La 기반의 ABO3 구조를 갖는 첨가물에 따른 Bi0.5(Na0.78K0.22)0.5TiO3의 압전 및 전기적인 특성 향상 연구 (The Study on the Improvement of Piezoelectric and Electrical Characteristics of Bi0.5(Na0.78K0.22)0.5TiO3 Ceramics Modified by the La-based ABO3 Pervskite Structure)

  • 이규탁;박정수;윤지선;조정호;정영훈;백종후
    • 한국전기전자재료학회논문지
    • /
    • 제27권11호
    • /
    • pp.707-711
    • /
    • 2014
  • The $0.99Bi_{0.5}(Na_{0.78}K_{0.22})_{0.5}TiO_3-0.01LaAlO_3$, $0.01LaMnO_3$ or $0.01LaFeO_3$ (0.99BNKT-0.01LA, 0.01LM or 0.01LF) ceramics were prepared by a conventional mixed mothod. The structure and morphology of the lead free ceramics were characterized by XRD (X-ray diffraction) and FE-SEM (field emission scanning electron microscopy). XRD results indicated that the BNKT ceramics modified by LA, LM or LF induced a transition from a ferroelectric tetragonal to a non-polar pseudo-cubic phase, leading to decrease in the remnant polarization ($P_r$) and coercive field ($E_c$) in the P-E hysterisis loops. The effects of the BNKT ceramics modified by La-based $ABO_3$ pervskite structure on the electric-field induced strain were investigated, and the largest normalized unipolar strain ($S_{max}/E_{max}$) was found in BNKT-0.01LF ceramic.

소결첨가제와 분위기가 $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$의 소결 및 압전 특성에 미치는 영향 (Effects of Sintering Additives and Atmospheres on the Piezoelectric and Sintering Properties of $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$)

  • 문종하;박진성;박현수
    • 한국세라믹학회지
    • /
    • 제33권11호
    • /
    • pp.1260-1266
    • /
    • 1996
  • The effects of SiO2 MnO2 and sintering atmospheres (O2, N2) on the piezoelectric properties and densification behaviors of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 were investigated. The addition of SiO2 to the system enhanced the rate of densification but supressed the rate of grain growth. On the other hand the addition of MnO2 to the system did not nearly affect the rate of densification but increased slightly the rate of grain growth The densification of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 was promoted with increasing the partial pressure of O2. The relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 sintered under O2 atmosphere were higher than under N2 atmosphere. Whereas the mechanical quality factor (Qm) of specimens sintered under O2 atmosphere were lower than under N2 atmosphere. Thus the sintering atmosphere of O2 and N2 in Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 acted as donor and acceptor respectively. As the amount of SiO2 increased the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 but the mechanical quality factor (Qm) did not nearly change, In the case of the addition of MnO2 to the system the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 sintered under O2 atmosphere decreased rapidly with increasing the amount of MnO2 but they were unchanged with increasing the amount of MnO2 under N2 sintering atmosphere. Therefore the differences of the relative dielect-ric constant ($\varepsilon$r) and piezoelectric constant (d33) due to sintering atmosphere were diminished as the amount of MnO2 increased.

  • PDF

CuO 첨가에 따른 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ 세라믹스의 압전특성과 미세조직의 변화 (Effect of CuO Additions on Microstructures and Piezoelectric Properties of the 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ Ceramics)

  • 전소현;김민수;정순종;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.194-194
    • /
    • 2008
  • Lead oxide based ceramics, represented by PZT, are the most widely used materials for piezoelectric actuators, sensors, and transducers due to their excellent piezoelectric properties. In particular, high-performance multilayered piezoelectric ceramics for advanced electronic components have drawn great attention. In order to develop piezoelectric ceramics capable of being sintered at low temperature for multilayer piezoelectric device applications, the effect of CuO additions on the microstructures and electromechanical properties of the 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ ceramics was investigated. The samples with CuO addition were synthesized by ordinary sintering technique. X-ray diffractions indicated that all samples formed a single phase perovskite structure. The addition of CuO improved the sinterability of the samples and caused an increase in the density and grain size at low temperature. The optimum sintering temperature was lowered by CuO additions. Excellent piezoelectric and electromechanical responses, $d_{33}$ ~ 663 pC/N, $k_p$ ~ 0.72, were obtained for the samples of high density with 0.1 wt% CuO addition sintered at $1050^{\circ}C$ for 4 h in air. These results show that the piezoelectric properties of PMNZT ceramics can be improved by controlling the microstructure and this system is potentially a good candidate as multilayer piezoelectric device for a wide range of electro-mechanical transducer applications.

