• 제목/요약/키워드: $Bi_2$$O_3$

검색결과 1,157건 처리시간 0.026초

$Bi_2O_3$ 첨가하여 소결한 $Y_1Ba_2Cu_3O_{7-y}$계의 초전도성질 (Properties of Superconducting Oxide $Y_1Ba_2Cu_3O_{7-y}$ Sintered with $Bi_2O_3$)

  • 박성;임호빈
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1988년도 춘계학술대회 논문집
    • /
    • pp.3-6
    • /
    • 1988
  • Electrical and magnetic properties of $Y_1Ba_2Cu_3O_7-y$ sintered with $Bi_2O_3$ have been investigated by levitation experiment and the measurement of electrical resistivity. The effects of $Bi_2O_3$ addition on the microstructure of the sintered specimens were also investigated. The electrical resistivity in the normal state is smaller in $Y_{0.85}Bi_{0.15}Ba_2Cu_3O_{7-y}$, where the Bi is substituted into Y site, than in the basic compound $Y_1Ba_2Cu_3O_{7-y}$ due to improved microstructure. On the other hand, the microstructure is poor and electrical resistivity is larger in the $Y_1Ba_2Cu_3O_{7-y}$ sintered with excess $Bi_2O_3$. It appears that the impurity in grain boundary affect the electrical properties significantly but has little effect on the magnetic property.

  • PDF

Ni를 첨가한 ZnO-Bi2O3-Sb2O3계의 소결과 전기적 특성 (Sintering and Electrical Properties of Ni-doped ZnO-Bi2O3-Sb2O3)

  • 홍연우;신효순;여동훈;김종희;김진호
    • 한국전기전자재료학회논문지
    • /
    • 제22권11호
    • /
    • pp.941-948
    • /
    • 2009
  • The present study aims at the examination of the effects of 1 mol% NiO addition on the reaction, microstructure development, resultant electrical properties, and especially the bulk trap and interface state levels of $ZnO-Bi_2O_3-Sb_2O_3$ (Sb/Bi=0.5, 1.0, and 2.0) systems (ZBS). The samples were prepared by conventional ceramic process, and characterized by density, XRD, SEM, I-V, impedance and modulus spectroscopy (IS & MS) measurement. The sintering and electrical properties of Ni-doped ZBS (ZBSN) systems were controlled by Sb/Bi ratio. Pyrochlore ($Zn_2Bi_3Sb_3O_{14}$) was decomposed more than $100^{\circ}C$ lowered in ZBS (Sb/Bi=1.0) by Ni doping. The reproduction of pyrochlore was suppressed by the addition of Ni in ZBS. Between two polymorphs of $Zn_7Sb_2O_{12}$ spinel ($\alpha$ and $\beta$), microstructure of ZBSN (Sb/Bi=0.5) composed of a-spinel was more homogeneous than $Sb/Bi{\geq}1.0$ composed of $\beta$-spinel phase. In ZBSN, the varistor characteristics were not improved drastically (non-linear coefficient $\alpha\;=\;6{\sim}11$) and independent on microstructure according to Sb/Bi ratio. Doping of Ni to ZBS seemed to form ${V_0}^{\cdot}$ (0.33 eV) as dominant bulk defect. From IS & MS, especially the grain boundaries of Sb/Bi=0.5 systems were divided into two types, i.e. sensitive to oxygen and thus electrically active one and electrically inactive intergranular one with temperature.

