Journal of the Microelectronics and Packaging Society
/
v.6
no.3
/
pp.45-50
/
1999
Copper has been widely used for the electronic parts, and especially spot welded one for the leads of condenser or resistor. However, copper is generally hard to be spot welded because of its low electrical resistivity. For this experiment, Sn-37%Pb solder which has relatively higher resistivity was coated on the Cu-sheet to improve the spot weldability of copper. As the experimental variables welding pressure was varied from 100 to 200kgf, welding time from 20 to 50ms, and welding current from 100 to 2500A. Experimental results showed that the solder coated Cu-sheet can be spot welded under the conditions of 400~2200A welding current, 100~200kgf pressure and 20-50ms welding time. The tensile shear strength of the spot welded joint increased with welding current up to the critical current, and after the critical value decreased with current.
Recently, more researches have been actively performed for the assessment of material degradation and residual-life of elevated temperature plant components, as some of domestic fossil power plants become older than 30 years. In this paper, results of on_site residual life assessment are reported for main steam pipes of Youngwol power station #2 which have operated since 1965. For critical weld locations such as butt welds branch welds, Y_sections and a T-section, replication technique and hardness measurement technique were employed for life_assessment. When cracks were detected by conventional NDT tests, crack growth life was calculated using a computer code. On the other hand, for matrix of pipes, residual life was quantitatively estimated by an analytic method and material degradation was estimated qualitatively using diameter measurement data and grain-boundary etching method. Also, direction in further improvement of on-site life assessment techniques are proposed.
Although Gas Tungsten Arc Welding (GTAW or TIG welding) is considered as high quality and precision welding process, it also has demerit of low melting rate. Narrow-gap TIG welding which has narrow joint width reduces the groove volume remarkably, so it could be shorten the welding time and decrease the overall shrinkage in heavy wall pipe welding. Generally Narrow-gap TIG welding is used as orbital welding process, it is important to select the optimum conditions for the automatic control welding This paper looks at the application and metallurgical properties on Narrow-gap TIG welding joint of heavy wall large austenitic stainless steel pipe to determine the deposition efficiency, the resultant shrinkage and fracture toughness. The fracture toughness depends slightly on the welding heat input.
Orthotropic steel decks are manufactured by welding thin plates therefore it is inevitable that there are abundant works of welding process. On connection of transverse rib web, crossing point of longitudinal rib, transverse rib and deck plate and cut-out parts of transverse rib are the significant position of stress concentration phenomenon because of out of plane and oil-caning deformation caused by longitudinal rib distortion with shear force and distortion. In order to reduce the stress concentration phenomenon and improving fatigue performance at the crosing point and cut-out, structural analysis was performed considering the existence of scalop at conection and diaphragm which have same plane with transverse rib placed inside of longitudinal rib. Result o f the analysis show that there are the largest efect of stres concentration reduction when diaphragms are installed without scallop at connection, therefore these detail can improve the fatigue performance of orthotropic steel decks.
Kim, Seung-Woo;Lee, Kang-Ho;Chin, Hui-cheol;Choi, Jae-In
Journal of the Korea Academia-Industrial cooperation Society
/
v.18
no.5
/
pp.151-159
/
2017
The aspect of modern warfare is gradually changing to a network of warfare, and its central information electronic warfare is evolving every day. Recently, domestic equipment of electronic warfare, which have succeeded in domestic localization, are strongly influenced by the nature of the environment. Therefore, the structural reliability of the antenna switching module that connects the mast and antenna of the ES equipment is the most important. This study proposed a structure that has an improved structure of antenna switching module by currently analyzing the structure of the antenna switching module and the environmental influence. By modifying the structure of the antenna switching module welding method and part of the reinforcement block, the structure was improved and the validity of the improved antenna switching module was simulated using a load test. The simulation showed that the safety factors of antenna switching module welding point and reinforced block part was enhanced 5.3 and 1.5 times compared to the existing values. These values were verified by load (181kg) test results, which was each 3.7Mpa and 64.4Mpa. The load test results were similar to the simulation results and load supporting capacity of the proposed antenna switching module was enhanced.
In steel bridges, there are several details that constrain the deformation such as buckling by external forces. Most of these details which are composed of the intersection members have scallops in order to exclude the weld defects inherently and to get the ease of fabrication and also to decrease the stress concentration. In this study, stress relief hole (SRH) near stress concentration zone with detail category D or under is proposed as a method to improve the resistance on the fatigue crack initiation to detail category C. And the effects of the appropriate size and location of SRH were examined and the applicability to improve the fatigue resistance of the floorbeam web and the rib wall at rib/floorbeam intersection in the orthotropic steel deck bridge was evaluated.
