Most studies on mechanical properties of concrete with recycled aggregate was focused on the concrete with compressive strength of less than 40 MPa. Therefore, this paper concerns the compressive strength and mechanical properties of concrete with compressive strength of greater than 40 MPa containing recycled coarse aggregate (RCA). The experimental parameters were compressive strength level and replacement ratio of RCA. Compressive strength level was 45 and 60 MPa, and replacement ratio of RCA was 30, 50, 70 and 100%. The results of the test were discussed: compressive strength, elastic modulus, split tensile strength and modulus of rupture. Test results of elastic modulus were compared to the design code predictions. The design code predictions for elastic modulus overestimated the experimental results. However, the design code predictions for modulus of rupture were generally in agreement with the measured values.
This paper is to investigate the mechanical characteristics of light-weighted soils (LWS) consisting of expanded polystyrene(EPS), dredged clays and cement by using both uniaxial and triaxial compression tests. The mechanical characteristics of the compressive strength of LWS are analysed with varying initial water contents of dredged clays, EPS ratio, cement ratio, and curing stress. In the triaxial compression state, it is found that the compressive strength of LWS containing EPS is independent on the effective confined stress. As the EPS ratio decreases($A_E$<2%) and cement ratio increases($A_c$>2%), the behavior characteristics of triaxial compressive strength-strain relationship is similar to that of cemented soil which decreases rapidly in compressive strength after ultimate compressive strength. For the applications of LWS to ground improvements which require the compressive strength of up to 200kPa, the optimized EPS ratio and initial water content of dredged clay are estimated to be 3~4% and 165~175%, respectively. Also, the ultimate compressive strength under both triaxial test and uniaxial compression states are almost constant for a cement ratio of up to 2% and then critical cement ratio of this LWS shall be 2%.
Proceedings of the Korea Institute of Fire Science and Engineering Conference
/
2009.04a
/
pp.147-154
/
2009
화재와 같은 고온의 환경에서 콘크리트의 고강도화는 폭렬(Explosive Spalling)이라는 큰 위험성을 가지고 있으며, 이러한 폭렬의 원인으로는 콘크리트 내부의 수증기압이 가장 큰 원인으로 제기되고 있다. 본 논문은 콘크리트의 폭렬발생 있어서 압축강도 및 함수율이 초기 폭렬특성에 미치는 영향을 실험적으로 검토하기위하여 건축구조물의 화재 온도조건인 ISO834 화재온도이력곡선을 15분, 30분 적용하여 콘크리트의 초기 폭렬특성을 검토하였다. 그 결과 압축강도 가열시간 함수율이 증가할수록 폭렬발생 및 폭렬현상이 증대되는 경향이 나타났으며, 15분, 30분 가열시간에 따른 잔존강도율을 나타내었다. 또한, 압축강도 및 함수율에 따른 폭렬발생영역을 분석하였으며, 압축강도 50${\sim}$100 MPa의 경우 함수율 3%이하, 100 MPa이상의 경우는 1%이하로 제어할 경우 폭렬현상이 발생하지 않을 것으로 판단되었다.
철근콘크리트부재의 강도는 여러 가지 요인으로 인하여 변이를 보이고 있다. 주요 요인들은 콘크리트나 철근의 강도 및 역학적 특성의 변이, 시공오차등이다. 이들중 콘크리트의 강도는 상대적으로 높은 불확실성을 가지며, 다양한 요인(배합, 운반, 타설, 양생등)에 의해 변화정도가 영향을 받는다. 본 연구에서는 국내 철근콘크리트 구조물이 가지는 신뢰도의 수준을 분석하기 위한 기초자료 조사로서, 현장에서 타설되는 콘크리트를 설계강도별로 직접채취하여 습윤양생과 현장조건양생을 통하여 콘크리트의 28일 압축강도의 확률적 특성을 분석하였다. 분석된 결과를 이용하여 현장타설 부재내에서의 콘크리트의 압축강도를 추정하였다.
A review is presented of experimental studies on the strength performance of concrete exposed at short-term and rapid heating as in a fire and after cooling. Emphasis is placed on concretes with high original compressive strengths, that is, high-strength concrete(HSC). The compressive strength-temperature relationships from the reviewed test programs are distinguished by the test methods used in obtaining the data(unstressed, unstressed residual strength, and stressed tests) and by the aggregate types(normal or lightweight), The compressive strength properties of HSC vary differently with temperature than those of NSC. HSC have higher rates of strength loss than lower strength concrete in the temperature range of between 20$^{\circ}C$ to about 400$^{\circ}C$. These difference become less significant at temperatures above 400$^{\circ}C$ compressive strengths of HSC at 800$^{\circ}C$ decrease to about 30 % of the original room temperature strength. A comparison of lest results with current code provisions on the effects of elevated temperatures on concrete compressive strength and elastic modulus shows that the CEN Eurocodes and the CEB provisions are unconservative.
