An experimental study of cutting efficiency of air-driven diamond burs on human tooth (수종 air-turbine 다이아몬드 버의 절삭 효과에 관한 실험적 연구)

  • Hong, Jin-Sun;Yeo, In-Sung;Kim, Sung-Hun;Lee, Jai-Bong;Han, Jung-Suk;Yang, Jae-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.1
    • /
    • pp.1-7
    • /
    • 2011
  • Purpose: The purpose of this study was to investigate the cutting efficiency of coarse grit diamond burs with air-turbine handpiece on natural tooth. Materials and methods: Four groups of coarse grit diamond bur were selected: Komet (A), Shofu (B), Premier (C), and Mani (D). The extracted maxillary central incisors were used, and ten cuts were made on each specimen, using the rotary diamond burs. The surface of each bur was measured at the upper, middle, and bottom of the bur with confocal laser scanning microscope and imaged with SEM. The data were analyzed with one-way ANOVA and t-test at the significance level of 0.05. Results: The surface roughness was measured. At the A diamond bur, the Sa values were $52.93\;{\mu}m$, $48.32\;{\mu}m$, $46.79\;{\mu}m$, $45.06\;{\mu}m$, and $43.43\;{\mu}m$ for control, test 1, 2, 3, and 4 respectively. The Sa values were $50.68\;{\mu}m$, $45.62\;{\mu}m$, $44.41\;{\mu}m$, $44.10\;{\mu}m$, and $42.46\;{\mu}m$ for B diamond bur, $58.02\;{\mu}m$, $55.53\;{\mu}m$, $52.22\;{\mu}m$, $48.26\;{\mu}m$, and $45.36\;{\mu}m$ for C diamond bur, and $50.11\;{\mu}m$, $46.73\;{\mu}m$, $45.46\;{\mu}m$, $42.58\;{\mu}m$, and $41.80\;{\mu}m$ for D diamond bur. Surface roughness after each bur use showed significant changes, but no significant difference was found in surface roughness change between bur systems. Conclusions: Surface roughness in the same bur system showed significant differences after each tooth preparation. However no statistically significant differences were found in surface roughness between bur systems. The SEM images between control and test 4 showed the abraded particles.

A study of burr formation on microgrooving for fresnel lens mould (프레넬렌즈 금형용 미세홈 가공에 있어서 버 발생 경향에 관한 연구)

  • 임한석;안중환
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.14 no.3
    • /
    • pp.28-34
    • /
    • 1997
  • The side burrs and shape distortion resulting from the micromachining of an array of V-shape microgrooves in fresnel lens mould were experimentally invesigated. The focus of this study is on the influence of depth of cut and prism angle on the burr growing rate. The main experiments were con- ducted on the single prism cutting for the convinient of measuring the burr shape and cutting force. From the observation of the burr shape and burr growing rate, it was found that there exits a critical depth of cut below which the burrs are more or less irregular and weak. But above that critical value, the burrs are re- latively clear and stiff.

  • PDF

Side Burr Generation Model of Micro-Grooving (미세홈 가공에 있어서 측면버 발생모델)

  • 임한석;안중환
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1997.04a
    • /
    • pp.987-992
    • /
    • 1997
  • Burrs always come out with the machining of ducterial with small size. Though the size of burrs is small, burrs dominate deterioration of the accuracy of the micro grooves. So the burr generation model especially side burr generation model was investigated to predict the size of the burrs at the given cutting conditions. The side shear plane is introduced to build the burr generation model and the width of side shear plane nomalized with cutting depth is defined with the shear angle. From the theoretical observation, the width of side shear plane can vary up 40% of the cutting depth. To determine the size of burr and stiffness, single groovings were carried out and it was found that there exist a critical depth of cut that the size or stiffness of the burr vary.

