• Title/Summary/Keyword: $H_2O$-Type

Search Result 1,740, Processing Time 0.03 seconds

Preparation of High Tc Superconductor Powders by Emulsion Drying Method (Emulsion 건조방법에 의한 고온초전도체 분말제조)

  • Eom, Woo-Sik;Kim, Ho-Gi
    • Korean Journal of Materials Research
    • /
    • v.1 no.2
    • /
    • pp.71-76
    • /
    • 1991
  • The superconducting powders in $YBa_2Cu_3O_{7-x}$ and Bi-Pb-Sr-Ca-Cu-O system were easily prepared from water in oil type emulsion by loading each cation into the aqueous phase. In $YBa_2Cu_3O_{7-x}$ system, the superconducting orthorhombic phase was formed by calcining at $750^{\circ}C$ for 10h in $O_2$. The size of the superconducting phase powders was submicron. The density of the sintered specimen using this powders was about 95% of the theoretical density and the resistance sharply decreases at about 90K, In Bi-Pb-Sr-Ca-Cu-O system the low Tc phase($(Bi, Pb)_2Sr_2Ca_1Cu_2O_y$) was formed by calcining at $800^{\circ}C$ for 10h in a low oxygen partial pressure of 1/20 atm The shape of clacined powder is thin plate of which size is about $2\mu\textrm{m}$ and thickness is smaller than $\mu\textrm{m}$. It was observed that the high Tc phase ($(Bi, Pb)_2Sr_2Ca_2Cu_3O_y$) was formed by sintering at $850^{\circ}C$ for 30h in oxygen pressure of 1/20 atm without intermediary grinding. The above sintered sample exhibited superconductivity with a Tc(zero)=105K.

  • PDF

Synthesis of P-type Zeolite Using Melting Slag from Municipal Incineration Ash (도시 소각재 용융슬래그로부터 P형 제올라이트 합성)

  • Lee Sung-Ki;Jang Young-Nam;Chae Soo-Chun;Ryu Kyoung-Won;Bae In-Kook
    • Journal of the Mineralogical Society of Korea
    • /
    • v.19 no.1 s.47
    • /
    • pp.7-14
    • /
    • 2006
  • Melting slag generated from the lots of municipal incineration ash, which causes the one of big urban problems in modern industrial society, was used as starting material for the hydrothermal synthesis of zeolite. P-type zeolite has been successfully synthesized by the combined process of both 'hydrogelation' and 'clay conversion' method. Commercial sodium silicate was used as Si source, and $NaAlO_2$ was prepared by the reaction in a $Na_{2}O/Al_{2}O_{3}$ molar ratio of 1.2. The optimum conditions for zeolite synthesis was found to be the $SiO_{2}/Al_{2}O_{3}$ ratio in the 3.2 and 4.2 range, the $H_{2}O/Na_{2}O$ ratio in the 70.7 and 80.0 range, and more than 15-hour reaction time at $80^{\circ}C$, In the synthesized zeolite, inhomogeneous melting slag particles were disappeared and homogeneous P-type zeolite crystal was grown. The cation exchange capacity of the synthesized zeolite was determined to be approx. 240 cmol/kg.

Reaction Characteristics of Combined Steam and Carbon Dioxide Reforming of Methane Reaction Using Pd-Ni-YSZ Catalyst (Pd-Ni-YSZ 촉매를 이용한 수증기-이산화탄소 복합개질 반응 특성)

  • Kim, Sung Su
    • Applied Chemistry for Engineering
    • /
    • v.29 no.4
    • /
    • pp.382-387
    • /
    • 2018
  • In this study, the reaction characteristics of combined steam and carbon dioxide reforming of methane (CSCRM) reaction using Pd-Ni-YSZ catalyst were investigated according to types of catalysts and gas compositions. Catalysts were prepared in the form of powder and porous disk. The injected gases were supplied at different ratios of $CH_4/CO_2/H_2O$. As a result, the conversion of $CH_4$ and $CO_2$ was improved as a result of using the porous disc type catalyst as compared with that of the powder type catalyst. When the $CH_4/CO_2/H_2O$ ratio of the feed gas was 1 : 0.5 : 0.5, the $H_2/CO$ ratio was adjusted close to 2. However, after 6 hours of the reaction, $CH_4$ conversion was partially reduced by the carbon deposition and the pressure drop increased from 0.1 to 0.8. This issue was then solved by optimizing the water content. As a result, it was confirmed that the durability was secured by preventing the carbon deposition when the gas was supplied at a $CH_4/CO_2/H_2O$ ratio of 1 : 0.5 : 1, and the conversion rate was maintained at a relatively high level.

