The encapsulation method of flexible organic light emitting devices (OLEDs) was investigated for the structure of ITO / 2-TNATA / NPB / $Alq_3$ : Rubrene (1 vol.%) / $Alq_3$ / LiF / Al / $Alq_3$ / LiF / Al (OLED #1), on which $SiN_x$ thin film was deposited and metal film was attached to protect the damage of OLED from oxygen and moisture. The $SiN_x$ thin film was deposited by plasma enhanced chemical vapor deposition (PECVD) method using $SiH_4$ of 20 sccm and $N_2$ of 15~35 sccm as reactor gases. The optimum $SiN_x$ deposition condition was found to be 20 sccm $SiH_4$ and 20 sccm $N_2$ from the Ca test of the fabricated $SiN_x$ thin film. The life time of OLED #1, OLED #1 / $SiN_x$ 200 nm, OLED #1 / $SiN_x$ 400 nm and OLED #1 / $SiN_x$ 400 nm / metal film was 7, 12, 25, and 45 hours, respectively. In conclusion, it has been shown that the lifetime of OLEDs can be improved more than 6 times by $SiN_x$ film and a metal film encapsulation.
Multilayer passivation film on OLED with organic/inorganic hybrid structure as to diminish the thermal stress and expansion was researched to protect device from the direct damage of $O_2$ and $H_2O$ and improve life time characteristics. Red OLED doped with 1 vol.% Rubrene in $Alq_3$ was used as a basic device. The films consist of ITO(150 nm)/ELM200_HIL(50 nm)/ELM002_HTL(30 nm)/$Alq_3$: 1 vol.% Rubrene(30 nm)/$Alq_3$(30 nm) and LiF(0.7 nm)/Al(100 nm) which were formed in that order. Using LiF/$SiN_x$ as a buffer layer was determined because it significantly improved life time characteristics without suffering damage in the process of forming passivation film. Multilayer passivation film on buffer layer didn't produce much change in current efficiency, while the half life time at 1,000 $cd/m^2$ of OLED/LiF/$SiN_x$/E1/$SiN_x$ was 710 hours which showed about 1.5 times longer than OLED/LiF/$SiN_x$/E1 with 498 hours. futhermore, OLED/LiF/$SiN_x$/E1/$SiN_x$/E1/$SiN_x$ with 1301 hours showed about twice than OLED/LiF/$SiN_x$/E1/$SiN_x$ which demonstrated that superior characteristics of life time was obtained in multilayer passivation film. Through the above result, it was suggested using LiF/$SiN_x$ as a buffer layer could reduce the damage from the difference of thermal expansion coefficient in OLED with protective films, and epoxy layer in multilayer passivation film could function like a buffer between $SiN_x$ inorganic layers with relatively large thermal stress.
저온 공정으로 제작되는 다결정 실리콘 박막 트랜지스터의 활성층을 이중 활성층(a-Si/a-SiN/sub x/)으로 제작하는 공정을 제안하고 다결정 실리콘 박막 트랜지스터를 제작하였다. 본 논문에서는 활성층의 아래쪽 실리콘 박막에 약간의 질소기를 첨가한 후 그 위에 순수한 비정질 실리콘 박막을 증착하여 엑시머 레이저의 에너지로 비정질 실리콘 박막을 결정화하여 사용하였다. 이중 활성층 (a-Si/a-SiN/sub x/)의 경우, 하부층의 NH₃/SiH₄ 유속비가 증가함에 따라, 상부 a-Si 층의 결정 성장이 촉진됨을 알 수 있었으나, n/sup +/ poly-SiN/sub x/ 층의 전도도 특성을 고려해 볼 때, NH₃/SiH₄ 유속비는 0.11의 상한치를 가짐을 알 수 있었다. 전계 방출 전류에 영향을 미치는 광학적 밴드갭의 경우, poly-Si 박막에 비해 증가하였으며, NH₃/SiH₄ 유속비가 0.11 이하에서도 0.1eV 정도의 증가를 보여, 이로 인하여 소자 제작시 전계 방출 전류가 억제될 것을 예상할 수 있다.
