Study on Properties of Natural Adhesives with Lacquer for Ceramic Conservation (옻을 활용한 토기 복원용 천연 접착재료의 특성 연구)

  • Jeong, Se Ri;Kim, Eun Kyung;Yu, Jae Eun
    • Journal of Adhesion and Interface
    • /
    • v.12 no.4
    • /
    • pp.111-116
    • /
    • 2011
  • The characteristics of natural resin, sap of the lacquer tree were examined as an adhesive for the ceramic conservation since it has such outstanding properties like corrosion resistance against acid and alkali, heat-resistance, waterproof, antiseptic and protection against insects. In order to utilize raw lacquer as an adhesive not under the hardening conditions of lacquer like high humidity (RH 75 to 85%) and high temperature (120 to $170^{\circ}C$), but under normal condition, isinglass and animal glue were added to raw lacquer at certain ratio. In addition, the viscosity and the drying time were measured and their possibilities of application were also investigated through measurement of tensile and adhesive strength. As a result of experiment, it was possible to dry at room temperature and RH $50{\pm}5%$ to mix with raw lacquer and glue, and the drying time of sample with animal glue was faster than that of isinglass. Furthermore, the adhesion of sample with glue was increased more than raw lacquer. It seems to be possible to use the environmental friendly traditional adhesive for the ceramic conservation and restoration, if there are studies or examinations of safety of applications on objects and weathering resistance.

Material Scientific Properties and Effects on Atmospheric Environment of Copper Rust Pigments (동록안료의 재료과학적 특성 및 대기환경 영향 평가)

  • Park, Ju Hyun;Kim, Myoung Nam;Park, Se Rin;Yu, Ji A;Kim, Su Kyoung;Lee, Sun Myung
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.33 no.4
    • /
    • pp.361-376
    • /
    • 2020
  • Atacamite and Verdigris were studied material scientific properties and durability that are used for traditional green pigment in traditional art painting work and Dancheong. As a result of ingrediant analysis, K-AA and K-VA identified Atacamite and Hoganite (or Verdigris) respectively. In order to find a factor of depressing the stability of pigment, we examined UV radiant exposure test, CO2/NO2 gas corrosion test and salt spray test. Salt spray test damaged both samples which were formed salt particle on the surface of the samples and it makes color disability. Furthermore, the results of gas corrosion test that both pigments change color enough to be perceived by the naked eyes showed that an air pollutant NO2 gas is also considered to be a major damage factor. In the case of K-VA, Hoganite that is main component of sample changes Tenorite with turn black after accelerated UV radiant exposure test. The consequences of the atmospheric environment effect test of the two pigments, K-VA showed relatetively weaker than K-AA.

Flexural Strength Analysis of RC T-Beams Strengthened Using Fiber Sheets (섬유시트로 보강된 T형 철근콘크리트보의 휨 강도 해석)

  • Park, Tae-Hyo;Lee, Gyu-Chul
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.2
    • /
    • pp.234-245
    • /
    • 2003
  • Most of the concrete bridge structures are exposed to damage due to the excessive traffic loading and the aging of the structure. The damage of concrete causes the further deterioration of the function in the concrete structure due to corrosion of the reinforced bars and decohesion between the concrete and the reinforced bar. The quick rehabilitation of the damaged concrete structures has become of great importance in the concrete structural system in order to avoid the further deterioration of the structures. Recently fiber sheets are used for strengthening the damaged concrete structures due to its many advantages such as its durability, non-corrosive nature, low weight, ease of application, cost saving, control of crack propagation, strength to thickness ratio, high tensile strength, serviceability and aesthetic. However, the lack of analytical procedures for assessing the nominal moment capacity by the fiber sheet reinforcement leads to difficulties in the effective process of decisions of the factors in the strengthening procedure. In this work, flexural strengthening effects by fiber sheets bonded on bottom face of the member are studied for the reinforced concrete T beam. In addition, auxiliary flexural strengthening effects by U-type fiber sheets bonded on bottom and side faces of the member to prevent delamination of the bottom fiber sheet are theoretically investigated. The analytical solutions are compared with experimental results of several references to verify the proposed approach. It is shown that the good agreements between the predicted results and experimental data are obtained.

A Study on Conservation and Material Characteristics of Outdoor Bronze Sculpture : Kim Chan Shik's 'Feeling' (야외 청동 조각작품의 보존과 재질특성 연구 - 김찬식 '정(情)'을 중심으로 -)

  • Kwon, Hee Hong;Kim, Ye Seung;Kim, Beom Jun;Choi, Nam Young;Park, Hye Sun;Kim, Jung Suk
    • Journal of Conservation Science
    • /
    • v.33 no.3
    • /
    • pp.155-165
    • /
    • 2017
  • As interest in the public display of art and outdoor sculptures is increasing, the conservation and treatment of these sculptures is becoming increasingly crucial. Long-term exposure to the natural elements and atmospheric pollution can cause corrosion and deterioration in outdoor sculptures. In the case of Kim Chan Shik's "Feeling", which was exhibited in the outdoor sculpture park at the National Museum of Modern and Contemporary Art (MMCA), the patina of the sculpture was damaged during a long outdoor exhibition. Therefore, the treatment process was as follows: recording of condition, sanding, repatination, and wax coating. Consequently, the sculpture was restored similar to the original. Chemical analysis revealed that the sculpture was crafted from bronze and was cast from a quaternary alloy of Cu-Pb-Sn-Zn. The welding is lower in Zn, Sn, and Pb content than the metal used in the sculpture itself. Bright strains contain about 13.0 wt% Sn and 10.5 wt% Pb. The strains are higher in Sn and Pb content than the rest of the metal in the sculpture (7.0 wt% Sn and 4.4 wt% Pb). As a result of component analysis and microstructure observation, the material is estimated to have been made by casting without artificial treatment.