Preparation of nanocrystalline CuO powders by hydrazine method and their gas sensing characteristics (Hydrazine 법에 의한 CuO 미분말의 합성 및 가스 감응성 평가)

  • Kim, Sun-Jung;Lee, Jong-Heun
    • Journal of Sensor Science and Technology
    • /
    • v.16 no.1
    • /
    • pp.11-16
    • /
    • 2007
  • CuO is an important transition metal oxide with many practical applications such as catalysts, p-type semiconductor, solar cells, magnetic storage media and cathode materials. In this contribution, nanocrystalline CuO powders were prepared by solution reduction method using copper chloride ($CuCl_{2}{\cdot}2H_{2}O$), hydrazine ($N_{2}H_{4}$) and NaOH and subsequent heat treatment. The gas sensor using nanocrystalline CuO powders showed high sensitivities to acetone and ethanol.

An experimental study of heat transfer in a submerged water jet (서브머지드 단일수분류의 열전달에 관한 실험적 연구)

  • Ohm, Ki-Chan
    • Journal of the Korean Solar Energy Society
    • /
    • v.25 no.4
    • /
    • pp.101-110
    • /
    • 2005
  • An experimental study of heat transfer of submerged water jet impinging normally on a flat plate is presented. Heat transfer measurements obtained with Reverse cone type nozzle(Rcone) were compared to those obtained with Cone type nozzle(Cone) and Square edged type nozzle(Vert) of the same diameter(D=8mm) for different jet velocities in the range of $3{\sim}7m/s(Re_D=30000{\sim}70000)$ and various nozzle-to target spacings($H/D=2{\sim}10$). The local Nusselt number profiles exhibited a sharp drop for $r/D{\leq}0.5$ and 2nd, 3rd peaks revealed at r/D=2, 3 respectively, followed by a slower decrease there after. The peaks were weakened with increasing the nozzle-to target spacing and decreasing the jet velocity. The stagnation Nusselt number of the Reverse cone type nozzle was larger than those of the other two nozzles for H/D=2. 10, but Cone type nozzle had the highest value for $H/D=4{\sim}8$. Also average Nusselt number of the Reverse cone type nozzle was higher than those of the other two nozzles at $H/D=2{\sim}10$, except for $V_o=7ms$ of H/D=6.

Current-voltage Characteristics of Water-adsorbed Imogolite Film

  • Park, Jae-Hong;Lee, Jung-Woo;Chang, Sun-Young;Park, Tae-Hee;Han, Bong-Woo;Han, Jin-Wook;Yi, Whi-Kun
    • Bulletin of the Korean Chemical Society
    • /
    • v.29 no.5
    • /
    • pp.1048-1050
    • /
    • 2008
  • Electric current flow was observed through imogolite film when imogolite ($(HO)_3Al_2O_3SiOH$) was exposed to water molecules and connected to external electrodes. Current flow was due to the bound water on the surface of imogolite. Current flow increased as the pH of the water decreased. The current-voltage (I-V) measurements from a field effective transistor (FET) using $H_2O$/imogolite film revealed that the current carrier in $H_2O$/ imogolite had p-type characteristics, i.e. the carrier was probably $H^+$. The possible mechanism for current transportation in imogolite/water was also suggested in this paper.

Epithermal Gold-Silver Mineralization and Depositional Environment of Carbonate-hosted Replacement Type Baegjeon Deposits, Korea (탄산염암 층준교대형 백전광상의 천열수 금-은 광화작용과 생성환경)

  • Lee, Chan Hee;Park, Hee-In
    • Economic and Environmental Geology
    • /
    • v.29 no.2
    • /
    • pp.105-117
    • /
    • 1996
  • The Baegjeon Au-Ag and Sb deposits, small of disseminated-type gold deposits are formed as a result of epithermal processes associated a shallow-seated Cretaceous Yeogdun granitoids intrusion. The orebodies are formed by the replacement of carbonate minerals in thin-bedded oolitic limestone beds favorable for mineralization within the upper-most Cambrian Pungchon Limestone Formation. The mineralization can be recognized one stage, ore minerals composed of base metal sulfides, electrum, AgSb-S, Ag-Cu-S, and Sb-S minerals. Gold-bearing minerals consist of electrum and submicroscopic invisible gold in pyrite and arsenopyrite. The composition of electrums ranges from 33.58 to 63.48 atomic % Ag. Fluid inclusion studies reveal that ore fluids were low saline $NaCl-CO_2-H_2O$ system. Temporary fluid mixing and boiling occured in later stage. Fluid inclusion data indicates the homogenization temperatures and salinities of NaCl eqivalent wt% were 176 to $246^{\circ}C$ and from 0.0 to 4.8 wt%, respectively. And $-logfs_2$, of mineralization obtained by thermodynamic considerations as 12.4 to 13.8 atm. The ${\delta}^{34}S_{H_2S}$, values of hydrothermal sulfides were calculated to be 6.8 to 10.2‰ which was of sedimentary origin. The ${\delta}^{18}O_{H_2O}$ and ${\delta}^{13}C_{CO_2}$, range from -3.9 to 9.6‰, from -1.1 to -2.2‰, and ${\delta}D$ range from -89 to -118‰, respectively. The Au deposition during mineralization seems to have occurred as a result of decrease of temperature, $fs_2$, $fo_2$, and pH probably due to oxidation by meteoric water mixing, which destabilized original $Au(HS)^-{_2}$. The mineralization of the Baegjeon deposits is similar to the Carlin-type deposits characterized by sediments-hosted epithermal bedding replacement disseminated gold deposits.

