• Title/Summary/Keyword: $UV/H_2O_2$ process

Search Result 195, Processing Time 0.033 seconds

Photo Catalytic Ability of Acicular Shaped TiO$_{2}$ Rutile Powder in Aqueous Metal-EDTA Solutions

  • Kim, Sun-Jae;chang-Joo choi;Park, Soon-Dong;Hwang, Jong-Sun;Han, Byung-Sung
    • Transactions on Electrical and Electronic Materials
    • /
    • v.2 no.2
    • /
    • pp.37-41
    • /
    • 2001
  • Photo catalytic characteristics of nano-sized TiO$_2$ powder with rutile phase produced using homogeneous precipitation process at low temperatures (HPPLT) were compared with those of commercial P-25 powder by Degussa Co. The TiO$_2$ powder by HPPLT showed very higher photoactivity in the removal rate, showing lower pH values in the solution, than the P-25 powder when eliminating metal ions such as Pb and Cu from aqueous metal-EDTA solutions. This can be inferred the more rapid photo-oxidation or -reduction of metal ions from the aqueous solution, together with relatively higher efficiencies in the use of electron-hole pair formed on the surface of TiO$_2$ particle, under UV light irradiation. Also, in the view of the TiO$_2$ particle morphology, compared to the well-dispersed spherical P-25 particle, the agglomerated TiO$_2$ particle by HPPL T consists of acicular typed primary particle with the thickness ranged of 3∼7 nm, which would be more effective to the photocatalytic reactions without electron-hole recombination on the surface of the TiO$_2$ particle under the UV light irradiation. It is, therefore, thought that the higher photo activity of the rutile TiO$_2$ powder by HPPLT in the aqueous solutions resulted from having its higher specific surface area as well as acicular shape primary particle with very thin thickness.

  • PDF

Semiconductor coupled solar photo-Fenton's treatment of dyes and textile effluent

  • Raji, Jeevitha R.;Palanivelu, Kandasamy
    • Advances in environmental research
    • /
    • v.5 no.1
    • /
    • pp.61-77
    • /
    • 2016
  • $NanoTiO_2$ was synthesized by ultrasonication assisted sol-gel process and subjected to iron doping and carbon-iron codoping. The synthesized catalysts were characterized by XRD, HR-SEM, EDX, UV-Vis absorption spectroscopy and BET specific surface area analysis. The average crystallite size of pure $TiO_2$ was in the range of 30 - 33 nm, and that of Fe-$TiO_2$ and C-Fe $TiO_2$ was in the range of 7 - 13 nm respectively. The specific surface area of the iron doped and carbon-iron codoped nanoparticles was around $105m^2/g$ and $91m^2/g$ respectively. The coupled semiconductor photo-Fenton's activity of the synthesized catalysts was evaluated by the degradation of a cationic dye (C.I. Basic blue 9) and an anionic dye (C.I. Acid orange 52) with concurrent investigation on the operating variables such as pH, catalyst dosage, oxidant concentration and initial pollutant concentration. The most efficient C-Fe codoped catalyst was found to effectively destruct synthetic dyes and potentially treat real textile effluent achieving 93.4% of COD removal under minimal solar intensity (35-40 kiloLUX). This reveals the practical applicability of the process for the treatment of real wastewater in both high and low insolation regimes.

Photocatalytic Property of Nano-Structured TiO$_2$ Thermal Sprayed Coating - Part II: TiO$_2$ -WO$_3$ Coating - (나노구조 TiO$_2$용사코팅의 미세조직 제어 공정기술 개발과 광촉매 특성평가 - Part II: TiO$_2$- WO$_3$ 코팅 -)