Three-dimensional digital recording of the conservation treatment and form analysis of an iron ring pommel (철제 환두부 보존처리 과정의 3차원 디지털기록 및 형상변화 분석)

  • Choi, Hyoryeong;Hong, Seonghyuk;Jo, Younghoon;Cho, Namchul
    • Conservation Science in Museum
    • /
    • v.25
    • /
    • pp.85-94
    • /
    • 2021
  • Conservation treatment of metallic artifacts contaminated with corrosion and foreign substances requires changes in the shape, characteristics, weight and thickness of the artifacts. Thus far, recording the changes after conservation treatment has mainly been performed through visual observation and photography, which lacks any quantitative description of the changes. In this study, the processes of removing foreign substances, joining cracks, and restoring an affected area were recorded using 3D scanning and then quantitatively analyzed to identify changes in form due to conservation treatment. The volume change after the conservation process was calculated based on the results of the 3D scanning, and numerical data on the changes to the form was analyzed. It was revealed that the foreign or corroded substances removed after the conservation accounted for 18.1 cm3, which is approximately 52% of the total volume of the ring pommel, and those substances were removed from about 98% of the surface of the ring pommel. This study confirmed that 3D form analysis was useful for recording the processes of conservation treatment and analyzing the results. It is therefore believed that this methodology can be applicable to not only metal artifacts, but to cultural heritage items in a range of materials.

Improved Treatment Technique for the Reuse of Waste Solution Generated from a Electrokinetic Decontamination System (동전기제염장치에서 발생한 폐액의 재사용을 위한 개선된 처리기술)

  • Kim, Wan-Suk;Kim, Seung-Soo;Kim, Gye-Nam;Park, Uk-Ryang;Moon, Jei-Kwon
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.12 no.1
    • /
    • pp.1-6
    • /
    • 2014
  • A large amount of acidic waste solution is generated from the practical electrokinetic decontamination equipments for the remediation of soil contaminated with uranium. After filtration of uranium hydroxides formed by adding CaO into the waste solution, the filtrate was recycled in order to reduce the volume of waste solution. However, when the filtrate was used in an electrokinetic equipment, the low permeability of the filtrate from anode cell to cathode cell due to a high concentration of calcium made several problems such as the weakening of a fabric tamis, the corrosion of electric wire and the adhension of metallic oxides to the surface of cathode electrode. To solve these problems, sulfuric acid was added into the filtrate and calcium in the solution was removed as $CaSO_4$ precipitate. A decontamination test using a small electrokinetic equipment for 20 days indicated that Ca-removed waste solution decreased uranium concentration of the waste soil to 0.35 Bq/g, which is a similar to a decontamination result obtained by distilled water.

The Gilt Bronze Saddle Accessory Excavated from Tomb No. 89 of Kyodong in Changnyong 75 - Reports on Conservation Treatment and Manufacturing Technique - (창녕(昌寧) 교동(校洞) 제 89호분 출토 금동제 안교장식 - 보존처리와 제작기법 조사 -)

  • Kim, Kyung-hee;Han, Man-sung;Ahn, Byong-chan
    • Conservation Science in Museum
    • /
    • v.1
    • /
    • pp.75-86
    • /
    • 1999
  • Conservation treatments were done for the gilt bronze saddle accessory excavated from Tomb No. 89 in Kyo-dong, Changnyong in Japanese rule period. The saddle accessory, broken into numerous pieces, was mixed with other remains. Principal aims of conservation treatments were to recover original shape of object and stabilize its material. In the process of treatments manufacturing technique of the remain was examined minutely. Thick layers of corrosion substances were peeled off and numerous pieces were pasted together to restore the original shape. And then the saddle accessory was mounted on an acrylic board to be handled and exhibited safely. In this process, it was confirmed that various ancient techniques of metalic crafts such as amalgam gilding, riveting, piercing, line engraving, stamping, chasing etc. had been used to make the saddle accessory.

