• 제목/요약/키워드: $Y_2O_3$ particles

검색결과 1,458건 처리시간 0.026초

$Al_2O_3/SiC$ Hybrid-Composite에서 SiC에 질화물 코팅의 영향 (The Effect of Nitride Coating on SiC Platelet in $Al_2O_3/SiC$ Hybrid-Composite)

  • 이수영;임경호;전병세
    • 한국세라믹학회지
    • /
    • 제34권4호
    • /
    • pp.406-412
    • /
    • 1997
  • Al2O3/SiC hybrid-composite has been fabricated by the conventional powder process. The addition of $\alpha$-Al2O3 as seed particles in the transformation of ${\gamma}$-Al2O3 to $\alpha$-Al2O3 provided a homogeneity of the microstructure. The grain growth of Al2O3 are significantly surpressed by the addition of nano-size SiC particles. Dislocation were produced due to the difference of thermal expansion coefficient between Al2O3 and SiC and piled up on SiC particles in Al2O3 matrix, resulting in transgranular fracture. The high fracture strength of the composite was contributed to the grain refinement and the transgranular fracture mode. The addition of SiC platelets to Al2O3/SiC nano-composite decreased the fracture strength, but increased the fracture toughness. Coated SiC platelets with nitrides such as BN and Si3N4 enhanced fracture toughness much more than non-coated SiC platelets by enhancing crack deflection.

  • PDF

Al2O3와 SiC 강화재가 첨가된 Al-Cu 기지 복합재료의 소결, 재압축 및 기계적 특성에 관한 연구 (Study on the Sintering, Repressing and Mechanical Properties of Al2O3 and Al-Cu-SiC Composites)

  • 박정수;이성규;안재환;정형식
    • 한국분말재료학회지
    • /
    • 제11권2호
    • /
    • pp.171-178
    • /
    • 2004
  • Effects of liquid phase and reinforcing particle morphology on the sintering of Al-6 wt%Cu-10 vol% $Al_2O_3$ or SiC particles were studied in regards to densification, structure and transverse rupture properties. The Al-Cu liquid phase penetrated the boundaries between the aluminum matrix powders and the interfaces with reinforcing particles as well, indicating a good wettability to the powders. This enhanced the densification during sintering and the resulting strength and ductility. Since most of the copper added, however, was dissolved in the liquid phase and formed a brittle $CuAl_2$ phase upon cooling rather than alloyed with the aluminum matrix, the strengthening effect by the copper was not fully realized. Reinforcing particles of agglomerate type were found less suitable for the liquid phase sintering than solid type particles. $Al_2O_3$ and SiC particles protluced little difference on the sintering behavior but their size had a large effect. Repressing of the sintered composites increased density and bending properties but caused debonding at the matrix-particle interfaces and also fracturing of the particles.

Mo첨가가 $Al_2O_3$ 세라믹스의 미세구조 및 기계적 성질에 미치는 영향 (Effects of Mo Addition on the Microstructures and Mechanical Properties of $Al_2O_3$ Ceramics)

  • 박정현;문성환;백승수;정동익
    • 한국세라믹학회지
    • /
    • 제25권3호
    • /
    • pp.201-206
    • /
    • 1988
  • Mo 입자의 첨가가 Al_2O_3$ 세라믹스의 미세구조와 기계적 성질에 미치는 영향을 알아보기 위하여 평균입경이 2-micron인 Mo와 6-micron인 Mo를 Al_2O_3$에 각 분산시켜 1$600^{\circ}C$, $H_2$ 분위기에서 5시간 소결하였다. Mo는 Al_2O_3$의 입자성장을 억제시켰으며 Mo의 입자가 작을 때 그 효과는 크게 나타났다. 2-micron Mo를 분산한 경우 꺽임강도와 파괴인성은 크게 증가하여하였으며, 6-micron Mo를 분산한 경우 강도는 증가하지 않았으나 파괴인성은 다소 증가하였다. Al_2O_3$-Mo계의 인성증진기구는 균열편향에 의한 파단면의 증가와 미세균열에 의한 균열전파에너지의 분산에 의한 것으로 보인다.

  • PDF

구형 SiO2@Y2O3: Eu 코어-쉘 복합체 형광체 합성 및 특성 (Synthesis and Characterization of Spherical SiO2@Y2O3 : Eu Core-Shell Composite Phosphors)

  • 송우석;양희선
    • 한국세라믹학회지
    • /
    • 제48권5호
    • /
    • pp.447-453
    • /
    • 2011
  • The monodisperse spherical $SiO_2$ particles were overcoated with $Y_2O_3:Eu^{3+}$ phosphor layers via a Pechini sol-gel process and the resulting $SiO_2@Y_2O_3:Eu^{3+}$ core-shell phosphors were subsequently annealed at $800^{\circ}C$ at an ambient atmosphere. The crystallographic structure, morphology, and luminescent property of core-shell structured $SiO_2@Y_2O_3:Eu^{3+}$ phosphors were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), and photoluminescence (PL). The spherical, nonagglomerated $SiO_2$ particles prepared by a Stober method exhibited a relatively narrow size distribution in the range of 260-300 nm. The thickness of phosphor shell layer in the core-shell particles can be facilely controlled by varying the coating number of $Y_2O_3:Eu^{3+}$ phosphors. The core-shell structured $SiO_2@Y_2O_3:Eu^{3+}$ phosphors showed a strong red emission, which was dominated by the $^5D_0-^7F_2$ transition (610 nm) of $Eu^{3+}$ ion under the ultraviolet excitation (263 nm). The PL emission properties of $SiO_2@Y_2O_3:Eu^{3+}$ phosphors were also compared with pure $Y_2O_3:Eu^{3+}$ nanophosphors.

