L/EPS, manufactured in the shape of block and used for civil engineering, is a lightweight material with an excellent resistance to compression, and provides a superb self-sufficient stability. EPS is a suitable material capable of resolving the problem of settlement and lateral flow if it is applied as the soil on soft ground. The Korean Standards (KS) has not yet proposed any testing method for use of EPS as an engineering banking material. Only its testing and quality ordinance as a heat insulation material has been standardized. The design criteria for EPS has been established and applied through the trial construction of KHC (Korea Highway Corporation) and quality test of manufacturer, but most studies on them have been confined to factory products. This study is focused on comparing and analyzing long-term durability by conducting cyclic load test, freezing and thawing test, absorption rate test and others. EPS used in the test was chosen from construction sites and factory products, focusing on the long-term durability of EPS depending on the passage of time. Unconfined compression test results indicated that the strength of collected samples was lower than factory products. While the triaxial compression test results indicated that the shear strength increased in proportion to the increase of confining pressure, and factory products had declining shear strength as the confining pressure rose.
Proceedings of the Korean Society of Disaster Information Conference
/
2022.10a
/
pp.427-428
/
2022
최근 대규모 항만 건설 및 기존 부두 리모델링과 같은 해안 공간 구조물 확충사업이 활발하게 진행되고 있으며 항만 구조물 거동 장기계측을 위한 센서에 대한 관심도 높아지고 있다. 기존의 항만에 적용한 전기식 센서들은 수개월 정도 단기간의 구조물 거동 측정은 가능하지만 수년 이상의 장기계측 시 염수분에 의한 부식 및 내구성에 취약하기 때문에 원활한 측정에 한계점이 있고 센서 설치를 위한 항만 외곽지역 구조물과 육상전원공급설비 배전반 사이의 거리로 인하여 긴 연장의 횡단로 가설전선 보호대 등을 설치해야 하는 어려움이 있다. 따라서, 본 연구에서는 항만 구조물 거동 장기계측을 위해 기존 전기식 센서들의 부식문제점을 파악하여 해수용 4종 센서 IoT 모듈 패키징을 설계하고 외부 전원공급 방해 영향을 최소화한 태양광 발전을 적용한 항만 구조물 거동 계측 시스템을 제안하였다.
Even if the exploitation of copper slag produced during the smelting process of copper as aggregate for construction purpose has been permitted since 2004 in Korea, the lack of sufficient data enabling to evaluate its long-term stability that is its durability has to date impeded its application. This study intends to investigate experimentally the durability characteristics of 18 and 27 MPa-class commercial concretes in which natural sand (fine aggregates) has been partially replaced by copper slag through accelerated and exposure tests so as to provide bases promoting the application of copper slag concrete. The experimental results revealed insignificant difference of the durability characteristics in most of the mix proportions in which 30% of natural sand was replaced by copper slag. In the case where crushed sand was adopted, tests verified similar characteristics for replacement ratio of 50%. Particularly, the results of the exposure test conducted during 8 years demonstrated that equivalent level of durability was secured compared to the case using natural sand. In the case of 18MPa-class lower grade concrete, exposure test verified also that the physical lifetime similar to 50 years could be secured until carbonation reaches cover depth of 20 mm.
For water barrier and reinforcing grout in soft ground, the verification of durability was conducted over the initial and long-term ages under various curing conditions. The grout was made of water glass system, fast-hardening mineral (FHM) system, and acrylic polymer system. There were three types of curing conditions that were tab water curing, artificial seawater curing, and atmospheric curing. And the various tests were performed for each sample by age, uniaxial compressive strength, length change, and weight change. As artificial seawater, MgCl2 and MgSO4 aqueous solutions were prepared and used, respectively. As the test results, the fast-hardening mineral system and acrylic polymer system were cured stably without significant change in durability in tap water and artificial sea water, whereas water glass system showed a very rapid drop in durability under artificial sea water conditions compared to tap water. In atmospheric curing conditions, durability is lowered compared to water curing in all cases, and in particular, the weight loss in the FHM system and water glass system is about 62% and 60%, respectively, resulting in a significant decrease in durability.
Ryu Keunchang;Lee Seong-Min;Kho Youngtai;Argent Colin
한국가스학회:학술대회논문집
/
2002.05a
/
pp.111-121
/
2002
천연가스 수송배관은 매설환경시의 방식 및 외부충격 등에 대비하여 배관을 보호할 목적으로 폴리에틸렌(polyethylene)으로 피복(coating)되어 있다. 가스배관이 전국으로 확장됨과 더불어 배관피복 기술도 초기 사용하던 1층(one-layer), 2층피복으로 발전되어 현재는 3층피복시스템을 적용한 배관들이 전국에 매설되고 없다. 그러나 강관에 적용된 폴리에틸렌 피복이 경우에 따라 장기간 사용에 따른 자연균열등이 발생하여 피복의 안정성에 문제를 일으키기도 하므로, 그동안 전국에 매설되어있는 배관 피복재들의 물성변화 여부를 확인하여 천연가스수송용 배관의 내성 데이터베이스를 구축, 향후 배간운영의 신뢰성 평가에 참고하고자 하였다. 이를 위하여 선진외국에서 폴리에틸렌 배관의 내구성과 장기사용 안정성 평가를 위해 오래전부터 활용되고 있는 저속균열저항성(slow crack growth resistance : SCGR) 측정과 배관 피복층의 산화유도시간(OIT : oxidation induction time)을 측정하여 국내 배관 피복재들의 내구성을 평가하고 이를 근거로 하여 국내사용판정에 적합하고 수출도 고려한 폴리에틸렌 물성치의 목표값을 제안하였다.
