• 제목/요약/키워드: $TeO_2$ glasses

검색결과 16건 처리시간 0.024초

$TeO_2-PbO-GeO_2$계 유리 내 비선셩 광학 특성의 구조 의존성 (Structural Dependence of Nonlinear Optical Properties in $TeO_2-PbO-GeO_2$)

  • 김원효;허종;김유성;류선윤
    • 한국세라믹학회지
    • /
    • 제33권5호
    • /
    • pp.507-513
    • /
    • 1996
  • Nonlinear optical properties of TeO2-PbO-GeO2 glasses were investigated and their correlation with struc-tural modification was investigated. Third-order nonlinear susceptibility $\chi$, ranged between 5.0$\times$10-13 esu and 10.7$\times$10-13 esu which are approximately 20-40 times larger than that of silica glass. The glass with a composition of 85(80TeO2-20PbO)-15GeO2(mol%) seemed to provide an optimum compromise between $\chi$and the stability against crystallization. Analyses of the Raman spectra suggested that these glasses are mainly composed of [TeO4] tbp, [TeO3]tp and [GeO4] tetrahedral structural units. It was concluded that the positive contribution of Pb2+ with high polarizability to $\chi$ in TeO2-PbO glasses overwhelmed the negative influence due to the structural modification of [TeO4]tbplongrightarrow[TeO3]tp. On the other hand addition of GeO2 in TeO2-PbO-GeO2 glasses resulted in the decrease of $\chi$ values. This behavior was attributed to the formation of [GeO4] polyhedra at the expense of [TeOn] polyhedra and Pb2+ ions which normally sowed a higher contribu-tion to $\chi$ than [GeO4] polyhedra.

  • PDF

Correlation between the concentration of TeO2 and the radiation shielding properties in the TeO2-MoO3-V2O5 glass system

  • Y. Al-Hadeethi ;M.I. Sayyed
    • Nuclear Engineering and Technology
    • /
    • 제55권4호
    • /
    • pp.1218-1224
    • /
    • 2023
  • We investigated the radiation shielding competence for TeO2-V2O5-MoO3 glasses. The Phy-X software was used to report the radiation shielding parameters for the present glasses. With an increase in TeO2 and MoO3 content, the samples' linear attenuation coefficient improves. However, at low energies, this change is more apparent. At low energy, the present samples have an effective atomic number (Zeff) that is relatively high (in order of 16.17-24.48 at 0.347 MeV). In addition, the findings demonstrated that the density of the samples is a very critical factor in determining the half value layer (HVL). The minimal HVL for each sample can be found at 0.347 MeV and corresponds to 1.776, 1.519, 1.391, 1.210 and 1.167 cm for Te1 to Te5 respectively. However, the highest HVL of these glasses is recorded at 1.33 MeV, which corresponds to 3.773, 3.365, 3.218, 2.925 and 2.908 cm respectively. The tenth value layer results indicate that the thickness of the specimens needs to be increased in order to shield the photons that have a greater energy. Also, the TVL results demonstrated that the sample with the greatest TeO2 and MoO3 concentration has a higher capacity to attenuate photons.

Na2O-Nb2O5-TeO2계 유리의 광학적 성질과 나노-결정화거동 (1) (Nano-crystallization Behavior and Optical Properties of Na2O-Nb2O5-TeO2Glasses (1))

  • 김현규;류봉기;차재민;김병관;이재성
    • 한국세라믹학회지
    • /
    • 제40권11호
    • /
    • pp.1078-1084
    • /
    • 2003
  • 비선형 광학재료 및 광촉매를 개발하기 위하여, $Na_2$O-Nb$_2$ $O_{5}$-Te $O_2$계 유리를 일반적인 용융 및 급냉하는 방법으로 제조하였다. 그리고 $Na_2$O-Nb$_2$ $O_{5}$-Te $O_2$계 유리의 광학적 성질과 나노-결정화거동을 조사하였다. $Na_2$O-Nb$_2$ $O_{5}$-Te $O_2$계 유리의 광학적 성질과 물리적 성질은 다음과 같다. 굴절률(n) 은 2.04$\pm$0.04, 밀도(g/㎤)는 4.87$\pm$0.58, 광 에너지 밴드(eV)는 3.14$\pm$0.04이였다. 나노결정으로 구성된 투명한 결정화유리는 3$50^{\circ}C$에서 l시간 열처리한 후, 이것을 다시 40$0^{\circ}C$에서 l 시간 열처리하여 얻었다. 나노결정으로 구성된 Cubie 결정상은 47$0^{\circ}C$ 이상의 온도에서 새로운 결정상으로 변화하였다.