MOCVD $Bi_4Ti_3O_{12}$ 박막의 실리콘 위에서의 증착기구 및 유기금속 원료의 펄스주입법에 의한 박막 특성 개선

  • 이석규;김준형;황민욱;엄명윤;김윤해;김진용;김형준
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2000년도 제18회 학술발표회 논문개요집
    • /
    • pp.103-103
    • /
    • 2000
  • 강한 결정 방향 의존성과 낮은 항정계를 갖는 Bi4Ti3O12 강유전체 박막은 NDRO형 비휘발성 강유전체 메모리 분야에서 매우 유망한 재료이다. 이를 위해서는 실리콘 기판과의 계면조절과 실리콘 기판성에서 고품질의 강유전성 박막을 성장시키는 기술이 필수적이다. MOCVD에 의한 Bi4Ti3O12 의 증착에서는 Bi 성분의 강한 휘발 특성과 낮은 반응성으로 인하여 조성과 두께 등의 조절이 매우 어렵다. 따라서 화학기상증착의 기구를 이해하고 제어하는 기술이 양질의 박막을 얻는데 필수적이다. 본 연구에서는 유기금속 원료 TPB, TIP 과 산소를 이용하여 실리콘 기판위에 Bi4Ti3O12 강유전체 박막을 증착할 때, 증착 변수의 변화에 따른 박막의 증착 거동과 구조적, 전기적 특성을 연계하여 분석하였다. 특히 기판부착력이 낮고 휘발성이 강한 Bi의 특성으로 인한 문제를 개선하기 위하여 TIP원료를 주기적으로 공급, 중단을 반복하는 펄스주입법을 고안하여 그 효과를 살펴보았다. 실리콘 기판위에서 TiO2의 증착속도는 실험온도 영역에서 온도에 따라 변화하지 않는 전형적인 물질 전달에 의해 지배되는 양상을 나타내었다. 반면 Bi2O3 경우에는 50$0^{\circ}C$ 이상에서 급격하게 증착속도가 감소하는 특이한 경향을 나타내었으며 이는 Bi2O3의 높은 휘발성 때문일 것이다. Bi4Ti3O12 박막은 온도증가에 따라 증착속도가 증가한 후 $600^{\circ}C$ 이상에서 포화되는 경향을 보였다. 이로부터 실리콘 기판위에서의 Bi4Ti3O12 박막의 증착 모델을 제시하였다. Bi2O3에 비해 상대적으로 표면 부착력이 월등히 큰 TiO2가 우선적으로 실리콘 펴면에 형성된 후 TPB 유기금속 원료가 이 TiO2와 반응하는 과정으로 Bi4Ti3O12 박막이 증착된다. $600^{\circ}C$이상에서는 증착 변수들을 바꾸어도 물성이 변하지 않는 자기조절기능이 있음을 알 수 있었는데 이는 고온에서의 Bi2O3의 강한 휘발성 때문일 것이다. 실리콘 기판에서 층상 페로브스카이트 상은 58$0^{\circ}C$ 이상에서 형성되며, 매우 좁은 온도 변화에도 결정구조, 박막현상 및 성분이 크게 바뀌는 온도에 민감한 증착거동이 관찰되었다. 증착 모델에서 예견되는 Bi의 불리함을 개선하기 위해 펄스주입법을 실시한 경우 Bi의 성분량이 증가되었고 결정성이 향상되었다. 이로부터 펄스주입법이 박막내에 부족하기 쉬운 Bi를 보충하여 박막의 특성을 개선함을 확인하였다. Bi4Ti3O12 박막의 증착온도에 따른 누설전류 특성 측정 결과 증착온도가 감소할수록 누설전류가 감소함을 알 수 있었고 펄스주입법이 연속주입법보다 더 낮은 누설전류를 보임을 알았다. 펄스주입법의 경우 -2.5V 인가 시의 누설전류는 7.4$\times$10-8A/cm2에서 1.3$\times$10+7A/cm2의 매우 우수한 값을 가졌다. 연속 주입법에 의해 증착된 박막은 C-V 측정 결과 강유전성 이력이 나타나지 않았으나, $600^{\circ}C$ 이상에서 펄스주입법에 의해 증착된 박박은 강유전성 이력을 나타내었다.

  • PDF

Pd 나노입자가 코팅된 β-Bi2O3 나노와이어의 NO2 검출 특성 (NO2 Sensing Properties of β-Bi2O3 Nanowires Sensor Coated with Pd Nanoparticles)