Kim, Jee-Sang;Jung, Sang-Hwa;Kim, Joo-Hyung;Lee, Kwang-Myong;Bae, Su-Ho
Journal of the Korea Concrete Institute
/
v.18
no.2
s.92
/
pp.239-248
/
2006
Recently, a variety of researches has been carried out to obtain a more controlled durability and long-term performance of concrete structures under chloride attack environments. In particular, new procedures for probability-based durability analysis/design have been noticed to be very valuable for the enhancement of service life of concrete structures. Although there is still a lack of relevant data, this approach has been successfully applied to some new concrete structures. In this paper, the diffusion equation based on Fick's second law has been solved with a time dependent diffusion coefficient and the probabilistic analysis of the durability performance has been carried out by using a Monte Carlo Simulation. From the results, the influence of each parameter on the durability of concrete structures was investigated and the new procedure for durability analysis was demonstrated in terms of chloride penetration data from various concrete structures. The new procedure might be very useful in designing important concrete structures and help to predict the remaining service life of existing concrete structures under chloride attack environments.
Proceedings of the Korean Society of Propulsion Engineers Conference
/
2009.05a
/
pp.335-337
/
2009
Internal Pressure Maintenance Equipment absorbs internal pressure variation for it's storage has developed. The bladder ; main item of Internal Pressure Maintenance Equipment, has developed with multi-layer to prevent a penetration and to improve durability. And durability test and environment test was carried out to verify the performance in the condition that could be happened in storage or operation.
Journal of the Korean Society of Hazard Mitigation
/
v.10
no.5
/
pp.17-25
/
2010
We studied on the watertightness improvement of cementitious material for durability enhancement of concrete. For improvement of watertightness of OPC and OPC with fly ash, we used various materials with watertightness properties to OPC and OPC with fly ash. The performance of watertightness improvement of cementitious materials closely related to formation of CSH by pozzolanic reaction and to reducing of size of contact angle in cement pore by using organic fatty acid. And volume of CSH formation at early hydration have an influence of watertightness improvement and reduction of long-term water absorption rate. In using of fly ash, improvement of workability by using the spherical fly ash caused to densify on the structures of cement material and CSH formation by pozzolanic reaction and cement using fly ash also caused watertightness improvement of cementitious materials. For improvement of concrete durability by watertightness, cementitious materials need using watertightness materials and at using fly ash, also it have to the effect of improvement of watertightness of cementitious materials by pozzolanic reaction.
KSCE Journal of Civil and Environmental Engineering Research
/
v.34
no.4
/
pp.1095-1104
/
2014
This paper presents the results of experimental work on both strength characteristics and durability of concrete or mortar having 50% ground granulate blastfurnace slag(GBS) with different fineness levels (4,450, 6,000 and $8,000cm^2/g$). Compressive and split tensile strength test results indicated that the concrete with a higher fineness level of GBS exhibited a better strength development due to the acceleration of latent hydraulic property at the later curing stage compared with ordinary portland cement concrete. Meanwhile, it was found that a higher fineness level of GBS showed some negative effects on the resistance against freezing-thawing action. However, incorporation of GBS to concrete, irrespective of fineness levels, significantly enhanced the chloride ions penetration resistance. The resistance against sulfate attack of mortar with GBS was greatly dependent on the attacking sources from sulfate environments.
Seo, Eun-A;Lee, Jang-Hwa;Lee, Ho-Jea;Kim, Do-Gyeum
Journal of the Korean Recycled Construction Resources Institute
/
v.5
no.1
/
pp.45-52
/
2017
This study evaluated the durability of nuclear power plant concrete. The main parameters were the water-to-binder ratio and admixture type. The results revealed that high-volume ground granulated blast-furnace slag(GGBS) concrete had lower initial strength, while the strength reached higher after 28 days. On the other hand, the initial strength of fly ash blended concrete was high, but the long-term strength of the robbery was low. The measured durability of GGBS blended concrete was found to be better than that of the existing concrete mix for use in the construction of nuclear power plants. Especially, the GGBS blended concrete was more durable than the fly ash blended concrete in terms of chloride attack, carbonation resistivity and freezing-thawing durability in low compressive strength. The effects of concrete compressive strength according to gamma rays were minor.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.