비메모리 반도체 미세 Cu배선의 전기적 신뢰성 향상을 위해 SiNx 피복층(capping layer)과 Cu 배선 사이 50 nm 두께의 Co 박막층 삽입이 계면 신뢰성에 미치는 영향을 double-cantilever beam (DCB) 접착력 측정법으로 평가하였다. DCB 평가 결과 SiNx/Cu 구조는 계면접착에너지가 0.90 J/㎡이었으나 SiNx/Co/Cu 구조에서는 9.59 J/㎡으로 SiNx/Cu 구조보다 약 10배 높게 측정되었다. 대기중에서 200℃, 24시간 동안 후속 열처리 진행한 결과 SiNx/Cu 구조는 0.93 J/㎡으로 계면접착에너지의 변화가 거의 없는 것으로 확인되었으나 SiNx/Co/Cu 구조에서는 2.41 J/㎡으로 열처리 전보다 크게 감소한 것을 확인하였다. X-선 광전자 분광법 분석 결과 SiNx/Cu 도금층 사이에 Co를 증착 시킴으로써 SiNx/Co 계면에 CoSi2 반응층이 형성되어 SiNx/Co/Cu 구조의 계면접착에너지가 매우 높은 것으로 판단된다. 또한 대기중 고온에서 장시간 후속 열처리에 의해 SiNx/Co 계면에 지속적으로 유입된 산소로 인한 Co 산화막 형성이 계면접착에너지 저하의 주요인으로 판단된다.
본 연구에서는 자기 공명 특성을 이용한 박막 센서의 멤브레인 및 박막 센서의 특성을 알아보았다. 멤브레인으로 유망한 물질로 $Si_xN_y$과 SiC가 있으며, 최적의 멤브레인 형성 조건을 알고자 박막의 잔류 응력 및 물성을 비교 분석하였다. 그 중에서 박막 센서에 적용 가능한 멤브레인으로 SiC보다 적절한 인장응력과 낮은 열팽창 계수를 가지는 $Si_xN_y$이 센서의 구조층으로 우수하였으며, $Si_xN_y$위에 박막 센서 물질을 증착 및 패턴닝(patterning)을 함으로써 센서의 자기 이력 곡선 및 자기 공진 주파수를 분석하였다. 센서에 인가되는 외부 자기장을 제거하면 자장에 의해 형성된 자화(magnetization)가 탄성 모드로 바뀌면서 에너지 방출에 의해 센서에서 전압이 발생하는데 이때 전압 발생 구간이 길어지면 기계적 진동이 야기되어 신호가 발생한다. 그리고 센서의 길이 및 폭이 증가할수록 자기공명 주파수가 감소하는 것을 볼 수 있다.
We has been studied the thin film encapsulation effect for organic light-emitting diodes (OLED). To evaluate the passivation properties of the passivation layer materials, we have carried out the fabrication of green light emitting diodes with ultra violet(UV) light absorbing polymer resin, $SiO_2,\;and\;SiN_x$, respectively. From the measurement results of shrinkage properties according to the exposure time to the atmosphere, we found that $SiN_x$ thin film is the best material for passivation layer. We have investigated the emission efficiency and life time of OLED device using the package structure of $OLED/SiN_x/polymer$ resin/Al/polymer resin. The emission efficiency of this OLED device was 13 lm/W and life time was about 2,000 hours, which reach 95 % of the performance for the OLED encapsulated with metal.