  • PDF

소결 온도에 따른 0.94(Na0.5K0.5)NbO3-0.06(Sr0.5Ca0.5)TiO3-0.1 MnO2의 압전 특성 (Piezoelectric Properties of 0.94(Na0.5K0.5)NbO3-0.06(Sr0.5Ca0.5)TiO3 with 0.1 MnO2 Addition at Varying Sintering Temperatures)

  • 정혜린;이성갑;이태호;김민호;조예원
    • 한국전기전자재료학회논문지
    • /
    • 제27권1호
    • /
    • pp.14-17
    • /
    • 2014
  • In this study, lead-free Piezoelectric $(Na_{0.47}K_{0.47}Sr_{0.03}Ca_{0.03})(Nb_{0.94}Ti_{0.06})O_3$-0.1 $MnO_2$ ceramics were fabricated using mixed oxide method and the effects of various sintering temperature on the structural and electrical properties were investigated. For the $(Na_{0.47}K_{0.47}Sr_{0.03}Ca_{0.03})(Nb_{0.94}Ti_{0.06})O_3$-0.1 $MnO_2$ (NKN-SCT-$MnO_2$) ceramics sintered at temperatures of $1,025{\sim}1,100^{\circ}C$. The results indicated that all specimens were perovskite single phase formation without any second phase. It has been shown that relative density is increased to increasing sintering temperature. When the sintered temperature at $1,075^{\circ}C$, highest sintered density and maximum value of $4.45g/cm^3$. Average grain size is increased to increasing sintering temperature. The electromechanical coupling factor, dielectric constant, dielectric loss, d33 and curie temperature at the sintering temperature $1,075^{\circ}C$ of NKN-SCT-$MnO_2$ specimens were 0.22, 511, 0.033, 103 and $380^{\circ}C$, respectively.

Pb(Ni1/3Nb2/3)O3-PZT 세라믹스 고용체에서 과잉 NiO첨가에 따른 압전특성 변화 (The Effect of NiO Addition to the PNN-PZT Piezoelectric Ceramics on Piezoelectric Properties)

  • 최용길;손영진;권준철;조경원;윤만순;김일호;김영민;어순철
    • 한국재료학회지
    • /
    • 제15권6호
    • /
    • pp.413-418
    • /
    • 2005
  • Perovskite $Pb(Ni_{1/3}Nb_{2/3})O_3-Pb(Zr,Ti)O_3[PNN-PZT]$ ceramics were synthesized by conventional ceramic processing technique. In order to modify piezoelectric properties for sensor application in this system, NiO addition was considered to provide $Ni^{+2}$ as an acceptor, which was known to occupy with B site in the structure. The effect of NiO addition up to $8\;mol\%$ on the following piezoelectric properties as well as sintering properties was investigated. When NiO added more than $1\;mol\%$, average grain size was decreased and second phase was found to form. Moreover, the second phase caused decrease in relative dielectric constant $(\varepsilon_{33}T/\varepsilon0)$, electro-mechanical coupling factor $(k_p)$, and piezoelectric charge constant $(d_{33})$, while increasing mechanical quality factor $(Q_m)$. When $1\;mol\%$ NiO was added, density, dielectric properties and piezoelectric properties were abruptly increased.

