• Title/Summary/Keyword: 변재

Search Result 87, Processing Time 0.028 seconds

Radial Variation of Sound Absorption Capability in the Cross Sectional Surface of Yellow Poplar Wood (백합나무 횡단면 흡음성능의 방사방향 변이)

  • Kang, Chun-Won;Lee, Youn-Hun;Kang, Ho-Yang;Kang, Wook;Xu, Huiran;Chung, Woo-Yang
    • Journal of the Korean Wood Science and Technology
    • /
    • v.39 no.4
    • /
    • pp.326-332
    • /
    • 2011
  • Radial variation of sound absorption capability and air permeability of yellow poplar (Liriodendron tulipifera) wood in cross sectional surface and effect of steam explosion treatment were estimated by the two microphone transfer function method and the capillary flow porometry, respectively. The sound absorption coefficients of steam explosion treated wood was higher than those of control wood and these values increased with frequency. Abundant and big vessel may behave as sound absorbing pore observed on the cross sectional surface of yellow poplar wood. The sound absorption coefficients and air permeability of sapwood were higher than those of heartwood for Liriodendron tulipifera.

Fixation characteristics of CCA and CCFZ in Japanese Red Pine, Japanese Larch, and Ezo Spruce Sapwood (소나무, 낙엽송, 북양가문비나무 변재부에서 CCA와 CCFZ의 정착특성)

  • Kim, Gyu-Hyeok;Kim, Hyung-Jun;Kim, Jae-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.29 no.1
    • /
    • pp.52-59
    • /
    • 2001
  • The fixation characteristics of CCA and CCFZ in Japanese red pine, Japanese larch, and ezo spruce sapwood were compared at various temperatures and fixation conditions (drying and nondrying fixation). Fixation was monitored by the rates of reduction of hexavalent chromium to trivalent one, and optimal fixation time was estimated based on the results. The rate of fixation was highly temperature dependent, and the fixation rate of treated wood conditioned under nondrying conditions was much more faster than that under drying conditions, especially when the moisture content of treated wood was below fiber saturation point. Preservative types affected fixation; CCA-Type B had the highest fixation rate, followed by CCA-Type C and then CCFZ. The differences in fixation rates of preservative components were also observed among wood species; Japanese red pine fixed the fastest, followed by Japanese larch and then ezo spruce. Time required to complete fixation according to the fixation temperature could be predicted successfully using the regression equations between the temperatures and fixation time, regardless of conditioning methods, preservative types, and wood species.

  • PDF

Physical Characteristics of Korean Red Pines According to Provinces (Goseong, Hongcheon and Bonghwa-gun) (한국산 소나무의 지역(고성, 홍천 및 봉화군)에 따른 물리적 특성)

  • Kim, Min-Ji;Kim, Byung-Ro
    • Journal of the Korean Wood Science and Technology
    • /
    • v.46 no.5
    • /
    • pp.437-448
    • /
    • 2018
  • Physical characteristics of Korean red pine (Pinus densiflora) were investigated with different cultivation locations in Taebaek Mountains as Goseong-gun, Hongcheon-gun and Bonghwa-gun as experimental sites. Moisture content based on air-dried or green (artificial) wood was no significant differences with different cultivation places. Specific gravities of both sapwood and heartwood of red pine from Bonghwa-gun were higher than those from other two sites (Hongcheon-gun or Goseong-gun). Specific gravity of heartwood of red pine from Goseong-gun was higher than it from Hongcheon-gun, but this trend was opposite in case of sapwood. Higher specific gravity of red pine heartwood from Goseong-gun maybe resulted in higher strength than those of other sites. In shrinkage ratio, there was no significant difference among different cultivation places in radial directions, but red pine from Bonghwa-gun was higher than those of other sites in tangential directions. Hygroscopicity was no significant differences with different cultivation places. These results will be helpful information for efficient use of pinewood and good quality of pinewood production for genetical breeding improved.

Anatomical and Physical Characteristics of Pinus densiflora Wood Damaged by Forest Fire - Difference by Damage Level - (산불 피해 소나무 목재의 해부 및 물리적 특성 - 피해 정도에 따른 차이-)

  • Kwon, Sung-Min;Chun, Kun-Woo;Kim, Nam-Hun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.36 no.4
    • /
    • pp.84-92
    • /
    • 2008
  • Anatomical and physical characteristics of Pinus densiflora woods damaged by forest fire at Yangyang-gun, Kangwon-do were investigated in present study. Even though the bark was severly carbonized, no trace of carbonization in the xylem was found. The amount of resin exudation was different by the degree of fire damage. Green moisture content of sapwood in the damaged wood was lower than that in the sound wood, but vice versa in the heartwood. Green density of heartwood in the damaged wood was higher than that in the sound wood, but there was no significant difference in sapwood. Cambial activities were found stopped in the severely damaged wood but were identified in the lightly damaged wood. In safranine staining process, epithelial and ray parenchyma cell walls in the damaged woods showed darker hue than those in the sound wood. Granular substances were observed in the lumina of ray parenchyma and epithelial cells of the severely damaged wood. Relative crystallinity of the outermost growth ring in the severely damaged wood was slightly higher than that in the sound wood.

