• 제목/요약/키워드: $Ta_2O_{5-X}$ thin films

검색결과 35건 처리시간 0.021초

RTMOCVD법에 의해 제조된 Ta2O5 박막의 특성 (Characteristics of Ta2O5 thin film prepared by RTMOCVD)

  • 소명기
    • 산업기술연구
    • /
    • 제19권
    • /
    • pp.101-105
    • /
    • 1999
  • Ultra thin $Ta_2O_5$ gate dielectrics were prepared by RTMOCVD (rapid thermal metal organic chemical vapor deposition) using Ta source $TaC_{12}H_{30}O_5N$ and $O_2$ gaseous mixtures. As a result, $Ta_2O_5$ thin films showed significantly low leakage current compared to $SiO_2$ of identical thickness, which was due to the stabilization of the interfacial layer by NO ($SiO_xN_y$) passivation layer. The conduction of leakage current in $Ta_2O_5$ thin films was described by the hopping mechanism of Poole-Frenkel (PF) type.

  • PDF

$IrO_2$를 하부전극으로 사용한 $Sr_{0.9}Bi_{2+x}Ta_2O_9$ 박막의 유전 및 전기적 특성 (Dielectric and Electrical Properties of $Sr_{0.9}Bi_{2+x}Ta_2O_9$ Thin Films on $IrO_2$ Electrode)

  • 박보민;송석표;정병직;김병호
    • 한국세라믹학회지
    • /
    • 제37권3호
    • /
    • pp.233-239
    • /
    • 2000
  • Sr0.9Bi2+xTa2O9(x=0, 0.1, 0.2, 0.3) thin films on IrO2/SiO2/Si or Pt/Ti/SiO2/Si substrate were prepared by spin coating method using SBT stock solutions synthesized by MOD process. SBT thin films on IrO2 transformed to layered perovskite phase at $700^{\circ}C$, but showed low breakdown voltage due to their porous microstructure. The smaple of Sr0.9Bi2+xTa2O9 composition showed the best dielectric and electrical properties. When the sample of the same composition was annealed at 80$0^{\circ}C$, the dielectric and electric properties were improved due to the grian growth and dense surface. the remanent polarization values(2Pr) at $\pm$3 V for IrO2 and Pt electrodes were 10.5, 7.15$\mu$C/$\textrm{cm}^2$, respectively. The SBT thin film with IrO2 electrode showed the lower coercive field. The leakage current density and breakdown voltage of SBT thin films on IrO2 were higher than those on Pt.

  • PDF

PREFERRED ORIENTATION AND MICROSTRUCTURE OF MOD DERIVED SrBi$_{2x}$Ta$_2$O$_9$ THIN FILMS WITH Bi CONTENT x

  • Yeon, Dae-Joong;Park, Joo-Dong;Oh, Tae-Sung
    • 한국표면공학회지
    • /
    • 제29권6호
    • /
    • pp.621-627
    • /
    • 1996
  • $SrBi_{2x}TaO_9$ ferroelectric thin films were prepared on platinized silicon substrates using MOD proces, and crystallization behavior of the films was investigated with variation of the annealing temperature and Bi content x. Crystalline phase of bismuth layered perovskite structure was formed even by baking the films at $800^{\circ}C$ for 5 minutes in air, and was not changed by annealing at temperatures raning from $700^{\circ}C$ to $900^{\circ}C$ for 1 hour in oxygen ambient. When $SrBi_{2x}TaO_9$ thin films ($0.8\lex\ie1.6$) were annealed at $800^{\circ}C$, Preferred orientation of the films along c-axis was observed with $x\ge1.2$. With increasing Bi content x, surface morphology of the films was changed from equiaxed grains to elongated grains.

  • PDF

Dielectric Properties of $Ta_2O_{5-X}$ Thin Films with Buffer Layers

  • Kim, In-Sung;Song, Jae-Sung;Yun, Mun-Soo;Park, Chung-Hoo
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • 제12C권4호
    • /
    • pp.208-213
    • /
    • 2002
  • The present study describe the electrical performance of amorphous T $a_2$ $O_{5-X}$ fabricated on the buffer layers Ti and Ti $O_2$. T $a_2$ $O_{5-X}$ thin films were grown on the Ti and Ti $O_2$ layers as a capacitor layer using reactive sputtering method. The X-ray pattern analysis indicated that the two as-deposited films were amorphous and the amorphous state was kept stable on the RTA(rapid thermal annealing) at even $700^{\circ}C$. Measurements of dielectric properties of the reactive sputtered T $a_2$ $O_{5-X}$ thin films fabricated in two simple MIS(metal insulator semiconductor), structures, (Cu/T $a_2$ $O_{5}$ Ti/Si and CuT $a_2$ $O_{5}$ Ti $O_2$Si) show that the amorphous T $a_2$ $O_{5}$ grown on Ti showed high dielectric constant (23~39) and high leakage current density(10$^{-3}$ ~10$^{-4}$ (A/$\textrm{cm}^2$)), whereas relatively low dielectric constant (~15) and tow leakage current density(10$^{-9}$ ~10$^{-10}$ (A/$\textrm{cm}^2$)) were observed in the amorphous T $a_2$ $O_{5}$ deposited on the Ti $O_2$ layer. The electrical behaviors of the T $a_2$ $O^{5}$ thin films were attributed to the contribution of Ti- $O_2$ and the compositionally gradient Ta-Ti-0, being the low dielectric layer and high leakage current barrier. In additional, The T $a_2$ $O_{5}$ Ti $O_2$ thin films exhibited dominant conduction mechanism contributed by the Poole-Frenkel emission at high electric field. In the case of T $a_2$ $O_{5}$ Ti $O_2$ thin films were related to the diffusion of Ta, Ti and O, followed by the creation of vacancies, in the rapid thermal treated thin films.films.

