• 제목/요약/키워드: 용접 열영향부

Search Result 350, Processing Time 0.025 seconds

Evaluation of Fracture Toughness in Steel Weldment for Inner Wall of LNG Storage Tank (LNG 저장탱크 내조용 강 용접부의 파괴인성 평가)

  • Jang J.-i.;Ju J.-B.;Yang Y.-c.;Kim W.-s.;Hong S. H.;Kwon D.
    • Journal of the Korean Institute of Gas
    • /
    • v.2 no.1
    • /
    • pp.7-13
    • /
    • 1998
  • In this study, for the safety performance of LNG storage tank, the fracture toughness in X-grooved weld HAZ(heat-affected zone) of $9\%$ Ni steel was evaluated qualitatively and quantitatively, and the relation with the change in microstructure was analyzed. The toughness assessment was peformed through the modified CTOD test proposed for thick weldment with X-groove. Additionally, microstructures of HAZ were evaluated by OM, SEM and XRD. From the results, HAZ toughness of SMA(shielded metal arc)-welded $9\%$ Ni steel decreased as the evaluated region approached the fusion line. The decrease in toughness was apparently caused by the increase in the fraction of coarse-grained zone within HAZ. On the other hand, toughness drop with decreasing test temperature in F.L.(fusion line) ${\~}$F.L.+3mm was larger than that in F.L.+5mm${\~}$F.L.+7mm region due to the fact that in the former regions, retained austenite had poor stability.

  • PDF

A study on the microstructure change during the welding of a cast iron with a Fe-Mn-Al steel powder (주철과 Fe-Mn-Al강 이종금속 용접부의 조직변화에 관한 연구)

  • 김경중;서정현
    • Journal of Welding and Joining
    • /
    • v.8 no.4
    • /
    • pp.35-45
    • /
    • 1990
  • Casting are widely used nodays as complicated and diversified forming materials due to its superior castability. However the welding of cast iron has not been accompaniced satisfactory resulting in an microstructure change happened in the heat affected zone (HAZ), especially the graphite are formed and shaped consecutively in the area and it has great impact on the crack occuring and growth together with martensite forming in this area. It case of gray cast iron welding, it is required for pre-heat treatment or specific welding consumables to restrain forming the martensite in the HAZ. In this study, by applying the plasma surface overlaid welding. Fe-Mn-Al steel powder has been used for improvement of anti-crackability in the HAZ and much attention has been paid to establish the overlaid welding method for gray cast iron so that optimum welding conditions may prevent the cracking. With our experiments, we have found that to prevent defects which may occur in the HAZ, the overlaid welding technique for gray cast iron has been developed.

  • PDF

Mechanism of Stress Corrosion Cracking of Hot Stove Shells and Preventive Measures (고로 열풍로에서의 응력부식발생 및 방지대책)

  • An, Gang-Hun;Park, Tae-Jo
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2002.05a
    • /
    • pp.279-284
    • /
    • 2002
  • The expected life of the hot stove equipments for #2 blast furnaces in Gwangyang Steel Works is about 40 years. However, the stress corrosion cracking(SCC) are founded in heat affected zone only 10 years operation. In this paper, the mechanism of SCC are investigated and the preventive measures are recommended.

  • PDF

AE Characteristics for Weld HAZ in SM 490A Steel (SM 490A 강의 용접 열영향부 음향방출 특성)

  • 이장규;우창기;박성완;김봉각;윤종희;인승현
    • Proceedings of the Korean Institute of Industrial Safety Conference
    • /
    • 2002.11a
    • /
    • pp.257-262
    • /
    • 2002
  • The object of this study is to investigate the effect of compounded welding through the AE (Acoustic Emission) characteristics for weld HAZ (Heat Affected Zone) on static tensile test. This study was carried out a SM 490A, high tension steel using the low hydrogen type E4316 of electronic shield metal arc welding, compound wire of $CO_2$ gas arc welding and tungsten electrode of TIG welding.

  • PDF

Effects of PWHT on the toughness of weld HAZ in Cu-bearing HSLA-100 steel (Cu를 함유한 HSLA-100강 용접 열 영향부의 인성에 미치는 PWHT의 영향)

  • 박태원;심인옥;김영우;강정윤
    • Proceedings of the KWS Conference
    • /
    • 1995.04a
    • /
    • pp.91-93
    • /
    • 1995
  • A study was made to examine the effects of post-weld heat treatment (PWHT) on the toughness and microstructures in the weld heat-affacted zone(HAZ) of Cu-bearing HSLA-100 steel. The Gleeble thermal/mechanical simulator was used to simulate the weld HAZ. The behavior of Cu-precipitates in HAZ is similar to that in base plate. PWHT at 55$0^{\circ}C$ shows highest hardness and lowest toughness, whereas PWHT at $650^{\circ}C$ shows reasonable toughness. Cu precipitated during agcing for increasing the strength of base metal is dissolved during single thermal cycle to 135$0^{\circ}C$ and is precipitated little on cooling and heating during subsequent weld thermal cycle. It precipitates by introducing PWHT.

