• Title/Summary/Keyword: 연삭마멸

Search Result 42, Processing Time 0.024 seconds

A Study on the Rolling Bearing Failure Mode of Automotive Transmission(I) (자동차 변속기용 구름베어링의 파손현상 고찰(I))

  • 현준수;문호근;박태조
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2001.06a
    • /
    • pp.406-411
    • /
    • 2001
  • This paper shows the failure(wear) phenomena of automotive transmission bearings and investigate their characteristics. It was found that the wear mechanism was mainly abrasive wear by the presence of particles in the gear box and the balls was weared more severely than the other tribological contacting parts. The wear of balls alter the bearing contact angle and load ratings, and finally it cause the bearing failure. With close examination of the failed bearing, various countermeasures could be suggested.

  • PDF

A scheme on roundness lmprovement in internal grinding of bearing inner race (베어링 내륜의 내면 연삭가공에서 진원도 개선 방안)

  • Kim, Jeong-Suk;Kang, Myeong-Chang;Bae, Jeong-Cheol
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.13 no.5
    • /
    • pp.60-66
    • /
    • 1996
  • Precision of bearing race is very important to maintain the clearance between ball and inner race. In internal grinding of bearing race, its roundness is dependent on shoe wear, accuracy of jig, dressing method and grinding conditions. In this study, the characteristics of shoe wear and eccentricity of workpiece were investigated experimentally. When wear of fornt shoe wear reaches at 100.mu. m and that of rear shoe reaches at 114 .mu. m, eccentricity of inner race is increased to 1.4 .mu. m. Roundness of race is mainly related to wear of rear shoe and ring type shoe is recommended to improve roundness of race.

  • PDF

Prediction of Wheel Wear when Surface Grinding by Dual Detection Methods (평면연삭시 복합검출방법에 의한 숫돌마멸 예측)

  • 왕덕현
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 1998.03a
    • /
    • pp.172-177
    • /
    • 1998
  • An experimental study on the prediction of grinding wheel wear by dual detection methods was conducted by the laser displacement and acoustic emission(AE) system. The laser displacement sensor was located above the head of the grinding wheel and the AE sensor was set under the workpiece, where the wheel were condition can be detected. It was found that the dual detection methods by laser displacement system and AE system made it possible to predict the wheel wear. From the experiments, the root mean square(RMS) values both methods was found to be proportional to the grinding wheel wear.

  • PDF

저순도 알루미나 예비소결체 절삭시의 공구 수명

  • 이재우
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2004.05a
    • /
    • pp.247-247
    • /
    • 2004
  • 세라믹의 완전 소결체는 높은 경도와 취성을 가지기 때문에 연삭과 같은 입자가공이 행해지게 되어, 가공능률이 매우 낮고, 복잡한 형상 창성이 어렵다. 완전소결된 세라믹의 절삭가공에서는, 공구수명이 짧고, 가공속도가 매우 늦어 일반의 부품가공에 적용하기 어렵다. 또한 소결이 전혀 행해지지 않은 성형체의 절삭가공은 공작물의 강도가 약하기 때문에 가공속도, 가공능률, 부품의 척킹 및 치수 정밀도 등에 문제가 있다고 할 수 있다 이러한 문제 때문에 엔지니어링 세라믹의 고능률, 고품위 절삭에 관한 연구가 필요하다.(중략)

  • PDF

Component and Bench Tests of Polyurethane Hydraulic Reciprocating Seal for Accelerated Life Testing (부품 및 벤치 실험을 통한 폴리우레탄 유압 왕복 실의 가속 실험)

  • Je, Youngwan;Kim, Hansol;Kim, Lyu-Woon;Chung, Koo-Hyun;An, Joong-Hyok;Jeon, Hong-Gyu
    • Tribology and Lubricants
    • /
    • v.30 no.5
    • /
    • pp.271-277
    • /
    • 2014
  • Hydraulic reciprocating seals have been widely used to prevent fluid leakage and to provide lubricant film on counter surface in various hydraulic system. The degradation of the seal may cause the catastrophic failure of the hydraulic system. To assess the durability of the seals and the compatibility with counter surface, accelerated life testing (ALT) has been typically employed from industry. However, ALT often takes up to a few months to cause a failure of the seals, and therefore, there is a need to develop more efficient ALT methods. In this work, the degradation characteristics of polyurethane (PU) seals from field test are investigated and they are compared to those from the component and bench tests, with an aim to contribute to the development of ALT method. From the comparison of the cross-sectional profiles of the sealing surface of the PU specimens before and after the tests, both wear and compression set are found to be responsible for degradation of the PU seals. It is also shown that the major wear mechanisms of the PU seals from the field is abrasive wear and formation of pits. The component and bench tests performed in this work are shown to reproduce such wear mechanisms, and therefore, those test methods can be used as an ALT method for PU seals. In particular, the bench test proposed in this work may be effectively utilized to assess the durability and the compatibility of the seals with the counter surface. The results of this work are expected to aid in the design of ALT for PU seal.