Gamma radiation attenuation properties of tellurite glasses: A comparative study

  • Al-Hadeethi, Y.;Sayyed, M.I.;Tijani, S.A.
    • Nuclear Engineering and Technology
    • /
    • 제51권8호
    • /
    • pp.2005-2012
    • /
    • 2019
  • This work investigated the radiation attenuation characteristics of three series of tellurite glass systems with the following compositions: 30PbO-10ZnO-xTeO2-(60-x)B2O3 where x = 10, 30, 40, 50 and 60 mol%, xBaO-xB2O3-(100-2x)TeO2 with x = 15-40 mol% and 50ZnO-(50-x)P2O5-xTeO2, where x = 0, 10, .40 mol%. The results revealed that the attenuation parameters in all the samples decrease with increase in the energy, which implied that all the samples have better interaction with gamma photons at low energies and thus higher photon attenuating efficiency. From the three systems, the samples coded as PbZnBTe60, BaBTe70 and ZnPTe40 have the lowest half value layer values and accordingly have superior photon attenuation efficacy. The maximum effective atomic number values were found for energy less than 0.1 MeV particularly near the K-edges absorption of the heavy atomic number elements such as Te, Ba and Pb. At the lowest energy, the Zeff values are found in the range of 62.33-66.25, 49.43-50.81 and 24.99-35.83 for series 1-3 respectively. Also, we found that the density of the glass remarkably affects the photon attenuation ability of the selected glasses. The mean free path results showed that the PbO-ZnO-TeO2-B2O3 glass system has better radiation shielding efficiency than the glass samples in series 2 and 3.

V2O5 및 TeO2 함유 유리를 이용한 염료감응형 태양전지 패널의 레이저 봉착 (Laser Sealing of Dye-Sensitized Solar Cell Panels Using V2O5 and TeO2 Contained Glass)

  • 조성진;이경호
    • 한국세라믹학회지
    • /
    • 제51권3호
    • /
    • pp.170-176
    • /
    • 2014
  • Effective glass frit compositions enabled to absorb laser energy, and to seal a commercial dye-sensitized solar-cell-panel substrate were developed by using $V_2O_5$-based glasses with various amounts of $TeO_2$ substitution. The latter was intended to increase the lifetime of the solar cells. Substitution of $V_2O_5$ by $TeO_2$ provided a strong network structure for the glasses via the formation of tetrahedral pyramids in the glass, and changed the various glass properties, such as glass transition temperature ($T_g$), dilatometric softening point ($T_d$), crystallization temperature, coefficient of thermal expansion (CTE), and glass flowage without any detrimental effect on the laser absorption property of the glasses. The thermal expansion mismatch (${\Delta}{\alpha}$) between the glass frit and the substrate could be controlled within less than ${\pm}5%$ by addition of 10 wt% of ${\beta}$-eucryptite. An 810 nm diode laser was used for the sealing test. The laser sealing test revealed that the VZBT20 glass frit with 10 wt% ${\beta}$-eucryptite was successfully sealed the substrates without interfacial cracks and pores. The optimum sealing conditions were provided by a beam size of 3 mm, laser power of 40 watt, scan speed of 300 mm/s, and 200 irradiation cycles.

