A rearing experiment of the olive flounder was performed in a set of water-reuse system to test the reusability of the water in culture system with (i) a foam fractionator to separate particles from water and (ii) a culture tank contain mineral particles to filter the metabolic wastes by adsorption and/or decomposition. Two kinds of commercially processed loess particles and a dolomite particle (all 50 ${\mu}$diameter) were tested. The mineral particles were suspended in the culture tank and the water was pumped into the foam fractionator, where the particles were separated and drained out with foam from the system. In a circular culture tank of 4.8 m in diameter with 10 d water, the juvenile olive flounders (23.1 g/fish, 5,555 fish, 128 kg total body weight) were stocked. 90 % of the rearing water was reused and turnover rate of the water in the tank was two times per hour. Water temperature was maintained 17${\pm}$1$^{\circ}C$. At the end of 75 day-experimental rearing, 5,532 flounders, weighing 468 kg, were harvested. An individual flounder grew to 84.6 g of body weight. The final stocking density was 26.0 kg/$m^2$. No diseases were observed during the experiment.
Kim Sang-Bae;Cho Sung-Baek;Kim Wan-Tae;Yoon Sung-Dae
Journal of the Mineralogical Society of Korea
/
v.18
no.1
/
pp.19-31
/
2005
A study on the beneficiation of illite occurring in Youngdong province is performed with applying selective grinding and air classification techniques. Quartz and illite are occurred as major components, and sulfide minerals such as pyrite, chalcopyrite are associated as minor components. The result of sieving test shows that contents of Al₂O₃, K₂O and ignition loss are increased, whereas SiO₂ is decreased with particle size decrease. Fe₂O₃ content is almost same in all the particle size range but slightly lower at coarse particles. The yield of fine particles is increased with increasing rotor speed in both grinding stage and air classification stage. When the selective grinding and air classification are carried out at optimal condition, yield of the concentrate is 76.16 wt.%. The chemical compositions of the concentrate are SiO₂70.13%, Al₂O₃ 19.40%, Fe₂O₃ 1.62%, K₂O 5.20%, and ignition loss 2.77%. The beneficiation process developed in the current study is very effective method which purification and particle size control can be achieved simultaneously.
The artificial rains having different pH and weathering simulation test were performed for Gyeongju Namsan granite and dacitic tuff to predict the role of acid rain in the deterioration of stone monuments located in Gyeongju area. The pH 4.0 rain reacted with the fresh granite showed near neutral pH at the early stage due to the hydrolysis of minerals in the rock surface. But the pH changed back to the initial pH in the later stage. On the other hand, the pH 5.6 rain showed the neutral pH for a longer time than the experiment with pH 4.0 rain, reflecting slower reaction of minerals due to the weaker acidity. When the pH 5.6 rain reacted with the weathered granite, the water showed neutral pH longer than the case of the fresh granite. The similar tendencies were observed in the experiment of dacitic tuff, except that the pH 4.0 rain reacted with dacitic tuff took a longer time to go back to the initial pH as compared with the case of granite. These results may due to the differences in mineral composition and texture of two rocks. Dacitic tuff contains more fine-grained or glassy groundmass than granite and is more reactive with weaker acid rain. It was predicted that the weight loss and strength decrease rate of dacitic tuff would be approximatetly twice relative to those of granite in the same experimental environment.
The Eoraesan area, Chungju, which is located in the northwestern part of Ogcheon Metamorphic Zone, Korea, mainly consists of the Neoproterozoic Gyemyeongsan Formation and the Mesozoic igneous rocks which intruded it. The metaacidic rocks (MAR) of the Gyemyeongsan Formation show a maximum radioactive value, and the Early Jurassic biotite granite is regionally distributed in this area. In this paper is researched the microstructure related to the growth of rare-earth mineral of allanite in the MAR, and is considered the source and occurrence time of rare-earth element (REE) mineralization. The MAR is mainly composed of alkalic feldspar (mainly microcline), quartz, iron-oxidizing mineral, biotite, muscovite, plagioclase, hornblende, allanite, zircon, epidote, fluorite, apatite, garnet, (clino)zoisite etc. The radioactive elements contained in the allanite cause a dark brown hale in the surrounding biotite, and the allinte also occurs as aggregate along the regional foliation. The deflection of regional foliation and the strain shadows, which are common to the pre-tectonic porphyroblast grown before the formation of regional foliation, can't be observed around most allanites (aggregates). The grain size and orientation of ironoxidizing mineral included in the allanite aggregate are the same as those in the matrix. It is recognized the hydrothermal conversion of hornblende to biotite due to the intrusion of igneous rock, and the secondary biotite occurs and contacts with allanite, zircon, epidote etc. These microstructures indicate that the rare-earth mineral of allanite (aggregate) grew by the hydrothermal alteration due to the intrusion of igneous rock after the formation of regional foliation. It is considered that the REE mineralization is closely related to the intrusion of Early Jurassic biotite granite which is regionally distributed in this area.