Mechanical Characteristics of Korean Red Pines according to Provinces (Goseong, Hongcheon and Bonghwa-gun) (한국산 소나무의 지역(고성, 홍천 및 봉화군)에 따른 역학적 특성)

  • Kim, Min-Ji;Kim, Ji-Yeol;Kim, Byung-Ro
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.5
    • /
    • pp.666-675
    • /
    • 2020
  • This study investigated mechanical characteristics of pine trees in Yeongdong (Goseong-gun), Yeongseo (Hongcheon-gun), and Yeongnam (Bonghwa-gun) to define differences in the material quality among pine trees of the three regions. The compressive strength, hardness and shear strength of pine trees of each region were measured. There were no differences in the compressive strength of the juvenile woods among the regions, while the heartwood and sapwood in Bongwha generally showed the highest compressive strength followed by those in Hongcheon and in Goseong. The hardness of the cross-section of pines in Bonghwa was the highest, and in terms of the hardness of the radial and tangential sections, pines in Goseong topped the list.. There were no difference among heartwoods of each region in terms of the shear strength, but, but sapwood from Bonghwa had higher shear strength than those of the other two regions, which may be attributed to differences in tracheid length and microfibril angle among pines in each region. This study identifies the quality differences among pines of different region, and therefore, is expected to add value by helping choose the domestic pine tree material effectively and selectively, and also select a plus tree.

Physical and Mechanical Properties of Major Korean Ash Species (한국산 물푸레나무속(屬) 주요 수종의 물리 및 역학적 특성)

  • Hwang, Won-Joong;Kwon, Goo-Joong;Kim, Nam-Hun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.30 no.2
    • /
    • pp.95-101
    • /
    • 2002
  • Physical and mechanical properties of major Korean ash species were examined. For Fraxinus rhynchophylla and Fraxinus sieboldiana, green moisture content of sapwood was almost the same value as heartwood. Heartwood of Fraxinus mandshurica, however, had slightly higher moisture content than sapwood. Green and oven dry densities of F. mandshurica were lower than those of F. rhynchophylla and F. sieboldiana. Swelling and shrinkage of sapwood in F. sieboldiana showed somewhat higher value than those of F. rhynchophylla. Longitudinal compressive strength and modulus of elasticity in F. sieboldiana were lower values than those in the other species. Shearing strength in radial section was higher than that in tangential section of all samples. It could be noted that shearing strength of F. sieboldiana demonstrated higher value than that of the other species. Three species had excellent bending properties in MOR and MOE. Impact bending absorbed energy for F. rhynchophylla and F. mandshurica did not show any significant differences.

Mechanical and Oven-drying Characteristics of Pinus densiflora Wood Damaged by Forest Fire (산불 피해 소나무재의 역학적 특성 및 급속오븐 건조특성)

  • Hwang, Won-Joung;Kwon, Gu-Joong;Park, Jong-Su;Kim, Nam-Hun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.4
    • /
    • pp.57-62
    • /
    • 2003
  • The Mechanical and drying characteristics of Pinus densiflora wood, which was damaged by forest fire, and sound wood were examined. There were no significant differences in axial compressive properties, shearing strength and impact bending absorbed energy between damaged and sound woods. But the bending properties of damaged wood were slightly higher than those of sound wood. The green moisture content of sapwood in damaged wood was lower than that in sound wood, but oven-drying rate was similar in both woods. Number of initial check in damaged wood was smaller than that in sound wood, and inner check in damaged and sound woods was not observed. Consequently, it is considered that mostly damaged wood by forest fire can be used for wood material after removing the bark.

Studies on the Properties of Populus Grown in Korea (포플러재(材)의 재질(材質)에 관(關)한 시험(試驗))

  • Jo, Jae-Myeong;Kang, Sun-Goo;Lee, Yong-Dae;Jung, Hee-Suk;Ahn, Jung-Mo;Shim, Chong-Supp
    • Journal of the Korean Wood Science and Technology
    • /
    • v.10 no.3
    • /
    • pp.68-87
    • /
    • 1982
  • In Korea, this is the situation at moment that the total demand of timber in 1972 is more than 5 million cubic meters. On the other hand, however, the available domestic supply of timber at the same year is only about, 1 million cubic meters. A great unbalancing between demand and supply of timber has been prevailing. To solve this hard problem, it has been necessitiated to build up the forest stocks as early as possible with fast grown species such as poplar. Under circumstances, poplar plantations which have been carryed on government and private have reached to large area of 116,603 hectors from 1962 up to date. It has now be come a principal timber resources in this country, and required the basic study on various properties of wood for it's proper utilization, since it has not been made of any systematic study on the properties of Populus grown in Korea. In order to investigate the properties such as anatomical, physical and mechanical properties of nine different species (P. euramericana Guiner I-214. P. euramericana Guiner I-476, P. deltoides Marsh, P. nigra var. italica (Muchk) Koeme, P. alba L.,P. alba $\times$ glandulosa P. maximowiczii Henry, P. koreana Rehder, P. davidiana Dode) of poplar for their proper use and development of new ways of grading processing and quality improving, this study has been made by the Forest Research Institute.

