• Title/Summary/Keyword: 양극산화 임플란트

Search Result 24, Processing Time 0.016 seconds

Osseointegration of the titanium implant coated with rhTGF-${\beta}2$/PLGA particles by electrospray: a preliminary microCT analyzing rabbit study (rhTGF-${\beta}2$/PLGA 복합체를 electrospray법으로 코팅한 타이타늄 임플란트 골 유착의 microCT 계측: a preliminary rabbit study)

  • Lee, Woo-Sung;Kim, Seong-Kyun;Heo, Seong-Joo;Koak, Jai-Young;Lee, Joo-Hee;Park, Ji-Man;Park, Yoon-Kyung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.52 no.4
    • /
    • pp.298-304
    • /
    • 2014
  • Purpose: This preliminary rabbit study was conducted to evaluate the effect of recombinant human transforming growth factor-${\beta}2$ (rhTGF-${\beta}2$)/poly lactic-co-glycolic acid (PLGA) coating on osseointegration of the titanium (Ti) implant. Materials and methods: Eight Ti implants were anodized with 300 voltages for three minutes. Four of those were coated with rhTGF-${\beta}2$/PLGA by an electrospray method as the experimental group. The implants were placed into tibiae of four New Zealand rabbits, two implants per a tibia, one implant per each group. After 3 and 6 weeks, every two rabbits were sacrificed and micro-computed tomography (microCT) was taken for histomorphometric analysis. Results: In scanning electron microscope (SEM) image, the surface of rhTGF-${\beta}2$/PLGA coated Ti implant showed well distributed particles. Although statistically insignificant, microCT analysis showed that experimental group has higher bone volume / total volume (BV/TV) and trabecular thickness (Tb.Th) values relatively. Cross sectional view also showed more newly formed bone in the experimental group. Conclusion: In the limitation of this study, rhTGF-${\beta}2$/PLGA particles coating on the Ti implant show the possibility of more favorable quantity of newly formed bone after implant installation.

Micromorphometric Influence of Anodic oxidation surface implant conditioned with tetracycline-HCI (양극 산화 임플란트 표면 구조에 대한 염산 테트라싸이클린의 영향)

  • Lim, Jeong-Taek;Chung, Jong-Hyuk;Kwon, Young-Hyuk;Park, Joon-Bong;Herr, Yeek
    • Journal of Periodontal and Implant Science
    • /
    • v.37 no.4
    • /
    • pp.767-777
    • /
    • 2007
  • The present study was performed to evaluate the effect of Tetracycline-HCI on the change of implant surface microstructure according to application time. Anodic oxidation surface were utilized. Implant surface was rubbed with 50mg/ml Tetracycline-HCI solution for ${\frac{1}{2}}min.$, 1min., $1{\frac{1}{2}}min.$, 2min., $2{\frac{1}{2}}min.$, and 3min. respectively in the test group. Then, specimens were processed for Ra Value test and scanning electron microscopic observation. The results of this study were as follows. 1. The anodic oxidation surface roughness tests don't show significant difference on conditioning with saline and Tetracycline-HCI. 2. The anodic oxidized surfaces showed the craterous structures. The surface conditioning with Tetracycline-HCI didn't influence on its micro-morphology. In conclusion, Anodic oxidation implant surface is stable to detoxificate with 50mg/ml Tetracycline-HCI of implant surface.

A Biocompatibility Evaluation of Hydroxyapaite·Titania Surface for Dental Implant (임플란트 적용을 위한 하이드록시아파타이트·이산화티탄 표면의 생체적합성 평가)

  • Kang, Min-Kyung;Bae, Sung-Suk
    • Journal of dental hygiene science
    • /
    • v.16 no.1
    • /
    • pp.70-76
    • /
    • 2016
  • The objective of this study was to fabricate hydroxyapatite (HA) containing titania layer by HA blasting and anodization method to obtain advantages of both methods and evaluated biocompatibility. To fabricate the HA containing titania layer on titanium, HA blasting treatment was performed followed by microarc oxidation (MAO) using the electrolyte solution of 0.04 M ${\beta}$-glycerol phosphate disodium salt n-hydrate and 0.4 M calcium acetate n-hydrate on the condition of various applied voltages (100, 150, 200, 250 V) for 3 minutes. The experimental group was divided according to the surface treatment procedure: SM (simple machined polishing treatment), HA, MAO, HA+MAO 100, HA+MAO 150, HA+MAO 200, HA+MAO 250. The wettability of surface was observed by contact angle measurement. Biocompatibility was evaluated by cell adhesion, and cell differentiation including alkaline phosphatase activity and calcium concentration with MC3T3-E1 cells. The porous titanium oxide containing HA was formed at 150 and 200 V. These surfaces had a more hydrophilic characteristic. Biocompatibility was demonstrated that HA titania composite layer on titanium showed enhanced cell adhesion, and cell differentiation. Therefore, these results suggested that HA containing titania layer on titanium was improved biological properties that could be applied as material for dental implant system.

Bioactivity of precalcified nanotubular $TiO_2$ layer on Ti-6Al-7Nb alloy (나노튜브 $TiO_2$ 층 생성 후 전석회화 처리한 Ti-6Al-7Nb 합금의 생체활성도)

  • Seo, Jae-Min
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.1
    • /
    • pp.16-21
    • /
    • 2011
  • Purpose: The purpose of this study was to investigate the bioactivity of precalcified nanotubular $TiO_2$ layer on Ti-6Al-7Nb alloy. Materials and methods: Anodic oxidation was carried out at a potential of 20 V and current density of 20 mA/$cm^2$ for 1 hour. The glycerol solution containing 1 wt% $NH_4F$ and 20 wt% deionized water was used as an electrolyte. Precalcification treatment was obtained by soaking in $Na_2HPO_4$ solution at $80^{\circ}C$ for 30 minutes followed by soaking in saturated $Ca(OH)_2$ solution at $100^{\circ}C$ for 30 minutes, followed by heat treatment at $500^{\circ}C$ for 2 hours. To evaluate the activity of precalcified nanotubular $TiO_2$ layer, specimens were immersed in a simulated body fluid with pH 7.4 at $36.5^{\circ}C$ for 10 days. Results: 1. Nanotubular $TiO_2$ layer showed the highly ordered dense structure by interposing small diameter nanotubes between large ones, the shape of nanotubes was enlarged as going down. 2. The mean length of nanotubes was $517.0{\pm}23.2\;nm$ innm glycerol solution containing 1 wt% $NH_4F$ and 20 wt% $H_2O$ at 20 V for 1 hour. 3. The bioactivity of Ti-6Al-7Nb alloy was improved with formation of nanotubular $TiO_2$ layer and precalcification treatment in $80^{\circ}C$ 0.5 M $Na_2HPO_4$ and saturated $100^{\circ}C$ $Ca(OH)_2$ solution. Conclusion: Bioactivity of precalcified nanotubular $TiO_2$ layer on Ti-6Al-7Nb alloy was improved.