Myeong, Hyeonah;Kim, Juhyeok;Lee, Jin-Yong;Kwon, Kideok D.
Korean Journal of Mineralogy and Petrology
/
v.34
no.4
/
pp.265-275
/
2021
Findings of microplastics and nanoplastics from diverse natural environments have increased demand for research of the fate and transport of the potentially toxic plastic particles in soils and groundwater. Weathering of microplastics would generate a significant amount of nanoplastics, but nanoplastics research is scarce because of technical difficulties in detecting nanoplastics in environments and analyzing nanoplastics adsorption to mineral surfaces. In the current study, we tested a possibility using quartz crystal microbalance (QCM) for application to nanoplastics adsorption analysis on mineral surfaces. In silica (SiO2)-packed column experiments, a measurable adsorption capacity for polystyrene nanoparticles often requires injection of unrealistically high ionic strengths or concentrated nanoplastic particles. The current test shows that QCM can measure polystyrene nanoplastics adsorbed onto SiO2 surface under the low ionic strengths and nanoplastics concentrations, where typical column experiments cannot. QCM is a promising tool for understanding the interaction between nanoplastics and mineral surfaces and thus transport of nanoplastics in soils and groundwater.
Quartz (SiO2) is among the major rock-forming minerals in the earth's crust. The atomistic structures of SiO2 may evolve during diverse frictional processes. The reduction of friction of quartz-rock accompanied by its amorphization, hydration, and formation of silica gel provides mineralogical insights into earthquakes and related phenomena. Ball milling, together with rotary shear experiments have been useful to infer the atomic origins of such processes. In this study, optimal experimental conditions for ball milling for amorphization of SiO2 were determined by taking into account various process variables. The crystallinity of SiO2 gradually decreased and became amorphous as the ball milling time increased at a high milling speed. The degree of wear of the milling media and its effect on the amorphization of SiO2 were analyzed using distinct milling materials (zirconia, stainless steel). The amount of ball wear increased with increasing milling time. Furthermore, the worn stainless steel particles from balls tend to interact with amorphized SiO2 to form Si-O-Cr. These results aid in understanding the process of atomistic structural changes caused by ball milling of divserse materials with relatively high hardness, such as SiO2, and understanding various geological friction processes.
The objectives of this study were to characterize the physicochemical properties and mineralogy of Hwangto (yellow residual soils) from the southwestern part of Korea and to understand the soil-forming processes of the residual soils from their parent rocks. Both the yellowish residual soils as well as the unweathered and weathered parent rocks were obtained from Jangdong-ri, Donggang-myun, Naju, Jeollanam-do, Korea. The soil samples were examined to analyze the said soil's physicochemical properties such as color, pH, and particle size distribution. A scanning electron microscopy (SEM) with energy dispersive X-ray (EDX) analysis, transmission electron microscopy (TEM) and X-ray diffraction (XRD) analysis were performed in order to understand the mineralogy, chemical composition, and morphology of the soils. Two thin sections of a parent rock were analyzed to study its mineral composition. A particle size analysis of the soils indicates that the residual soil consists of mainly silt and clay (approximately 95%) and that soil textures are silty clay or silt clay loam. The soil colors of the residual soil are dark brown (7.5YR 3/4) through yellowish red (5YR 4/6). The pH of the residual soil ranges from 4.3 to 5.1. The major minerals of the parent rocks were quartz, biotite, chlorite, and plagioclase. The mineralogy of the sand fraction of the residual soil was quartz, biotite, muscovite and sanidine. The mineralogy of the silt fraction of the residual soil was quartz, biotite, muscovite, Na-feldspar, K-feldspar, and sanidine. The clay mineralogy of the soil was goethite, kaolinite, ilite, hydroxy-interlayed vermiculite(HIV), vermiculite, mica, K-feldspar and quartz. The mineral composition of the residual soil and the parent rock indicates that feldspar and mica in the parent rock weathered into illite, vermiculite and hydroxy-interlayed vermiculite(HIV), and finally changed into kaolinite and halloysite in the yellowish residual soils.
