• 제목/요약/키워드: 수중불분리

검색결과 91건 처리시간 0.027초

플라이애쉬를 사용한 수중불분리성 콘크리트의 수화열에 관한 연구 (A Study on the Hydration Heat of Antiwashout Underwater Concrete Using Fly Ash)

  • 권중현
    • 한국해양공학회지
    • /
    • 제14권4호
    • /
    • pp.30-34
    • /
    • 2000
  • The concretes cast in the sea water would be likely to be rich mix and mass concrete. Therefore it is important to check out the hydration heat of concrete and to reduce it to prevent the concrete from processing the temperature crack. Recently the antiwashout agent is used on underwater concrete for preventing from the segregation of concrete in the water. The experimental studies were done for the combined cement replaced by fly ash 30%unit weight of binder to study on the characteristics of hydration heat of antiwashout underwater concrete, and its characteristic was discussed by comparing on cast in sea water with anther one in air. The present paper showed that the hydration heat concrete replaced by 30%of fly ash was more significantly reduced than the normal concrete. The hydration heat of antiwashout underwater concrete was highter than that of normal concrete, but it was reduced lower than the normal concrete by adding fly ash.

  • PDF

해사 혼합율 변화에 따른 수중불분리콘크리트의 특성에 관한 실험적 연구 (An Experimental Study on the Characteristics of Antiwashout Underwater Concrete with Variation of Blend Ratio of Sea Sand)

  • 윤재범;이상명;김광민;어영선;김명식
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표논문집(II)
    • /
    • pp.342-349
    • /
    • 1998
  • The objective of this study is to investigate the characteristic change of antiwashout underwater concrete with variation of blend ratio of sea sand and fine aggregate percentage through experimental researches. According to the experiments results, when sea sand are mixed in antiwashout underwater concrete mixture by about 40% per total fine aggregate, in fine aggregate percentage of 40%, it is found that the flowability fit and the compressive strength is higher others.

  • PDF

고로슬래그미분말을 혼입한 수중불분리콘크리트의 특성에 관한 연구 (A Study on the Characteristics of Antiwashout Underwater Concrete Using Finely Ground Granulated Furnace Blast Slag)

  • 이상명;최홍윤;이환우;김명식
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.95-98
    • /
    • 1999
  • Recently, the use of the underwater concrete constructions with the antiwashout underwater concrete is increasing. In this study, we investigate the properties of pH, suspended solids, slump flow, box test, air contents of fresh antiwashout underwater concrete and the Unit weight, compressive strength of hardened antiwashout underwater concrete which Ground Granulated Blast Furnace Slag contents 0%, 10%, 20%, 30%, 50%, 60% at 7days and 28days age which is produced and cured in the water and sea water. As a result, Ground Granulated Blast Furnace Slag contents 30% was excellent.

  • PDF

고로슬래그미분말을 활용한 수중불분리성콘크리트 (Properties of Antiwashout Underwater Concrete Using the GGBF Slag)

  • 문한영;김성수;이병덕;이재준
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표회 논문집(I)
    • /
    • pp.83-86
    • /
    • 1998
  • Recently, underwater concrete constructions are increasing. Therefore it is considered important to control the quality of underwater concrete. In this paper, we have an intention of evaluating fundamental properties of underwater concrete using the Ground Granulated Blast Furnace Slag (GGBF Slag). Thus, it has been investigated that the slump flow of the concrete, pH value and suspended solids in solution, compressive strength on both of specimens made above and below water. Also the percentage of GGBF Slag was found to alter the filling-up in underwater concrete.

  • PDF

수중불분리성 콘크리트의 염화물이온 침투저항성에 대한 고찰 (Diffusion of Chloride Ion in Antiwashout Underwater Concrete)

  • 김성수;김진철;김홍삼;김종필;김동현
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.451-454
    • /
    • 2000
  • Recently, the antiwashout underwater concrete has been increasingly used for underwater structure such as high strength massive concrete structures. However, Concrete has poor quality ad durability due to dilution with separating cementitious material. In this study, specimens were made with antiwashout underwater concrete replaced with mineral admixtures to improve their properties and were placed in air, water, and salt water. To estimation the chloride ion permeation in concrete, ASTM C 1202 Test was performed. The experimental results demonstrate that the increase of the admixtures improved the properties of antiwashout underwater concrete.

