  • The development of dry etching process for sapphire wafer with plasma has been key issues for the opto-electric devices. The challenges are increasing control and obtaining low plasma induced-damage because an unwanted scattering of radiation is caused by the spatial disorder of pattern and variation of surface roughness. The plasma-induced damages during plasma etching process can be classified as impurity contamination of residual etch products or bonding disruption in lattice due to charged particle bombardment. Therefor, fine pattern technology with low damaged etching process and high etch rate are urgently needed. Until now, there are a lot of reports on the etching of sapphire wafer with using $Cl_2$/Ar, $BCl_3$/Ar, HBr/Ar and so on [1]. However, the etch behavior of sapphire wafer have investigated with variation of only one parameter while other parameters are fixed. In this study, we investigated the effect of pressure and other parameters on the etch rate and the selectivity. We selected $BCl_3$ as an etch ant because $BCl_3$ plasmas are widely used in etching process of oxide materials. In plasma, the $BCl_3$ molecule can be dissociated into B radical, $B^+$ ion, Cl radical and $Cl^+$ ion. However, the $BCl_3$ molecule can be dissociated into B radical or $B^+$ ion easier than Cl radical or $Cl^+$ ion. First, we evaluated the etch behaviors of sapphire wafer in $BCl_3$/additive gases (Ar, $N_2,Cl_2$) gases. The behavior of etch rate of sapphire substrate was monitored as a function of additive gas ratio to $BCl_3$ based plasma, total flow rate, r.f. power, d.c. bias under different pressures of 5 mTorr, 10 mTorr, 20 mTorr and 30 mTorr. The etch rates of sapphire wafer, $SiO_2$ and PR were measured with using alpha step surface profiler. In order to understand the changes of radicals, volume density of Cl, B radical and BCl molecule were investigated with optical emission spectroscopy (OES). The chemical states of $Al_2O_3$ thin films were studied with energy dispersive X-ray (EDX) and depth profile anlysis of auger electron spectroscopy (AES). The enhancement of sapphire substrate can be explained by the reactive ion etching mechanism with the competition of the formation of volatile $AlCl_3$, $Al_2Cl_6$ or $BOCl_3$ and the sputter effect by energetic ions.

  • PDF

고밀도 유도결합형 $Cl_2/BCL_3/Ar$ 플라즈마를 이용한 sapphire의 식각 특성

  • 성연준;이용혁;김현수;염근영;이재원;채수희;박용조
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2000년도 제18회 학술발표회 논문개요집
    • /
    • pp.31-31
    • /
    • 2000
  • Al2O3는 높은 화학적, 열적 안정성으로 인하여 미세전자 산업에서 절연막이나 광전자소자의 재료로써 널리 이용되고 있다. 특히, 사파이어는 고위도의 LED, 청색 LD의 재료인 GaN 계열의 III-Nitride 물질을 성장시킬 때 필요한 기판으로 보편적으로 사용되고 있다. 이러한 GaN계열의 광소자 제조에서 사파이어 기판을 적용시 지적되는 문제점들 중의 하나는 소자제조 후 사파이어의 결정 구조 및 높은 경도에 의해 나타나는 cutting 및 backside의 기계적 연마가 어렵다는 것이다. 최근에는 이온빔 식각이나 이온 주입 후 화학적 습식 시각, reactive ion etching을 통한 사파이어의 건식 식각이 소자 분리 및 backside 공정을 우해 연구되고 있다. 그러나 이러한 방법을 이용한 사파이어의 식각속도는 일반적으로 15nm/min 보다 작다. 높은 식각율과 식각후 표면의 작은 거칠기를 수반한 사파이어의 플라즈마 식각은 소자 제조 공정시 소자의 isolation 및 lapping 후 연마 공정에 이용할 수 있다. 본 연구에서는 평판 유도결합형 플라즈마를 이용하여 Cl2/BCL3/Ar 의 가스조합, inductive power, bias voltage, 압력, 기판온도의 다양한 공정 변수를 통하여 (0001) 사파이어의 식각특성을 연구하였다. 사파이어의 식각속도는 inductive power, bias voltage, 그리고 기판 온도가 증가할수록 증가하였으며 Cl2에 BCl3를 50%이하로 첨가할 때 BCl3 첨가량이 증가할수록 식각속도 및 식각마스크(photoresist)와의 식각선택비가 증가하는 것을 관찰하였다. 또한, Cl3:BCl3=1:1의 조건에 따라 Ar 첨가에 따른 식각속도 및 표면 거칠기를 관찰하였다. 본 연구의 최적 식각조건인 40%Cl2/40%BCl3/20%Ar, 600W의 inductive power, -300V의 bias voltage, 30mTorr의 압력, 기판온도 7$0^{\circ}C$에서 270nm/min의 사파이어 식각속도를 얻을수 있었다. 그리고 이러한 식각조건에서 표면의 거치기를 줄일수 있었다. 사파이어 식각은 보편적인 사파이어 lapping 공정시 수반되어 형성된 표면의 거치기를 줄이기 위한 마지막 공정에 응용될수 있다. 사파이어의 식각시 나타나는 식각 부산물은 플라즈마 진단방비인 optical emission spectroscopy (OES)를 통하여 관찰하였고, 식각시 사파이어의 표면성분비 변화 및 표면의 화학적 결합은 X-ray photoelectron spectroscopy(XPS)를 사용하여 측정하였다. 시각 전, 후의 표면의 거칠기를 scanning electron microscopy(SEM)을 통하여 관찰하였다.