MOD법에 의한 강유전성 $Sr_xBi_yTa_2O_{9+\alpha}$(SBT) 박막의 제조 및 후열처리 효과에 관한 연구 (Fabrication and Post-Annealing Effects of Ferroelectric $Sr_xBi_yTa_2O_{9+\alpha}$(SBT) Thin Films by MOD Process)

  • 정병직;신동석;윤희성;김병호
    • 한국전기전자재료학회논문지
    • /
    • 제11권3호
    • /
    • pp.229-236
    • /
    • 1998
  • Ferroelectric $Sr_xBi_yTa_2O_{9+\alpha}$/(0.7$\leqSr\leq1.0,\; 2.0\leqBi\leq2.6)$ solutions were prepared by MOD (Metalorganic Deposition) process. These solutions were made into thin films with thickness ranging from 1500~2000${\AA}$ by spin coating. The phase transformation of the SBT thin films by variation of annealing temperature and annealing time were observed using high temperature XRD and SEM. The crystallization and grain growth of SBT thin film were accomplished at $800^{\circ}C$ for 30 minutes after deposition of Pt top electrode by sputtering to prevent electrical breakdown. Ferroelectric properties of the SBT thin films were measured in the range of $\pm$3V\; and\; \pm5V$. The specimen with composition ratio of Sr/Bi/Ta (0.8/2.4/2.0) has the excellent ferroelectric properties ; $2P_r = 10.5,\; 13.2\muC/cm^2 \;at\; \pm3V\; and\; \pm5V$ respectively. Observing the post annealed Pt/SBT/Pt interface by SEM, it was found that Pt electrode sputtered on to the SBT thin film penetrated into the hollow on the SBT thin film, thus decreasing the effective insulation thickness. The effective insulation thickness recovered by post annealing, and this was confirmed by leakage current density measurement.

  • PDF

솔 - 젤법을 이용한 Bismuth Layered Structure를 가진 강유진성 박막의 제조 및 특성평가에 관한 연구 (II. MOD법으로 제조한 강유전성 $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ 박막의 유전특성) (The Preparation and Characterization of Bismuth Layered Ferroelectric Thin Films by Sol-Gel Process (II. Dielectric Properties of Ferroelectric $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ Thin Films Prepared by MOD Process))

  • 최무용;송석표;정병직;김병호
    • 한국전기전자재료학회논문지
    • /
    • 제12권1호
    • /
    • pp.62-68
    • /
    • 1999
  • Ferroelectric $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$(x=0, 0.1, 0.2, 0.3) thin films were deposited on $Pt/SiO_2/Si$ substrate by MOD(Metalorganic Decomposition) process. Metal carboxylate and metal alkoxide were used as precursors, and 2-methoxyethanol, xylene as solvents. After spin coating, thin films were pre-annealed at $400^{\circ}C$, followed by RTA(Rapid Thermal Annealing) and final annealing at $800^{\circ}C$ in oxygen atmosphere. These procedures were repeated three times to obtain thin films with the thickness of $2000{\AA}$. To enhance the nucleation and growth of layered-perovskite phase, thin films were rapid-thermally annealed above $720^{\circ}C$ in oxygen atmosphere. As RTA temperature increased, fluorite phase was transformed to layered-perovskite phase. And the change of Nb contents affected dielectric / electrical properties and microstructure. The ferroelectric characteristics of $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ thin film were Pr=8.67 $\mu{C}/cm^2$, Ec=62.4kV/cm and $I_{L}=1.4\times10^{-7}A/cm^2$ at the applied voltage of 5V, respectively.

  • PDF

산화물 박막 커패시터의 RTA 처리와 유전 특성에 관한 연구 (The Study on Dielectric and RTA Property of Oxide Thin-films)

  • 김인성;이동윤;조영란;송재성
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.23-25
    • /
    • 2001
  • In this work, the $Ta_2O_5$ thin films were deposited on Pt/n-Si substrate by reactive magnetron sputtering and the RTA treatment at temperatures range from 650 to $750^{\circ}C$ in $O_2$ and vacuum. X-ray diffraction analysis, FE SEM, dielectric properties and leakage current density have been used to study the structural and electrical properties of the $Ta_2O_5$ thin films. XRD result showed that as- deposited films were amorphous and the annealed films crystallized (<$700^{\circ}C$) into ${\beta}-Ta_2O_5$. The crystallinity increased with temperature in terms of an increase in the intensity of the diffracted peaks(${\beta}-Ta_2O_5$) and annealing in oxygen reduced defect dang1ing Ta-O bonds. As deposited $Ta_2O_5$ films show the leakage current density $10^{-7}$ to $10^{-8}$ (A/$cm^2)$ at low electric fields (<200 kV/cm) However, it was found leakage current density of $Ta_2O_5$ thin films decreased with $O_2$ ambient annealing. The dielectric constant of the as deposited $Ta_2O_5$ thin films was ${\varepsilon}_r$ $9{\sim}11$ but the dielectric constant was increased after RTA treatment in $O_2$ ambient more then in vacuum.