  • 박성훈;강우승
    • 한국표면공학회지
    • /
    • 제48권6호
    • /
    • pp.303-308
    • /
    • 2015
  • Pd-functionalized ${\beta}-Bi_2O_3$ nanowires are synthesized by thermal evaporation of Bi powder using VLS mechanism followed by Pd coating and annealing. In this study, sensing properties of Pd-functionalized ${\beta}-Bi_2O_3$ nanowires sensor to selected concentrations of $NO_2$ gas were examined. Scanning electron microscopy showed that the nanowires with diameters in a range of 100 - 200 nm and lengths of up to a few tens of micrometers. Transmission electron microscopy and X-ray diffraction confirmed that the products corresponded to the nanowires of ${\beta}-Bi_2O_3$ crystals and Pd nanoparticles. Pd-functionalized ${\beta}-Bi_2O_3$ nanowires sensor showed an enhanced sensing performance to $NO_2$ gas compared to as-synthesized ${\beta}-Bi_2O_3$ nanowires sensor. As synthesized and Pd-functionalized ${\beta}-Bi_2O_3$ nanowire sensors showed responses of 178% - 338% and 196% - 535% at $300^{\circ}C$, respectively, to 0.05 - 2 ppm $NO_2$. In addition, the underlying mechanism of the enhancement of the sensing properties of ${\beta}-Bi_2O_3$ nanowires by Pd-functionalization is discussed.

$Bi_2O_3$ 첨가에 따른 (Na,K,Li)$NbO_3$계 무연 압전 세라믹스의 압전특성 (The Piezoelectrc properties of (Na,K)$NbO_3$-system Pb-free Piezoelectric Ceramics with $Bi_2O_3$ Addition)

  • 류성림;이호일;배세환;김주현;김용주;서상현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.216-217
    • /
    • 2005
  • In this paper, in order to develop Pb-free piezoelectric ceramics, $(Li_{0.05}Na_{0.57}K_{0.38})NbO_3$ ceramic was fabricated with the variation of $Bi_2O_3$ addition. Piezoelectric properties of the ceramic were varied with the amount of $Bi_2O_3$ addition and showed the maximum kp value at.0.2 wt% $Bi_2O_3$ addition. Qm of $Bi_2O_3$ added ceramics showed lower values than the non-added ceramics, however, the kp was increased by the addition of $Bi_2O_3$ up to 0.2 wt%. At the sintering temperature of 1110$^{\circ}C$ and the calcination temperature of 850$^{\circ}C$, the optimal values of density=4.52g/$cm^3$, kp=0.47, $\varepsilon_r$=400 were obtained.

  • PDF

펄스레이저 증착법으로 제작된 $Bi_4Ti_3O_{12}/LaAlO_3$ 박막과 $Bi_4Ti_3O_{12}/YBa_2Cu_3O_{7-x}/LaAlO_3$ 복합구조의 에피 성장 (Epitaxial Growth of Pulsed-Laser Deposited Bi4Ti3O12/LaAlO3 Thin Films and Bi4Ti3O12/YBa2Cu3O7-x/LaAlO3 Heterostructure)

  • 조월렴;조학주;노태원
    • 한국결정학회지
    • /
    • 제5권2호
    • /
    • pp.85-92
    • /
    • 1994
  • 펄스 레이저 증착법을 이용하여 강유전체 Bi4T13012 박막을 laA109(001) 위에 성장시켰다. 넓은 영역의 온도에서 증착한 박막의 상 형성과 구조적 성질을 X선 회절법을 이용하여 조사하였다. 740℃에서 증착한 박막은 박막의 c-축이 기판에 수직한 형태의 에피 성장의 경향을 보인다. 펄스 레이저 증착법을 이용하여 Bi4Ti3O12/YBa2Cu3O7-x/LaAlO3 복합구조를 in-situ 성장시켰다. Yba2Cu3O7-x의 a-, b-축이 LaAlO3와 완벽하게 평행하게 배열되어 있지 않음에도 불구하고, Bi4Ti3012 박막은 에피 성장의 경향을 보인다.