The silicon nitride ($SiN_x$) film for surface passivation and anti-reflection coating of crystalline silicon solar cell is very important and it is generally deposited by plasma enhanced chemical vapor deposition (PECVD). PECVD can be divided into low and high frequency method. In this paper, the $SiN_x$ film deposited by low and high frequency PECVD method was studied. First, to optimize the $SiN_x$ film deposited by low frequency PECVD method, the refractive index was measured by varying the process conditions like $SiH_4$, $NH_3$, $N_2$ gas rate, and RF power. When $SiH_4$ gas rate was increased and $NH_3$ gas rate was decreased, the refractive index was increased. The refractive index was also increased with RF power decline. Second, to compare the characteristics of the low and high frequency PECVD $SiN_x$ film, the refractive index was measured by varying $NH_3/SiH_4$ gas ratio and RF power and the minority carrier lifetime of before and after high temperature treatment process was also measured. The refractive index of both low and high frequency PECVD $SiN_x$ film was decreased with increase in $NH_3/SiH_4$ gas ratio and RF power. After high temperature treatment process, the minority carrier lifetime of both low and high frequency PECVD $SiN_x$ film was increased and increased degree was similar. The minority carrier lifetime of low frequency PECVD $SiN_x$ was increased from $11.03{\mu}m$ to $28.24{\mu}m$ and that of high frequency PECVD $SiN_x$ was increased from $11.60{\mu}m$ to $27.10{\mu}m$.
한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권1호
/
pp.659-662
/
2007
The characteristics of a $SiN_x$ passivation layer grown by a specially designed catalyzer enhanced chemical vapor deposition (CECVD) system and electrical and optical properties of OLEDs passivated with the $SiN_x$ layer are described. Despite the low substrate temperature, the single $SiN_x$ passivation layer, grown on the PC substrate, exhibited a low water vapor transmission rate of $2{\sim}6{\times}10^{-2}\;g/m^2/day$ and a high transmittance of 87 %. In addition, current-voltage-luminescence results of an OLED passivated with a 150 nm-thick $SiN_x$ film compared to nonpassivated sample were identical indicating that the performance of an OLED is not critically affected by radiation from tungsten catalyzer during the $SiN_x$ deposition.
3차원 패키지용 고종횡비 TSV(through-Si via)를 이용한 배선 공정에서 via 충진을 위한 대표적인 방법중의 하나가 via 내부에 $SiO_2$ 절연막을 형성한 다음 Sputtering법으로 접착/확산방지막 및 씨앗층을 형성하고 전해도금법으로 Cu를 충진하는 방법이다. 본 연구에서는 Cu 박막과 $SiO_2$ 절연막 사이에 reactive sputtering법으로 증착한 $TaN_x$ 박막의 조성에 따른 접착특성 및 확산방지막특성을 연구하였다. $TaN_x$ 박막의 질소함량에 따른 Cu 박막과 $SiO_2$ 절연막사이의 접착력을 $180^{\circ}$ peel test와 topple test를 이용하여 정량적으로 측정하였다. $TaN_x$ 박막 내 질소함량이 증가함에 따라 접착력은 더욱 증가하였는데, 이는 질소함량이 증가함에 따라 $TaN_x$ 박막과 $SiO_2$ 절연막사이의 계면에서 계면반응물의 생성이 증가하였기 때문으로 해석된다. 고온에서 열처리를 통하여 Cu에 대한 확산방지막으로서의 특성을 조사한 결과, $TaN_x$ 박막은 Ta 박막에 비하여 우수한 Cu에 대한 확산방지 특성을 보였으며 N/Ta성분비 1.4까지는 $TaN_x$ 박막내 질소함량의 증가에 따라 확산방지특성도 향상되었다.
In this study, the influences of silicon-based gas barrier films fabricated by using a facing target sputtering(FTS) system on the gas permeability for flexible displays have been investigated. Under these optimum conditions on the $SiO_x$ film with oxygen concentration($O_2/Ar+O_2$) of 3.3% and the $SiO_xN_y$ film with nitrogen concentration($N_2/Ar+O_2+N_2$) of 30% deposited by the FTS system, it was found that the films were grown about 4 times higher deposition rate than that of the conventional sputtering system and showed high transmittance about 85% in the visible light range. Particularly, the polyethylene naphthalate(PEN) substrates with the $SiO_x$ and/or $SiO_xN_y$ films showed the enhanced properties of decreased water vapor transmission rate (WVTR) over $10^{-1}\;g/m^2{\cdot}day$ compared with the PEN substrate without any gas barrier films, which was due to high packing density in the Si-based films with high plasma density by FTS process and/or the denser chemical structure of Si-N bond in the $SiO_xN_y$ film.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.