• Title/Summary/Keyword: $Y_2O_3$ powder

Search Result 2,384, Processing Time 0.029 seconds

Improvement of Powder Feeding Characteristics of Fine$5\mu\textrm{m}$ $Al_2O_3$ Powder by Modification of the Powder Feeding Systems and Characterization of the Coating Layer depending on Plasma Spraying Conditions (분말송급장치의 개조에 의한 미세$5\mu\textrm{m}$ $Al_2O_3$분말의 송급 특성개선 및 플라즈마 용사조건에 따른 코팅층의 특성분석)

  • 설동욱;김병희;정민석;임영우;서동수
    • Journal of Welding and Joining
    • /
    • v.15 no.1
    • /
    • pp.116-124
    • /
    • 1997
  • A scope of this study is to establish the optimum plasma spray conditions for fine ($5\mu\textrm{m}$) $Al_2O_3$ powder. However, the flowability of the $Al_2O_3$ powder is not so good because of irregular particle shape and fine particle size. Therefore, powder feeding system was modified by 1) change of powder feeding line material from polymer to copper 2) shorten the powder feeding tube length 3) heating the powder feeding system to $80^{\circ}C$4) vibrating the powder feeding line continuously, in order to feed the fine powder homogeneously. The homogeneous powder feeding conditions were obtained with the modified powder feeding system by controlling the powder carrier gas flow and the powder flow rate indicator. The best plasma spraying conditions for the fine $Al_2O_3$ powder were found out as 40kw gun power, 80 g/min. powder feed rate and 50 mm working distance after characterizing the microstructure, hardness and wear loss of the $Al_2O_3$ coating layer.

  • PDF

Changes in the Surface Characteristics of Gas-atomized Pure Aluminum Powder during Vacuum Degassing

  • Yamasaki, Michiaki;Kawamura, Yoshihito
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1039-1040
    • /
    • 2006
  • Vacuum degassing is essential in the preparation of RS P/M aluminum alloys to remove adsorbates and for the decomposition of hydrated-$Al_{2}O_3$ on the powder surface. Changes in the surface characteristics during vacuum degassing were investigated by X-ray photoelectron spectroscopy and temperature-programmed desorption measurement. Hydrated-$Al_{2}O_3$ decomposition to crystalline-$Al_{2}O_3$ and hydrogen desorption on the surface of argon gas-atomized aluminum powder occurred at 623 K and 725 K, respectively. This temperature difference suggests that the reaction converting hydrated-$Al_{2}O_3$ to crystalline-$Al_{2}O_3$ during vacuum degassing should be divided into the two reactions $"2Al+Al_{2}O_3{\cdot}3H_2O\;2Al_{2}O_3+6H_{surf}"and"6H_{surf}3H_2"$.

  • PDF

Hydrothermal Precipitation of PZT Powder (PZT분말의 수열합성에 관한 연구)

  • 이경희;이병하;대문정기;천하희흥지;강원호;박한수
    • Journal of the Korean Ceramic Society
    • /
    • v.24 no.4
    • /
    • pp.397-403
    • /
    • 1987
  • Pb(Zr0.52Ti0.48)O3 powders were prepared by hydrothermal synthesis. Using soluble salts such as Pb(NO3)2, TiCl4 and ZrOCl2$.$8H2O and oxide such as PbO and TiO2 as starting materials, PZT powder was hydrothermally synthesized at the temperature range between 150$^{\circ}C$ and 200$^{\circ}C$. The result showed that reactivity by alkali was decreased in the sequence of Pb(NO3)2, TiCl4, ZrOCl2, PbO, TiO2 and ZrO2. Using the first three soluble salts, PZT powder was synthesiged at 150$^{\circ}C$ for 1hr. In PbO-TiCl4-ZrOCl2 system, PZT powder was synthesized at 150$^{\circ}C$ for 8rs. In Pb(NO3)2-TiO2-ZrOCl2 system, PZT powder was synthesized at 150$^{\circ}C$ for 16hrs, in PbO-TiO2-ZrOCl2 system, the powder was synthesized at 200$^{\circ}C$ for 8hrs.

