Recently, trouble of sand supplying is occurred according to exhaustion of natural sand resources. Therefore various measures are proposed for solution of trouble of sand supply and crushed sand among measures is used as one of most universal measures. But because crushed sand have poor particle shape and plenty of makes micro particle, the quality of concrete using crushed sand deteriorated. Therefore, this study evaluated engineering property of concrete with replacement ratio of crushed sand and EEZ sand and applied evaluation result to fundamental data for quality control of concrete using crushed sand and EEZ sand. The result of this study have shown that quality of concrete using crushed sand and EEZ sand and The compressive strength of concrete up to 50, 70% EEZ sand replacement by crush sand, nearly equal to that of general sand.
경량콘크리트는 자중을 경감할 수 있다는 특징을 활용하여 다양한 용도로 건축 및 토목 구조물에 적용할 수 있다. 그러나 경량콘크리트의 성능은 사용된 경량골재의 물리적 특성에 의해 크게 좌우되어진다. 따라서 본 연구에서는 일반적인 콘크리트의 물결합재비부터 고강도 영역의 낮은 물결합재비까지의 콘크리트 배합범위를 대상으로 하여 국내외에서 제조 생산되고 있는 대표적인 구조용 인공경량골재 3종류의 품질 특성에 따른 경량콘크리트의 프레쉬 및 경화성상의 검토를 하였다. 그 결과 보통콘크리트에 비해 경량골재를 사용한 콘크리트의 경우가 슬럼프 로스가 다소 큰 것을 알 수 있었으며 재령별 강도발현은 보통콘크리트에 비해 경량콘크리트가 다소 낮은 것을 알 수 있으나 큰 차이를 나타내지는 않았다. 경량골재의 비조립형 및 조립형 골재에 따라서는 조립형 경량골재를 사용한 경우 비조립형 보다 양호한 콘크리트 성상을 나타냈으며 향후 철근부착 및 철근정착 등의 구조 부재성능 차원의 검토를 통해 판단될 필요가 있다.
As a part of efforts for conformity of demand to high quality of concrete and for solution of economic problem, blast-furnace slag has been utilized by means of cement replacement. With utilization of blast-furnace slag, superior performance can be ensured, environmental pollution can be prevented and economical advantage can be obtained. But blast-furnace slag has a lot of disadvantages like retardation of strength manifestation etc. in field construction, so properties examination of concrete using blast-furnace slag instead of cement is necessary. For upper necessity, it is planed that basic data for utilization and performance management of blast-furnace slag by means of cement replacement is presented with experimental comparison and investigation of engineering properties of concrete according to the replacement ratio and fineness of blast-furnace slag.
본 연구에서는 황토에 시멘트나 유기계 접착제를 첨가하지 않은 천연재료 황토결합재를 사용하여 황토경화체를 제작하고, 배합조건에 따른 강도성상을 평가하였다. 황토와 석회의 결합재에 천연재료를 첨가할 경우 사용한 천연재료는 모두 물리적 성능을 개선하는 효과가 있었다. 천연재료 중에서 석회는 황토경화체의 물성을 증가시키는데 가장 큰 영향을 미치고 있다. 황토경화체의 물리적 특성은 적용한 배합비 중에서 W/B 45%, 단위수량 $285kg/m^3$, 석회첨가율 60%일 때 가장 우수하게 나타나고 있다.
Sewage facilities are positively necessary for environment improvement such as rainwater removal, sewage disposal, preservation of the quality of water and health of the citizens in present-day. Meanwhile, a deterioration of the concrete sewer pipe is increasing rapidly due to the chemical and physical attack and especially biochemical attack that is to say biodeterioration. So, in advanced countries, prediction techniques and corrosion inhibition system for sewer concrete are developed and are being applied. Also, antibiotics were developed already but application of that is low because it is not economical and has no practical use. But, in domestic, countermeasures for the corrosion of sewage concrete are not sufficient and biochemical attack is not reflected in those essentially. In this study, to prevent biochemical corrosion of the sewer concrete, surface of the concrete was spread with liquefied inorganic antibiotics and then its engineering properties were experimentally investigated. As a result, compressive strength of the specimen spread with antibiotics were similar to those of non spread, Both bond strength and abrasion amount of the specimen spread with antibiotics were inferior to non spread. Properties of absorption and air permeability of the specimen spread with antibiotics were superior to non spread. Finally, carbonation depth, chloride ion penetration depth and weight change ration of the specimen spread with antibiotics were smaller than non spread.