  • PDF

Studies on the Pulping Characteristics of Larchwood (Larix leptolepis Gordon) by Alkaline Process with Additives (첨가제(添加劑) 알칼리 법(法)에 의한 일본 잎갈 나무의 펄프화(化) 특성(特性)에 관(關)한 연구(硏究))

  • Lim, Kie-Pyo;Shin, Dong-Sho
    • Journal of the Korean Wood Science and Technology
    • /
    • v.7 no.2
    • /
    • pp.3-30
    • /
    • 1979
  • Larch ($\underline{Larix}$ $\underline{leptolepis}$ GORDON), one of the major afforestation species in Korea in view of its growing stock and rate of growth, is not favored as a raw material for pulp due to its low yield of pulp and difficulties with bleaching arising from the high content of extractives in wood, and the high heartwood ratio and the active phenolics, respectively. The purpose of this study is to investigate the characteristics of firstly pulping with various additives of cellulose protector for the yield of pulp, and secondly bleaching with oxygen for chlotination-alkali extraction of five stage-sequence to reduce chlorine compounds in bleaching effluents. The kraft cooking liquor for five age groups of larchwood was 18 percent active alkali with 25 percent sulfidity and 5 : 1 liquor-to-wood ratio, and each soda liquor for sap-and heart-wood of the 15-year-old larchwood was 18 percent alkali having one of the following cellulose protectors as the additive; magnesium sulfate ($MgSO_4$, 2.5%), zinc sulfate ($ZnSO_4$, 2.5%), aluminium sulfate ($Al_2(SO_4)_3$, 2.5%), potasium iodide (KI, 2.5%), hydroquinone (HQ, 2.5%), anthraquinone (AQ, 0.1%) and ethylene diamine (EDA, 2.5%). Then each anthraquinone-soda liquor for the determination of suitable cooking condition was the active alkali level of 15, 17 and 19 percent with 1.0, 0.5 and 0.1 percent anthraquinone, respectively. The cooking procedure for the pulps was scheduled to heat to 170$^{\circ}C$ in 90 minutes and to cook 90 minutes at the maximum temperature. The anthraquinone-soda pulps from both heartwood and sapwood of 15-year-old larchwood prepared with 0.5 percent anthraquinone and 18 percent active alkali were bleached in a four-stage sequency of OCED. (O: oxygen bleaching, D: chlorine dioxide bleaching and E: alkali extraction). In the first stage oxygen in atmospheric pressure was applied to a 30 percent consistency of pulp with 0.1 percent magnesium oxide (MgO) and 3, 6, and 9 percent sodium hydroxide on oven dry base, and the bleached results were compared pulps bleached under the conventional CEDED (C: chlorination). The results in the study were summarized as follows: 1. The screened yield of larch kraft pulp did not differ from particular ages to age group, but heartwood ratio, basic density, fiber length and water-extractives contents of wood and the tear factor of the pulp increased with increasing the tree age. The total yield of the pulp decreased. 2. The yield of soda pulp with various chemicals for cellulose protection of the 15-year-old larchwood increased slightly more than that of pure soda pulp and was slightly lower than that of kraft pulp. The influence of cellulose protectors was similar to the yield of pulps from both sapwood and heartwood. The effective protectors among seven additives were KI, $MgSO_4$ and AQ, for which the yields of screened pulp was as high as that of kraft pulp. Considering the additive level of protector, the AQ was the most effective in improving the yield and the quality of pulp. 3. When the amount of AQ increased in soda cooking, the yield and the quality of the pulp increased but rejects in total yield increased with decreasing the amount of active alkali from 19 to 15 percent. The best proportion of the AQ seemed to be 0.5 percent at 17 percent active alkali in anthraquinone-soda pulping. 4. On the bleaching of the AQ-soda pulp at 30 percent consistency with oxygen of atomospheric pressure in the first stage of the ODED sequence, the more caustic soda added, the brighter bleached pulp was obtained, but more lignin-selective bleaching reagent in proportion to the oxygen was necessary to maintain the increased yield with the addition of anthraquinone. 5. In conclusion, the suitable pulping condition for larchwood to improve the yield and quality of the chemical pulp to the level for kraft pulp from conventional process seemed to be. A) the selection of young larchwood to prevent decreasing in yield and quality due to the accumulation extractives in old wood, B) the application of 0.5 percent anthraquinone to the conventional soda cooking of 18 percent active alkali, and followed, C) the bleaching of oxygen in atmospheric pressure on high consistency (30%) with 0.1 percent magnesium oxide in the first stage of the ODED sequence to reduce the content of chlorine compounds in effluent.

  • PDF