용한 경우에 침출수CODcr 처리율 62%, 과산화수소의 분해율 52%를 나타내었다. FeSO$_4$.7($H_2O$)를 산화반응 촉매로 사용한 경우에는 약 65-70%정도의 다소 높은 처리효율을 나타낸 반면에 과산화수소의 소비량은 제강분진의 경우보다 약 20%이상의 높은 값을 나타내었다. 연속산화공정 실험에서는 운전 3시간 이후에 유출수 중의 CODcr과 $H_2O$$_2$의 농도가 안정된 값을 나타내었다. 이 때 산화 반응조의 침출수 CODcr 제거효율은 약 43%이었으며, 처리수의 농도는 현재의 침출수 방류기준 이하로 나타났다. 결론적으로 침출수의 연속식 산화처리 실험결과, 처리효율과 경제성에서 제강분진의 산화촉매활용 공정의 개발 가능성이 매우 높은 것으로 나타났다.ell에 의해 완전분해 되었으며, 함께 존재시 TC는 Fe$^{\circ}$만으로는 분해가 되지 않았지만 cell에 의해 완전분해 되었으며, 함께 존재시 TCE분해에 저해작용을 미치는 것으로 나타났다.술의 첨가가 요구되고 있다. 따라서, 산성광산배수 오염지대에 대해 획일적으로 같은 처리방법을 채택하여 사용하는 것보다 각 지역 또는 광산산성폐수가 유출되어 나오는 광산폐기물의 특성 등을 고려하여 거기에 맞는 기술들을 복합적으로 또는 단독으로 사용하되 처리방법 채택 시 신중을 기할 것이 요망된다.정시에는 SeaWiFS 위성과 관련된 global algorithms 중에서 490nm와 555nm의 복합밴드를 포함하는 OC2 알고리즘(ocean color chlorophyll 2 algorithm)을 사용하는 것이 OC2 series 및 OC4 알고리즘보다 좋은 추정 값을 도출할 수 있을 것으로 기대된다.환경에서는 5일에서 7월에 주로 이 충체의 유충이 발육되고 전파되는 것으로 추측되었다.러 가지 방법들을 적극 적용하여 금후 검토해볼 필요가 있을 것이다.잡은 전혀 삭과가 형성되지 않았다. 이 결과는 종간 교잡종을 자방친으로 하고 그 자방친의 화분친을 사용할 때만 교잡이 이루어지고 있음을 나타내고 있다. 따라서 여교잡을 통한 종간잡종 품종육성 활용방안을 금후 적극 확대 검토해야 할 것이다하였다.함을 보이고 있다.X> , ZnCl$_{3}$$^{-}$같은 이온과 MgCl$^{+}$, MgCl$_{2}$같은 이온종을 형성하기 때문인것 같다. 한편 어떠한 용리액에서던지 NH$_{4}$$^{+}$의 경우 Dv값이 제일 작았다. 바. 본 연구의 목적중의 하나인 인체유해 중금속이온인 Hg(II), Cd(II)등이 NaCl같은 염화물

  • PDF

Characteristics of Polyester Polymer Concrete Using Spherical Aggregates from Industrial By-Products(II)(Use of Fly Ash and Atomizing Reduction Steel Slag) (산업부산물 구형골재를 사용한 폴리에스테르 폴리머 콘크리트의 특성(II) (플라이 애쉬와 아토마이징 제강 환원슬래그 사용))

  • Hwang, Eui-Hwan;Kim, Jin-Man
    • Korean Chemical Engineering Research
    • /
    • v.53 no.3
    • /
    • pp.364-371
    • /
    • 2015
  • For the cost down of polymer concrete, It is very important to reduce the use amount of polymer binder, which occupies most of the production cost of polymer concrete. Fly ash and atomizing reduction steel slag are spherical materials obtained from industrial by-products. Spherical atomizing reduction steel slag was manufactured using steel slag from reduction process of ladle furnace by atomizing technology. To investigate the physical properties of polymer concrete, polymer concrete specimens were prepared with the various proportions of polymer binder and replacement ratios of atomizing steel slag. Results showed that compressive and flexural strengths of the specimens were remarkably increased with the addition amount of polymer binder and the replacement ratios of atomizing steel slag. In the hot water resistance test, compressive strength, flexural strength, bulk density and average pore diameter decreased but total pore volume and pore diameter increased. We found that polymer concrete developed in this study reduced the amount of polymer binder by 18.2% compared to the conventional product because of the remarkable improvement of workability of polymer concrete using spherical fly ash and atomizing reduction steel slag instead of calcium carbonate (filler) and river sand (fine aggregate).