  • PDF

유도 결합 플라즈마를 이용한 TiN 박막의 식각 특성 (Etch Characteristics of TiN Thin Films in the Inductively Coupled Plasma System)

  • 엄두승;강찬민;양성;김동표;김창일
    • 한국표면공학회지
    • /
    • 제41권3호
    • /
    • pp.83-87
    • /
    • 2008
  • This study described the effects of RF power, DC bias voltage, chamber pressure and gas mixing ratio on the etch rates of TiN thin film and selectivity of TiN thin film to $SiO_2$ with $BCl_3$/Ar gas mixture. When the gas mixing ratio was $BCl_3$(20%)/Ar(80%) with other conditions were fixed, the maximum etch rate of TiN thin film was 170.6 nm/min. When the DC bias voltage increased from -50 V to -200 V, the etch rate of TiN thin film increased from 15 nm/min to 452 nm/min. As the RF power increased and chamber pressure decreased, the etch rate of TiN thin film showed an increasing tendency. When the gas mixing ratio was $BCl_3$(20%)/Ar(80%) under others conditions were fixed, the intensity of optical emission spectra from radical or ion such as Ar(750.4 nm), $Cl^+$(481.9 nm) and $Cl^{2+}$(460.8 nm) was highest. The TiN thin film was effectively removed by the chemically assisted physical etching in $BCl_3$/Ar ICP plasma.

Effects of red ginseng oil(KGC11ℴ) on testosterone-propionate-induced benign prostatic hyperplasia

  • Lee, Jeong Yoon;Kim, Sohyuk;Kim, Seokho;Kim, Jong Han;Bae, Bong Seok;Koo, Gi-Bang;So, Seung-Ho;Lee, Jeongmin;Lee, Yoo-Hyun
    • Journal of Ginseng Research
    • /
    • 제46권3호
    • /
    • pp.473-480
    • /
    • 2022
  • Background: Benign prostatic hyperplasia (BPH) is a disease characterized by abnormal proliferation of the prostate, which occurs frequently in middle-aged men. In this study, we report the effect of red ginseng oil (KGC11o) on BPH. Methods: The BPH-induced Sprague-Dawley rats were divided into seven groups: control, BPH, KGC11o 25, 50, 100, 200, and finasteride groups. KGC11o and finasteride were administered for 8 weeks. The BPH biomarkers, DHT, 5AR1, and 5AR2, androgen receptor, prostate-specific antigen (PSA), Bax, Bcl-2, and TGF-β were determined in the serum and prostate tissue. The cell viability after KGC11o treatment was determined using BPH-1 cells, and, androgen receptor, Bax, Bcl-2, and TGF-β were confirmed by western blotting. Results: In the in vivo study, administration of KGC11o reduced prostate weight by 18%, suppressed DHT (up to 22%) and 5AR2 (up to 12%) levels from administration of 100 mg/kg KGC11o (P < 0.05). PSA was significantly downregulated dose-dependently from at the concentration of 50 mg/kg KGC11o (P < 0.05). BPH-1 cell viability significantly reduced through the treatment with KGC11o. In vitro and vivo, AR, Bcl-2 TGF-β levels reduced significantly but Bax was increased (P < 0.05). Conclusion: These results suggest that KGC11o may inhibit the development of BPH by significantly reducing the levels of BPH biomarkers via 5ARI, anti-androgenic effect, and anti-proliferation effect, serving as a potential functional food for treating BPH.

