0.5$Ba_2Ti_9O_{20}$-0.5Mg$TiO_3$ 세라믹스의 마이크로파 유전특성 (Microwave Dielectric Properties of 0.5$Ba_2Ti_9O_{20}$-0.5Mg$TiO_3$ Ceramics)

  • 김재식;최의선;임성수;정장호;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2002년도 하계학술대회 논문집 C
    • /
    • pp.1491-1493
    • /
    • 2002
  • The 0.5$Ba_2Ti_9O_{20}$-0.5Mg$TiO_3$ ceramics were prepared by the conventional mixed oxide method. The structural properties were investigated with sintering temperature by XRD. According to the X-ray diffraction patterns, major phases of the 0.5$Ba_2Ti_9O_{20}$-0.5Mg$TiO_3$ ceramics were coexisted. Also the secondary phase of Mg$Ti_2O_5$, Ba$Mg_6Ti_6O_{19}$ and the unreacted $TiO_2$ phase were existed. In the case of 0.5$Ba_2Ti_9O_{20}$-0.5Mg$TiO_3$ ceramics sintered $1350^{\circ}C$, dielectric constant, quality factor and temperature coefficient of resonant frequency were 33.7, 54,900GHz, -12.5ppm/$^{\circ}C$, respectively.

  • PDF

솔젤법으로 제작한 $TiO_2-V_2O_5$ 세라믹스의 물성 (Properties of $TiO_2-V_2O_5$ Ceramics Prepared by Sol-Gel Method)

  • 유도현
    • 전기학회논문지
    • /
    • 제56권7호
    • /
    • pp.1255-1260
    • /
    • 2007
  • [ $TiO_2-V_2O_5$ ] sol was prepared using sol-gel method. Sol changed to gel with hydrolysis and polymerization. DTA properties of gel powder had endothermic reaction due to evaporation of propanol about $80^{\circ}C$, had exothermic reaction due to combustion of propanol about $230^{\circ}C$ and had exothermic reaction due to combustion of alkyl group about $350^{\circ}C$. Crystalline properties of gel powder retained amorphous phase at $50^{\circ}C$, retained anatase phase from $400^{\circ}C\;to\;600^{\circ}C$ and had all rutile phase over $700^{\circ}C$ at 0.01mole $V_2O_5$ additive. The capacitance of thin films increased with increasing heat treatment temperature and thin films had best properties at $700^{\circ}C$. The capacitance of thin films increased a lot with decreasing measurement frequency.

TiO2 전극 표면의 전자상태 계산 (Calculation on Surface Electronic State of $TiO_2$ Electrode)

  • 이동윤;이원재;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.1
    • /
    • pp.259-262
    • /
    • 2003
  • The surface electronic state of rutile $TiO_2$, which is an oxide semiconductor and has a wide band gap of 3.1 $\sim$ 3.5 eV, was calculated by DV-$X_{\alpha}$ method, which is a sort of the first principle molecular orbital method and uses Hartre-Fock-Slater approximation. The $[Ti_{15}O_{56}]^{-52}$ cluster model was used for the calculation of bulk state and the $[OTi_{11}O_{34}]^{-24}$ model for the surface state calculation. After calculations, the energy level diagrams and the deformation electron density distribution map were compared in both models. As results, it was identified that the surface energy levels are found between the valence and conduction band of bulk $TiO_2$ on the surface area. The energy values of these surface-induced levels are lower than conduction band of bulk $TiO_2$ by 0.1 $\sim$ 1 eV. From this fact, it is expected that the surface energy levels act as donar levels in n-type semiconductor.

  • PDF

$TiO_2$ 첨가에 따른 $Mg_4Ta_2O_9$ 세라믹스의 마이크로파 유전특성과 유전체 공진기 거동에 관한 연구 (Study on the Microwave Dielectric Properties and Dielectric Resonator Performance of the $Mg_4Ta_2O_9$ Ceramics with $TiO_2$ Addition)