  • PDF

Bi 함량에 따른 $SrBi_{2x}Ta_2O_9$ 박막의 전기적 특성 (Electrical properties of S$SrBi_{2x}Ta_2O_9$ thin films with Bi content)

  • 연대중;권용욱;박주동;오태성
    • 한국진공학회지
    • /
    • 제8권3A호
    • /
    • pp.224-230
    • /
    • 1999
  • $SrBi_{2x}Ta_2O_9$ (SBT) thin films were prepared on platinized silicon substrates by MOD process, and their ferroelectric and leakage current characteristics were investigated. The grain size of the MOD derived SBT films increased with increasing the BI/Ta mole ration. Although the SBT films with x of 0.8~1.2 were composed of the equiaxed grains, the elongated grains were also observed for the SBT films with x of 1.4 and 1.6. The SBT film with x of 1.2 exhibited the optimum ferroelectric properties of 2PR : 9.79 $\muC/\textrm{cm}^2$ and Ec : 24.2kV/cm at applied voltage of 5V. The leakage current density of the SBT films increased with increasing the BI/Ta mole ratio. With post annealing process, 2Pr and $E_c$of the SBT film with x of 1.2 increases 11.3 $\muC/\textrm{cm}^2$ and 39.6kV/cm, respectively. decrement of the leakage current density by post annealing process increased remarkably with increasing the Bi/ta mole ratio, and the SBT film with x=1.6 exhibited the lowest leakage current density after post annealing process.

  • PDF

MOS구조에서의 원자층 증착 방법에 의한 $Ta_2O_{5}$ 박막의 전기적 특성에 관한 연구 (A Study on the Electrical Properties of $Ta_2O_{5}$ Thin Films by Atomic Layer Deposition Method in MOS Structure)

  • 이형석;장진민;임장권;하만효;김양수;송정면;문병무
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제52권4호
    • /
    • pp.159-163
    • /
    • 2003
  • ln this work, we studied electrical characteristics and leakage current mechanism of $Ta_2O_{5}$ MOS(Metal-Oxide-Semiconductor) devices. $Ta_2O_{5}$ thin film (63 nm) was deposited by ALD(Atomic Layer Deposition) method at temperature of 235 $^{\circ}C$. The structures of the $Ta_2O_{5}$ thin films were examined by XRD(X-Ray Diffraction). From XRD, it is found that the structure of $Ta_2O_{5}$ is single phase and orthorhombic. From capacitance-voltage (C-V) anaysis, the dielectric constant was 19.4. The temperature dependence of current density-electric field (J-E) characteristics of $Ta_2O_{5}$ thin film was studied at temperature range of 300 - 423 K. In ohmic region (<0.5 MV/cm), the resistivity was 2.456${\times}10^{14}$ ($\omega{\cdot}cm$ at 348 K. The Schottky emission is dominant at lower temperature range from 300 to 323 K and Poole-Frenkel emission is dominant at higher temperature range from 348 to 423 K.

원자층 증착 방법에 의한 $Ta_2O_5$ 박막의 전기적 특성 (The Electrical Properties of $Ta_2O_5$ Thin Films by Atomic Layer Deposition Method)

  • 이형석;장진민;장용운;이승봉;문병무
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 유기절연재료 전자세라믹 방전플라즈마 일렉트렛트 및 응용기술
    • /
    • pp.41-46
    • /
    • 2002
  • In this work, we studied electrical characteristics and leakage current mechanism of Au/$Ta_2O_5$/Si metal-oxide-semiconductor (MOS) devices. $Ta_2O_5$ thin film (63nm) was deposited by atomic layer deposition (ALD) method at temperature of $235^{\circ}C$. The structures of the $Ta_2O_5$ thin films were examined by X-Ray Diffraction (XRD). From XRD, the structure of $Ta_2O_5$ was single phase and orthorhombic. From capacitance-voltage (C-V) analysis, the dielectric constant was 19.4. The temperature dependence of current-voltage (I-V) characteristics of $Ta_2O_5$ thin film was studied from 300 to 423 K. In ohmic region (<0.5 MVcm${-1}$), the resistivity was $2.4056{\times}10^{14}({\Omega}cm)$ at 348 K. The Schottky emission is dominant in lower temperature range from 300 to 323 K and Poole-Frenkel emission dominant in higher temperature range from 348 to 423 K.

  • PDF