  • PDF

Powder Chracteristics and Sintering Behavior of $SiO_2$ Coated $BaTiO_3$

  • Park, Jae-Sung;Han, Young-Ho
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1097-1098
    • /
    • 2006
  • The Powder characteristics and sintering behavior of $SiO_2$ coated $BaTiO_3$ were studied. Silica coated $BaTiO_3$ powders were prepared by sol-gel method. The particle size of the $BaTiO_3$ powders were $\sim35$ nm and the thickness of the $SiO_2$ coating layer was $\sim5$ nm. As the $SiO_2$ content increased, the $SiO_2$ layers improved the powder dispersion. The Zeta potential of $SiO_2$ coated $BaTiO_3$ was getting close to that of pure silica with a more negative charge, compared with that of the uncoated $BaTiO_3$. The onset temperature of shrinkage curves shifted to higher temperatures with increasing $SiO_2$ contents

  • PDF

Sintering Properties of Renewed ${Al_2}{O_3}$Ceramics with Particle Size and Addition Amount of Recycling Powder (재활용원료의 첨가량과 입경에 따른 재생 ${Al_2}{O_3}$ 세라믹스의 소결 특성)

  • 신대용;한상목;김경남
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.12
    • /
    • pp.1123-1131
    • /
    • 2001
  • The sintering behaviors of the renewed $Al_2$O$_3$ceramics were investigated as functions of the addition amount and particle size of recycling $Al_2$O$_3$powder, such as crushed powder of structural $Al_2$O$_3$ceramics and waste $Al_2$O$_3$adsorbent, were investigated. Pure $Al_2$O$_3$sample was fabricated by sintered at 1,$650^{\circ}C$ for 5h and it was crushed into powder (-40${\mu}{\textrm}{m}$and +40${\mu}{\textrm}{m}$ in particle size) by thermal shock treatment and crushing. Then, 10~50wt% of crushed $Al_2$O$_3$powder and waste $Al_2$O$_3$adsorbent were mixed with pure $Al_2$O$_3$powder and were subjected to re-sintering to renewed $Al_2$O$_3$sample. The density and the 3-point bending strength increased with increasing the sintering temperature without regard to the addition amount and particle size of recycling $Al_2$O$_3$powder, and that of the samples at the same sintering temperature decreased with increasing the addition amount and particle size of recycling $Al_2$O$_3$powder. Samples over 200 Mpa of 3-point bending strength were obtained by mixing ~30wt% of crushed $Al_2$O$_3$powder(-40${\mu}{\textrm}{m}$), ~20wt% of crushed $Al_2$O$_3$powder (+40${\mu}{\textrm}{m}$) and 10wt% of waste $Al_2$O$_3$adsorbent. 5~20wt% of waste glass powder containing renewed $Al_2$O$_3$samples for densification were fabricated by sintered at 1200~1$650^{\circ}C$ for 5h. The temperature of maximum density and 3-point bending strength decreased with increasing the addition amount of waste glass powder, however, these samples at above 140$0^{\circ}C$ showed lower density and bending strength than renewed $Al_2$O$_3$samples. The addition of waste glass powder did not improved the densification of renewed $Al_2$O$_3$sample.

  • PDF

Microstructures and Texture of Al/Al2O3 Composites Fabricated by a Powder-in Sheath Rolling Method (분말시스압연법에 의해 제조한 Al/Al2O3 복합재료의 미세조직 및 집합조직)

  • 이성희;이충효
    • Journal of Powder Materials
    • /
    • v.10 no.2
    • /
    • pp.103-107
    • /
    • 2003
  • Aluminum-based $Al/Al_2O_3$ composites were fabricated by a powder-in sheath rolling method. A stainless steel tube with outer diameter of 12 mm and wall thickness of 1 mm was used as a sheath. A mixture of aluminum powder and $Al_2O_3$ particles of which volume content was varied from 5 to 20%, was filled in the tube by tap filling and then rolled by 75% reduction in thickness at ambient temperature. The rolled specimen was then sintered at 56$0^{\circ}C$ for 0.5 h. The mixture of Al powders and $Al_2O_3$ particles was successfully consolidated by the sheath rolling. The $Al/Al_2O_3$ composite fabricated by the sheath rolling showed a recrystallized structure, while unreinforced Al powder compact fabricated by the same procedure showed a deformed structure. The unreinforced Al powder compact was characterized by a deformation (rolling) texture of which main component is {112}<111>, while the $Al/Al_2O_3$ composite showed a mixed texture oi deformation and recrystallization. The sintering resulted in recrystallization in Al powder compact and grain growth in the composite.

