Characteristics of micronized blue ceramic pigments using electric arc furnace dust (제강분진을 활용한 청색 세라믹 안료의 미립화 거동에 관한 연구)

  • Kim, Hye-Jin;Han, Kyu-Sung;Hwang, Kwang-Taek;Nahm, Sahn;Kim, Jin-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.29 no.3
    • /
    • pp.115-122
    • /
    • 2019
  • Electric arc furnace dust (EAFD), which is a dust waste generated in the steel manufacturing process, contains heavy metals. Recently, researches of recycling a large amount of valuable metals such as zinc and iron in EAFD are being actively carried out. In this study, EAFD is used as a substitute for cobalt in blue ceramic pigments without any pretreatment. Then, the synthesized blue ceramic pigment using EAFD was micronized and formulated as a ceramic ink for inkjet printer. The particle size distribution, crystal structure and color characteristics during the micronization process were investigated for the development of ceramic ink. $Co_{0.75}Zn(EAFD)_{0.25}Al_2O_4$ ceramic pigments showed excellent blue coloric properties and monomodal distribution through micronization process. The average particle size of $Co_{0.75}Zn(EAFD)_{0.25}Al_2O_4$ ceramic pigments after 3 hours of milling was $0.271{\mu}m$, which is smaller than $0.303{\mu}m$, which is the average particle size of $CoAl_2O_4$ ceramic pigments without EAFD after 5 hours of milling. Especially, it was confirmed that $Co_{0.75}Zn(EAFD)_{0.25}Al_2O_4$ ceramic pigments showed a color difference (${\Delta}E{^*}_{ab}$) value of 5.67, which smaller than ${\Delta}E{^*}_{ab}$ value of $CoAl_2O_4$ during micronization. These results show that EAFD can be used as a raw material for a blue ceramic pigment by replacing expensive cobalt without any pretreatment.

Removal of Aqueous Cyanide through the Utilization of Industrial By-products (산업부산물(제강 Sludge, 제강 Slag)을 이용한 시안 흡착 제거)

  • 이정원;현재혁;조재범
    • Journal of Korea Soil Environment Society
    • /
    • v.3 no.2
    • /
    • pp.89-99
    • /
    • 1998
  • Sorption of the aqueous cyanide onto steel mill sludge and steel mill slag, both of which are the by-products from the converter furnace, was studied. In the study, the influence of temperature, activation energy, concentration and pH on sorption of cyanide was investigated. Three different temperature($25^{\circ}C$ > $37^{\circ}C$> $50^{\circ}C$) was chosen to represent that of landfill leachate. Initial concentration was 1 mg/$\ell$ 5 mg/$\ell$, 10 mg/$\ell$, and 20 mg/$\ell$. In addition, pH was set to three different level, that is, 3, 7, and 11 respectively. As the result of batch mode experiment for cyanide adsorption, the removal rate was found to be proportional to the initial concentration of cyanide. The order of removal rate was 20 mg/$\ell$> 10 mg/$\ell$> 5 mg/$\ell$> 1 mg/$\ell$. Similarly the influence of pH was proportional because of the change in solubility of cyanide. The order of removal rate was pH 11 > pH 7 > pH 3. As the temperature increased, so did the removal rate. The reaction was endothermic and the value of activation energy(Ea) was 127.93 J/mole and 59.44 J/mole respectively at 1 mg/ιand 20 mg/ιof initial concentration. From the experiment, it can be postulated that the capability of steel mill by-products to attenuate aqueous cyanide is enough to be used as substitute for clay liner of landfill site in the aspect of pollutant removal.

  • PDF

A Study on the Separation and Recovery of Useful Metallic Elements(Zn, Pb) from the 2nd Dust in Refining of Crude-Zinc Oxide (조산화아연의 정제과정에서 발생된 2차분진으로부터 유용금속원소(Zn, Pb)의 분리회수에 관한 연구)