Journal of the Earthquake Engineering Society of Korea
/
v.5
no.2
/
pp.73-82
/
2001
본 연구는 실험적 방법과 해석적 방법을 통하여 반복하중을 받는 ├형 철근콘크리트 접합부의 전단특성을 파악함을 목적으로 한다. ├형 접합부는 고강도 재료의 사용으로 인한 체적의 감소 뿐만 아니라, 지진발생 시 반복하중의 작용으로 인한 변동축력 등으로 , 구조적으로 취약한 부분이 될 가능성이 있다. 따라서 본 연구에서는 ├형 접합부의 전단특성을 파악하기 위하여 기동축력, 콘크리트 압축강도, 접합부 전단보강근비를 변수로 한 12개의 실험체를 제작하여 가력실험을 수행하였다. 또한, 유한요소 해석을 수행하여 본 실험결과와의 비교 검토를 통하여 타당성을 검토한 후, 기둥축력과 콘크리트 압축강도의 변화에 대한 변수해석을 통하여 접합부의 전단강도에 미치는 변수는 영향을 파악하였으며, 실험에 의한 실험체의 전단내력을 기존에 제안된 AIJ, ACI 규준 등과 비교 검토하였다. 본 연구의 결로부터 기둥축력과 콘크리트 압축강도가 ├형 철근콘크리트 접합부의 전단강도에 미치는 영향을 확인하였다.
재생콘크리트의 압축강도와 휨강도는 재생골재의 혼입량이 증가할수록 감소하였으며 플라이애쉬를 혼화재로 사용할 때 그 양이 증가할수록 재생콘크리트의 조기 압축강도는 떨어졌다. 골재원에 따른 압축강도는 재생골재의 혼입량이 적을수록, 양생기간이 길어질수록 증가하엿으나, 전반적으로 비슷한 강도변화의 경향을 보여주고 있다. 재생콘크리트의 휨강도 발현은 보통 콘크리트와 비슷하나, 휨강도에 대한 압축강도비는 보통 콘크리트에 비하여 낮았다. 재생콘크리트의 건조수축은 재생골재의 혼입량이 증가할수록 증가하였으며 , 특히 재령2주와3주사이에 건조수축량이 보통 콘크리트에 비해 월등히 높았다.
Journal of the Korea institute for structural maintenance and inspection
/
v.25
no.5
/
pp.135-140
/
2021
In this study, the concrete aggregate shape features were extracted from the cross-section of a normal concrete strength cylinder, and the compressive strength of the cylinder was predicted using artificial neural networks and image processing technology. The distance-angle features of aggregates, along with general aggregate shape features such as area, perimeter, major/minor axis lengths, etc., were numerically expressed and utilized for the compressive strength prediction. The results showed that compressive strength can be predicted using only the aggregate shape features of the cross-section without using major variables. The artificial neural network algorithm was able to predict concrete compressive strength within a range of 4.43% relative error between the predicted strength and test results. This experimental study indicates that various material properties such as rheology, and tensile strength of concrete can be predicted by utilizing aggregate shape features.
프리텐션 방식 원심력 고강도콘크리트 말뚝이 KS F4306 규격에 제정되어 콘크리트의 압축강도가 800kg/$ extrm{cm}^2$ 이상의 제조가 불가한 실정이 것으로 평가 된다. 따라서 본 연구에서는 고강도콘크리트 말뚝 제조에 적용하기 위한 고황산염 시멘트의 실험적 연구로써 석고계 첨가량 및 단위 시멘트량 변화가 증가양생 콘크리트의 제 강도 특성에 미치는 영향을 규명하는데 목적이 있다. 연구결과로부터 석고첨가량이 증대하면 콘크리트강도가 향상되지만, 7.5% 이상 첨가시에는 오히려 강도 저하현상이 나타나는 것으로 분석되었으며, 특히 단위 시멘트량 변화에 따른 압축강도 영향은 그다지 크지 않은 것으로 나타났다. 한편 최고 압축강도 발현은 석고첨가량 5~7.5% 첨가와 단위시멘트량 500~540kg/㎥ 조건에서 800kg/$\textrm{cm}^2$ 이상의 고강도 콘크리트 제조가 가능함을 확인하였다.
Journal of the Korean Recycled Construction Resources Institute
/
v.5
no.3
/
pp.313-319
/
2017
In general, various factors such as grain size, chemical composition, amorphous amount, amorphous Si and Al content of fly ash affect the reaction with cement. In this study, we investigate the effect of fly ash particle characteristics on compressive strength. The standard sand was pulverized to a particle size similar to that of fly ash and the compressive strength was measured by blending with the cement as in fly. Using the measured compressive strength results, strength enhancement by cement hydration reaction and strength enhancement by particle filling effect were confirmed. Strength increment by pozzolanic reaction of fly ash was calculated by using the compressive strength results of mortar substituted with standard powder. As a result of comparison between compressive strengths and the particle characteristics of fly ash, the blaine showed a weak correlation with the compressive strength and the PI(Pozzolanic Index) showed good correlation with the 10% penetration diameter(D10) and the 50% Respectively. Therefore, it is expected that PI will be a good means to evaluate the fly ash characteristics together with the chemical characteristics of fly ash.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.