  • We investigated the quantum well intermixing (QWI) of a compressively strained InGaAs/InGaAsP multiple quantum well (MQW) by using impurity free vacancy diffusion technique. The samples with InGaAs/$SiO_2$ capping layer showed a higher degree of intermixing compared to that of InP/$SiO_2$ capping layer after rapid thermal annealing (RTA). Band-gap shift difference as large as 123 meV (195 nm) was observed between samples capped with InGaAs/$SiO_2$ and with InP/$SiO_2$ layer at RTA temperature of $700^{\circ}C$. Using the InGaAs/$SiO_2$ cap layer, the band-gap wavelength of MQW was changed by the intermixing from 1.55 $\mu\textrm{m}$ band to 1.3 $\mu\textrm{m}$ band with a wavelength shift of a 237 nm. The transform from MQW structure to homogenous alloy was observed above the RTA temperature of $700^{\circ}C$.

  • PDF

Effects of SiO2 on the High Temperature Resistivities of AIN Ceramics (SiO2 첨가가 AIN 세라믹스의 고온 비저항에 미치는 영향)

  • Lee, Won-Jin;Kim, Hyung-Tae;Lee, Sung-Min
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.1
    • /
    • pp.69-74
    • /
    • 2008
  • The effects of $SiO_2$ impurity on the high temperature resistivities of AIN ceramics have been investigated. When $SiO_2$ was added into 1 wt% $Y_2O_3$-doped AIN, DC resistivities have decreased and electrode polarizations disappeared. Impedance spectroscopy showed two semi-circles at $600^{\circ}C$, which were attributed to grain and grain boundary, respectively. $SiO_2$ doping had more significant effects on the grain resistivity than grain boundary resistivity, implying that doped Si acted as a donor in AIN lattice. In addition, voltage dependency of DC resistivity was observed, which might be related to dependency of size of grain boundary semi-circle on the bias voltage in impedance spectroscopy.

Studies of the $TiO_2-Si$ Interface Bombarded by $Ar^+$ Ion Beam

  • Zhang, J.;Huang, N.K.;Lu, T.C.;Zeng, L.;Din, T.;Chen, Y.K.
    • Journal of the Korean Vacuum Society
    • /
    • v.12 no.S1
    • /
    • pp.63-66
    • /
    • 2003
  • It is experimentally shown that a $TiO_2$ film on Si(111) substrate was prepared by using the technique of D.C. reaction sputter deposition with $Ar^{+}$ ion beam bombardment, and a layer-like structure was observed from the depth profile of the interface between $TiO_2$ film and Si substrate with Scanning Electron Microscopy and Electron Probe. It was also surprisingly discovered that Ti atoms could be detected at about 9 $\mu$m depth. The $TiO_2$-Si interface bombarded by $Ar^{+}$ ion beams revealed multi-layer structures, a mechanism might be caused by defect diffusion, impurity and matrix relocation. Multi-relocations of impurity and matrix atoms were as a result of profile broadening of the $TiO_2$-Si interface, and the spread due to matrix relocation in this system is shown to exceed much more the spread due to impurity relocation.

Effects of Composition and Temperature on the Descaling Characteristics in Si Containing Steel (Si 첨가강의 Descaling 특성에 미치는 강조성 및 가열온도의 영향)

  • Choi J. W.;Kwon S. J.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.08a
    • /
    • pp.277-284
    • /
    • 2004
  • Low carbon steels containing Si of up to $1.2\;wt\%$ were oxidized in air at 1373 K and 1523 K, i.e. below and above the eutectic temperature of FeO and $Fe_2SiO_4$. The influence of a impurity element, S on behavior of scale formation during oxidation was investigated by using $M\"{o}chssbauer$ spectroscopy and EDS. This allowed establishment of an interface oxidation model of Si-added steel depending on temperature and an impurity element. A compound of FeO and FeS was formed in the scale/matrix interface of low carbon steels containing S of up to $0.03\;wt\%$ oxidized above 1213 K of the eutectic temperature. This was flat formed between $Fe_2SiO_4$ nodules along the scale/matrix interface without selective oxidation. It is due to low viscosity and high wettability of the compound of FeO and FeS in liquid. Conventional metallographic examinations revealed that roughness of the scale/matrix interface in Si-added steels became flat as the content of S increased. It was independent of oxidizing temperature and Si content. Effects of oxidizing temperature and an impurity element content on descaling characteristics in Si-added steels were evaluated by using a hydraulic descaling simulator. Good descaling characteristics was attributable to this flatness of the scale/matrix interface.