Conservation of a Bronze Incense Burner from Chungung-dong, Hanam (하남시 춘궁동 출토 청동현향로(靑銅懸香爐)의 제작기술과 보존처리)

  • Jeong, Subin;Park, Haksoo
    • Conservation Science in Museum
    • /
    • v.16
    • /
    • pp.32-45
    • /
    • 2015
  • The bronze incense burner, discovered in Chungung-dong, Hanam, Gyeonggi-do in 1971, is a hanging incense burner dating from the Goryeo period. The incense burner was covered with a thick layer of clay. The object was in a severely deteriorated state, affected by bronze disease which resulted in extensive corrosion. Numerous cracks were present across its surface, and some parts had been broken off. To preserve and display the bronze incense burner in a stable condition, deposits of foreign material were removed from the surface, and the weakened metal was strengthened. Cracked and broken areas were reinforced using woven glass fiber, followed by the application of epoxy resin to restore the shape. To investigate the method of production, a chemical analysis was performed, and the microstructure was examined. The chemical analysis revealed that the body of the incense burner as well as the ear, loop, lid and the knob were cast in a ternary alloy of Cu-Sn-Pb. Moreover, copper nails with high copper content were used to securely join the ear to the body of the incense burner. The microstructure was mainly α-phase, and non-intermetallic inclusions composed of Cu and S were detected.

Study of the Production Techniques Used in the Goryeo-period Gilt-Bronze Case for Acupuncture in the Collection of the Royal Museums of Art and History, Belgium (벨기에 왕립예술역사박물관 소장 고려시대 금동침통의 과학적 보존처리를 통한 제작기법 연구)

  • Lee, Jaesung;Park, Younghwan
    • Conservation Science in Museum
    • /
    • v.27
    • /
    • pp.147-164
    • /
    • 2022
  • Over 200,000 Korean cultural heritage items are currently located abroad. They have made their way to 22 countries under different circumstances and with unique backgrounds. While some of them continue to contribute to promoting Korean culture around the world, others cannot be exhibited due to damage or poor condition. In view of these circumstances, the Overseas Korean Cultural Heritage Foundation (OKCHF) has since 2013 provided museums and art galleries abroad with support for the conservation, restoration, and utilization of the Korean cultural heritage items that they house. As a part of these efforts and on the occasion of the 120th anniversary of the diplomatic relationship between the Republic of Korea and the Kingdom of Belgium in 2021, a gilt-bronze case for acupuncture needles dating to the Goryeo period (918-1392) from the collection of the Royal Museums of Art and History (RMAH), Belgium was brought to Korea for conservation treatment. The primary purpose of this conservation treatment was to restore the original form of the relic and slow to the degree possible the progress of corrosion. The conservation treatment of the gilt-bronze case followed the fundamental order of conservation treatment: removal of corrosive substances, stabilization, and reinforcement. Since this was the first case of restoring metallic cultural properties under the abovementioned support program by the OKCHF, special methodologies distinct from those available in overseas institutions were required. Diverse scientific methods (e.g., X-ray inspection, CT scanning, 3D microscopy) were applied to identify the metalcraft techniques used in the Goryeo period. The analysis found that several designs, including lotus and scrollwork, were exquisitely engraved on the surface of the case by making dots using a round-edged chisel. A bronze plate engraved with designs was rolled into a cylindrical form. The ends were overlapped by 2 to 3 centimeters and then attached to each other by silver soldering. The overlapping ends were welded flat with nearly no gaps. As the final process in the production, the case was lavishly gilt with gold powder using amalgam gilding. The conservation treatment of the gilt-bronze case for acupunctural needles in the RMAH collection restored the original form of the relic and arrested further corrosion. Above all, it revived the historic and academic value of the overseas Korean cultural heritage through scientific analysis.

Relationship between the Aboveground Vegetation Structure and Fine Roots of the Topsoil in the Burnt Forest Areas, Korea (산화적지에서 지상부 식생구조와 표토에 분포하는 세근의 관계)

  • Lee, Kyu-Song;Park, Sang-Deog
    • The Korean Journal of Ecology
    • /
    • v.28 no.3
    • /
    • pp.149-156
    • /
    • 2005
  • This study was conducted to elucidate the relationship between the aboveground vegetation structure and fine roots of the topsoil (<15m), and thereafter to obtain the regression models for the estimation of the fine roots of the topsoil using the aboveground vegetation values in the burned forest areas, Korea. The FRT (fine roots of the top soil) as well as the aboveground vegetation structure showed spatial variation in the earlier successional stages after forest fire. The fine roots (<2 mm) of the topsoil in the earlier successional stages than the first 3 year after forest fire showed the range from 3 to 166 g $DM/m^2$. The FRT in the naturally regenerated sites and planted sites after forest fire was closely correlated with the vegetation indices, especially lvc, representing the development status of the aboveground vegetation. The FRT in the terrace seeding work sites after forest fire was closely correlated with year elapsed after terrace seeding work. The FRT in the terrace seeding work sites showed the much higher values because of the vigorous growth of grass species than the other sites. In the naturally regenerated sites, the FRT showed the parabola form according to the increment of aboveground vegetation value (Ivc). Although the aboveground vegetation value (Ivc) showed a tendency to increase logarithmically during the secondary succession after forest fire, the estimated fine roots of the topsoil was depicted the parabola form showing the gradual increment until the first 15 years and slight decrease thereafter. Decrease of FRT in the later successional stage showing the high vegetation value may be caused by increment of the woody species contribution to the vegetation value (Ivc). Our results represented that the aboveground vegetation value (Ivc) can be used to the estimation of the fine roots of the topsoil in burned forest areas.