  • PDF

플라이애쉬를 혼입한 굳지않은 수중불분리성 콘크리트의 특성에 관한 연구 (The Characteristic of Fresh Properties of Antiwashout Underwater Concrete with Variation of Fly Ash)

  • 정병훈;최병우;장희석;김명식
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.41-46
    • /
    • 2000
  • In recently, though the development of antiwashout admixture, if's possible to construct in underwater with the concrete which is improved segregation resistance of material, filling and self-leveling. It is generally to use this method with Europe and Japan as the central figure, and also the construction case is reported in korea. There's some advantages to add the fly ash in plain concrete. The objective of this study is to find the characteristics of fresh underwater antiwashout concrete which is followed by the blend rate of fly ash.

  • PDF

고로슬래그 미분말 치환율에 따른 수중불분리성 콘크리트의 압축강도 발현에 관한 실험적 연구 (An Experimental Study on the Compressive Strength Development of antiwashout underwater Concrete with Blended Ratio of Finely Ground Granulated Blast Furnace Slag)

  • 김명식;이환우;양영인;정해동
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.57-61
    • /
    • 2000
  • This experimental study was carried out to estmate the effects of mixing dosage rate and blain on the compressive strength properties of antiwashout underwater concrete admixed with finely ground granulated blast furnace slag. The experimental parameters are slag contents(0, 20, 30, 40, 50, 60%). As a result the compressive strength have a high correlation with slag blended ratio. Thus, it is possible to calculate the modulus of modified age using compressive strength of antiwashout underwater concrete blended with slag.

  • PDF

수중불분리성 혼화재의 종류에 따른 콘크리트의 성능 비교연구 (Comparative Study on the Underwater Concrete Properties using various Anti-washout Admixtures)

  • 백승준;박희민;성상래;윤영수;이승훈
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1996년도 가을 학술발표회 논문집
    • /
    • pp.366-372
    • /
    • 1996
  • This paper persents the characteristics and properties of the five domestic and foreign-made anti-washout admixtures commercially available in Korea. These admixtures have been analysed by experiments to compare among others specifically on the following items : air content, slump-flow, hardening time, pH, filling condition, turbidity, content of chloride, compressive strength of underwater concrete and ratio of ambient / underwater concrete compressive strength. The mix design for comparison has been set according to the Japanese practicesince there is still no guideline concerning underwater concrete available domestically.

  • PDF

공기 불요 연료전지 동력 시스템 (Air-independent Fuel Cell Power System)

  • 김태규
    • 한국추진공학회:학술대회논문집
    • /
    • 한국추진공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.331-334
    • /
    • 2009
  • 본 연구에서는 우주 및 수중 동력원을 위한 연료전지 기반 공기 불요 추진 시스템을 개발하였다. 공기 불요 동력 시스템을 위해 과산화수소를 산화제로 선택하였고, 촉매 분해 반응을 통해 산소와 물을 발생하였다. 순수한 산소는 연료전지에 공급되고, 물은 분리한 후 저장된다. 본 연구에서는 고체 상태의 수소화붕소나트륨을 수소원으로 사용하였고, 촉매 가수분해 반응을 통해 순수한 수소를 발생할 수 있었다. 연료전지 기반 공기 불요 동력 시스템을 검증하기 위해 연료전지 시스템을 구축하였고 다양한 조건에서 평가를 수행하였다.

  • PDF

수중온도가 수중불분리성 콘크리트의 초기상도에 미치는 영향에 관한 실험적 연구 (Water temperature effects on the early strength characteristics of antiwashout underwater concrete)

  • 이승훈;정재홍;안태송;원종필
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 가을 학술발표논문집(II)
    • /
    • pp.324-329
    • /
    • 1998
  • Recently the use of the underwater concrete with the antiwashout admixture is increased considerably. When we intend to apply it to the field, we must consider the water temperature effect. In this study, we investigate the properties of setting time, early strength, hydration temperature history and core strength with the antiwashout underwater concrete in the water temperature 8$^{\circ}C$, 14$^{\circ}C$ and 22$^{\circ}C$ respectively. As a result of experiment, as the water temperature is decreasing, setting time is delayed twice of three times and early strength is lower from 10% to 50%. Therefore to compensate the decrease of the early strength, we used the accelerator and investigated the concrete properties.

  • PDF