  • PDF

Effects of Titania Whisker Precipitation on Wear Property of the Glass-Ceramic (타이타니아 단섬유상의 석출이 결정화유리의 마모특성에 미치는 영향)

  • 이경호
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.2
    • /
    • pp.192-202
    • /
    • 1996
  • In Li0.4Ca0.05AlP0.5Si0.75O4.5 composition glass, glass-ceramic having a near 100% crystallinity after nucleation heat treatment of 74$0^{\circ}C$/2 h and crystallization heat treatment of 90$0^{\circ}C$/2 h and in-situ TiO2 whisker reinforced glass-ceramic after heat treatment of 105$0^{\circ}C$ for 20 h were fabricated with the addition of 4% TiO2 as a nucleating agent. With these materials a ball-on-disc type wear test was conducted in order to examine the effect of TiO2 whisker prepcipitation on ambient and high temperature wear properties of the glass-ceramic. Wear test results indicated that all specimens exhibited micro-fracture wear mechanism in ambient temperature. As temperature increased the wear rates of the materials were increased. However the in-situ TiO2 whisker reinforced glass-ceramic exhibited the lowest wear rate over the test temperature range. This resulted from the improvement of harness and fracture toughness of the material as the glass converted into the glass-ceramic followed by precipitation of TiO2 whiskers throughout the glass-ceramic matrix.

  • PDF

Experimental of Absorption Performance Enhancement for Binary Nanofluids($NH_3/H_2O$ + Nano Particles) (이성분 나노유체($NH_3/H_2O$+나노입자)의 흡수성능 촉진실험)

  • Lee, Jin-Ki;Jung, Chung-Woo;Koo, June-Mo;Kang, Yong-Tae
    • Proceedings of the SAREK Conference
    • /
    • 2008.06a
    • /
    • pp.124-129
    • /
    • 2008
  • The objectives of this paper are to examine the effect of nano-particles on the pool type absorption heat transfer enhancement and to find the optimal conditions to design a highly effective compact absorber for $NH_3/H_2O$ absorption system. The effect of $Al_2O_3$ and CNT particles on the absorption performance is studied experimentally. The experimental ranges of the key parameters are 20% of $NH_3$ concentration, $0{\sim}0.08%$ (volume fraction) of CNT particles, and $0{\sim}0.06%$ (volume fraction) of $Al_2O_3$ nano-particles. For the $NH_3/H_2O$ nanofluids, the heat transfer rate and absorption rate with 0.02 vol% $Al_2O_3$ nano-particles were found to be 28.9% and 17.8% higher than those without nano-particles, respectively. It is recommended that the concentration of 0.02 vol% of $Al_2O_3$ nano-particles be the best candidate for $NH_3/H_2O$ absorption performance enhancement.

  • PDF

Thermal Deactivation of Plate-type V2O5-WO3/TiO2 SCR Catalyst (Plate-type V2O5-WO3/TiO2 SCR 촉매의 열적 비활성화 특성)

  • Cha, Jin-Sun;Park, Jin-Woo;Jeong, Bora;Kim, Hong-Dae;Park, Sam-Sik;Shin, Min-Chul
    • Applied Chemistry for Engineering
    • /
    • v.28 no.5
    • /
    • pp.576-580
    • /
    • 2017
  • In the present paper, the thermal deactivation characteristics of plate-type commercial $V_2O_5-WO_3/TiO_2$ SCR catalyst were investigated. For this purpose, the plate-type catalyst was calcined at different temperatures ranging from $500^{\circ}C$ to $800^{\circ}C$ for 3 hours. Structural and morphological changes were characterized byXRD, specific surface area, porosity, SEM-EDS and also NOx conversion with ammonia according to the calcine temperature. The NOx conversion decreased with increasing calcine temperature, especially when the catalysts were calcined at temperatures above $700^{\circ}C$. This is because the crystal phase of $TiO_2$ changed from anatase to rutile, and the $TiO_2$ grain growth and $CaWO_4$ crystal phase were formed, which reduced the specific surface area and pore volume. In addition, $V_2O_5$, which is a catalytically active material, was sublimated or vaporized over $700^{\circ}C$, and a metal mesh used as a support of the catalyst occurred intergranular corrosion and oxidation due to the formation of Cr carbide.