  • 이창훈;최한신;이창희;김형준;신동우
    • Journal of Welding and Joining
    • /
    • v.21 no.4
    • /
    • pp.46-55
    • /
    • 2003
  • TiO$_2$-WO$_3$(8.2wt%) coatings were prepared by the APS (Atmospheric Plasma Spraying) process to clarify the relationship between the process parameters(H$_2$ gas flow rate of plasma 2nd gas and spraying distance) of the APS coating and photo-decomposition efficiency kinetics of the MB(methylene blue) aqueous solution decomposition and to understand the effect of addition of WO$_3$ on photocatalytic properties of TiO$_2$ sprayed coating. Further, the temperature and velocity of flying particles were measured by DPV-2000 to investigate the relationship between microstructure of coatings and process parameters. Properties of coatins were investigated by XRD, SEM, XPS, RAMAN, UV/VIS spectrometer. In case of the TiO$_2$-WO$_3$(8.2wt%) coating, it had a lower anatase fraction than that of pure-TiO$_2$ coatings because of flying in the higher temperature plasma plume by the heavy weight of TiO$_2$, WO$_3$. And, when WO$_3$ added powders were spayed, the doping effects of W ions substituted into the Ti ion sites was not occured during melting and solidification cycles of spraying. It was found that the addition of WO$_3$ was ineffective effective on increasing photo-decomposition efficiency of TiO$_2$ sprayed coating.

Synthesis, Characterization and DNA Interaction Studies of (N,N'-Bis(5-phenylazosalicylaldehyde)-ethylenediamine) Cobalt(II) Complex

  • Sohrabi, Nasrin;Rasouli, Nahid;Kamkar, Mehdi
    • Bulletin of the Korean Chemical Society
    • /
    • v.35 no.8
    • /
    • pp.2523-2528
    • /
    • 2014
  • In the present study, at first, azo Schiff base ligand of (N,N'-bis(5-phenylazosalicylaldehyde)-ethylenediamine) ($H_2L$) has been synthesized by condensation reaction of 5-phenylazosalicylaldehyde and ethylenediamine in 2:1 molar ratio, respectively. Then, its cobalt complex (CoL) was synthesized by reaction of $Co(OAc)_2{\cdot}4H_2O$ with ligand ($H_2L$) in 1:1 molar ratio in ethanol solvent. This ligand and its cobalt complex containing azo functional groups were characterized using elemental analysis, $^1H$-NMR, UV-vis and IR spectroscopies. Subsequently, the interaction between native calf thymus deoxyribonucleic acid (ct-DNA) and CoL complex was investigated in 10 mM Tris/HCl buffer solution, pH = 7 using UV-vis absorption, thermal denaturation technique and viscosity measurements. From spectrophotometric titration experiments, the binding constant of CoL complex with ct-DNA was found to be $(2.4{\pm}0.2){\times}10^4M^{-1}$. The thermodynamic parameters were calculated by van't Hoff equation.The enthalpy and entropy changes were $5753.94{\pm}172.66kcal/mol$ and $43.93{\pm}1.18cal/mol{\cdot}K$ at $25^{\circ}C$, respectively. Thermal denaturation experiments represent the increasing of melting temperature of ct-DNA (about $0.93^{\circ}C$) due to binding of CoL complex. The results indicate that the process is entropy-driven and suggest that hydrophobic interactions are the main driving force for the complex formation.

A Study OH the Character and Activity of $TiO_2$ Photocatalysts Prepared With Various Condition (다양한 조건에서 제조된 $TiO_2$ 광촉매 특성 및 활성에 관한 연구)

  • Kim, Seung-Min;Youn, Tae-Kawun;Hong, Dae-Il;Kim, Sung-Kuk;Park, Sang-Won
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.27 no.9
    • /
    • pp.932-938
    • /
    • 2005
  • [ $TiO_2$ ] nanoparticles were prepared from the precipitation in $TiCl_4$ and the sol-gel profess in $Ti(OC_3H_7)_4$ as starting materials with various synthetic conditions. The samples were characterized by XRD, SEM, and TEM testing techniques. The photocatalytic degradation of congo red has been investigated in $TiO_2/UV$ process to evaluate photocatalytic activities for the samples. $TiO_2$ nanoparticles calcined at $400^{\circ}C$ had the best photocatalytic activity with the rate constant of the degradation of congo red as $0.0319\;min^{-1}$. The rate constant of $TiO_2$ photocatalysts was increased with the calcination temperature under $400^{\circ}C$ and decreased with the calcination temperature upper $400^{\circ}C$. In the case of $TiO_2$ photocatalysts, the photocatalytic activity wasn't greatly affected by the frequencies of usage. In the similar synthesis condition, the degradation efficiency of the $TiO_2$ particle prepared by $TiCl_4$ was increased to 8.8%, when the rate was compared with the sample prepared by $Ti(OC_3H_7)_4$. The photocatalytic activities of $TiO_2$ photocatalysts synthesized by $Ti(OC_3H_7)_4$ with various conditions were also discussed.