  • Yoon, Jae-hong;Yoon, Chi-hyun
    • Resources Recycling
    • /
    • v.30 no.1
    • /
    • pp.66-76
    • /
    • 2021
  • Electric arc furnace dust (EAFD) contains compounds, such as oxides and chlorides, including large quantities of Zn, Pb and Fe. An efficient and stable method for the extraction of metal elements from EAFD is the Rotary Kiln Process. This method is used to recover Zn in the form of crude ZnO (approximately 60%) via the addition of a reducing agent (coke, anthracite) and limestone (for basicity control) to EAFD. This process is commonly used in industry as well as in research and development. Currently, this method is used in many Korean commercial plants, producing approximately 150,000 tons of Crude ZnO per year. The majority of Zn is found in crude ZnO (approximately 76%). In addition components such as Pb, Cd, Sn, In, Fe, Cl, and F are present as oxides, chlorides, and alkaline compounds. This elements have an adverse effect on the zinc smelting process. Therefore, a refining process that eliminates these impurities is essential. In this study, we developed a process technology that efficiently separates Zn and Pb from byproducts (mainly chlorides). A bag filter was used to collect Zn and Pb generated during the dry purification process of crude ZnO. Pure components were recovered as metals or metal carbonate.

A Study on the Recycling of Molten Ladle Slag Residue into LF Process (Ladle내 잔류(殘留) 용융(熔融)슬래그의 LF 공정(工程)으로 재활용(再活用)에 관한 연구(硏究))

  • Kim, Young-Hwan;Yoo, Jung-Min;Kim, Dong-Sik;Lim, Jong-Hoon;Yang, Sung-Ho
    • Resources Recycling
    • /
    • v.22 no.1
    • /
    • pp.36-41
    • /
    • 2013
  • LF slag is formed by EAF carryover slag and slag former(such as lime, dolomite) put into the ladle during the tapping molten metal. After LF process, continuous casting is started when molten steel is sent from ladle to tundish through bottom nozzle of ladle. Conventionally, remained molten slag and steel in ladle are poured into a slag port and they are transferred to a slag yard and then recycled. In this study, we investigated about recycling of molten LF slag residue(including Fe residue to reuse) which is made in steelmaking process. As a result, lime usage was decreased about 2.2~3.2 kg/steel-ton and also molten steel yield rate was increased about 0.3 ~ 0.5 percent point.

Smelting and Refining of Silicon (실리콘의 제련과 정제)

  • Sohn, Ho-Sang
    • Resources Recycling
    • /
    • v.31 no.1
    • /
    • pp.3-11
    • /
    • 2022
  • Silicon is the most abundant metal element in the Earth's crust. Metallurgical-grade silicon (MG-Si) is an important metal that has wide industrial applications, such as a deoxidizer in the steelmaking industry, alloying elements in the aluminum industry, the preparation of organosilanes, and the production of electronic-grade silicon, which is used in the electronics industry as well as solar cells. MG-Si is produced industrially by the reduction smelting of silicon dioxide with carbon in the form of coal, coke, or wood chips in electric arc furnaces. MG-Si is purified by chemical treatments, such as the Siemens process. Most single-crystal silicon is produced using the Czochralski method. These smelting and refining methods will be helpful for the development of new recycling processes using secondary silicon resources.

The Properties of Underwater-Hardening Epoxy Mortar Used the Rapidly Cooled Steel Slag (RCSS) (급냉 제강슬래그를 사용한 수중 경화형 에폭시 모르타르의 특성)

  • Kim, Jin-Man;Kwak, Eun-Gu;Bae, Kee-Sun
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.5
    • /
    • pp.549-555
    • /
    • 2007
  • Although blast furnace slag has been widely used in concrete as a cementitious admixture or aggregate for many years, the slowly cooled steel slag is not used in concrete but mainly in road. Its use in concrete operates problem such as the lack of volume stability due to high free CaO content, which can be potentially hazardous in concrete. However, the rapidly cooled steel slag by atomization has a low free CaO content, a high density, and a spherical shape, so it is expected to use in concrete so much. This paper is to understand the probability that the rapid cooled steel slag can replace the silica sand used as aggregate in the epoxy mortar. We did the experimental study on the properties of the epoxy mortar having various replacement proportion of rapidly cooled steel slag. This study shown that increasing content of the rapidly cooled steel slag in epoxy mortar lead to increase largely the passing time of nozzle by O-lot, compressive strength and flexural strength. However except the flow is almost same level. So we understand that the rapidly cooled steel slag has positive effect on increasing of properties in epoxy mortar.