Wear Behaviors of ${Si_3}{N_4}$ under Various Sliding Conditions (미끄럼 환경의 변화에 따른 ${Si_3}{N_4}$의 마멸거동)

  • Lee, Yeong-Jae
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.20 no.6
    • /
    • pp.1753-1761
    • /
    • 1996
  • The wear behaviors of ${Si_3}{N_4}$ under the different sliding conditions were investigated. The cylinder-on-disc wear tester was used. Using the servo-metor, the sliding speed did ot alternate due to the frictional forces. Threekinds of loads and speeds were selected to watch the variation of the wear rates and the frictional forces. Also three kinds of sliding condition under a constant speed were used to see the effects of the oxidationand the abrasion. The contact pressure was more effective than the repeated cycle on the wear behavior of ${Si_3}{N_4}$. With the low loads, the effect of the asperity-failure was more dominant than that of oxidation and abrasion. As increasing the load, the effects of oxidation and abrasion were increased, but the asperity-failure effects were decreased. The wear particles destroyed the ozide layers formed on sliding surfaces. The wear rate could be decreased due to delaying the oxidation. The frictional power and the wear weight per time were usefuel to see the transition of wear.

Indentation and Sliding Contact Analysis between a Rigid Ball and DLC-Coated Steel Surface: Influence of Supporting Layer Thickness (강체인 구와 DLC 코팅면 사이의 압입 및 미끄럼 접촉해석: 지지층 두께의 영향)

  • Lee, JunHyuk;Park, TaeJo
    • Tribology and Lubricants
    • /
    • v.30 no.4
    • /
    • pp.199-204
    • /
    • 2014
  • Various heat-treated and surface coating methods are used to mitigate abrasion in sliding machine parts. The most cost effective of these methods involves hard coatings such as diamond-like carbon (DLC). DLC has various advantages, including a high level of hardness, low coefficient of friction, and low wear rate. In practice, a supporting layer is generally inserted between the DLC layer and the steel substrate to improve the load carrying capacity. In this study, an indentation and sliding contact problem involving a small, hard, spherical particle and a DLC-coated steel surface is modeled and analyzed using a nonlinear finite element code, MARC, to investigate the influence of the supporting layer thickness on the coating characteristics and the related coating failure mechanisms. The results show that the amount of plastic deformation and the maximum principal stress decrease with an increase in the supporting layer thickness. However, the probability of the high tensile stress within the coating layer causing a crack is greatly increased. Therefore, in the case of DLC coating with a supporting layer, fatigue wear can be another important cause of coating layer failure, together with the generally well-known abrasive wear.

A Study on the Wear Characteristics and Lifetime Of High Chromium Roll (고크롬 롤의 수명과 마멸특성에 관한 연구)

  • Kim, M.K.;Kim, S.K.;Jeon, E.C.
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.14 no.2
    • /
    • pp.58-65
    • /
    • 1997
  • Work rolls used in cold rolling mills must have outstanding wear resistance and very little plastic defor- mation. Thus, these rolls require a higher surface hardness and harding to a greater depth. To meet these requirements, the rolls, in general, have basic chemical composition of 0.7 to 1.0% carbon and 1.0 to 5.0% Cr(chromium), plus a small amounts of special elements, and are subjected to intensive water quenching and tempering at low temperature to provide a surface hardness of over 90 shore. This test results are as follows. Deflection and fracture load of 5% Cr material are than those of 3% Cr material and show flat curve from surface to subsurface. It will be clear that 5% Cr work roll has a superior resisti- bility against wear and abrasion comparing with 3% Cr work roll. The improvement of wear and abrasion in 5% Cr work roll will be achieved by the large amount of wpheroidal carbide. In grindability and polish, 5% Cr work roll will be a little inferior comparing with 3% Cr work roll.

  • PDF

A Study on the Monitoring Technology for the Continuous Detection of Grinding Process (연삭 공정의 연속 진단을 위한 모니터링에 관한 연구)

  • 강재훈
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.8 no.1
    • /
    • pp.74-80
    • /
    • 1999
  • Recently, manufacturing work has been transformed to small scale production form with various types to act up to user's expectation from mass production with a little items required in the past. Then FMS using NC type machinaries has been applied actively also in domestic manufacturing line to meet thus tendency, but there are many machining troubles occured during work process not be settled yet. Nowdays high efficiently has been required no less than high precision in grinding work for the improvement of productivity. In this study, to represent more advance FMS can be adapted to thus situation In-process type monitoring method using AE and Current sensors is suggested to investigate the machining condition in grinding process. As results form this experimental study, it is recognized well that grinding conditions and dressing point of in time cab be estimated effectively using monitoring method suggested. Furthermore, surface shape of grinding wheel on voluntary point of in time can be predicted indirectly through the observation and comparison of AE signal waveform obtained as performance of continuous dressing work.

  • PDF

Non-lithographic Micro-structure Fabrication Technology and Its Application (Non-lithography 방법에 의한 마이크로 구조물 제작 및 응용)

  • 성인하;김진산;김대은
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2002.05a
    • /
    • pp.956-959
    • /
    • 2002
  • In this work, a new non-lithographic micro-fabrication technique is presented. The motivation of this work is to overcome the demerits of the most commonly used photo-lithographic techniques. The micro-fabrication technique presented in this work is a two-step process which consists of mechanical scribing followed by chemical etching. This method has many advantages over other micro-fabrication techniques since it is simple, cost-effective, rapid, and flexible. Also, the technique can be used to obtain a metal structure which has sub-micrometer width patterns. In this paper, the concept of this method and its application to microsystem technology are described.

  • PDF