  • PDF

Characteristics of TaN Film as to Cu Barrier by PAALD Method (PAALD 방법을 이용한 TaN 박막의 구리확산방지막 특성)

  • 부성은;정우철;배남진;권용범;박세종;이정희
    • Journal of the Semiconductor & Display Technology
    • /
    • v.2 no.2
    • /
    • pp.5-8
    • /
    • 2003
  • In this study, as Cu diffusion barrier, tantalum nitrides were successfully deposited on Si(100) substrate and $SiO_2$ by plasma assisted atomic layer deposition(PAALD) and thermal ALD, using pentakis (ethylmethlyamino) tantalum (PEMAT) and NH$_3$ as precursors. The TaN films were deposited at $250^{\circ}C$ by both method. The growth rates of TaN films were 0.8${\AA}$/cycle for PAALD and 0.75${\AA}$/cycle for thermal ALD. TaN films by PAALD showed good surface morphology and excellent step coverage for the trench with an aspect ratio of h/w -1.8:0.12 mm but TaN films by thermal ALD showed bad step coverage for the same trench. The density for PAALD TaN was 11g/cmand one for thermal ALD TaN was 8.3g/$cm^3$. TaN films had 3 atomic % carbon impurity and 4 atomic % oxygen impurity for PAALD and 12 atomic % carbon impurity and 9 atomic % oxygen impurity for thermal ALD. The barrier failure for Cu(200 nm)/TaN(10 nm)/$SiO_2$(85 nm)/ Si structure was shown at temperature above $700^{\circ}C$ by XRD, Cu etch pit analysis.

  • PDF

Oxidation of CVD β-SiC in Impurity-Controlled Helium Environment at 950℃ (950℃ 불순물을 포함한 헬륨 환경에서 CVD β-SiC의 산화)

  • Kim, Dae-Jong;Kim, Weon-Ju;Jang, Ji-Eun;Yoon, Soon-Gil;Kim, Dong-Jin;Park, Ji-Yeon
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.5
    • /
    • pp.426-432
    • /
    • 2011
  • The oxidation behavior of CVD ${\beta}$-SiC was investigated for Very High Temperature Gas-Cooled Reactor (VHTR) applications. This study focused on the surface analysis of the oxidized CVD ${\beta}$-SiC to observe the effect of impurity gases on active/passive oxidation. Oxidation test was carried out at $950^{\circ}C$ in the impurity-controlled helium environment that contained $H_2$, $H_2O$, CO, and $CH_4$ in order to simulate VHTR coolant chemistry. For 250 h of exposure to the helium, weight changes were barely measurable when $H_2O$ in the bulk gas was carefully controlled between 0.02 and 0.1 Pa. Surface morphology also did not change based on AFM observation. However, XPS analysis results indicated that a very small amount of $SiO_2$ was formed by the reaction of SiC with $H_2O$ at the initial stage of oxidation when $H_2O$ partial pressure in the CVD ${\beta}$-SiC surface placed on the passive oxidation region. As the oxidation progressed, $H_2O$ consumed and its partial pressure in the surface decreased to the active/passive oxidation transition region. At the steady state, more oxidation did not observable up to 250 h of exposure.

Origin of Charge Puddle of Graphene on α - SiO2: First Principles Study.

  • Shim, Yoon Su
    • Proceeding of EDISON Challenge
    • /
    • 2015.03a
    • /
    • pp.338-342
    • /
    • 2015
  • Ripples and charge impurity effect of graphene are considered as the origin of charge puddles in graphene sheet on SiO2. However, this topic is very controversial among researchers in graphene community. In this study, by using density functional theory, we calculate the band structure of the rippled graphene model and charged impurity model that is located close to the (0001) ${\alpha}$-quartz surface. We expect that this study will provide great insight on this matter.

