Failure Behaviors Depending on the Notch Location of the Impact Test Specimens on the HAZ (용접열영향부 충격시험편 노치 위치에 따른 파괴거동)

  • Jang, Yun-Chan;Hong, Jae-Keun;Park, Ji-Hong;Kim, Dong-Wook;Lee, Young-Seog
    • Proceedings of the KSME Conference
    • /
    • 2007.05a
    • /
    • pp.706-711
    • /
    • 2007
  • Numerical studies were performed to examine the effects of notch location of impact specimens on the failure behavior of HAZ (heat affected zone) when Charpy V-notch impact test were made at a low temperature ($1^{\circ}C$). Carbon steel plate (SA-516 Gr. 70) with thickness of 25mm for pressure vessel was welded by SMAW (shielded metal-arc welding) and specimens were fabricated from the welded plate. Charpy tests were then performed with specimens having different notch positions of specimens varying from the fusion line through HAZ to base metal. A series of finite element analysis which simulates the Charpy test and crack propagation initiating at the tip of V-notch was carried out as well. The finite element analysis takes into account the irregular fusion line and non-homogenous material properties due to the notch location of the specimen in HAZ. Results reveals that the energies absorbed during impact test depend significantly on the notch location and direction of specimen. Finite element analysis also demonstrates that the notch location of specimens, to a great extent, influences the reliability and consistency of the test.

  • PDF

Evaluation of Reheat Cracking Susceptibility with Simulated Heat Affected Zones in Cr-Mo-V Turbine Rotor Steel (CrMoV 터빈로터강에서 모의 열영향부 시험편을 이용한 재열균열 민감도평가)

  • 김광수
    • Journal of Welding and Joining
    • /
    • v.13 no.1
    • /
    • pp.89-102
    • /
    • 1995
  • The evaluation of reheat cracking susceptibility in CrMoV turbine rotor steel was performed using thermally simulated heat affected zones. The examinations were carried out in terms of microstructural characterization, microhardness measurement and a Charpy type notch opening three point bend test. It was found that reheat cracking susceptibility increased as the peak temperature increased. This effect was due to the combined effects of the carbide dissolution and unrestricted grain growth at 1350.deg. C peak temperature. Reheat cracking susceptibility was estimated based on microhardness measurement and prior austenite grain size. It was established that for this particular material, reheat cracking in coarse grained heat affected zone can be eliminated if the microhardness is below about 360DPH and the grain size is below about 30.mu.m. It is evident that reheat cracking susceptibility can be eliminated or reduced by carefully controlling the welding parameters such that a refined structure is produced in the coarse grained heat affected zone.

  • PDF

A study on the variation of physical properties of line heated classification DH32 thick plate steel (선상가열한 선급 DH32 후판 강재의 물성 변화에 관한 연구)

  • Kim, Jeong-Tae;Chung, Han-Shik;Jeong, Hyo-Min;Lee, Kwang-Sung
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.40 no.9
    • /
    • pp.774-779
    • /
    • 2016
  • This study was performed to study the possibility of TMCP's application for side shell plating curved structures through mechanical property testing to understand if the rules and regulations of DNV and the quality standard of IACS after line heating for TMCP steel and normalizing DH32 material steel could be satisfied. Experimental results showed that TMCP's strength was measured to YS = 385 MPa, 18% higher than the required 315 MPa and TS = 525 MPa, complying with the required range of between 440 and 570 MPa. The minus 20 degree impact test for the Charpy V-Notch complied with the required standard and in addition the hardness test satisfied the requirement of 'Hv10 = 130 ~ 320' by reaching an average of T : 216 and L : 275 respectively.

A Study on the Safety of Lifting Cable for Construction of Coastal Structures (항만건설을 위한 케이슨 들고리의 안전성에 관한 연구)

  • Kwak, Kae Hwan;Jang, Ki Woong;Kim, Jong Hyo
    • Journal of Korean Society of Steel Construction
    • /
    • v.10 no.1 s.34
    • /
    • pp.85-99
    • /
    • 1998
  • This paper describes an experimental study to examine collapse causes of the lifting cable due to brittle failure of an fitting anchor under the lifting works. Also, in this study an collapse mechanism that was obtained from stress analysis was compared with an actual collapse procedure. Fractographical analysis as well as chemical component test, tension test and Charpy V-Notch impact test for the fractured steel members were carried out. And then, its results were compared with that of normal steel members. Circumferential surface flaws were developed at internal facets of the fitting anchor before tensile stress occurred. Hence, a higher stress than nominal stress was occurred at flaws by stress concentration at the crack tip. Also, stress intensity factor of members increased by crack size of the potential flaws. Because the stress intensity factor at the crack tip was greater than critical values(fracture toughness), brittle fracture occurred under the lifting works. It is judged that the main collapse of the lifting cable is due to brittle fracture of the fitting anchor.