The Influence of Current Flow on OH Radical Generation in a Photocatalytic Reactor of TiO2 Nanotube Plates (전류흐름에 따른 TiO2 nanotube 광촉매의 OH radical 생성량 평가)

  • Kim, Da-Eun;Lee, Yong-Ho;Kim, Dae-Won;Pak, Dae-Won
    • Journal of the Korean Applied Science and Technology
    • /
    • v.34 no.2
    • /
    • pp.349-356
    • /
    • 2017
  • OH radical generation is one of the common method to evaluate photocatalytic activity. In many of previous studies, only the UV(Ultraviolet) light was applied to test photocatalytic ability of $TiO_2$ nanotubes by studying probe compound(4-Chlorobenzoic acid) concentration change in solution. Also, $TiO_2$ nanotubes were found to show some electrochemical characteristics when the flow of electric current was applied. In this study, the flow of electric current and UV light were applied at the same time to determine whether electrochemical characteristics of $TiO_2$ nanotube plate can give synergetic effect on the photocatalytic activity. $TiO_2$ nanotube was grown on Ti by anodic oxidation to create $TiO_2$ nanotube plate which can be used as a photocatalyst and a electrode that can undergo AOP(Advanced Oxidation Process) for water treatment. Probe compound solution was prepared using 4-chlorobenzoic acid and $H_2O$ as a solvent. NaCl was added to give conductivity to work as electrolyte. As a result, enough level of electric current flow was found to give synergetic photocatalytic effect which can be used for efficient AOP water treatment method.

Oxidation of Organic Compounds through the Electrochemical Reaction Using $TiO_{2}$ Photocatalytic Membranes ($TiO_{2}$ 광촉매 막의 전기화학 반응에 의한 유기물의 산화)

  • 현상훈;이기홍
    • Membrane Journal
    • /
    • v.6 no.2
    • /
    • pp.101-108
    • /
    • 1996
  • The oxidation/degradation efficiency of formic acid through the photoelectrochemical reaction has been investigated as a basic research in order to develope the process for degrading toxic organic compounds dissolved in water. A $TiO_{2}$ photoelectro-membrane reactor for purification of water, in which filtration as well as photoelectrocatalytic oxidation of organic compounds could be carried out simultaneously, was developed. Porous $SnO_{2}$ tubes prepared by slip casting and commercial porous stainless steel tubes, being electrically conductive, were used as not only supports but also working electrodes. The UV light with the wavelength of 365 nm was applied as a light source for photocatalytic reactions. The photoelectrocatatytic composite membranes were prepared by coating the support surface with the $TiO_{2}$ sol of pH 1.45. The oxidation efficiency of formic acid increased with the reaction time and the applied voltage, but was almost independent of the solution flux. The results showed that more than 90% of formic acid could he dograded at 27V using the $TiO_{2}$/stainless steel composite membrane, while about 77% in case of the $TiO_{2}/SnO_{2}$ Composite membrane. It was also concluded that the oxidation efficiencies of formic acid could be significantly improved by about 6~7 times by the photoelectrochemical reaction in comparison with those by the photocatalytic reaction only.