Nano-sized iron colloids are formed as acid mine drainage is exposed to surface environments and is introduced into surrounding water bodies. These iron nanomaterials invoke aesthetic contamination as well as adverse effects on aqueous ecosystems. In order to control them, the characteristics of their behaviour should be understood first, but the cumulative research outputs up to now are much less than the expected. Using zero-valent iron (ZVI) and magnetite, this study aims to investigate the behaviour of iron nanomaterials according to the change in the composition and pH of background electrolyte and the concentration of natural organic matter (NOM). The size and surface zeta potential of iron nanomaterials were measured using dynamic light scattering. Characteristic behaviour, such as aggregation and dispersion was compared each other based on the DLVO (Derjaguin, Landau, Verwey, and Overbeek) theory. Whereas iron nanomaterials showed a strong tendency of aggregation at the pH near point of zero charge (PZC) due to electrostatic attraction between particles, their dispersions became dominant at the pH which was higher or lower than PZC. In addition, the behaviour of iron nanomaterials was likely to be more significantly influenced by cations than anions in the electrolyte solutions. Particularly, it was observed that divalent cation influenced more effectively than monovalent cation in electrostatic attraction and repulsion between particles. It was also confirmed that the NOM enhanced the dispersion nanomaterials with increasing the negative charge of nanomaterials by coating on their surface. Under identical conditions, ZVI aggregated more easily than magnetite, and which would be attributed to the lower stability and larger reactivity of ZVI.
In this study we propose that the ‘enclaves’ which occur in the granites should be translated into ‘Po-yu-am’in Korean. Also we suggest some criteria to discriminate the mafic microgranular enclaves (MME) of igneous origin from the xenoliths, which possibly come from the plutonic, volcanic and sedimentary country rocks. The color of the MME is gray green∼dark gray and the mineral grains are fine and equigranular. The MME are generally of ellipsoidal shape and can be easily found within the granites. They do not show any evidence of contact metamorphism by granite host. On the other hand. the xenoliths are generally of angular shape and are of the same mineral assemblage and texture as the country rocks around the granites. The distribution of the xenoliths is mostly concentrated along the intruding plane of the granites near the country rocks. The xenoliths were partly metamorphosed by the granite intrusion. The xenoliths from the plutonic rocks are easily distinguished from the MME in terms of their angular shape and coarser grain size, but they do not have any metamorphic mineral assemblage and texture. The xenoliths from the tuffaceous rocks show angular shape and porphyritic and pyroclastic textures. Large size xenoliths from the sedimentary rocks specifically preserve bedding structure which are indicative of the sedimentary strata. However, the sedimentary xenoliths of small size are often difficult to distinguish from the MME. Metamorphic minerals and texture are a useful key to discriminate the small-sized sedimentary xenoliths from the MME. In summary the xenoliths in the granites can be megascopic ally distinguished from the MME by comparing their color, shape, grain size and remnant original structure like bedding. Additionally the metamorphic mineral assemblage and texture are microscopic discriminators between the xenoliths and the MME in the granites.
The Sea:JOURNAL OF THE KOREAN SOCIETY OF OCEANOGRAPHY
/
v.18
no.3
/
pp.122-130
/
2013
To examine floc characteristics of cohesive bed sediment of the Yeongsan River estuary, a floc camera system has been developed and utilized to observe flocs under varying conditions. In order to validate the floc camera system, sand particles were passed through 88-125 and $63-88{\mu}m$ sieves and observed within the laboratory. Mean grain size and settling velocities were found to be 102 and $56.2{\mu}m$ and 6.7 and 5.9 mm/s, respectively. Artifacts of particles estimated outside of the sieve range are attributed to being imaged out of the depth of focus. However, as mean grain size and settling velocity of each size class were within the confidence interval, the floc camera system was confidently used to examine cohesive bed sediments of Yeongsan River estuary. The bed sediment sample was prepared with a concentration of 0.1 g/L in 0 psu deionized water. The mean grain size, settling velocity and fractal dimension of flocs were $40.6{\pm}0.66{\mu}m$, 14 mm/s, and 2.86, respectively. Experiments were also conducted using different salinities (10 and 34 psu) and sediment concentrations (0.1 and 0.3 g/L). Despite changing these parameters, the mean observed grain size and settling velocities were found to be the same within the error range of the system. The relatively higher values of settling velocity and fractal dimension are considered a result of the sediment containing relatively small concentrations of organic matter. Moreover, consistent floc size over various grain sizes and concentrations may be the result of insufficient turbulence to aggregate flocs.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.