  • 최의선;류기원;이영희;김재식
    • 전기학회논문지
    • /
    • 제56권4호
    • /
    • pp.756-760
    • /
    • 2007
  • The $(1-x)Mg_4Ta_2O_9-xwt%TiO_2\;(x=5\sim20)$ microwave dielectric ceramics were prepared by solid-state reaction method and sintered at $1450^{\circ}C$. According to the X-ray diffraction data, the $Mg_4Ta_2O_9-xwt%TiO_2$ ceramics had main phase of $Mg_4Ta_2O_9$ and $MgTi_2O_5$ peaks were added by increasing of $TiO_2$ addition. Microwave dielectric properties of the $Mg_4Ta_2O_9-xwt%TiO_2$ ceramics were influenced by $MgTi_2O_5$ phase and properties of $TiO_2$. There was a little decrement of the quality factor from 116,800GHz of pure $Mg_4Ta_2O_9$ to 100,100GHz of 15wt% $TiO_2$ added one. But there was excellent improvement in temperature coefficient of the resonant frequency (TCRF) by addition of 15wt% $TiO_2$. The dielectric constant quality factor and TCRF of the $Mg_4Ta_2O_9-xwt%TiO_2$ ceramics sintered at $1450^{\circ}C$ were $13.08\sim16.41,\;45,000\sim165,410GHz,\;-24.82\sim+3.88ppm/^{\circ}C$, respectively, depending on the value of x. Simulated dielectric resonator (DR) with $Mg_4Ta_2O_9-15wt%TiO_2$ ceramics had the operating frequency of 11.97GHz and $S_{2,1}$ of -35.034dB.

$TiO_2-Nb_2O_5$ 솔의 물성에 대한 분석 (Analysis on Properties of $TiO_2-Nb_2O_5$ Sol)

  • 유도현
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제55권7호
    • /
    • pp.349-353
    • /
    • 2006
  • [ $TiO_2-Nb_2O_5$ ] sol was prepared using sol-gel method. Crystalline properties of gel powder changed from rutile phase to anatase phase with increasing $Nb_2O_5$ additives at $800^{\circ}C$, while they retained rutile phase regardless of $Nb_2O_5$ additives at $900^{\circ}C,\;1,000^{\circ}C$. They retained amorphous phase from $50^{\circ}C\;to\;400^{\circ}C$, retained anatase phase from $500^{\circ}C\;to\;600^{\circ}C$ and had rutile phase over $700^{\circ}C$ at 1mole% $Nb_2O_5$ additive. After $TiO_2-Nb_2O_5$ sol retained low viscosity with normal chain structure for a long time, its viscosity increased fast with network structure. DTA properties of gel powder had endothermic reaction due to evaporation of propanol and water about $78^{\circ}C$, had exothermic reaction due to propanol combustion about $290^{\circ}C$ and had exothermic reaction due to changing of $TiO_2$ phase about $640^{\circ}C$.

복합 전기방사법을 이용한 Fe-doped TiO2/α-Fe2O3 이중구조 나노와이어의 합성 및 자성 특성 (Synthesis of Fe-Doped TiO2/α-Fe2O3 Core-Shell Nanowires Using Co-Electrospinning and Their Magnetic Property)

  • 구본율;안효진
    • 한국재료학회지
    • /
    • 제24권8호
    • /
    • pp.423-428
    • /
    • 2014
  • We synthesized Fe-doped $TiO_2/{\alpha}-Fe_2O_3$ core-shell nanowires(NWs) by means of a co-electrospinning method and demonstrated their magnetic properties. To investigate the structural, morphological, chemical, and magnetic properties of the samples, X-ray diffraction, scanning electron microscopy, transmission electron microscopy, and X-ray photoelectron spectroscopy were used, as was a vibrating sample magnetometer. The morphology of the nanostructures obtained after calcination at $500^{\circ}C$ exhibited core/shell NWs consisting of $TiO_2$ in the core region and ${\alpha}-Fe_2O_3$ in the shell region. In addition, the XPS results confirmed the formation of Fe-doped $TiO_2$ by the doping effect of $Fe^{3+}$ ions into the $TiO_2$ lattice, which can affect the ferromagnetic properties in the core region. For comparison, pure ${\alpha}-Fe_2O_3$ NWs were also fabricated using an electrospinning method. With regard to the magnetic properties, the Fe-doped $TiO_2/{\alpha}-Fe_2O_3$ core-shell NWs exhibited improved saturation magnetization(Ms) of approximately ~2.96 emu/g, which is approximately 6.1 times larger than that of pure ${\alpha}-Fe_2O_3$ NWs. The performance enhancement can be explained by three main mechanisms: the doping effect of Fe ions into the $TiO_2$ lattice, the size effect of the $Fe_2O3_$ nanoparticles, and the structural effect of the core-shell nanostructures.