Jung, Jong Hyeon;Jung, Yu Jin;Lee, Sang Man;Lee, Jung Hee;Shon, Byung Hyun;Lim, Hyun Sul
Clean Technology
/
v.20
no.2
/
pp.171-178
/
2014
In this study we have examined the health risk factors and analyzing data of laborers working at the welding operation at large-sized casting process. In order to improve the working environment of workplace, an effective ventilation method was proposed after performing CFD (computational fluid dynamics) modeling and measurement of pollutants. As a result of examining the health risk factors of workers, oxidized steel dust is the main pollution source in the company A, welding fume in the companies B and C, and welding fume and oxidized steel dust in the company D. The fume concentration in the workers' breathing zone was $0.05{\sim}4.37mg/m^3$, and the fume concentration in the indoor air at the welding process was $0.13{\sim}7.54mg/m^3$. From a result of CFD, a local exhaust with an exhaust duct adjacent to welding point was found to be most effective in case of the exhaust process. In case of air supply, we found that a desired location of air supply fan would be at the end of the opening. If a standardizing the ventilation system for tunnel-type semi-enclosed space at a large-sized casting process is introduced in welding work places in the future, it would be more effective to protect the health of welding workers working at the casting industry and shipbuilding industry and improve the work environment.
Song, Tae-Kwang;Choi, Young Hwan;Park, Jeong Soon;Chung, Hae-Dong;Oh, Chang-Young
Transactions of the Korean Society of Pressure Vessels and Piping
/
v.7
no.4
/
pp.1-11
/
2011
This paper presents the effects of preventive maintenance schemes on the residual stress distributions in dissimilar metal welds. Dissimilar metal weld is known susceptible to PWSCC and thus, effective maintenance schemes to prevent PWSCC are needed. Three preventive maintenances schemes, i.e. weld overlay, MSIP and inlay weld which are widely used in nuclear power plants, are selected and their effects on welding residual stresses are investigated via finite element analyses. As results, weld overlay and MSIP were proved effective method to mitigate residual stresses and inlay weld, on the other hand, produces strong tensile residual stresses in the inner surface. Although Alloy 690 known to be resistant to PWSCC are used in inlay weld, continuous careful observation are needed since tensile welding residual stresses are key parameter for PWSCC.
Both impact and fracture toughnesses were investigated with root gaps in FCAW weld metals at room temperature and 0.deg.C. The maximum impact value was obtained at the root gap of 16mm for 1G position weld metal, and the impact value of 3G position weld metals also showed the maximum impact value at the root gap of 12mm. However, the fracture toughnes(CTOD)values tend to decrease with increasing root gaps at both temperatures in 1G weld metal. Bending test also showed satisfactory results with all of root gaps investigated. Based on this result, it becomes possible to apply wide root gaps in real projects in both aspects of toughness and bending resistance.
최근 전세계적으로 유가 상승 및 배기가스 배출 저감과 관련된 각종 환경규제에 대응하기 위하여 선진 자동차회사들은 $CO_2$ 배출 저감 기술과 기존 내연기관 차량의 연비향상을 위해 엔진성능 개선, 구동시스템의 최적화, 차량 경량화, 공기저항 감소 등에 초점을 맞춰 차량의 연비향상과 배기가스 규제에 대응하고 있다. 특히, 자동차 중량의 30%를 차지하는 차체의 경량화는 엔진효율을 높여 자동차의 성능향상을 극대화시키고, 그로 인해 연비향상을 도모할 수 있으므로 환경오염 방지와 연료절감에 가장 적합하고 효과적인 방법이다. 이에 기존의 강재에 비해 비중이 낮으면서 유사한 강도와 내식성이 뛰어난 알루미늄 합금의 차체 적용에 대한 연구가 진행되고 있다. 본 연구에서는 자동차 Door에 알루미늄 합금(Al 5052)의 적용 가능성을 판단하기 위해 반응표면분석법(Response surface methodology)을 이용하여 저입열 Pulse MIG 용접 공정변수를 최적화하였다. 첫째, 저입열 Pulse MIG 용접에서 용접 공정 변수(용접전압, 용접속도, Gap)의 변화가 비드 형상에 미치는 영향에 대해 평가하였다. 요인분석법을 이용하여 용접 공정 변수와 비드 형상 변수와의 주효과와 교호작용효과를 분석하였고, 이를 통해 비드 형상 변수에 영향을 크게 미치는 용접 공정변수를 선별하여 다중회귀분석을 통해 용접 공정 변수 변화에 따른 비드형상 예측 회귀모델을 제안하였다. 둘째, 자동차 Door 생산 현장에서 박판 알루미늄 합금 겹치기 용접 이음부의 0~1 mm 갭 발생에 대해 강건한 용접조건을 제시하기 위해 반응표면법(Response surface methodology)을 이용하여 저입열 Pulse MIG 용접 공정 변수를 최적화하였고, 그 적용 가능성을 확인하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.