고밀도 플라즈마를 이용한 $HfAlO_3$ 박막의 식각 특성 연구 (Dry Etching Characteristics of $HfAlO_3$ Thin Films using Inductively Coupled Plasma)

  • 하태경;우종창;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.382-382
    • /
    • 2010
  • The etch characteristics of the $HfAlO_3$ thin films and selectivity of $HfAlO_3$ to $SiO_2$ in $Cl_2/BCl_3$/Ar plasma were investigated in this work. The maximum etch rate was 108.7 nm/min and selectivity of $HfAlO_3$ to $SiO_2$ was 1.11 at $Cl_2$(3sccm)/$BCl_3$(4sccm)/Ar(16sccm), RF power of 500 W, DC-bias voltage of - 100 V, process pressure of 1 Pa and substrate temperature of $40^{\circ}C$. As increasing RF power and DC-bias voltage, etch rates of the $HfAlO_3$ thin films increased. Whereas as decreasing of the process pressure, those of the $HfAlO_3$ thin films were increased. The chemical reaction on the surface of the etched the $HfAlO_3$ thin films was investigated with X-ray photoelectron spectroscopy (XPS).

  • PDF

Etching Characteristics of HfAlO3 Thin Films Using an Cl2/BCl3/Ar Inductively Coupled Plasma

  • Ha, Tae-Kyung;Woo, Jong-Chang;Kim, Chang-Il
    • Transactions on Electrical and Electronic Materials
    • /
    • 제11권4호
    • /
    • pp.166-169
    • /
    • 2010
  • In this study, we changed the etch parameters (gas mixing ratio, radio frequency [RF] power, direct current [DC]-bias voltage, and process pressure) and then monitored the effect on the $HfAlO_3$ thin film etch rate and the selectivity with $SiO_2$. A maximum etch rate of 108.7 nm/min was obtained in $Cl_2$ (3 sccm)/$BCl_3$ (4 sccm)/Ar (16 sccm) plasma. The etch selectivity of $HfAlO_3$ to $SiO_2$ reached 1.11. As the RF power and the DC-bias voltage increased, the etch rate of the $HfAlO_3$ thin film increased. As the process pressure increased, the etch rate of the $HfAlO_3$ thin films increased. The chemical state of the etched surfaces was investigated with X-ray photoelectron spectroscopy. According to the results, the etching of $HfAlO_3$ thin film follows the ion-assisted chemical etching.

고밀도 플라즈마를 이용한 ZnO 박막의 식각 특성 분석 (Etching mechanism of ZnO films using high density plasma)

  • 강찬민;김관하;김창일
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 제37회 하계학술대회 논문집 C
    • /
    • pp.1382-1383
    • /
    • 2006
  • ZnO 박막은 wide band gap(Eg=3.37eV)의 derect band gap을 갖고 있기 때문에 여러 소자로의 응용가능성에 큰 기대를 하고 있는 물질이다. 본 논문에서는 소자 제조과정에서 요구되는 ZnO 박막의 식각변수에 따른 식각율과 식각특성에 관하여 연구하였으며 Inductively coupled plasma(ICP)를 사용하여 $BCl_3$/Ar 가스를 혼합하여 식각을 하였다. $BCl_3$/Ar=8/2 플라즈마에서 화학적 식각의 도움을 받아 ZnO 박막의 식각률은 1724 ${\AA}/min$ 로 최고를 보였으며 이때의 공정 조건은 800 W 의 RF power, 400 W 의 bias power, 1 Pa 의 공정 압력이었다. 식각시에 플라즈마 내부의 이온 거동상태를 측정하기위해 quadrupolemass spectrometer(QMS)를 사용하여 분석하였고 식각후 ZnO 박막의 식각률은 surface profiler(KLA fencer, ${\alpha}$-step 500)을 이용하여 측정하고 ZnO 박막과 B, Cl 라디칼과의 표면 반응 상태를 고찰하기 위하여 식각된 ZnO 박막의 표면을 X-ray photoelectron spectroscopy(XPS)로 분석하였다. XPS를 통하여 ZnO 박막과 Cl 라디칼과 반응을 하여 식각된다는 것과 낮은 휘발성으로 인하여 Ar 이온에 의한 스퍼터링 효과의 도움에 의해서 식각이 진행됨을 확인하였다.

