  • Microcracking of type 304 stainless steel at $593^{\circ}C(1,100^{\circ}F)$ has been studied, in particular, initiation, growth, and coalescence of fatigue and creep microcracks on smooth specimens and small notch specimens via surface replicas and photomicrographs. Quantitative information, such as, initiation period, growth, and coalescence behavior, statistical distributions of crack length, density of cracks, distribution patterns and crack growth properties, were obtained. From this study, the fracture process, fatigue life, and creep life prediction characterized by the growth of surface microcracks have been analysed by a new approach unifying the conventional approaches based on the final fracture of materials with the fracture mechanics approach. Knowledge of these parameters is critical for the application of fracture mechanics to fatigue and creep life assessment, and the damage evaluation of structures at elevated temperature.

  • PDF

Hydration Heat and Crack-Reducing Properties of Cement Mortar Added Fluosilicate Salt Based Hydration Heat Reducer (규불화염계 수화열 저감제가 첨가된 시멘트 모르타르의 수화열 변화 및 균열저감 특성)

  • Kim, Jin-Yong;Lee, Hyo-Song;Rhee, Young-Woo;Kim, Do-Su;Lee, Byoung-Ky;Khil, Bae-Su;Han, Seung-Gu
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.3 s.274
    • /
    • pp.198-204
    • /
    • 2005
  • Fluosilicate salts based hydration heat reducer(SWP-HR), used in this study, is composed of fluosilicate salts, soluble silica, aromatic polymer condensate and nitrate salt based inorganic compound with latent heat property. Effects of SWP-HR addition on the hydration heat and anti-crack property of cement mortar were investigated. Adiabatic hydration temperature and drying shrinkage length of SWP-HR added cement mortar had a tendency to decrease compared to those of cement mortar without SWP-HR addition. Also, it was confirmed through crack pattern experiment of plate-form specimen for elucidating crack-reducing characteristic that anti-crack property of SWP-HR added cement mortar was improved.

Fracture Characteristics of Polypropylene Fiber Reinforced Concrete (폴리프로필렌 섬유보강 콘크리트의 파괴특성 연구)

  • Shin-Won Paik
    • Journal of the Korean Society of Safety
    • /
    • v.12 no.4
    • /
    • pp.230-240
    • /
    • 1997
  • An experimental research investigation of the fracture properties of polypropylene fiber reinforced concrete is reported. Fibers used in this experiment were two types, monofilament and fibrillated polypropylene fibers. Fiber length was 19 mm, and volume fractions were 0, 1, 2, and 3%. Also, as initial notch depths influence the fracture properties of fiber reinforced concrete, the notch depth ratios by specimen height were 0.15, 0.30 and 0.45. The main objective of this experimental program is to obtain the load-deflection and the load-CMOD curves, to investigate the fracture properties of the polypropylene fiber reinforced concretes. Therefore, the flexural specimen testings on the four-point bending were conducted. Then, the load-load point displacement and the load-crack mouth opening displacement curves were measured. The effects of different volume fractions of the monofilament and the fibrillated polypropylene fiber reinforced concrete on the compressive strength, flexural strength and toughness, stress intensity factor, and fracture energy were investigated through the experimental results.

  • PDF

Safety Margin Improvement Against Failure of Zr-2.5Nb Pressure Tube (Zr-2.5Nb압력관 파손에 대한 안전여유도 개선)

  • Jeong, Yong-Hwan;Kim, Young-Suk
    • Nuclear Engineering and Technology
    • /
    • v.27 no.5
    • /
    • pp.775-783
    • /
    • 1995
  • This study is to assess the effects of increasing wall thickness on the safety margin of pressure tube in operating and of lowering initial hydrogen concentration on the DHC growth in respect to the improvement of the reliability of pressure tube in CANDU reactors. The pressure tube with thicker wall of 5.2 mm shows much higher safety margin for flaw tolerance by 25% than the current 4.2mmm tube. The thicker pressure tubes have a great benefit in LBB assessment including the initial crack depth at which DHC occurs, the crack length at onset of leaking and the available time for action. The resistance for the pressure tube ballooning at LOCA accident is also increased with the thicker tube. The calculations for Heq concentration after 20 years of operation as a function of wall thickness and initial hydrogen concentration show that the 5.2 mm nil thickness tube with 5 ppm initial hydrogen concentration is the most resistant to DHC. with the lower initial hydrogen concentration, TSS temperature for the precipitation or hydride decreases and the crack growth during cooldown reduces.

  • PDF

Investigation of Detectable Crack Length in a Bolt Hole Using Eddy Current Inspection (와전류탐상검사를 이용하여 탐지 가능한 볼트홀 내부 균열 길이 연구)

  • Lee, Dooyoul;Yang, Seongun;Park, Jongun;Baek, Seil;Kim, Soonkil
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.41 no.8
    • /
    • pp.729-736
    • /
    • 2017
  • In this study, the physics-based model and machine learning technique were used to conduct model-assisted probability of detection (MAPOD) experiments. The possibility of using in-service cracked parts was also investigated. Bolt hole shaped specimens with fatigue crack on the hole surface were inspected using eddy current inspection. Owing to MAPOD, the number of experimental factors decreased significantly. The uncertainty in the crack length measurement for in-service cracked parts was considered by the application of Monte Carlo simulation.