Desulfurization Reaction according to Ladle Slag Recycling Method in Shaft-Type EAF Operation (Shaft형 전기로 공정에서 ladle 슬래그 재활용 방법에 따른 탈황반응)

  • Jung-Min Yoo
    • Resources Recycling
    • /
    • v.33 no.2
    • /
    • pp.46-53
    • /
    • 2024
  • The residual heat and high CaO content present in the slag remaining in the ladle after the completion of continuous casting in the electric arc furnace (EAF) steelmaking process have been utilized to reduce power consumption and lime usage in the ladle furnace (LF) process. However, if the timing of such processes does not align with the LF and continuous casting operations, the recycling rate will decrease. To increase the slag recycling rate, the effect of ladle slag recycling methods, specifically pouring ladle slag into the slag pot in advance for subsequent recycling, on LF operations was analyzed. The slag liquefaction rate was calculated using the thermodynamic program Factsage 8.3 for ladle molten slag recycling methods. By applying each of the 10 heats operations for the ladle slag recycling methods, the desulfurization ability and LF operation performance were compared. It was found that when slag was immediately recycled into the ladle after continuous casting was completed, power consumption decreased by 0.3 MWh, LF operation time was shortened by 1.2 minutes, and the desulfurization rate increased by 5.8%.

Environmental Characteristics of Leachates from Steel Slag (제강슬래그 침출수의 환경적 특성)

  • Park, Jong-Beom;Lee, Byoung-Chan;Jang, Min-Ho;Na, Hyun-Ho
    • Journal of the Korean Geosynthetics Society
    • /
    • v.11 no.2
    • /
    • pp.31-38
    • /
    • 2012
  • The recycled aggregate for construction, slag, coal ash and such may elute leachates by chemical reaction when in touch with water, and to confirm this, generally the waste process test is executed. If the test result criteria are met, it can be used as replacement aggregate. In case of steel slag, however, the chemical reaction does not end in a short term, but occurs over a long time, generating eluted leachate. Thus, in this study, the leachate from steel slag were analyzed for heavy metal, and the pH change and environmental characteristics of eluted leachate were analyzed. According to the experiment result, the chemical reaction of free CaO and water within the steel slag occurred more actively when stirred, and the smaller the grain size, the higher the pH was. As the result of waste process test, all test items for the two types of specimen were found to have no heavy metal, but from the ICP test analysis result, heavy metals such as Al, Pb, Zn, Fe were detected. It could be confirmed that chemical reaction would occur upon contact of steel slag and water, and heavy metal may be detected depending on experiment conditions and analysis methods, the long-term environmental characteristics should be examined for utilization of steel slag.

Characteristics of Polyester Polymer Concrete Using Spherical Aggregates from Industrial By-Products(II)(Use of Fly Ash and Atomizing Reduction Steel Slag) (산업부산물 구형골재를 사용한 폴리에스테르 폴리머 콘크리트의 특성(II) (플라이 애쉬와 아토마이징 제강 환원슬래그 사용))

  • Hwang, Eui-Hwan;Kim, Jin-Man
    • Korean Chemical Engineering Research
    • /
    • v.53 no.3
    • /
    • pp.364-371
    • /
    • 2015
  • For the cost down of polymer concrete, It is very important to reduce the use amount of polymer binder, which occupies most of the production cost of polymer concrete. Fly ash and atomizing reduction steel slag are spherical materials obtained from industrial by-products. Spherical atomizing reduction steel slag was manufactured using steel slag from reduction process of ladle furnace by atomizing technology. To investigate the physical properties of polymer concrete, polymer concrete specimens were prepared with the various proportions of polymer binder and replacement ratios of atomizing steel slag. Results showed that compressive and flexural strengths of the specimens were remarkably increased with the addition amount of polymer binder and the replacement ratios of atomizing steel slag. In the hot water resistance test, compressive strength, flexural strength, bulk density and average pore diameter decreased but total pore volume and pore diameter increased. We found that polymer concrete developed in this study reduced the amount of polymer binder by 18.2% compared to the conventional product because of the remarkable improvement of workability of polymer concrete using spherical fly ash and atomizing reduction steel slag instead of calcium carbonate (filler) and river sand (fine aggregate).