본 연구에서는 유물의 보존 처리 과정에서 결손 부위의 복원을 위해 적용 가능한 다목적용 복원재료로써 Epoxy Putty를 개발하고자 하였다. 기존에 사용되고 있는 재료의 물성에서 드러난 높은 강도로 인한 가공성의 문제, 작업 과정 중 긴 경화 시간으로 인한 처짐 현상, 도구나 장갑에 묻어 유물의 표면을 오염시키는 등의 문제점을 해결하기 위해, 1차적으로 현재 많이 사용되고 있는 Epoxy Putty 형태의 복원 재료 물성을 파악한 후 이를 비교 대상으로 선택하여 경화제와 충전제의 종류에 따른 Epoxy Putty를 개발하였다. 개발 된 Epoxy Putty는 기존 재료의 문제점 해결 및 유사한 물성을 지니기 위해 성상(性狀)이 다른 2종의 경화제를 선정하여 물성 실험을 실시하였다. 경화제로는 Mercaptan 계열의 경화제와 Aliphatic amine 계통의 경화제 2종을 선택하여 개발하였다. 연구 결과 2종 모두 Paste 형태로 경화 시간은 5~10분 내외로 기존 재료에 비해 약 3~10배 정도 짧아 작업의 편리성을 높였으며, 가공성을 높이기 위한 마모율은 약 3배 정도 향상시켜 쉽게 사용할 수 있도록 하였으며, 작업 중 발생하는 표면 오염 등의 단점을 보완하기 위해 충전제로 백색의 Micro-balloon을 첨가하여 사용 중 손에 묻어 나오는 끈적거리는 현상을 줄여주었을 뿐만 아니라 Coloring, 경량성, 절삭력 등이 높은 저수축 및 가공성이 우수한 다목적 복원 재료를 개발하였다.
최근 $CO_2$ 배출의 저감을 위한 활동으로 시멘트의 사용량을 줄이고, 고로슬래그 및 플라이 애시 등과 같은 산업부산물을 적극 활용하여 건설분야에 적용하고자 하는 움직임이 활발하게 진행되고 있으며, 이를 통해 환경부하저감 및 자원재활용을 도모하고 있다. 이에 본 연구에서는 자원재이용 및 환경부하저감을 위한 기초적 연구로서 고로슬래그 및 플라이 애시를 사용하여 부산물의 치환율에 따른 경화성상 및 내구성상을 비교 분석하고 고로슬래그와 플라이애시의 3성분계를 치환한 콘크리트 성상을 검토함으로서 결합재로서의 상성관계를 평가하여 향후, 대량활용을 위한 기초자료를 제시하고자 하였다. 고로슬래그 미분말 및 플라이애시를 대체한 콘크리트의 압축강도는 재령 7일 초기강도에서는 무혼입 콘크리트에 비해 현저히 낮은 수준으로 발현하고 있으나, 28일 이후에는 무혼입 콘크리트에 비해 유사하거나 높은 압축강도를 발현하였다. 또한 고로슬래그 미분말의 대체율이 증가함에 따라 염해 저항성이 향상되는 것으로 나타났으며, 이는 기존 연구결과에 따라 고로슬래그 미분말에 의해 염화물 이온이 콘크리트 표면에 고정화됨으로서 염해 저항성이 향상되는 것으로 판단된다.
The performance of concrete mainly depend upon its water-cement ratio. If water percentage is excess in concrete, it may cause the degradation of performance. Because of these reasons, the change of water content is managed by using various evaluation method of unit water content. And criterion for the change of water content is regulated and used. However the criterion is set only considering production error and measurement error but criterion does not consider performance degradation of concrete. Therefore this study tries to investigate degradation of performance while adding extra water by artificial manipulation or management error in concrete, The contents of extra water for tests are set as 0, 20, 40, 60kg/m3, to examine the performance degradation of concrete, strength, shrinkage, cracks, carbonation are tested This study conclude that, when extra water content is excess than 20kg/m3 in concrete, then performance level of concrete declined rapidly. 80 it is very important to maintain quality of concrete for its better performance.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.