중공구의 크기에 의한 hollow TiO2/polyacrylate 복합체의 열차단 특성 (Effect of Hollow Sphere Size on Heat Shield Properties of hollow TiO2/polyacrylate Composites)

  • 김종석
    • 공업화학
    • /
    • 제32권6호
    • /
    • pp.690-694
    • /
    • 2021
  • 본 연구에서는 글루코스를 전구체로 사용하여 수열합성방법을 통해 구형탄소입자(carbon sphere, CS)를 제조하였다. 200 nm, 500 nm, 1,200 nm 크기의 중공형 TiO2 (H-TiO2)는 CS/TiO2 core-shell 구조를 졸-겔 법과 열처리 방법으로 합성하였다. FE-SEM, HR-TEM, XRD 분석을 통하여 H-TiO2의 물리적 특성을 측정하였다. H-TiO2/polyacrylate (PA) 복합체의 UV-Vis-NIR 분석을 통해 색상변화와 일사반사율을 얻었으며, 실험실에서 제작한 차열온도 측정기를 통해 차열온도를 측정하였다. H-TiO2/PA 복합체는 열전도도가 낮은 건조공기로 채워진 중공구조에 의한 우수한 차열 특성과 근적외선 반사율을 보였다. H-TiO2/PA 복합체에서 중공구의 크기가 증가함에 따라 열차단 특성이 증가하였다. 1,200 nm 중공 크기의 H-TiO2를 혼합한 PA 필름에서 측정된 차열온도가 투명 유리판의 차열온도보다 26 ℃ 감소하였다.

N 도핑된 TiO2 광촉매 박막의 제조 및 특성분석 (Manufacturing and Characterization of N-doped TiO2 Photocatalytic Thin Film)

  • 박상원;남수경;허재은
    • 한국환경과학회지
    • /
    • 제16권6호
    • /
    • pp.683-688
    • /
    • 2007
  • In this study, N doped $TiO_2$ (TiO-N) thin film was prepared by DC magnetron sputtering method to show the photocatalytic activity in a visible range. Various gases (Ar, $O_2\;and\;N_2$) were used and Ti target was impressed by 1.2 kW -5.8 kW power range. The hysteresis of TiO-N thin film as a function of discharge voltage wasn't observed in 1.2 and 2.9kW of applied power. Cross sections and surfaces of thin films by FE-SEM were tiny and dense particle sizes of both films with normal cylindrical structures. XRD pattern of $TiO_2$ and TiO-N thin films was appeared by only anatase peak. Red shift in UV-Vis adsorption spectra was investigated TiO-N thin film. Photoactivity was evaluated by removal rate measurement of suncion yellow among reactive dyes. The photodegradation rate of $TiO_2$ thin film on visible radiation was shown little efficiency but TiO-N was about 18%.

리튬용액 침투방법에 의한 Li2TiO3 페블 제조 (Fabrication of Li2TiO3 Pebbles by Lithium Solution Penetration Method)

  • 유민우;박이현;이상진
    • 한국세라믹학회지
    • /
    • 제50권5호
    • /
    • pp.333-340
    • /
    • 2013
  • To fabricate spherical lithium titanate ($Li_2TiO_3$) pebbles which are used for a breeder material in fusion reactor, titanium oxide ($TiO_2$) granules were used as a starting material. The granules were pre-sintered, and then aqueous lithium nitrate solution infiltrated into the granules at vacuum condition. The granules were crystallized to $Li_2TiO_3$ after sintering under the control of process parameters. In this study, the concentration of lithium in the solution, as well as the number of penetration times and sintering temperature affected the final crystallite phase and the microstructure of the pebbles. In particular, the sphericity and size of the pebbles were effectively controlled by a technical rolling process. The useful spherical $Li_2TiO_3$ pebbles which have 10~20% porosity and 60~120 N compressive strength were obtained through the sintering at $1000{\sim}1100^{\circ}C$ in the multi-times infiltration process with 50 wt% solution. The physical properties of pebbles such as density, porosity and strength, can be controlled by a selection of $TiO_2$ powders and control of processing parameters. It can be thought that the lithium penetration method is a useful method for the fabrication of mass product of spherical $Li_2TiO_3$ pebbles.

(Sr.Pb)TiO$_3$계 세라믹의 유전특성에 미치는 Bi$_2$O$_3$.3TiO$_2$의 영향 (Effects of Bi$_2$O$_3$.3TiO$_2$ on the Dielectric Properties of Ceramics in the system (Sr.Pb)TiO$_3$)

  • 최운식;김충혁;홍진웅;김재환;이준웅
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1990년도 추계학술대회 논문집
    • /
    • pp.68-70
    • /
    • 1990
  • (1-X)(Sr$\_$7/9/Pb$\_$2/9/)$\_$(1-y)/(Ca$\_$1/5/Mg$\_$4/5/)$\_$y/TiO$_3$+X(BiO$_2$O$_3$$.$3TiO$_2$) (y=0.145, 0$\leq$X$\leq$0.08) ceramics were fabricated by the mixed oxide method. The sintering temperature and time were 1180∼1230[$^{\circ}C$], 2[hr], respectly. The grain size were grown with increasing the contents of Bi$_2$O$_3$$.$3TiO$_2$, but decreased more and less in the specimens which had more than 0.04[mol].