Magnetic and Temperature-Sensitive Composite Polymer Particles and Adsorption Behavior of Emulsifiers and Trypsin

  • Ahmad, Hasan;Rahman, M.Abdur;Miah, M.A. Jalil;Tauer, Klaus
    • Macromolecular Research
    • /
    • 제16권7호
    • /
    • pp.637-643
    • /
    • 2008
  • A combination of magnetic and temperature-responsive properties in the same polymer composites is expected to increase their potential applications in the biomedical field. Accordingly, micron-sized magnetite/polystyrene/poly(2-dimethylaminoethyl methacrylate-ethyleneglycol dimethacrylate), which are abbreviated as $Fe_3O_4$/PS/P (DM-EGDM) composite polymer particles, were prepared by the seeded copolymerization of DM and EGDM in the presence of magnetite/polystyrene ($Fe_3O_4$/PS) particles. $Fe_3O_4$/PS/P(DM-EGDM) composite particles with magnetic properties showed a temperature-sensitive phase transition at approximately $31^{\circ}C$. The adsorption behavior of the low molecular weight emulsifiers and trypsin (TR) as biomolecules were examined on $Fe_3O_4$/PS/P(DM-EGDM) composite polymer particles at different temperatures. The native conformation of TR was followed by measuring the specific activity under various adsorption conditions. The activity of the adsorbed TR on composite polymer particles was higher than those of the tree TR and TR adsorbed on $Fe_3O_4$/PS particles.

1997~2001년 제주도 고산지역 PM2.5 미세분진의 오염 특성 (Pollution Characteristics of PM2.5 Fine Particles Collected at Gosan Site in JeJu Island during 1997~2001)

  • 강창희;김원형;한진석;선우영;문길주
    • 한국대기환경학회지
    • /
    • 제19권3호
    • /
    • pp.263-273
    • /
    • 2003
  • P $M_{2.5}$ fine particles have been collected at the Cosan measurement station in Jeju Island, and the major water-soluble components have been analyzed in order to Investigate the aerosol compositions and pollution characteristics. The mean concentrations of the components were in the order of S $O_4$$^{2-}$> N $H_4$$^{+}$> N $O_3$$^{[-10]}$ > N $a^{+}$> $K^{+}$>C $l^{[-10]}$ >C $a^2$$^{+}$>M $g^2$$^{+}$. The major components were S $O_4$$^{2-}$, N $H_4$$^{+}$ and N $O_3$$^{[-10]}$ , whose compositions were 58%, 18% and 10% of the total ions, respectively. Most of the components showed higher concentrations in spring season, and especially $Ca^2$$^{+}$, N $O_3$$^{[-10]}$ and S $O_4$$^{2-}$ concentrations were increased 2.8, 1.9 and 1.2 times higher than the annual mean concentrations. The most parts of S $O_4$$^{2-}$ and N $H_4$$^{+}$ were distributed in fine particles below 2.1 ${\mu}{\textrm}{m}$ size, but the $Ca^2$$^{+}$, N $a^{+}$ and C $l^{[-10]}$ showed relatively higher concentrations in coarse particles. Based on the factor analysis, the P $M_{2.5}$ fine particles were considered to be largely influenced by anthropogenic sources, and followed by sea salt and soil sources. In the variations of concentrations as a function of wind direction, most components have shown higher concentrations notably as the northwesterly prevails.thwesterly prevails.

분무열분해 공정에서 붕소 농도에 따른 Gd2O3:Eu 형광체의 GdBO3:Eu 형광체로의 전환 (Transition of Gd2O3:Eu Phosphor to GdBO3:Eu Phosphor with Boron Concentration in the Spray Pyrolysis)

  • 구혜영;정대수;주서희;홍승권;강윤찬
    • 한국재료학회지
    • /
    • 제16권3호
    • /
    • pp.163-167
    • /
    • 2006
  • The transition of europium-doped gadolinium oxide phosphor to gadolinium borate phosphor with the concentration of boron in the spray pyrolysis was investigated. The particles prepared from spray solution below 10 wt% boric acid of prepared phosphor had crystal structure of $Gd_2O_3:Eu$ phosphor, in which the crystallinity of the particles decreased with increasing the boron concentration. A single phase $GdBO_3:Eu$ phosphor particles were prepared from spray solution above 50 wt% boric acid of prepared phosphor. The phosphor particles prepared from spray solution with 20 wt% boric acid of prepared phosphor had no XRD peaks of $Gd_2O_3:Eu$ and $GdBO_3:Eu$ Therefore the phosphor particles prepared from spray solution with 20 wt% boric acid of prepared phosphor had the lowest photoluminescence intensity under ultraviolet and vacuum ultraviolet. $GdBO_3:Eu$ and $Gd_2O_3:Eu$ phosphor particles prepared from spray solutions with proper concentrations of boric acid had good photoluminescence intensity under vacuum ultraviolet. The morphology of the phosphor particles were strongly affected by the concentrations of boric acid added into spray solution.

