• Title/Summary/Keyword: 순환 굵은 골재

Search Result 127, Processing Time 0.024 seconds

Effects of Low-quality Aggregates in the Same Workability Conditions on the Engineering Properties of Concrete (저품질 골재가 동일 작업성 조건에서 콘크리트 공학적 특성에 미치는 영향)

  • Min, Kyeong-Chul;Han, Cheon-Goo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.3
    • /
    • pp.299-306
    • /
    • 2016
  • In this research, influence of low quality aggregate on engineering properties of concrete was evaluated experimentally. From the experiment, the fresh properties of slump and air content were controlled with unit water and AE dosage and all mixture were designed to have similar fresh properties of slump and air content with various quality of aggregate. Under this conditions, comparing with the mixture with high quality aggregate, the mixture with low quality aggregate showed the unit water and AE dosage were increased about 18 and 98%, respectively, because of poor grading and quantity of fines. For compressive strength, the low quality aggregate, specifically, exploded debris, clay sand, and sea sand contributed on decreasing compressive strength about 20~35%. Additionally, the concrete mixture including low quality fine and coarse aggregate showed adverse quality in not only compressive strength but also durability of freeze-thawing resistance, drying shrinkage, carbonation, and chloride ingression. Therefore, it is considered that for low quality aggregate, extra treatment processes such as washing or controlling gradation, and regulation to limit the use of low quality aggregate are needed.

Fundamental Performance Evaluation of Recycled Aggregate Concrete with Varying Amount of Fly Ash and Recycled Fine Aggregate (순환잔골재 및 플라이애쉬 혼입률에 따른 순환골재 콘크리트의 압축강도, 염소이온 투과 및 중성화 저항성 평가)

  • Sim Jongsung;Park Cheolwoo;Moon Il-Whan;Lee Hee-Chul
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.5 s.89
    • /
    • pp.793-801
    • /
    • 2005
  • This study investigates fundamental properties of recycled aggregate concrete which incorporated 100% recycled coarse aggregate and various amount of recycled fine aggregate. In addition, for the purpose of the improvement of long term strength and durability, a part of cement was replaced with fly ash. Compressive strength and resistance to chloride ion penetration and carbonation were investigated. When the coarse aggregate was completely replaced with the recycled the replacement ratio of the fine aggregate with the recycled was recommended to be limited below 60% in the consideration of strength. The strength of the steam-cured specimen was very comparable to the wet-cured at 28 days. As fly ash content increased the resistance to chloride ion penetration was increased. The chloride ion penetrability based on the charge passed was found to be low at 21 days and very low at 56 days, respectively. Carbonation depth and carbonation velocity coefficient increased as the fly ash content increased and the relationship between the carbonation depth and recycled fine aggregate replacement ratio was not clear. Up to 28days, however, the measured carbonation depth was mostly less than 10mm which could be considered as low.

Structural Behaviors of Precast Concrete Box Structures Using Recycled Aggregate (순환골재 콘크리트 박스 구조의 거동)

  • Byun, Keun-Joo;Song, Ha-Won;Kim, Ho-Jin;Nam, Jin-Won;Kim, Ki-Hwan
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.1
    • /
    • pp.93-102
    • /
    • 2006
  • In order to use a recycled aggregate concrete for precast concrete box structures, the structural behaviors should be analytically and experimentally evaluated. In this study, full-scale precast concrete box structures are manufactured using the recycled aggregate (30% replacement) and natural aggregate. Then, the flexural failure test and shear failure test as well as water leakage lest for the structures arc carried out. First of all, test results of compressive strength show that recycled aggregate concrete is only 4% lower than normal concrete. In the flexural and shear failure test, the structural performances of precast box using the recycled aggregate concrete are 95% of the capacities of normal precast concrete box or more. Especially, the water leakage test shows that leakage pressure of recycled concrete box is more than the critical value, 60kPa, as well as 9% higher than normal precast concrete box. These test results are analyzed and compared with results of finite clement analysis. The comparison shows that test results are more excellent than analytical results. Also, the comparison confirms the applicability of recycled aggregate concrete for the use as practical precast concrete box structure.

  • PDF

The Optimal Mixing Design of the PHC Piles Utilizing the Air Cooled Blast Furnace Slag as Coarse Aggregate (서냉 고로슬래그 굵은골재를 활용한 PHC 파일의 최적배합 및 물리적 특성)

  • Park, Yong-Kyu;Kim, Hyun-Woo;Kim, Seung-Il;Hur, Kab-Soo;Yoon, Ki-Won
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.2
    • /
    • pp.137-144
    • /
    • 2014
  • The PHC pile utilizing the air-cooled blast-furnace slag as coarse aggregate was studied. This research was progressed with the range from the indoor mixing design evaluation into the actual goods production. The physical properties of the PHC pile are determined to satisfy through the appropriate mixing design adjustments. However, it should eliminate the aggregates including CaO and MgO in SG when it utilize in an AC (autoclave) type manufacturing process. It satisfied the bending moment, shear strength, and compressive strength of KS F 4306 except the surface states of the pile.

