This study presents a simple method to control the seed orientation which leads to the various growth characteristics of a single grain REBCO (RE: rare-earth elements) bulk superconductors. Seed orientation was varied systematically from c-axis to a-axis with every 30 degree rotation around b-axis. Orientations of a REBCO single grain was successfully controlled by placing the seed with various angles on the prismatic indent prepared on the surface of REBCO powder compacts. Growth pattern was changed from cubic to rectangular when the seed orientation normal to compact surface was varied from c-axis to a-axis. Macroscopic shape change has been explained by the variation of the wetting angle of un-reacted melt depending on the interface energy between $YBa_2Cu_3O_{7-y}$ (Y123) grain and melt. Higher magnetic levitation force was obtained for the specimen prepared using tilted seed with an angle of 30 degree rotation around b-axis.
$YBa_2Cu_3O_{7-x}$ oxide superconductors were fabricated by the hot isostatic pressing (HIP). It was shown that their structures were orthorombic and constited of a single (123) phase. While as-sintered compacts had many pores, they were remarkably reduced by Hiping. The on-set and off set temperature of (123) compound sintered at $950^{\circ}C$ in oxygen and hiping at $880^{\circ}C$ were the highest and it showed 0 resistance at $90^{\circ}K$. The critical current density ($J_c$) of the above superconductor was $27A/cm^2$ and it also showed a number of twin structures, which are typical of high $T_c$ superconductor. It seemed that the low current density may be due to the many pores of starting-sintered compacts.
We investigated the quench characteristics of thin film type SFCLs with shunt layers of various thickness. The SFCLs ware based on 2 inch diameter YBa$_2$Cu$_3$O$_{7}$ thin films coated in-situ with a gold shunt layer. The shunt layer thickness was varied by Ar ion milling. The limiters were tested with simulated fault currents at various source voltages. The thinner the shunt layer was, the slower was the rise of SFCL temperatures. This means SFCLs of thinner shunt layers had higher voltage ratings. The voltage rating was approximately inversely proportional to the square root of the shunt layer thickness. This result could be understood through the concept of heat balance.e.
Step-edge Josephson junctions (SEJ) have been fabricated on sapphire substrates with in situ deposited films of CeO$_2$ buffer layer and YBa$_2$Cu$_3$O$_{7}$ films on the low angle steps. Direct coupled SQUID magnetometers with the SEJ were formed on 1 cm X 1 cm R-plane sapphire substrates. Typical 5-${\mu}{\textrm}{m}$-wide Josephson junctions have R$_{N}$ of 3 Ω and I$_{c}$ of 50 $mutextrm{A}$ at 77 K. The direct coupled SQUID magnetometers were designed to have pickup coils of 50-${\mu}{\textrm}{m}$-wide 16 parallel loops on the 1 cm X 1 cm substrates with outer dimension of 8.8 mm X 8.8 mm. The SEJ SQUID magnetometers exhibit relatively low 1/f noise even with dc bias control, and could be stably controlled by flux-locked loops in the magnetically disturbed environment. Field noise of the do SQUID was measured to be 200∼300 fT/Hz$^{1}$2/in the white noise region and about 2 pT/Hz$^{1}$2/ at 1 Hz when measured with dc bias method.hod.d.
Ion-beam assisted deposition (IBAD) technology has been successfully applied to high-temperature superconductor coated conductors (CC) as textured substrates. Since the coated conductors were proposed as a potential framework for utilizing the superior transport characteristics of $YBa_2Cu_3O_7$ and related cuprate oxides, several methods including rolling-assisted bi-axial textured substrates (RABiTS) and inclined substrate deposition (ISD), as well as IBAD, have been attempted. As of 2016, most companies that are trying to commercialize CC adapt IBAD technology except for American Superconductors who use RABiTS predominantly. For the materials in the IBAD process, initial efforts to use yttria-stabilized zirconia (YSZ) or related fluorites in Fujikura in Japan have quickly given way to MgO which technique was developed by Stanford University in the USA. In this review, we present a historical overview of IBAD technology, in particular, for the application of CC. We describe the key scientific understanding of nucleation, the texturing mechanism, and the growth of large bi-axial grains and discuss some potential new IBAD materials and systems for large-scale production.