주형법으로 제조된 Gd2O3:Eu3+ 적색 형광체의 나노입자 분산 및 형상제어 (Dispersion and Shape Control on Nanoparticles of Gd2O3:Eu3+ Red Phosphor Prepared by Template Method)

  • 박정민;반세민;정경열;최병기;강광중;김대성
    • 한국재료학회지
    • /
    • 제27권10호
    • /
    • pp.534-543
    • /
    • 2017
  • $Gd_2O_3:Eu^{3+}$ red phosphors were prepared by template method from crystalline cellulose impregnated by metal salt. The crystallite size and photoluminescence(PL) property of $Gd_2O_3:Eu^{3+}$ red phosphors were controlled by varying the calcination temperature and $Eu^{3+}$ mol ratio. The nano dispersion of $Gd_2O_3:Eu^{3+}$ was also conducted with a bead mill wet process. Dependent on the time of bead milling, $Gd_2O_3:Eu^{3+}$ nanosol of around 100 nm (median particle size : $D_{50}$) was produced. As the bead milling process proceeded, the luminescent efficiency decreased due to the low crystallinity of the $Gd_2O_3:Eu^{3+}$ nanoparticles. In spite of the low PL property of $Gd_2O_3:Eu^{3+}$ nanosol, it was observed that the photoluminescent property was recovered after re-calcination. In addition, in the dispersed nanosol treated at $85^{\circ}C$, a self assembly phenomenon between particles appeared, and the particles changed from spherical to rod-shaped. These results indicate that particle growth occurs due to mutual assembly of $Gd(OH)_3$ particles, which is the hydration of $Gd_2O_3$ particles, in aqueous solvent at $85^{\circ}C$.

공침법에 의한 $Ni_2Y$ 자성 분말의 합성 (Synthesis of $Ni_2Y$ magnetic particles by coprecipitation method)

  • 김한근;사공건
    • E2M - 전기 전자와 첨단 소재
    • /
    • 제9권9호
    • /
    • pp.906-910
    • /
    • 1996
  • Ferroxplana N $i_{2}$Y(B $a_{2}$N $i_{2}$F $e_{12}$ $O_{22}$ ) magnetic particles, which is one of the hexagonal ferrite were synthesized by a coprecipitation method. The coprecipitates were prepared by adding aqueous solution of BaC $I_{2}$ - 2 $H_{2}$O, NiC $I_{2}$ - 6 $H_{2}$O and FeC $I_{3}$ - 6 $H_{2}$O(of which the mole ratio is $Ba^{+2}$ : N $i^{+2}$ : F $e^{3+}$= 1 : 1 : 6) to a mixture of NaOH and N $a_{2}$C $O_{3}$. The shape of Ferroxplana N $i_{2}$Y magnetic particles obtained at 1, 100(.deg. C) was hexagonal plate-like, average particle size and aspect ratio were 2(.mu.m) and 7, respectively.y.

  • PDF

침전법으로 제조한 Al2O3-ZrO2-Y2O3계 분말의 특성 (Properties of the Powders of the System Al2O3-ZrO2-Y2O3 Prepared by Precipitation Method)

  • 김준태;홍기곤;이홍림
    • 한국세라믹학회지
    • /
    • 제25권2호
    • /
    • pp.117-124
    • /
    • 1988
  • The properties of the powders of the system Al2O3-ZrO2-Y2O3 prepared by precipitation method were investigated. Al2(SO4)3$.$18H2O3, ZrOCl2$.$8H2O and YCl3$.$6H2O were used as starting materials. Amorphous aluminum hydrate prepared by precipitation method was completely transformed to alpha Al2O3 as a result of calcining at 1100$^{\circ}C$ for 1 hr and gamma, delta and theta phases appeared as transition phases. In ZrO2-Y2O3 system prepared by co-precipitation method, the crystallization temperature of ZrO2 was increase with Y2O3 contents. The coupled crystallization occured in coprecipitated Al2O3-ZrO2-Y2O3 system, therefore the formation temperature of alpha Al2O3 and ZrO2-Y2O3 system. In this ternary system, the powder morphology showed a particular shape which was composed of large Al2O3 grains having small spherical ZrO2 particles within large Al2O3 grain and relatively large ZrO2 particles along the grian boundaries.

  • PDF