  • This paper deals with a fatigue life prediction of a surface crack based on the experimentally obtained relationship between surface crack length ratio $a/a_{f}$ and cycle ratio $N/N_{f}$ using micro computer. Firstly $a/a_{f}$-$N/N_{f}$ curves obtained from experimental tests, were assumed as three curves UC(the upper limit curve), LC(the lower limit curve) and MC(the middle curve), and these were utilized to predict the fatigue life. Comparing the calculated values which represent the characteristics of crack growth behaviors from the three assumed curves with the experimental ones, it has been found that in the stable crack growth region, they coincide reasonably well each other. And the differences between the fatigue lives obtained from the assumed curves and the experimental fatigue life did not exceed 20%. Using the characteristics of $a/a_{f}$-$N/N_{f}$ curves, it is possible to predict the da/dN-Kmax curves and the S-$N_{f}$ curves.

작은 표면균열의 성장특성에 의한 수명예측 (A Fatigue Life Prediction by Growth Characteristics of a Small Surface Crack)

  • 서창민;임창순;강용구
    • 한국해양공학회지
    • /
    • 제3권2호
    • /
    • pp.108-117
    • /
    • 1989
  • This paper deals with a fatigue life prediction of a surface crack based on the experimentally obtained relationship between surface crack length ratio $a/a_{f}$ and cycle ratio $N/N_{f}$ using micro computer. Firstly $a/a_{f}$-$N/N_{f}$ curves obtained from experimental tests, were assumed as three curves UC(the upper limit curve), LC(the lower limit curve) and MC(the middle curve), and these were utilized to predict the fatigue life. Comparing the calculated values which represent the characteristics of crack growth behaviors from the three assumed curves with the experimental ones, it has been found that in the stable crack growth region, they coincide reasonably well each other. And the differences between the fatigue lives obtained from the assumed curves and the experimental fatigue life did not exceed 20%. Using the characteristics of $a/a_{f}$-$N/N_{f}$ curves, it is possible to predict the da/dN-Kmax curves and the S-$N_{f}$ curves.

  • PDF

2024-T3 및 황동의 작은 표면결함재의 피로균열 성장특성에 관한 연구 (A study on the growth behaviors of surface fatigue crack initiated from a small-surface defect of 2024-T3 and brass)

  • 서창민;오명석
    • 한국해양공학회지
    • /
    • 제10권1호
    • /
    • pp.53-64
    • /
    • 1996
  • In this paper, rotating bending fatigue tests have been carried out to investigate the growth behabiors of surface fatigue crack initiated from a small artificial surface defect, that might exist in real structures, on 2024-T3 and 6:4 brass. The test results are analysed in the viewpoints of both strength of materials and fracture mechanics, it can be concluded as follows. The effect of a small artificial surface defect upon the fatigue strength is very large. The sensitivity of 2024-T3 on the defect is higher than that of 6:4 brass. The growth behavior of the surface fatigue crack of 2024-T3 is different from that of 6:4 brass. The growth rate of the surface fatigue crack of 2024-T3 is considerably rapid in the early stage of the fatigue life and apt to decrease in the later stage. It was impossible to establish a unifying approach in the analysis of crack growth begabior of 2024-T3 and 6:4 brass using the maximum stress intensity factor because of their dependence on stress level. But if the elastic strain and cyclic total strain intensity factor range were applied to obtain the growth rate of surface fatigue cracks of the materials, the data were found to be nearly coincided.

  • PDF

Hydroxyapatite 소결체의 가소제 첨가에 따른 특성 (Properties of hydroxyapatite sintered body added with plasticizer)

  • 류수착;김재규;김승현
    • 한국결정성장학회지
    • /
    • 제29권4호
    • /
    • pp.167-172
    • /
    • 2019
  • HAp의 성형성과 열처리를 용이하게 하는 유기가소제를 사용하여 첨가량에 따른 강도(MPa)와 경도(Hv), 수축율(%) 및 생물학적 특성 중 항균력을 측정하였다. 가소제의 첨가량이 증가할수록 기계적 특성인 압축강도와 굽힘강도, 경도 등이 증가하였으나 가소제의 첨가량이 7%를 넘을 경우 오히려 기계적 특성이 감소하였다. 이는 허용치 이상의 가소제의 첨가는 성형 시 균열을 발생시키고 이러한 균열은 소결 시 내부에 미세균열 및 산화 시 기공의 발생을 촉진시켜 기계적 특성의 감소를 유발한다. 항균성 측정 결과 가소제 첨가량 에 관계없이 균은 검출되지 않았으며 우수한 항균력을 발휘하였다.

열응력, 내력 및 균열 경계하중을 고려한 2차원 균열문제의 에너지방출율 (The Energy Release Rate of the Two Dimensional Cracked Body Under Thermal Stresses, Body Forces and Crack-Face Tractions)

  • 이태원
    • 대한기계학회논문집
    • /
    • 제17권9호
    • /
    • pp.2172-2180
    • /
    • 1993
  • Under general loadings, including body forces, crack-face tractions and thermal loading, the energy release rate equation for a two-dimensional cracked body is presented. Defining the virtual crack extension as the variation of the geometry, the equation is directly derived by a shape design sensitivity of the potential energy. Although the form of the derived energy release rate equation is different from other researchers's results, the three example show that the former is exactly the same as the latter. However, the final integral equation do not involve the derivative of the displacement on the crack surface and crack tip region, thereby improving the numerical accuracy in the computation of the energy relase rate. Moreover, as it was derived from the governing equation including non-linear elasticity without special assumptions, the energy release rate of a elasto-plastic fracture can be obtained and any numerical stress analysis method can be applied.