레이저 열-압착 본딩을 위한 압전 액추에이터로 구동되는 용융실리카 헤더의 취성특성에 관한 연구 (A study on the brittle characteristics of fused silica header driven by piezoelectric actuator for laser assisted TC bonding)

  • 이동원;하석재;박정연;윤길상
    • Design & Manufacturing
    • /
    • 제13권4호
    • /
    • pp.10-16
    • /
    • 2019
  • Semiconductor chip is bonded to the substrate by melting solder bumps. In general, the chip bonding is applied by a Reflow process or a Thermo-Compression(TC) bonding process. In this paper, we introduce a Laser Assisted Thermo-Compression bonding (LATCB) process to improve the anxiety of the existing process(Reflow, TC bonding). In the LATCB process, the chip is bonded to the substrate by irradiating a laser with a uniform energy density in the same area as the chip to melt only the solder bumps and press the chip with a Transparent Compression Module (TCM). The TCM consists of a fused silica header for penetrating the laser and pressurizing the chip, and a piezoelectric actuator (P.A.) coupled to both ends of the header for micro displacement control of the header. In addition, TCM is a structure that can pressurize the chip and deliver it to the chip and solder bumps without losing the energy of the laser. Fused silica, which is brittle, is vulnerable to deformation, so the header may be damaged when an external force is applied for pressurization or a displacement differenced is caused by piezoelectric actuators at both ends. On the other hand, in order to avoid interference between the header and the adjacent chip when pressing the chip using the TCM, the header has a notch at the bottom, and breakage due to stress concentration of the notch is expected. In this study, the thickness and notch length that the header does not break when the external force (500 N) is applied to both ends of the header are optimized using structural analysis and Coulomb-Mohr failure theory. In addition, the maximum displacement difference of the P.A.s at both ends where no break occurred in the header was derived. As a result, the thickness of the header is 11 mm, and the maximum displacement difference between both ends is 8 um.

하이드로폰용 결정화 유리의 제조 및 전기적 특성 (Preparation and Electrical Properties of Piezoelectric Glass-Ceramics for Application in Hydrophones)

  • 박성수;이창희;이현;이헌수;손명모;박희찬
    • 한국재료학회지
    • /
    • 제8권12호
    • /
    • pp.1146-1151
    • /
    • 1998
  • 열처리 온도 및 시간의 변화에 따라 $PbO-TiO_2$-$A1_2O_3$-$SiO_2$유리계의 열처리된 시편들에서 perovskite $PbTiO_3$ 결정의 결정화 거동을 X선 회절 (XRD)과 주사 전자 현미경 (SEM)에 의하여 조사하였다 고온에서 장시간 동안 열처리된 시편은 높은 결정화도를 나타내었다. 열처리 시간이 증가할수록 $610^{\circ}C$$650^{\circ}C$ 에서 열처리된 시편들의 유전 상수는 증가했지만, $800^{\circ}C$에서 열처리된 시편의 유전 상수는 감소하였다. 시편들의 손실 정접은 열처리 조건에 거의 영향을 받지 않았다. $800^{\circ}C$에서 1h, 2h 및 8h 동안 열처리된 시편들의 압전 계수는 $1.0\times10^{-12}~8.0$\times$10^{-12}C/N$ 정도 이었다.

  • PDF

AlGaN/GaN HEMT의 채널폭 스케일링에 따른 협폭효과 (Narrow channel effect on the electrical characteristics of AlGaN/GaN HEMT)

  • 임진홍;김정진;심규환;양전욱
    • 전기전자학회논문지
    • /
    • 제17권1호
    • /
    • pp.71-76
    • /
    • 2013
  • 본 연구에서는 AlGaN/GaN HEMT (High electron mobility transistor)를 제작하고 채널폭의 감소에 따른 특성의 변화를 고찰하였다. AlGaN/GaN 이종접합구조 기반의 기판 위에 채널의 길이는 $1{\mu}m$, 채널 폭은 각각 $0.5{\sim}9{\mu}m$가 되도록 전자선 리소그라피 방법으로 트랜지스터를 제작하였다. 게이트를 형성하지 않은 상태에서 채널의 면저항을 측정한 결과 sub-${\mu}m$ 크기로 채널폭이 작아짐에 따라 채널의 면저항이 급격히 증가하였으며, 트랜지스터의 문턱전압은 $1.6{\mu}m$$9{\mu}m$의 채널폭에서 -2.85 V 이었으며 $0.9{\mu}m$의 채널폭에서 50 mV의 변화, $0.5{\mu}m$에서는 350 mV로 더욱 큰 변화를 보였다. 트랜스컨덕턴스는 250 mS/mm 내외의 값으로부터 sub-${\mu}m$ 채널에서 150 mS/mm로 채널폭에 따라 감소하였다. 또한, 게이트의 역방향 누설전류는 채널폭에 따라 감소하였으나 sub-${\mu}m$ 크기에서는 감소가 둔화되었는데 채널폭이 작아짐에 따라 나타는 이와 같은 일련의 현상들은 AlGaN 층의 strain 감소로 인한 압전분극 감소가 원인이 되는 것으로 사료된다.