Performance of Recycled Coarse Aggregate Concrete with Nylon Fiber (나일론 섬유를 적용한 순환 굵은골재 콘크리트의 성능 평가)

  • Lee, Seung-Tae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.2
    • /
    • pp.28-36
    • /
    • 2019
  • The adhered mortars in recycled aggregate may lower the performance of the concrete, such as by reducing in strength and durability, and cracking. In the present study, the effects of nylon fiber (NF) on the mechanical and durable properties of 100% ordinary portland cement (OPC) and 50% ground granulated blast furnace slag (GGBFS) concretes incorporating recycled coarse aggregate (RA) were experimentally investigated. Concrete was produced by adding 0 and $0.6kg/m^3$ of NF and then cured in water for the predetermined period. Measurements of compressive and split tensile strength, water permeable pore and total charge passed through concrete were carried out, and the corresponding test results were compared with those of concrete incorporating crushed coarse aggregate (CA). In addition, the microstructures of 28-day concretes were observed by using SEM technique. Test results revealed that the RA concrete showed lower performance than CA concrete because of the adhered mortars in RA. However, it was obvious that the addition of NF in RA concrete was much effective in enhancing the performance of the concretes due to the bridge effect from NF. In particular, the application of NF2 (19 mm) exhibited a somewhat beneficial effect compared with concrete incorporating NF1 with respect to mechanical properties, especially for RA concrete.

Compressive Strength Evaluation of Concrete with Mixed Plastic Waste Aggregates Filled with Blast Furnace Slag Fine Powder (무기충진재를 혼입한 복합 폐플라스틱 골재를 활용한 콘크리트 압축강도 특성)

  • Lee, Jun;Kim, Kyung-Min;Cho, Young-Keun;Kim, Ho-Kyu;Kim, Young-Wook
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.3
    • /
    • pp.253-259
    • /
    • 2021
  • Plastic wastes generated from household waste are separated by mixed discharge with foreign substances, and recycling is relatively low. In this study, the effect of the ratio and content of mixed plastic waste coarse aggregate(MPWCA)s and mixed plastic waste fine aggregate(MPWFA)s filled with blast furnace slag fine powder on the slump and compressive strength of concrete was evaluated experimentally. The MPWCAs were found to have a similar fineness modulus, but have a single particle size distribution with a smaller particle size compared to coarse aggregates. However, the MPWFAs were found to have a single particle size distribution with a larger fineness modulus and particle size compared to fine aggregates. Meanwhile, the effect of improving the density and filling pores by the blast furnace slag fine power was found to be greater in the MPWFA compared to the MPWCA. As the amount of the mixed plastic waste aggregate(MPWA)s increased, the slump and compressive strength of concrete decreased. In particular, the lower the slump and compressive strength of concrete was found to decrease the greater the amount of MPWFA than MPWCA when the amount of MPWA was the same. This is because of the entrapped air and voids formed under the angular- and ROD-shaped aggregates among the MPWFAs. On the other hand, the addition of the admixture and the increase in the unit amount of cement were found to be effective in improving the compressive strength of the concrete with MPWAs.

The Effect of Combinations of Electric Arc Furnace Slag and Lime Stone aggregates on Engineering Properties of Ultra High Strength Concrete with 80MPa (전기로 산화슬래그 잔골재와 석회암 골재의 조합사용이 80MPa급 초고강도 콘크리트의 공학적 특성에 미치는 영향)

  • Han, Min-Cheol;Moon, Byeong-Yong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.3
    • /
    • pp.253-260
    • /
    • 2017
  • The aim of research is to investigate various physical properties of ultra high strength concrete of 80MPa class using a combination of limestone aggregate and electronic arc furnace oxidizing slag aggregate. For aggregate combinations, granite and limestone are used for coarse aggregate, granite and limestone are also used for fine aggregate. And also, limestone fine aggregate is replaced by electronic arc furnace oxidizing slag aggregate of 25% and 50%. Test results indicated that flowability and compressive strength increased when limestone fine aggregate was used compared to that using granite fine aggregate due to higher modulus of elasticity by limestone. Also substitution of electronic arc furnace oxidizing slag aggregate resulted in a decrease of compressive strength slightly. It is found that the use of electronic arc furnace oxidizing slag aggregate and limestone aggregate would be favorable for reducing the autogenous shrinkage by as much as 9~25%.

Monitoring on Compressive Strength and Carbonation of Reinforced Concrete Structure with 100% Recycled Aggregate (순환골재를 100% 사용한 철근콘크리트 구조물의 압축강도 및 탄산화 진행 모니터링)

  • Lee, Sang-Yun;Kim, Gyu-Yong;Yoon, Min-Ho;Na, Chul-Sung;Lee, Sang-Kyu;Shin, Sung-Gyo;Nam, Jeong-Soo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.5
    • /
    • pp.383-389
    • /
    • 2019
  • The supply of natural aggregate for concrete has been difficult, and the amount of construction waste has been continuously increasing. Therefore, the necessity of using recycled aggregate made of construction waste as aggregate is rised. Therefore, many studies on the characteristics of concrete using recycled aggregate have been made and positive studies have been reported mainly in recent studies. A study on the chlorides binding effect of the mortar with recycled coarse aggregate has been reported. However, due to the user's perception of waste, most of the recycled aggregate currently produced is used only for low value-added products. In order to improve the recognition of recycled aggregate and the user's perception of recycled aggregate concrete, long-term monitoring of the structure with 100% recycled aggregate was conducted to confirm the applicability of the recycled aggregate concrete.