  • PDF

X-선 광전자 분광법(XPS)을 이용한 $PbO-Bi_2O_3-Ga_2O_3$계 적외선 투과 유리의 구조해석 (Structural Investigation of Infrared Transmitting $PbO-Bi_2O_3-Ga_2O_3$ Glasses by X-ray Photoelectron Spectroscopy)

  • 허종;김춘곤;김유성
    • 한국세라믹학회지
    • /
    • 제30권11호
    • /
    • pp.911-918
    • /
    • 1993
  • X-ray photoelectron spectroscopy(XPS) has been empolyed to investigate the structure of PbO-Bi2O3-Ga2O3 glasses. XPS OIS spectra recorded from binary PbO-Ga2O3 glasses clearly showed the presence of two peacks due to bridging and non-bridging oxygens, respectively. Gaussin best-fit deconvolution of the OIS peaks suggested there are substaintial amount of non-bridging oxygens in the structure. Therefore, in addition to the glassforming and charge compensating roles of PbO as suggested from the previous works, role of PbO as network modifiers needs to be considered. Addition of Bi2O3 to binary glasses resulted in the rapid decrease in the amount of non-bridging oxygens as well as in values of FWHM (Full Width at the Half Maximum intensity). It is believed that Bi2O3 form distorted BiO6 octahedra and therefore, work as intermediates. Infrared spectra also suggested that Ga2O3 behave as network-formers in the form of GaO4- tetrahedra.

  • PDF

열처리에 따른 ZnO 바리스터의 비직선 계수의 영향 (Effect of Heat Treatment on the Nonlinear Exponents in ZnO Varistors)

  • 안충선;심영재;조병두
    • 한국세라믹학회지
    • /
    • 제29권2호
    • /
    • pp.161-165
    • /
    • 1992
  • Nonlinear exponents and electron trap density variations were observered in ZnO-Bi2O3-MnO2 ternary ZnO varistors as a function of heat treatment temperature. Three kinds of ZnO varistor compositions were selected; i.e. 99.0 ZnO-0.5 Bi2O3-0.5 MnO2, 98.5 ZnO-1.0 Bi2O3-0.5 MnO2, and 98.0 ZnO-1.5 Bi2O3-0.5 MnO2 in mol%. Sintering was done at 1150$^{\circ}C$ for three hours, and heat treatments were done at 500$^{\circ}C$, 700$^{\circ}C$, and 900$^{\circ}C$. When heat treated at 500$^{\circ}C$, nonlinear exponents were increased regardless of the Bi2O3 amount. Increasing heat treatment temperature above 500$^{\circ}C$ resulted in lowering nonlinear exponents. Nonlinear exponents seem to be related to the 0.17 and 0.33 eV electron traps which are possibly of intrinsic origin.

  • PDF

ZnO-Bi2O3 세라믹스의 비오옴 특성에 대한 Intergranular Layer의 영향 (The Effects of Intergranular Layer on the Nonohmic Characteristics of ZnO-Bi2O3 Ceramics)

  • 김경남;한상목
    • 한국세라믹학회지
    • /
    • 제26권4호
    • /
    • pp.487-492
    • /
    • 1989
  • The microstructure and electrical properties of ZnO-Bi2O3 system with Bi2O3(0.5~5mol%) content have been investigated in relatin to sintering temperature and atmosphere. The grain size of ZnO increases sharply with Bi2O3(0.5~5mol%) content, but over 0.5mol% Bi2O3 increased less rapidly when sintered at 120$0^{\circ}C$. Electrical characteristics varied with sintering atmosphere and air-sintered conditions showed comparatively lower nonlinear exponents than the double-crucible conditions. Calculated barrier voltage was about 1.7V.

  • PDF

공침법에 의한 지르코니아분말의 합성 및 특성 III) ZrO2-Y2O3-Bi2O3의 특성 및 소결성 (A Synthesis and Characteristics for Zirconia Powders by Coprecipitation Method ; III) The Properties and Sinterabilities of ZrO2-Y2O3-Bi2O3)

  • 윤종석;이동인;오영제;이희수
    • 한국세라믹학회지
    • /
    • 제26권5호
    • /
    • pp.655-660
    • /
    • 1989
  • The physical properties and sinterabilities of ZrO2-Y2O3-Bi2O3 ternary system powder prepared by coprecipitation were investigated. The crystallization temperatures of ternary system were increased and the specific surface areas were decreased with increasing Bi2O3 amount as sintering agents both PSZ and FSZ. Especially, the partially stabilized zirconia showed monoclinic phase. The sinterability was increased with the amount of Bi2O3 added which caused liquid phase sintering.

  • PDF