  • PDF

Study of $MgB_2$ Films Grown on Various Impurity Layers by using HPCVD Method (혼성물리화학기상 증착법으로 여러가지 불순물층 위에 제조한 $MgB_2$ 박막에 대한 연구)

  • Park, S.W.;Seong, W.K.;Jung, Soon-Gil;Kang, W.N.
    • Progress in Superconductivity
    • /
    • v.10 no.1
    • /
    • pp.35-39
    • /
    • 2008
  • By using the hybrid physical-chemical vapor deposition (HPCVD) technique, we have fabricated $MgB_2$ thick films on $Al_{2}O_3$ substrates with various impurity layers of Ni, Ti, and SiC. We have found a significant enhancement of the critical current density ($J_c$) for $MgB_2$ films grown on impurity layered substrates, indicating that additional impurity layers were provided as possible pinning sites by chemical doping in $MgB_2$ films. All samples doped by Ni, Ti, and SiC were observed to have high superconducting transition temperatures of 39 - 41 K. The $J_c$ of $MgB_2$ films grown on SiC impurity layered substrates showed three times higher than that of undoped films at high magnetic fields above 1 T.

  • PDF

PAALD 방법을 이용한 TaN 박막의 구리확산방지막 특성

  • 부성은;정우철;배남진;권용범;박세종;이정희
    • Proceedings of the Korean Society Of Semiconductor Equipment Technology
    • /
    • 2002.11a
    • /
    • pp.14-19
    • /
    • 2002
  • In this study, as Cu diffusion barrier, tantalum nitrides were successfully deposited on Si(100) substrate and SiO2 by plasma assisted atomic layer deposition(PAALD) and thermal ALD, using pentakis (ethylmethlyamino) tantalum (PEMAT) and $NH_3$ as precursors. The TaN films were deposited on $250^{\circ}$C by both method. The growth rates of TaN films were $0.8{\AA}$/cycle for PAALD and $0.75{\AA}$/cycle for thermal ALD. TaN films by PAALD showed good surface morphology and excellent step coverage for the trench with an aspect ratio of h/w - $1.8 : 0.12 \mu\textrm{m}$ but TaN films by thermal ALD showed bad step coverage for the same trench. The density for PAALD TaN was $11g/\textrm{cm}^3$ and one for thermal ALD TaN was $8.3g/\textrm{cm}^3$. TaN films had 3 atomic % carbon impurity and 4 atomic % oxygen impurity for PAALD and 12 atomic % carbon impurity and 9 atomic % oxygen impurity for thermal ALD. The barrier failure for Cu(200nm)/TaN(l0nm)/$SiO_2(85nm)$/Si structure was shown at temperature above $700^{\circ}$C by XRD, Cu etch pit analysis.

  • PDF

Analysis and Reduction of Impurity Contamination Induced by Plasma Etching on Si Surface (플라즈마 식각에 의하여 실리콘 표면에 유기된 불순물 오염의 분석 및 제거)

  • Cho, Sun-Hee;Lee, Won-Jong
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.12
    • /
    • pp.1078-1084
    • /
    • 2006
  • Impurity contamination induced by $CF_4\;and\;HBr/Cl_2/O_2$ plasma etching on Si surface was examined by using surface spectroscopes. XPS(x-ray photoelectron spectroscopy) surface analysis showed that F of 0.4 at % exists in the surface layer in the form of Si-F bonding but Br and Cl are below the detection limit $(0.1{\sim}1.0%)$ of the spectroscope. Static-SIMS(secondary ion mass spectrometry) surface analysis showed that the etched Si surface was contaminated with etching gas elements such as H, F, Cl and Br, and they existed to the depth of about $20{\sim}40nm$. The etched Si surface was treated with three different methods that were HF dip, thermal oxidation followed by HF dip and oxygen-plasma oxidation followed by HF dip. They showed an effect in reducing the impurity contamination and the oxygen-plasma oxidation followed by HF dipping method appears to be a little bit more effective.