  • PDF

Properties of ZnO/TiO2 Bilayer Thin Films with a Low Temperature ALD Process (저온 원자층증착법으로 제조된 ZnO/TiO2 나노이층박막의 물성 연구)

  • Noh, Yunyoung;Han, Jeungjo;Yu, Byungkwan;Song, Ohsung
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.6
    • /
    • pp.498-504
    • /
    • 2011
  • We examined the microstructure and optical properties of crystallized ~30 nm-ZnO/~10 nm amorphous $TiO_2$ nano bilayered films as nano electrodes were deposited at extremely low substrate temperatures of $150-210^{\circ}C$. The bilayered films were deposited on silicon substrates with 10 cm diameters by ALD (atomic layer deposition) using DEZn (diethyl zinc(Zn(C2H5)2)) and TDMAT (tetrakis dimethyl-amid $titanium(Ti(N(CH_3)_2)_4)$ as the ZnO and $TiO_2$ precursors, respectively, and $H_2O$ as the oxidant. The microstructure, phase, and optical properties of the bilayered films were examined by FE-SEM, TEM, XRD, AES, and UV-VIS-NIR spectroscopy. FE-SEM and TEM showed that all bilayered films were deposited very uniformly and showed crystallized ZnO and amorphous $TiO_2$ layers. AES depth profiling showed that the ZnO and $TiO_2$ films had a stoichiometric composition of 1:1 and 1:2, respectively. These bilayered films have optical absorption properties in a wide range of ultraviolet wavelengths, 250-390 nm, whereas the single ZnO and $TiO_2$ films showed an absorption range of 350-380nm.

A clean technology development using the molybdenum dissolution reaction with hydrogen peroxide/UV/Ozone ($오존/UV/H_2O_2$를 이용한 몰리브덴(Mo) 용해 반응에 따른 청정기술 개발에 관한 연구)

  • 김재우;홍종순;신대윤
    • Journal of environmental and Sanitary engineering
    • /
    • v.14 no.4
    • /
    • pp.143-149
    • /
    • 1999
  • In the tungsten industry as light source material, tungsten filament which used as light source material could form after molybdenumwire which used as the center supporter for coil shape tungsten wire was removed. This process uses hydrogen peroxide, Ozone and UV(Ultraviolet)Lamp, for the quantity of hydrogen peroxide decrease. The results were as follows : 1. An incandescent electric Lamp type : FL(FL-20) type : A standard of commodity (P.W.: $19{\pm}1.0mg$, $C.R:4.5{\pm}0.3{\Omega}$) 1) Only hydrogen peroxide treated ; Reaction Time : 65Min., P.W.: 18.60mg, $C.R.:4.60{\Omega}$ 2) Ozone/Ultraviolet/70% of hydrogen peroxide; Reaction Time : 64Min., P.W.: 18.61mg, C.R.: $4.61{\Omega}$ 2. A Fluorescent Lamp Type : GLS(GLS-40) Type : A standard of commodity(P.W.: $11.8{\pm}0.2mg$$65{\pm}1.5{\Omega}$) 1) Only hydrogen peroxide treated ; Reaction Time: 72Min, P.W.:11.88mg, C.R.: $65.62\Omega$ 2) Ozone/Ultraviolet/70% of hydrogen peroxide;Reaction Time:71Min., P.W.:11.88mg, C.R.: $65.63\Omega$

  • PDF

Treatment Characteristics of 1,4-Dioxane by Advanced Oxidation Process System (AOP에 의한 1,4-다이옥산의 처리 특성에 관한 연구)

  • Lee, Soo;Kang, Hak-Su;Choi, Jae-Hyuk
    • Journal of the Korean Applied Science and Technology
    • /
    • v.25 no.1
    • /
    • pp.32-40
    • /
    • 2008
  • 1,4-Dioxane is an EPA priority pollutant often found in contaminated ground waters and industrial effluents. Conventional water treatment techniques are limited to decompose this compound effectively. Therefore, an advanced oxidation process system (AOP) was used for the degradation of 1,4-dioxane. This research investigates the effect of adding oxidants, such as ozone, air, and $H_2O_2$ during the UV irradiation of 1,4-dioxane solution. In order to analyze 1,4-dioxane, a modified 8270 method, which is an improved method of U.S EPA 8720, was used. Degradation efficiencies of 1,4-dioxane by only UV irradiation at various temperatures were not significant. However, The addition of oxidants and air bubbling in the UV irradiation system for 1,4-dioxane decomposition showed the higher 1,4-dioxane degradation rate. And, during AOP treatment the tendency of TOC changes was similar to that of 1,4-dioxane decomposition rate.