Improvement of $^{4}I_{11/2}{\to}^{4}I_{13/2}$ Transition Rate and Thermal Stabilities in $Er^{3+}-Doped\;TeO_2-B_2O_3\;(GeO_2)-ZnO-K_2O$ Glasses

  • Cho, Doo-Hee;Choi, Yong-Gyu;Kim, Kyong-Hon
    • ETRI Journal
    • /
    • 제23권4호
    • /
    • pp.151-157
    • /
    • 2001
  • Spectroscopic and thermal analysis indicates that tellurite glasses doped with $B_2O_3$ and $GeO_2$ are promising candidate host materials for wide-band erbium doped fiber amplifier (EDFA) with a high 980 nm pump efficiency. In this study, we measured the thermal stabilities and the emission cross-sections for $Er^{3+}:^{4}I_{13/2}\;{\to}\;^{4}I_{15/2}$ transition in this tellurite glass system. We also determined the Judd-Ofelt parameters and calculated the radiative transition rates and the multiphonon relaxation rates in this glass system. The 15 mol% substitution of $B_2O_3$ for $TeO_2$ in the $Er^{3+}-doped\;75TeO_2-20ZnO-5K_2O$ glass raised the multiphonon relaxation rate for $^4I_{11/2}\;{\to}\;^4I_{13/2}$ transition from 4960 $s^{-1}$ to 24700 $s^{-1}$, but shortened the lifetime of the $^4I_{13/2}$ level by 14 % and reduced the emission cross-section for the $^4I_{13/2}\;{\to}\;^4I_{15/2}$ transition by 11%. The 15 mol% $GeO_2$ substitution in the same glass system also reduced the emission cross-section but increased the lifetime by 7%. However, the multiphonon relaxation rate for $^4I_{11/2}{\to}^4I_{13/2}$ transition was raised merely by 1000 $s^{-1}$. Therefore, a mixed substitution of $B_2O_3$ and $GeO_2$ for $TeO_2$ was concluded to be suitable for the 980 nm pump efficiency and the fluorescence efficiency of $^4I_{13/2}{\to}^4I_{15/2}$ transition in $Er^{3+}-doped$ tellurite glasses.

  • PDF

Er3+ 첨가 유리의 1.55μm 형광특성에 미치는 Thermal Poling의 영향 (Effect of Thermal Poling on the 1.55 μm Emission Characteristics of Er3+-doped Glasses)

  • 이태훈;정운진;허종
    • 한국세라믹학회지
    • /
    • 제40권5호
    • /
    • pp.423-427
    • /
    • 2003
  • 1.55$\mu$m 파장대 광증폭용 재료의 이득 파장대역 증대를 목적으로 Er$^{3+}$ 첨가 유리에 대해 thermal poling이 형광스펙트럼 의 반가폭(full width at half maximum)에 미치는 영향을 분석하였다. 텔루라이트 유리(TeO$_2$-ZnO)의 경우 poling후 약 6%의 형광 반가폭 증가가 관찰된 반면 다른 유리에서는 감소하거나 변화가 없었다. 이와 같은 형광스펙트럼의 변화는 알려진 바와 같이 poling으로 인해 유리내에 생성된 전하 결핍층과 이러한 결핍층에 발생하는 잔류 정전기장 때문으로 판단된다. 실리케이트 등과 같은 다른 유리와는 달리 텔루라이트 유리에서만 Er$^{3+}$ 의 형광 반가폭이 증가한 것은 유리를 구성하고 있는 TeO$_4$에 존재하는 비공유 전자쌍과 밀접하게 관련되어 있을 것으로 추측된다.