  • PDF

EFFECT OF CUTTING INSTRUMENTS ON THE DENTIN BOND STRENGTH OF A SELF-ETCH ADHESIVE (상아질 삭제기구가 자가부식 접착제의 결합강도에 미치는 효과)

  • Lee, Young-Gon;Moon, So-Ra;Cho, Young-Gon
    • Restorative Dentistry and Endodontics
    • /
    • v.35 no.1
    • /
    • pp.13-19
    • /
    • 2010
  • The purpose of this study was to compare the microshear bond strength of a self-etching primer adhesive to dentin prepared with different diamond points, carbide burs and SiC papers, and also to determine which SiC paper yield similar strength to that of dentinal surface prepared with points or burs. Fifty-six human molar were sectioned to expose the occlusal dentinal surfaces of crowns and slabs of 1.2 mm thick were made. Dentinal surfaces were removed with three diamond points, two carbide burs, and three SiC papers. They were divided into one of eight equal groups (n = 7); Group 1: standard diamond point(TF-12), Group 2: fine diamond point (TF-12F), Group 3: extrafine diamond point (TF-12EF), Group 4: plain-cut carbide bur (no. 245), Group 5: cross-cut carbide bur (no. 557), Group 6 : P 120-grade SiC paper, Group 7: P 220-grade SiC paper, Group 8: P 800-grade SiC paper. Clearfil SE Bond was applied on dentinal surface and Clearfil AP-X was placed on dentinal surface using Tygon tubes. After the bonded specimens were subjected to uSBS testing, the mean uSBS (n = 20 for each group) was statistically compared using one-way ANOV A and Tukey HSD test. In conclusion, the use of extrafine diamond point is recommended for improved bonding of Clearfil SE Bond to dentin. Also the use of P 220-grade SiC paper in vitro will be yield the results closer to dentinal surface prepared with fine diamond point or carbide burs in vivo.

EFFECT OF MICROLEAKAGE OF A SELF-ETCHING PRIMER ADHESIVE ACCORDING TO TYPES OF CUTTING INSTRUMENTS (삭제기구가 자가 산부식 접착제의 미세누출에 미치는 영향)

  • Kim, Yong-Hee;Park, Jae-Gu;Cho, Young-Gon
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.4
    • /
    • pp.327-334
    • /
    • 2007
  • The purpose of this study was to evaluate the effect of burs on microleakage of Class V resin restorations when a self-etching primer adhesive was used. Forty Class V cavities were prepared with four different cutting burs on extracted third molars, and divided into one of four equal groups (n = 10); Group 1-plain cut carbide bur (no. 245), Group 2-cross cut carbide bur (no. 557), Group 3-fine diamond bur (TF-21F), Group 4-standard diamond bur (EX-41). The occlusal and gingival margin of cavities was located in enamel and dentin, respectively. Cavities were treated with Clearfil SE Bond and restored with Clearfil AP-X. Specimens were thermocycled, immersed in a 2% methylene blue solution for 24 hours, and bisected longitudinally. They were observed leakages at enamel and dentinal margins. Data were analyzed using Mann-Whitney and Wilcoxon signed ranked test. The results of this study were as follows; 1. At enamel margin, microleakage of group 4 was statistically higher than those of group 1, 2 and 3 (p < 0.01). 2. At dentinal margin, microleakage of group 4 was statistically higher than group 3 (p < 0.01), but group 1 and 2 were not statistically different with group 3 and 4. 3. Enamel microleakage was statistically higher than dentinal microleakage in group 1, 2 and 3 (p < 0.05), but statistical difference between the microleakage of enamel and dentinal margin was not in Group 4. In conclusion, the use of coarse diamond bur showed high microleakage at both enamel and dentinal margin when Clearfil SE Bond was used in class V cavity.

Grinding Characteristics of Diamond Burs in Dentistry (AE에 의한 치과용 다이아몬드 버의 연삭가공 특성)

  • 이근상;임영호;권동호;소의열
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.8 no.3
    • /
    • pp.76-82
    • /
    • 1999
  • This study was carried out to verify finding performance of dental diamond bur and investigate the possibility of AE application in density field. Work pieces were made of acryl and bovine respectively for the experiments in this study. Grinding test was conducted to get the data of grinding resistance and specific finding energy of low different types of diamond bur by using tool dynamometer. AE signal was acquired to verify grinding process in the AE measuring system. AErms value was increased as the grinding velocity and depth were increasing, but it decreased as the feed rate was increasing. The case of the small value of AE signal is due to abnormal grinding in D type diamond bur. By analyzing AErms start and finish time of grinding working, abnormal grinding state can be confined. Abnormal state can be found through the behavior of AE signal in the finding working. As a result, it is expected that forecast of abnormal state is possible using AE equipments under real time process.

