Park, Gi-Joon;Kim, Won-Woo;Park, Jung-Jun;Moon, Jae-Heum;Kim, Sung-Wook
Journal of the Korea institute for structural maintenance and inspection
/
v.22
no.3
/
pp.31-37
/
2018
This study evaluates the dynamic tensile behavior of HPFRCC according to compressive strength levels of 100, 140 and 180 MPa. Firstly, the compressive stress-strain relationship of 100, 140 and 180 MPa class HPFRCC was analyzed. As a result, the compressive strengths were 112, 150 and 202 MPa, respectively, and the elastic modulus increased with increasing compressive strength. The static tensile strengths of HPFRCC of 100, 140 and 180 MPa were 10.7, 11.5 and 16.5 MPa, and tensile strength also increased with increasing compressive strength. On the other hand, static tensile strength and energy absorption capacity at 100 and 140 MPa class HPFRCC showed no significant difference according to the compressive strength level. It was influenced by the specification of specimen and the arrangement of steel fiber. As a result of evaluating the dynamic impact tensile strength of HPFRCC, tensile strength and dynamic impact factor of all HPFRCCs tended to increase with increasing strain rate from 10-1/s to 150/s. In the same strain rate range, the DIF of the tensile strength was measured higher as the compressive strength of HPFRCC was lower. It is considered that HPFRCC of 100 MPa is the best in terms of efficiency. Therefore, it is advantageous to use HPFRCC with high compressive strength when a high level of tensile performance is required, and it is preferable to use HPFRCC close to the target compressive strength for more efficient approach at a high strain rate such as explosion.
The Journal of the Convergence on Culture Technology
/
v.6
no.4
/
pp.655-661
/
2020
In this study, the correlation between concrete core compressive strength and rebound hardness of urban railway underground structures was analyzed. The equations for the range of rebound hardness were derived and compared with the measured concrete core strengths for each range of rebound hardness to confirm the adequacy of the estimated compressive strength. As the result, the linear regression analysis results of the average compressive strength by the Gaussian probability density function (representative compressive strength estimation formula) and the estimation formula by the rebound hardness range were founded to match well within 3% of the experimental concrete core compressive strength test results. Therefore, the stochastic statistical analysis using the rebound hardness measurement results suggested in this study could be help to secure the confidence level of the correlation between the rebound hardness and the concrete compressive strength which are relatively large deviation according to the estimation equations.
Proceedings of the Korea Concrete Institute Conference
/
2008.04a
/
pp.781-784
/
2008
Recently as application of high-strength concrete on concrete structures has been on the rise, use of non-standard specimen is increasing. Therefore, this study investigated the effect of specimen's size effect, ratio of height/diameter and curing conditions on concrete compressive strength. Results of experiments showed that as size of specimen increased as much as 1 mm, standard design compressive strength of 24MPa fell as much as0.15MPa 40MPa fell as much as 0.1MPa 80MPa fell as much as 0.3MPa, and it indicates that as the level of strength is intensified, the decrement of compressive strength increases. As ratio of height/diameter increased as much as 1.0, compressive strength of 24MPa fell as much as 2.9MPa 40MPa fell as much as 3.7MPa 80MPa fell as much as 9.8MPa, and it means that as strength of concrete is higher, influence of ratio of height/diameter becomes bigger.
철근콘크리트부재의 강도는 여러 가지 요인으로 인하여 변이를 보이고 있다. 주요 요인들은 콘크리트나 철근의 강도 및 역학적 특성의 변이, 시공오차등이다. 이들중 콘크리트의 강도는 상대적으로 높은 불확실성을 가지며, 다양한 요인(배합, 운반, 타설, 양생등)에 의해 변화정도가 영향을 받는다. 본 연구에서는 국내 철근콘크리트 구조물이 가지는 신뢰도의 수준을 분석하기 위한 기초자료 조사로서, 현장에서 타설되는 콘크리트를 설계강도별로 직접채취하여 습윤양생과 현장조건양생을 통하여 콘크리트의 28일 압축강도의 확률적 특성을 분석하였다. 분석된 결과를 이용하여 현장타설 부재내에서의 콘크리트의 압축강도를 추정하였다.
The reduction phenomena of concrete compressive strength with the size of specimens have been extensively investigated, but till now the adequate analysis technique is not fixed. The existing research results show that the bigger the member size, the smaller the strength. This means the nonlinear fracture mechanics theory is needed in order to analyze the fracture behaviors of concrete and the size effect. There is a few model equations that is to predict the size effect of compressive strength of standard and non-standard cylindrical specimen. However, theses equations did not considered the difference of fracturing mechanism which depends on the strength level. In this paper, model equations to predict compressive strength of concrete considering the size effect and strength level are suggested. The size effect model suggested in this paper shows good prediction compared with the existing test data of various concrete size and strength level.