Structural Modification of Alkali Tellurite Binary Glass System and Its Characterization

  • Lee, Kyu-Ho;Kim, Tae-Ho;Kim, Young-Seok;Jung, Young-Joon;Na, Young-Hoon;Ryu, Bong-Ki
    • 한국재료학회지
    • /
    • 제18권5호
    • /
    • pp.235-240
    • /
    • 2008
  • This paper presents results and observations obtained from a study of the optical and thermal properties of alkali tellurite depending on the composition. Fourier transform infrared (FT-IR) spectra showed evidence of chemical modification from $TeO_4$ trigonal bipyramids (tbp) to $TeO_3$ trigonal pyramids (tp) in tellurite glasses. The optical band gaps of the different glass samples calculated using Tauc's method were found to range from 3.5-3.8 eV. The glass transition temperature (Tg) and glass stability (${\Delta}T$) of alkali tellurite glasses were investigated, as $M_2O$ [M: Li, Na, K] amounted to 25 mol%, through the use of differential thermal analysis (DTA). The coefficient of thermal expansion (CTE) was measured in a thermo mechanical analysis (TMA) with a slow heating rate after the glass samples were annealed. The results confirm that the optical band gap of alkali tellurite glasses depends on the Te-O-Te structural relaxation related to the ratio of bridging/non bridging oxygen (BO/NBO). In contrast, the thermal properties are related to the ionic field strength of the Te-O-M and M-O-M bonds, and the Te-O-Te breakage depends on the ratio of BO/NBO.

Role of modifiers on the structural, mechanical, optical and radiation protection attributes of Eu3+ incorporated multi constituent glasses

  • Poojha, M.K. Komal;Marimuthu, K.;Teresa, P. Evangelin;Almousa, Nouf;Sayyed, M.I.
    • Nuclear Engineering and Technology
    • /
    • 제54권10호
    • /
    • pp.3841-3848
    • /
    • 2022
  • The effect of modifiers on the optical features and radiation defying ability of the Eu3+ ions doped multi constituent glasses was examined. XRD has established the amorphous nature of the specimen. The presence of various functional/fundamental groups in the present glasses was analyzed through FTIR spectra. The physical, structural and elastic traits of the glasses were explored. The variation in the structural compactness of the glass structure according to the incorporated modifier was enlightened to describe their suitability for a better shielding media. For the examined glasses, the metallization criterion value varied in the range 0.613-0.692, indicating the non-metallic character of the glasses with possible nonlinear optical applications. The computed elastic moduli expose the Li-containing glass (BTLi:Eu) to be tightly packed and rigid, which is a requirement for a better shielding channel. Furthermore, the optical bandgap and the Urbach energy values are calculated based on the optical absorption spectra. The evaluated bonding parameters revealed the nature of the fabricated glasses covalent. In addition, we investigated the radiation attenuation attributes of the prepared Eu3+ ions doped multi constituent glasses using Phy-X software. We determined the linear attenuation coefficient (LAC) and reported the influence of the five oxides Li2O3, CaO, BaO, SrO, and ZnO on the LAC values. The LAC varied between 0.433 and 0.549 cm-1 at 0.284 MeV. The 39B2O3-25TeO2-15Li2O3-10Na2O-10K2O-1Eu2O3 glass has a much smaller LAC than the other glasses.

Bismuth modified gamma radiation shielding properties of titanium vanadium sodium tellurite glasses as a potent transparent radiation-resistant glass applications

  • Zaid, M.H.M.;Matori, K.A.;Sidek, H.A.A.;Ibrahim, I.R.
    • Nuclear Engineering and Technology
    • /
    • 제53권4호
    • /
    • pp.1323-1330
    • /
    • 2021
  • This work reported the radiation shielding characteristic of the bismuth titanium vanadium sodium tellurite glass system. The density of the specially-developed glass samples was increased from 2.21 to 4.01 g/cm3 with the addition of Bi2O3, despite the fact the molar volume is decease within 85.43-54.79 cm3/mol. The WinXcom program was used to approximate the effect of Bi2O3 on the gamma radiation shielding parameters of bismuth titanium vanadium sodium tellurite glasses. The ㎛ values decrease with the increase of Bi2O3 concentration. The computed data shows that the glass sample with 20 mol.% of Bi2O3 content has the greatest radiation attenuation performance in comparison to other selected glasses. The Bi2O3-TiO2-V2O5-Na2O-TeO2 glass system shows excellent neutron shielding material with high long-term light transmittance and discharge resistance and could be potentially used as transparent radiation-resistant shielding glass applications.