  • PDF

Grinding Characteristic of Diamond Burs in Dentistry (치과용 다이아몬드 버의 연삭 가공 특성)

  • 이근상
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.04a
    • /
    • pp.414-418
    • /
    • 1996
  • This paper aims at reviewing the possibility application over normal or abnormal, detection used by AE and the characteristics of grinding process. In this study, when diamond bur in dentistry with chosen grinding conditions were tuned at grinding. The variation of grinding resistance and AE signal is detected by the use of AE measuring system. The tests are carried out in accordance with diamond burs and workpiece: arcyl and cowteeth. According to the experiment results, the following can be expected; AE has the possibility to detect the state normality and abnormality. However, the grinding resistance measuring can find it difficult to detect it. It can be accurately excepted from AE occurrence pattern in contact start point of diamond but and cowteeth, grinding condition and derailment point. It is known that AErms is well compatible with grinding resistance.

  • PDF

Wear Characteristic of Diamond Burs in Dentistry (치과용 다이아몬드 버의 마멸 특성)

  • 이근상;임영호;권동호;최만용;김교한;최영윤
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.11a
    • /
    • pp.80-84
    • /
    • 1996
  • This paper aims at reviewing the Possibility application over normal or abnormal, detection used by AE and the wear characteristics of grinding process. In this study, when diamond bur in dentistry with chosen grinding conditions were tuned at grinding. The variation of grinding resistance and hE signal is detected by the use of AE measuring system. The tests are carried out in accordance with diamond burs and workpiece; arcyl and bovine. According to the experiment results, the following can be expected; AE has the possibility to detect the state normality and abnormality. However, the grinding resistance measuring can find it difficult to detect it. It can be accurately excerpted from AE occurrence pattern in contact start point of diamond bur and bovine, grinding condition and derailment point. It is known that AE$\_$rms/ is well compatible with grinding resistance. According to the increase of the material removal rate, the specific energy of the diamond bur is inclined to decrease and the grinding resistance has a tendency to increase.

  • PDF

Wear of Diamond Dental Burs (치과의술용 다이아몬드 전착공구의 마멸)

  • Lee, Keun-Sang;Lim, Young-Ho;Kwon, Dong-Ho;So, Eui-Yeorl
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.16 no.4 s.97
    • /
    • pp.148-154
    • /
    • 1999
  • This study was carried out to verify grinding performance of dental diamond bur and investigate the possibility of AE application in dentistry field. Workpieces were made of acryl and bovine respectively for the experiments in this study. Grinding test was conducted to get the data of grinding resistance and specific grinding energy of four different types of diamond bur by using tool dynamometer. AE signal was acquired to verify grinding process in the AE measuring system. Tool wear was observed to find parameters about grinding characteristics of diamond bur by means of SEM picture. It was found that the wear of dental diamond bur could be detected with polishing of grinding material, removal of adhesive parts, wear of particles neighboring cutting nose, loss of material and elevation of temperature. The wear of B, C, D type diamond bur is due to wear and fracture of grain size. Abnormal state can be found through the behavior of AE signal in the grinding working. As a result, it is expected that forecast of abnormal state is possible using AE equipments under real time process.

  • PDF

Grinding Characteristics of Diamond Burs in Dentistry (치과용 다이아몬드 버의 연삭가공 특성)

  • Lee, Keun-Sang;Lim, Young-Ho;Kwon, Dong-Ho;Choi, Man-Yong;Kim, Kyo-Han;Choi, Young-Yun
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.14 no.12
    • /
    • pp.66-72
    • /
    • 1997
  • This paper aims at reviewing the possibility application over normal or abnormal, detection used by AE and the wear characteristics of grinding process. In this study, when diamond bur in dentistry with chosen grinding conditions were tuned at grinding. The variation of grinding resistance and AE signal is detected by the use of AE measuring system. The tests are carried out in accordance with diamond burs and workpiece: arcyl and bovine. According to the experiment results, the following can be expected: AE has the possibility to detect the state normality and abnormality. Hpwever, the grinding resistance measuring can find it difficult to detect it. It can be accurately excepted from AE occurrence pattern in contact start point of diamond bur and bovine, grinding condition and derailment point. It is known that AErms is well compatible with grinding resistance. According to the increase of the material removal rate, the specific energy of the diamond bur is inclined to dectease and the grinding resistance has a tendency to increase.

  • PDF