  • PDF

An Experimental Study on High Temperature Material Properties of Welded Joint (용접부의 고온 재료물성에 대한 실험적 연구)

  • Baek, Un-Bong;Yun, Gi-Bong;Seo, Chang-Min;Lee, Hae-Mu
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.12
    • /
    • pp.3096-3103
    • /
    • 2000
  • High temperature material properties of a welded joint were experimentally studied. Tensile and creep properties were measured for each part of weld metal. HAZ(heat affected zone) and parent metal at 538$^{\circ}C$. HAZ metal was obtained by a simulated heat treatment. Results showed that the order of tensile strength is weld>HAZ> parent both at 24$^{\circ}C$ and at 538$^{\circ}C$. Creep resistance was also the highest for weld metal and lowest for parent metal. Creep rupture life curves were obtained and converted to Monkman-Grant relation which is useful for life assessment. Use of the data obtained in this study is discussed.

Crush Strength Analysis of a Spacer Grid for PWR Nuclear Fuel Considering Mechanical Properties in Weld Zone (용접부 기계적 물성치를 고려한 경수로 핵연료 지지격자의 충격해석)

  • Song, Kee-Nam;Lee, Sang-Hoon
    • Transactions of the Korean Society of Pressure Vessels and Piping
    • /
    • v.8 no.2
    • /
    • pp.7-13
    • /
    • 2012
  • A spacer grid which is one of the most important structural components in a pressurized water reactor fuel is an interconnected array of slotted grid straps, welded at the intersections to form an egg-crate structure. The spacer grid is required to not only protect fuel rods stably but also have sufficient lateral crush strength for the sake of enabling shut-down of the nuclear reactor during abnormal operating environments. Then, the lateral crush strength of the spacer grid is closely related with welding quality of the spacer grid. Previous research on the crush strength analysis of the spacer grid had been performed using only parent material properties. In this study, to investigate the effect on the crush strength of the spacer grid when used mechanical properties in weld zone instead of parent material properties, crush strength analysis considering mechanical properties in weld zone obtained from the instrumented indentation technique was performed and compared the results with the previous research.

Effect of weld thermal cycle on the HAZ toughness and microstructure of a Ti-oxide bearing steel (Ti산화물강의 HAZ인성 및 미세조직에 미치는 용접열 cycle의 영향)

  • 정홍철;한재광;방국수
    • Journal of Welding and Joining
    • /
    • v.14 no.2
    • /
    • pp.46-56
    • /
    • 1996
  • HAZ impact toughness of Ti-oxide steel was investigated and compared to that of a conventional Ti-nitride steel. Toughness variations of each steel with weld peak temperatures and cooling rates were interpreted with microstructural transformation characteristics. In contrast to Ti-nitride steel showing continuous decrease in HAZ toughness with peak temperature, Ti-oxide steel showed increase in HAZ toughness above $1400^{\circ}C$ peak temperature. The HAZ microstructure of the Ti-oxide steel is characterized by the formation of intragranular ferrite plate, which was found to start from Ti-oxide particles dispersed in the matrix of the steel. Large austenite grain size above $1400^{\circ}C$ promoted intragranular ferrite plate formation in Ti-oxide steel while little intragranular ferrite plate was formed in Ti-nitride steel because of dissolution of Ti-nitrides. Ti-oxides in the Ti-oxide steel usually contain MnS and have crystal structures of TiO and/or $Ti_2O_3$.

  • PDF

Stress Distributions at the Dissimilar Metal Weld of Safety Injection Nozzles According to Safe-end Length and SMW Thickness (안전단 길이 및 동종금속용접부 두께 변화에 따른 안전주입노즐 이종금속용접부의 응력분포)

  • Kim, Tae-Jin;Jeong, Woo-Chul;Huh, Nam-Su
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.39 no.10
    • /
    • pp.979-984
    • /
    • 2015
  • In the present paper, we evaluate the effects of the safe-end length and thickness of the similar metal weld (SMW) of safety injection nozzles on stress distributions at the dissimilar metal weld (DMW). For this evaluation, we carry out detailed 2-D axisymmetric finite element analyses by considering four different values of the safe-end length and four different values of the thickness of SMW. Based on the results obtained, we found that the SMW thickness affects the axial stresses at the center of the DMW for the shorter safe-end length; on the other hand, it does not affect the hoop stresses. In terms of the safe-end length, the values of the axial and hoop stresses at the inner surface of the DMW center increase as the safe-end length increases. In particular, for the cases considered in the present study, the stress distributions at the DMW center can be categorized according to certain values of safe-end length.