Removal of Heavy Metals from Wastewater Using Steelmaking Slag and Sludge (제강 슬래그 및 분진에 의한 폐수 중 중금속 제거)

  • Hyun, Jae-Hyuk;Kim, Min-Gil;Nam, In-Young;Baek, Jung-Sun
    • Resources Recycling
    • /
    • v.8 no.1
    • /
    • pp.11-17
    • /
    • 1999
  • This study was carried out to investigate the efficiency of stcclmaldng slag and sludge in removing metals existing in wastewater or leachate. Laboratory experiments were performed as a function of initial concentration of metals. pH a and temperature of the background solution and the presence of che1ating agent, EDTA. The test conditions were temperatures r ranging from $25^{\circ}C$ to $50^{\circ}C$; initial concentrations varying from 5mg/L to 50 mg/L; pH between 3 and 11; and Cu. Cd‘ and Pb a as adsorbates. The results of tests showed that overall rates of metals removal were 20~30% at pH 3 and greater than 90% at p pH 7 and 11. Metals were removed from the solution predominantly via adsorption in acidic conditions, and the combined e effects of adsorption and precipitation in neutral and alkaline conditions. In view of the test results and other engineering c characteristics of steelmaking slag and sludg$\xi$, these industrial by-products from steel industry have a high potential to be used l in wastewater treatment and are particularly beneficial when used as landfill liner additives due to thelJ ability to remove heavy m metals from leachate.

  • PDF

Strength Development Characteristics of Clay Stabilized with Electric Furnace Steel Slag (전기로 제강슬래그로 안정화된 연약점토의 강도 발현 특성)

  • Hyeongjoo Kim;Taegew Ham;Taewoong Park;Taeeon Kim
    • Journal of the Korean GEO-environmental Society
    • /
    • v.25 no.5
    • /
    • pp.29-37
    • /
    • 2024
  • This study aimed to investigate the changes in chemical components that occur when weak clay is mixed with steel slag modified with calcium oxide, and to understand the expression characteristics of compressive strength according to hydrophilicity and curing time. XRF testing, SEM imaging, vane shear strength and uniaxial compressive strength testing were conducted. Calcium (Ca) released from the steel slag increases the Ca content in clay by increasing the number of crystal particles and forming a coating layer known as calcium silicate hydrate (CaO-SiO2-H2O) through chemical reactions with SiO2 and Al2O3 components. The weak clay stabilized with steel slag is classified into an initial inactive zone where strength relatively does not increase and an activation zone where strength increases over curing time. The vane shear strength of the initial inactive area was found to be 4.4 to 18.4 kN/m2 in the state of the weight mixing ratio Rss 30% (steel slag 30% + clay 70%). In the case of the active area, the maximum uniaxial compressive strength increased to 431.8 kN/m2 after 480 hours of curing time, which increased due to the apparent adhesion strength of clay through pozzolanic reaction. Therefore, considering the strength expression characteristics of stabilized mixed clay based on the mixing ratio (Rss) during the recycling of steel slag can enhance its practicality in civil engineering sites.

The adsorption efficiency of ceramic filter media prepared with the steel-making slag for the removal of VOCs (휘발성 유기화합물 제거를 위한 제강슬래그로 제조된 세라믹 여재의 흡착효율)

  • Sin, Jun-Ho;Kim, Tae-Heui;Park, Kyung-Bong
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.20 no.3
    • /
    • pp.153-157
    • /
    • 2010
  • We studied the adsorption efficiency of steelmaking slag in removing volatile organic compounds (VOCs) for increasing the recycling rate of steel-making slag. Ceramic filter was prepared by mixing the steel-making slag and the diatomite which is used as adsorbents due to the advantage of the high specific surface area and regular mesopores. The adsorption efficiency for VOCs removal was about 80%, 96% and 85% in acetaldehyde, formaldehyde and ammonia, respectively. The adsorption efficiency over 80% for all The gases showed the practical possibility as the adsorption filter.