  • PDF

유도결합 플라즈마를 이용한 TiN 박막의 식각 특성 연구 (The etch characteristic of TiN thin films by using inductively coupled plasma)

  • 박정수;김동표;엄두승;우종창;허경무;위재형;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.74-74
    • /
    • 2009
  • Titanium nitride has been used as hardmask for semiconductor process, capacitor of MIM type and diffusion barrier of DRAM, due to it's low resistivity, thermodynamic stability and diffusion coefficient. Characteristics of the TiN film are high intensity and chemical stability. The TiN film also has compatibility with high-k material. This study is an experimental test for better condition of TiN film etching process. The etch rate of TiN film was investigated about etching in $BCl_3/Ar/O_2$ plasma using the inductively coupled plasma (ICP) etching system. The base condition were 4 sccm $BCl_3$ /16 sccm Ar mixed gas and 500 W the RF power, -50 V the DC bias voltage, 10 mTorr the chamber pressure and $40\;^{\circ}C$ the substrate temperature. We added $O_2$ gas to give affect etch rate because $O_2$ reacts with photoresist easily. We had changed $O_2$ gas flow rate from 2 sccm to 8 sccm, the RF power from 500 W to 800 W, the DC bias voltage from -50 V to -200 V, the chamber pressure from 5 mTorr to 20 mTorr and the substrate temperature from $20\;^{\circ}C$ to $80\;^{\circ}C$.

  • PDF

Pb 함량에 따른 PZT 박막의 식각 및 유전특성에 관한 연구 (A study on the Etching and Dielectric Properties of PZT Thin Films with Excess Pb Contents)

  • 김경태;이성갑;김창일;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 춘계학술대회 논문집 전자세라믹스 센서 및 박막재료 반도체재료 일렉트렛트 및 응용기술
    • /
    • pp.56-59
    • /
    • 2000
  • In this study, Ferroelectric $Pb(Zr_x,Ti_{1-x})O_3$(x=0.53) thin films were fabricated by the spin-coating on the Pt/Ti/$SiO_2$/Si substrate using the PZT metal alkoxide solutions with various excess Pb contents. Etching of PZT film was performed using planar inductively coupled Ar(20)$/Cl_2/BCl_3$ plasma. The etch rate of PZT film was 2450 ${\AA}/min$ at Ar(20)$/BCl_3$(80) gas mixing ratio and substrate temperature of $80^{\circ}C$. The leakage current densities of before etching and after etching PZT thin film were $6.25\times10^{-8}A/cm^2$, $8.74\times10^{-7}A/cm^2$ with electric field of 0.07MV/em, respectively.

  • PDF

The Dry Etching Properties on TiN Thin Film Using an N2/BCl3/Ar Inductively Coupled Plasma

  • Woo, Jong-Chang;Joo, Young-Hee;Park, Jung-Soo;Kim, Chang-Il
    • Transactions on Electrical and Electronic Materials
    • /
    • 제12권4호
    • /
    • pp.144-147
    • /
    • 2011
  • In this work, we present a study regarding the etching characteristics on titanium nitride (TiN) thin films using an inductively coupled plasma system. The TiN thin film was etched using a $N_2/BCl_3$/Ar plasma. The studied etching parameters were the gas mixing ratio, the radio frequency (RF) power, the direct current (DC)-bias voltages, and the process pressures. The baseline conditions were as follows: RF power = 500 W, DC-bias voltage = -150 V, substrate temperature = $40^{\circ}C$, and process pressure = 15 mTorr. The maximum etch rate and the selectivity of the TiN to the $SiO_2$ thin film were 62.38 nm/min and 5.7, respectively. The X-ray photoelectron spectroscopy results showed no accumulation of etching byproducts from the etched surface of the TiN thin film. Based on the experimental results, the etched TiN thin film was obtained by the chemical etching found in the reactive ion etching mechanism.