Evaluation of Crack Width Based on the Actual Bond Stress-Slip Relationship in Structural Concrete Members (부착응력-미끌림 관계에 기반한 철근콘크리트 부재의 균열폭 산정)

  • Kim, Woo;Lee, Ki-Yeol;Kim, Jang-Hyun
    • Journal of the Korea Concrete Institute
    • /
    • v.18 no.1 s.91
    • /
    • pp.91-100
    • /
    • 2006
  • This paper presents an analytical model for evaluation of crack widths in structural concrete members. The model is mathematically derived from the actual bond stress-slip relationships between the reinforcement and the surrounding concrete, and the relationships summarized in CEB-FIP Model Code 1990 are employed in this study together with the assumption of a linear slip distribution along the interface at the stabilized cracking stage. With these, the actual strains of the steel and the concrete are integrated respectively along the embedment length between the adjacent cracks so as to obtain the difference in the axial elongation. The model is applied to the test specimens available in literatures, and the predicted values are shown to be in good agreement with the experimentally measured data.

A Study on the Fatigue Crack Evaluation Method of Railway Bogie Frame (철도차량 대차를 피로균열 평가법 연구)

  • Jun, Hyun-Kyu;Seo, Jung-Won;Lee, Dong-Hyong;Kim, Hyeong-Jin
    • Journal of the Korean Society for Railway
    • /
    • v.12 no.1
    • /
    • pp.16-24
    • /
    • 2009
  • In this study, fatigue crack growth rate of a cracked railway bogie frame under variable amplitude loading is predicted by applying linear elastic fracture mechanics. For this purpose, we find the critical points by reference surveying on cracked railway bogie frames. And we make an effective load history by synthesizing the dynamic load measured from the critical points of railway bogie frame during commercial line operation and the static load calculated from structural analysis. Crack growth analyses are performed at the 3 critical points under the commercial operation loading condition by assuming an initial crack size as 40 mm. and the results are compared with the experimental results from Japanese railway bogie frame crack growth case. From the analysis results, we find that around 500,000 km operating distance is necessary to bring crack growth from the initial crack to unstable crack. And it takes around 3.8 normal operating years. We conclude that it is enough time to detect the crack between normal maintenance period.

Evaluation of Fatigue Crack Growth Rate on the Surface of Steel Members Using COD(Crack Opening Displacement) Measurement (COD(Crack Opening Displacement) 측정에 의한 강재표면의 피로균열진전속도 평가)

  • Kim, Kwang Jin;Kim, In Tae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.15 no.2
    • /
    • pp.179-188
    • /
    • 2011
  • Steel structures have been allowed to have fatigue damage tolerance in fact. If it would be assessed whether fatigue crack is growing or not and How fast fatigue crack is propagating, we should make a rational decision on methods and a period of reinforcement in the maintenance. In this study, fatigue crack growth tests on two kinds of through-thickness cracked steel plates and a out-of-plane gusset welded joint were conducted to evaluate fatigue crack growth rate using the COD(Crack Opening Displacement), and COD measurement using strain gauges was examined to offer a practical method. As a result, we proposed a reasonable assessing method for fatigue crack growth rate using the COD and it was experimentally proved practical to estimate the COD through measuring strains.

Fatigue Strength of In-plane Welded Attachments (면내 거셋 용접연결부의 피로강도)

  • Bae, Doobyong
    • Journal of Korean Society of Steel Construction
    • /
    • v.15 no.6 s.67
    • /
    • pp.629-637
    • /
    • 2003
  • This s paper presented the results of the three phases of fatigue tests to determine the fatigue strength of in-plane welded gusset joints, which are the most common details inevitably existing in the region of high stress range. A total of 57 fatigue specimens with varying thickness and strengths were made and tensile fatigue tests performed. One full-scale beam fatigue test was also performed. The validity of the fatigue strength of those details in the specification was confirmed, with the effects of thickness of flanges and welded attachments, length of attachments, and strength of applied steel examined. The characteristics of crack initiation and propagation were also observed. The test result was evaluated by comparing it with other test data and fatigue criteria of other countries. To determine the degree of stress concentration in the weld toe depending on geometric configuration such as attachment length and transition radius, analyses were performed. Compared to the present specification, analytical results indicate the need to revise and subdivide the detail categories.

A Study of Shrinkage Characteristics of Low Shrinkage Normal Strength Concrete With Boundary Restraint Condition (4변 구속조건을 갖는 초저수축 일반강도 콘크리트의 수축특성 연구)

  • Jeong, Jun-Young;Min, Kyung-Hwan;Lee, Dong-Gyu;Choi, Hong-sik
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.6
    • /
    • pp.693-699
    • /
    • 2016
  • In this study, the replacement effects of cementitious materials (fly ash, blast furnace slag, and blended mixtures) were assessed for normal strength concrete with very low shrinkage properties under $350{\mu}{\varepsilon}$ strain using a powder type shrinkage reducing agent. In addition, through mock-up tests of actual size walls restrained with four sides, the shrinkage characteristics using the power type shrinkage reducing agent were measured and the crack reducing ability was assessed. The slump and air contents were measured as the properties of fresh concrete, and the length changes of the prismatic specimens, $100{\times}100{\times}400mm$ in size, were measured for the shrinkage characteristics. To reduce the shrinkage of concrete, the maximum replacing ratio of the fly ash is effective to 20 percent; however, the use of blast furnace slag and ternary mixtures did not reduce the shrinkage.