한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
/
pp.91-94
/
1999
A new type of high-T$_c$ superconducting Josephson junctions has been prepared by Ar ion beam etching and electron beam lithography. YBa$_2Cu_3O_{7-x}$ (YBCO) films deposited on (001) SrTiO$_3$ single crystal substrate by pulsed laser deposition were patterned by Ar ion milling with photolithography. The narrow slit with a electroresist mask, about 1000 ${\AA}$ wide, was constructed over a 3 ${\sim}$ 5 ${\mu}$m bridge of a 1200-${\AA}$-thick YBCO film by electron beam lithography. The slit was then etched by the Ar ion beam to form a damaged 600-${\AA}$-thick YBCO. Thus prepared structure forms an S-N-S (YBCO - damaged YBCO - YBCO) type Josephson junctions. Those junctions exhibit RSI-like I-V characteristics at 77 K. The properties of the Josephson junctions such as I$_c$ R$_N$, and J$_c$ were characterized.
We investigated quench distribution in SFCLs of two different sizes. YBa$_2$Cu$_3$O$_{7}$ films coated in-situ with a gold layer were patterned into meander lines of two different sizes by photolithography. The limiters were tested with simulated fault currents at various source voltages. The values of resistivity and their time dependence were similar at similar electric fields. The resistivity was nearly uniform except at the edges in both smaller and larger SFCLs. In particular, the resistivity gradient was smaller in larger SFCLs. However, differences between stripe resistivities were larger in larger SFCLs. The results were quantitatively explained with a heat transfer concept.t.
We investigated the properties of a hybrid type superconducting fault current limiter (SFCL), which consists of a transformer with multiple secondary windings and resistive $YBa_2Cu_3O_7$ (YBCO) thin film stripes. The secondary windings of the transformer were coupled with each other, and a superconducting current limiting unit of YBCO stripes was connected to each of them as a switch. Simple connection in series of SFCL units tends to produce imbalance in power among the units due to slight differences in quench current. In current design, magnetic coupling between the SFCL units provides a solution to power dissipation imbalance, inducing simultaneous quench by current redistribution in the YBCO films.
The combination of methane-chemical activation and Self-propagating High-temperature synthesis (SHS) has widened the possibilities for both methods. For YBCO systems the investigation showed that a short-term mechano-chemical activation of initial powders before SHS leads to single-phase and ultra-fine products. A new technique for preparation ultra-fine high-temperature superconductors of YBCO composition with a grain size d < $1{\mu}m$ is developed. The specific feature of the technique is formation of the $YBa_2Cu_3O_{7-x}$ crystalline lattice directly from an X-ray amorphous state arising as a result of mechanical activation of the original oxide mixture. The technique allows the stage of formation of any intermediate reaction products to be ruled out. X-ray and magnetic studies of ultra-fine high temperature superconductors (HTS) are carried out. Dimension effects associated with the microstructure peculiarities are revealed. A considerable enhancement of inter-grain critical currents is found to take place in the ultra-fine samples investigated.
Dual mode ring resonators(DMRR) have been fabricated using laser ablated $YBa_2Cu_3O_{7-x}$ superconducting thin films. The transition temperature of YBCO thin films were 85 - 88 K and the film thicknesses were about 5,000 $\AA$. Dual mode ring resonators were patterned by standard photolithography process and wet-etching. Then two-layer metal thin films (Ti/Ag) have been deposited for the ground plane on the back side of substrate by e-beam and thermal evaporation. The input/output feedline angles of each resonator were $60^{\circ}$, $100^{\circ}$, $180^{\circ}$. A network analyzer was used for testing the performance of the resonators in the frequency range of 6-13 GHz at 77 K.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.