탄소강의 피로균열 진전거동 평가에 관한 실험적 연구 (An Experimental on the Evalution of Fatigue Crack Propagation of Carbon Steel)

  • 김희송;안병욱
    • 대한기계학회논문집
    • /
    • 제13권5호
    • /
    • pp.938-946
    • /
    • 1989
  • 본 연구에서는 CT시험편을 이용하여 소규모 항복조건하에서 하한계(near threshold)영역과 안전균열성장(제II)영역의 균열진전거동을 파악하고 피로균열 진전속도와 음향방출거동, 파단면 특성을 각각 비교, 고찰하여 각 파라미터간의 상관 관계 및 유용성을 검토하고자 한다.

인공경량골재 내부에 발생하는 방사형 균열의 억제 방법에 관한 연구 (Study on the prevention methods of radial cracks generated in artificial lightweight aggregate)

  • 강지민;김강덕;강승구
    • 한국결정성장학회지
    • /
    • 제25권5호
    • /
    • pp.199-204
    • /
    • 2015
  • 본 연구에서는 잔사회와 준설토로 제조된 구형의 인공경량골재 내부에 생성되는 방사형 균열의 원인 및 그 억제 방법에 대하여 연구하였다. 인공경량골재는 잔사회와 준설토를 각각 7 : 3의 무게 비로 혼합하고 직경이 5~20 mm인 구 형태로 성형한 후 $1200^{\circ}C$에서 10분간 직화소성법으로 제조하였다. 골재 내부의 균열은 골재 지름이 작을수록 발생이 억제되었다. 또한 $SiO_2$ 분말을 첨가한 경우, 분말의 크기가 클수록 또는 첨가량이 증가할수록 방사형 균열 발생이 억제되었다. 균열이 억제된 인공경량골재의 비중은 1.3~1.6이고, 흡수율은 5~20 %의 범위를 나타내었다. 따라서 본 논문에서 제조된 인공경량골재는 건설 및 환경소재 등 여러 분야에 적용 가능할 것으로 보이며, 더불어 잔사회 및 준설토의 재활용율을 높이는데 크게 기여할 것으로 기대된다.

원전 이종금속 맞대기용접부 PWSCC 균열건전성평가 (Evaluation of PWSCC at Dissimilar Metal Butt Welds in NPP)

  • 이성호;이경수;오창영
    • 대한기계학회논문집A
    • /
    • 제36권9호
    • /
    • pp.1047-1052
    • /
    • 2012
  • 가압경수로형 원전의 Alloy 600 원자로압력용기헤드 관통노즐 및 Alloy 82/182 이종금속 맞대기 용접부에서 일차수응력부식균열(PWSCC)이 보고된 이후 전 세계적으로 PWSCC에 의한 용접부 파단을 예방하기 위해 강화검사를 적용하고 있다. 본 이종금속용접부에 대한 가동중검사에서 균열이 발견된 경우 건전성평가 결과가 도출되기까지 발전소가 정지 상태에 있게 됨에 따라 원전 이용율 저하가 발생할 수 있는데, 이를 예방하기 위해서는 균열건전성평가 관련 기술의 정립뿐만 아니라 신속하게 평가 결과를 도출할 수 있는 시스템의 구축이 필요하다. 본 연구에서는 이종금속 맞대기 용접부를 대상으로 진행하고 있는 PWSCC 균열건전성평가 기준 정립 및 전산 시스템 개발 결과를 제시하였다. 본 연구를 통해 이종금속 맞대기 용접부 PWSCC 균열건전성평가 기술이 정립되고 전산 시스템으로 구현되어 원자로압력용기 주변 이종금속 맞대기 용접부에서의 PWSCC 균열에 대한 기술적 건전성평가 수단을 확보하였다.

단일과대하중하의 부식피로균열진전거동에 관한 연구 (A Study on Corrosion Fatigye Crack Propagation Behaviors due to a Single Overload)

  • 강동명;이하성;우창기
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 춘계학술대회 논문집
    • /
    • pp.481-485
    • /
    • 1997
  • 6063-T5 alloys are tested in laboratory air, water and 3% NaCl solution to investigate the effects of corrosive environment on the retardation behavior through single overload fatigue test. Also, the fatigue crack propagation and the crack closure behavior are studied. The results obtained in this experimental study are summarized as follows: 1) Behaviors of fatigue crack growth retardation are observed in water and 3% NaCl solution as they do in air. The number of delay cycles and the size of affected region by single overload decrease greatly in water and 3% NaCl compared with those in air. 2) In fractographic results, the overload marking by single overload appear remarkably in air, but indistinctly in water and 3% NaCl solution. 3) The effect of crack closure on crack propagation is most remarkable in the beginning of crack propagation. With crack propagation, the crack closure level and its effect decrease greatly.

  • PDF

非規則性 短纖維强化 SMC複合材料의 疲勞龜裂 進展에 관한 硏究 (A Study on Fatigue Crack Propagation of Random Short Fiber SMC Composite)

  • 김광수;김상태
    • 대한기계학회논문집
    • /
    • 제13권1호
    • /
    • pp.87-95
    • /
    • 1989
  • 본 연구에서는 국내산 비규칙성 짧은 섬유로 강회된 SMC 복합재료의 피로파괴 특성에 대한 기초자료로서 피로균열의 진전특성을 나타내는데 기존파괴 역학의 적용여부를 살펴보며, 서로 다른 피로모드 상태 하에서 하중크기의 상태에 따른 피로균열진전의 특성을 나타내었으며, 또한 주사형 전자현미경(scanning electron microscope)을 사용한 파단면 관찰을 통해 파괴 메카니즘을 살펴보았다.