초음파 진동자용 MnO2가 Doping된 PZT-PSN 세라믹스의 구조 및 압전 특성 (Structural and Piezoelectric Properties of MnO2-Doped PZT-PSN Ceramics for Ultrasonic Vibrator)

  • 차유정;김창일;김경준;정영훈;이영진;이해근;백종후
    • 한국재료학회지
    • /
    • 제19권4호
    • /
    • pp.198-202
    • /
    • 2009
  • For use in ultrasonic actuators, we investigated the structural and piezoelectric properties of $(1\;-\;x)Pb(Zr_{0.515}Ti_{0.485})O_3$ - $xPb(Sb_{1/2}Nb_{1/2})O_3$ + 0.5 wt% $MnO_2$ [(1 - x)PZT - xPSN + $MnO_2$] ceramics with a variation of x (x = 0.02, 0.04, 0.06, 0.08). All the ceramics, which were sintered at $1250^{\circ}C$ for 2 h, showed a typical perovskite structure, implying that they were well synthesized. A homogeneous micro structure was also developed for the specimens, and their average grain size was slightly decreased to $1.3{\mu}m$ by increasing x to 0.8. Moreover, a second phase with a pyrochlore structure appeared when x was above 0.06, which resulted in the deterioration of their piezoelectric properties. However, the 0.96PZT-0.04PSN+$MnO_2$ ceramics, which corresponds with a morphotropic phase boundary (MPB) composition in the (1 - x)PZT - xPSN + $MnO_2$ system, exhibited good piezoelectric properties: a piezoelectric constant ($d_{33}$) of 325 pC/N, an electromechanical coupling factor ($k_p$) of 70.8%, and a mechanical quality factor ($Q_m$) of 1779. The specimens with a relatively high curie temperature ($T_c$) of $305^{\circ}C$ also showed a significantly high dielectric constant (${\varepsilon}_r$) value of 1109. Therefore, the 0.96PZT - 0.04PSN + $MnO_2$ ceramics are suitable for use in ultrasonic vibrators.

IDT 전극 패턴 임베디드 압전 에너지 하베스터의 특성 (Energy Harvesting Characteristics of Interdigitated (IDT) Electrode Pattern Embedded Piezoelectric Energy Harvester)

  • 이민선;김창일;윤지선;박운익;홍연우;백종후;조정호;박용호;장용호;최범진;정영훈
    • 한국전기전자재료학회논문지
    • /
    • 제29권9호
    • /
    • pp.581-588
    • /
    • 2016
  • Piezoelectric thick films of a soft $Pb(Zr,Ti)O_3$ (PZT) based commercial material were produced by a conventional tape casting method. Thereafter, the interdigitated (IDT) Ag-Pd electrode pattern was printed on the $25{\mu}m$ thick piezoelectric film at room temperature. Co-firing of the 10-layer laminated piezoelectric thick films was conducted at $1,100^{\circ}C$ and $1,150^{\circ}C$ for 1 h, respectively. Piezoelectric cantilever energy harvesters were successfully fabricated using the IDT electrode pattern embedded piezoelectric laminates for 3-3 operation mode. Their energy harvesting characteristics were investigated with an excitation of 120 Hz and 1 g under various resistive loads (ranging from $10k{\Omega}$ to $200k{\Omega}$). A parabolic increase of voltage and a linear decrease of current were shown with an increase of resistive load for all the energy harvesters. In particular, a high output power of 3.64 mW at $100k{\Omega}$ was obtained from the energy harvester (sintered at $1,150^{\circ}C$).