RECYCLING PROCESS OF U3O8 POWDER IN MnO-Al2O3 DOPED LARGE GRAIN UO2 PELLETS

  • Oh, Jang Soo;Kim, Dong-Joo;Yang, Jae Ho;Kim, Keon Sik;Rhee, Young Woo;Koo, Yang-Hyun
    • Nuclear Engineering and Technology
    • /
    • v.46 no.1
    • /
    • pp.117-124
    • /
    • 2014
  • The effect of various process variables on the powder properties of recycled $U_3O_8$ from MnO-$Al_2O_3$ doped large grain $UO_2$ pellets and the effect of those recycled $U_3O_8$ powders on the sintered density and grain size of MnO-$Al_2O_3$ doped large grain $UO_2$ pellets have been investigated. The evolution of morphology, size, and BET surface area of the recycled $U_3O_8$ powders according to the respective variation of the thermo-mechanical treatment variables of oxidation temperature, powder milling, and sequential cyclic heat treatment of oxidation and then reduction was examined. The correlation between the BET surface area of recycled $U_3O_8$ powder and the sintered pellet properties of MnO-$Al_2O_3$ doped pellets showed that the pellet density and grain size of doped pellets were increased and then saturated by increasing the BET surface area of the recycled $U_3O_8$ powder. The density and grain size of the pellets were maximized when the BET surface area of the recycled $U_3O_8$ powder was in the vicinity of $3m^2/g$. Among the process variables applied in this study, the cyclic heat treatment followed by low temperature oxidation was a potential process combination to obtain the sinter-active $U_3O_8$ powder.

Mechanical Properties of Al/Al2O3 Composite Fabricated by a Powder-in Sheath Rolling Method (분말시스압연법에 의해 제조된 Al/Al2O3 복합재료의 기계적 성질)

  • 이성희;이충효
    • Journal of Powder Materials
    • /
    • v.10 no.2
    • /
    • pp.97-102
    • /
    • 2003
  • The powder-in sheath rolling was applied to the fabrication of $Al/Al_2O_3$ composite. A stainless steel tube with outer diameter of 12 mm and wall thickness of 1 mm was used as a sheath. Mixture of aluminum powder and $Al/Al_2O_3$ particles of which volume content was varied from 5 to 20 vol.% was filled in the tube by tap filling and then rolled to 75% reduction at ambient temperature. The re]]ed specimen was sintered at 56$0^{\circ}C$ for 0.5 hr. The $Al/Al_2O_3$ composite fabricated by the sheath rolling and subsequent sintering showed the relative density higher than 0.96. The tensile strength of the composite increased with the volume content of $Al_2O_3$ particles, and it reached a maximum of 90 MPa which is 1.5 times higher than unreinforced material. The elongation decreased with the volume content of $Al_2O_3$ particles. It is concluded that the powder-in sheath rolling is an effective method for fabrication of $Al/Al_2O_3$ composite.

Microstructure and Properties of Nano-Sized Ni-Fe Alloy Dispersed Al2O3 Composites (Ni-Fe 합금입자 분산 Al2O3 나노복합재료의 미세조직 및 특성)

  • 남궁석;정재영;오승탁;이재성;이홍재;정영근
    • Journal of Powder Materials
    • /
    • v.9 no.3
    • /
    • pp.161-166
    • /
    • 2002
  • Processing and properties of $Al_2O_3$ composites with Ni-Fe content of 10 and 15 wt% were investigated. Homogeneous powder mixtures of $Al_2O_3$/Ni-Fe alloy were prepared by the solution-chemistry route using $Al_2O_3$, $Ni(NO_3)_2{\cdot}6H_2O$ and $Fe(NO_3)_3{\cdot}9H_2O$ powders. Microstructural observation of composite powder revealed that Ni-Fe alloy particles with a size of 20nm were homogeneously dispersed on $Al_2O_3$ powder surfaces. Hot-pressed composites showed enhanced fracture toughness and magnetic response. The properties are discussed based on the observed microstructural characteristics.

Fabrication of Mo-Cu Powders by Ball Milling and Hydrogen Reduction of MoO3-CuO Powder Mixtures (MoO3-CuO 혼합분말의 볼 밀링 및 수소분위기 열처리에 의한 Mo-Cu 복합분말 제조)

  • Kang, Hyunji;Oh, Sung-Tag
    • Journal of Powder Materials
    • /
    • v.25 no.4
    • /
    • pp.322-326
    • /
    • 2018
  • The hydrogen reduction behavior of $MoO_3-CuO$ powder mixture for the synthesis of homogeneous Mo-20 wt% Cu composite powder is investigated. The reduction behavior of ball-milled powder mixture is analyzed by XRD and temperature programmed reduction method at various heating rates in Ar-10% $H_2$ atmosphere. The XRD analysis of the heat-treated powder at $300^{\circ}C$ shows Cu, $MoO_3$, and $Cu_2MoO_5$ phases. In contrast, the powder mixture heated at $400^{\circ}C$ is composed of Cu and $MoO_2$ phases. The hydrogen reduction kinetic is evaluated by the amount of peak shift with heating rates. The activation energies for the reduction, estimated by the slope of the Kissinger plot, are measured as 112.2 kJ/mol and 65.2 kJ/mol, depending on the reduction steps from CuO to Cu and from $MoO_3$ to $MoO_2$, respectively. The measured activation energy for the reduction of $MoO_3$ is explained by the effect of pre-reduced Cu particles. The powder mixture, hydrogen-reduced at $700^{\circ}C$, shows the dispersion of nano-sized Cu agglomerates on the surface of Mo powders.