Journal of the Korean Recycled Construction Resources Institute
/
v.8
no.2
/
pp.198-203
/
2020
Cracking due to material behavior like drying shrinkage easily occurs since tensile strength in concrete is very low at initial curing stage. In this paper, workability such as air content and slump was evaluated on CFC(Cellulose Fiber Concrete) with 0.0 ~ 2.0% of fiber addition, and the tests for tensile/compressive strength were performed. With increasing addition ratio of fiber, air content and slump kept similar level to 1.0kg/㎥ of addition ratio, and this trend was effective to 2 hours after mixing. Strength was enhanced with increasing addition ratio, which showed 7.0 ~ 9.0% for compressive strength and 7.0 ~ 22.0% for tensile strength, respectively. The tensile strength increased relatively more, which show the addition of cellulose fiber was very effective to crack resistance. The workability in CFC can be guaranteed for 2 hours in the following conditions like 2 minutes of mixing period and 1.0kg/㎥ of addition ratio of fiber.
Proceedings of the Computational Structural Engineering Institute Conference
/
2009.04a
/
pp.379-382
/
2009
횡방향으로 구속된 콘크리트의 응력-변형률 거동은 구속되지 않은 콘크리트와는 다른 거동을 한다. 보통강도 콘크리트에서 구속효과를 고려한 콘크리트 재료모델로는 Mander 모델이 대표적이며 고강도 콘크리트의 구속효과의 경우 여러 연구자들에 의하여 제안된 모델 중 공시체 수준의 실험결과와 잘 일치하는 Sakino-Sun 모델을 사용하였다. 보통강도에서는 Mander모델을 고강도 콘크리트에서는 Sakino-Sun 모델을 사용하였으나 중간 강도인 30-40MPa의 강도에서 Mander 모델과 Sakino-Sun 모델의 적용시 실험결과와 해석결과가 다소 차이를 보이며 또한 두 모델은 적용할 수 있는 최대 또는 최소 콘크리트 압축강도의 한계범위가 명확하지 않다. 따라서 이 연구에서는 30-40MPa의 강도의 횡방향으로 구속된 콘크리트의 비선형 재료모델을 제안하고 실제 30-40MPa의 압축강도를 갖는 콘크리트 공시체의 일축압축시험 결과와의 비교를 통해 그 적용성을 검토하였다.
Park, Chan-Kyu;Lee, Seung-Hoon;Kim, Han-Jun;Kim, Sang-Jun;Lee, Tae-Wang
Proceedings of the Korea Concrete Institute Conference
/
2008.11a
/
pp.637-640
/
2008
In this study, the characteristics of strength development on high volume fly ash concrete(HVFAC)with Type 4 cement was experimentally investigated. Three levels of W/B were selected. Four levels of fly ash replacement ratios and two levels of silica fume replacement ratios were adopted. In the concrete mix, the water content of 125kg/m$^3$ was used, which is less than that of usual water content. As a result, it appeared that the compressive strength gradually decreased with increasing fly ash replacement ratio until 91days. However, regarding the compressive strength, the proper replacement ratio is about 20%, which is low compared to Type I cement case. It was observed that the tensile strength is proportional to the 0.72 power of the compressive strength. It appears that the prediction equation presented in Concrete Standard Specification overestimate the tensile strength in the low strength range, underestimate the tensile strength in the hi호 strength range.
Kim, Kyung-Hwan;Oh, Sung-Rok;Choi, Wook;Choi, Yun-Wang
Journal of the Korea Concrete Institute
/
v.26
no.5
/
pp.591-598
/
2014
In this study, the relationship between compressive strength and water-cement ratio according to water reducing ratio was evaluated, concrete mix was prepared according to 3 level of water reducing ratio (0%, 8% and 16%) and 3 level of water-cement ratio (40%, 45% and 50%). In addition, concrete mix was carried out repetition test of three times in order to secure the reliability. As a result, compressive strength according to water reducing ratio was shown that difference of strength was about 20% occurred, effect of compressive strength according to water reducing ratio was found more than the water-cement ratio. Therefore, reflected the effect of water reducing ratio, relationship equation between new compressive strength and water-cement ratio was proposed.
Proceedings of the Korea Concrete Institute Conference
/
2009.05a
/
pp.571-572
/
2009
Current design codes regarding compression lap splice dose not utilize merits of the improved strength of ultra-high strength concrete. Especially, a compression lap splice can be calculated longer than a tension lap splice according to the codes because they do not consider effects of strength of concrete and transverse reinforcement. Design equation is proposed for compression lap splice in 40 to 70 MPa of compressive strength of concrete. The proposed equation is based on 51 specimens. Through two-variable non-linear regression analysis of measured splice strengths, a splice strength equation is derived, which is converted into a splice length equation.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.