Microstructure and Phase Transition of ZnO Varistor Ceramics (ZnO 바리스터 세라믹스의 미세구조와 상전이)

  • 김경남;한상목
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.2
    • /
    • pp.160-166
    • /
    • 1991
  • Microstructure and phase changes during the sintering of ZnO varistors were studied in ZnO-Bi2O3-CoO-Sb2O3 and ZnO-Bi2O3-CoO-Sb2O3-Cr2O3 systems using acanning electron microscopy (SEM) with an energy dispersive X-ray analysis (EDAX), X-ray diffraction (XRD) and differential thermal analysis (DTA). The spinel phase and the Bi2O3 phase were formed by the decomposition of the pyrochlore phase during heating. The spinel particles (2-4$\mu\textrm{m}$), which were formed both along ther grain boundaries and within the ZnO grain, were always found near the pyrochlore phase. Intergranular phases (Bi2O3 and pyrochlore) were precipitated from the liquid phase during cooling. The Bi2O3 phases were located at the triple (or multiple) point of the ZnO grains. Cr2O3 played a role in decreasing the formation temperature of the spinel phase and Bi2O3 phase during sintering, and inhibited the grain growth.

  • PDF

Distribution Behavior of Bi and Pb Between Molten PbO-SiO2 Slag and Bi (용융(熔融) PbO-SiO2계(系) 슬래그와 Bi 사이의 Bi와 Pb의 분배거동(分配擧動))

  • Kim, Se-Jong;Kim, Eung-Jin;Sohn, Ho-Sang
    • Resources Recycling
    • /
    • v.21 no.5
    • /
    • pp.65-71
    • /
    • 2012
  • The equilibrium distribution of bismuth and lead between molten PbO-$SiO_2$ slag and bismuth phase was studied in the temperature range of $775^{\circ}C$ to $850^{\circ}C$ in a MgO crucible. The oxygen partial pressure of atmosphere was controlled by $P_{CO2}/P_{CO}$ ratio. The value of $(%PbO)_{slag}/[%Pb]_{metal}$ increased with increasing $SiO_2$ content of slag, and the value of $(%Bi_2O_3)_{slag}/[%Bi]_{metal}$ decreased with increasing $SiO_2$ content of slag. The concentration of Pb in metal increased with increasing temperature. These experimental results agreed well with the thermodynamic prediction.

The Phse Stability and the Electrical Properties of $3Bi_2O_3.WO_3$ Solid Electrolyte ($3Bi_2O_3.WO_3$ 고체전해질의 상안정성과 전기적 특성)

  • 백현덕;이윤직;박종욱
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.2
    • /
    • pp.248-256
    • /
    • 1995
  • The electrical conducton in the sintered 3Bi2O3.WO3 solid electrolyte was investigated by measuring the conductivity and ionic transport number. The electrical conductivity was about three to ten times higher than that of YSZ at temperatures between 300 and 80$0^{\circ}C$. D.C. polarization method confirmed that 3Bi2O3.WO3 was predominantly an ionic conductor. Unlike the instability of high conductive fcc phase in the rare-earth oxide-Bi2O3 or Y2O3-Bi2O3 systems at temperature below $700^{\circ}C$, fcc phase in the 3Bi2O3.WO3 exhibited no transformation even after annealing over 900 hrs at 600 and $650^{\circ}C$. Two samples which had different grain sizes showed almost the same conductivity. This result suggests that the electrical properties of grain and grain boundry were very similar.

  • PDF

Effect of $M_2O_3$ on the Sinterbility and Electrical Conductivity of $ZrO_2(Y_2O_3)$ System (I): Ceramics of the:$ZrO_2-Y_2O_3-Bi_2O_3$ System ($ZrO_2(Y_2O_3)$ 계 세라믹스의 소결성과 전기전도도에 대한 $M_2O_3$의 영향 (I):$ZrO_2-Y_2O_3-Bi_2O_3$계 세라믹스)

  • 오영제;정형진;이희수
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.3
    • /
    • pp.87-93
    • /
    • 1986
  • Yttria-bismuth-stabilized zirconia was investigated with respect to the amount of $Bi_2O_3$ addition in the ran-ge of 0.5~5mol% to the base composition of $(ZrO_2)_{0.92}(Y_2O_3)_{0.08}.Bismuth was introduced into the ma-terial with $Bi_2O_3-SiO_2$ glasses in order to reduce the evaporation of components. The sinterbility evaporation of components phase formation and microstructure were evaluated depending on the amount of $Bi_2O_3-SiO_2$ glass addition. Two probe A. C conductivity measurement was subjected to all the specimens and the result was discussed on the possible substitution of $Bi^{3+}$ for $Zr^{4+}$ and interistial $Si^{4+}$ in the fluorite structure of zirconia crystal there-upon the possible change in the capability of oxygen transference within the material. It was found that the addition of $Bi_2O_3$ could improve the sinterbility of material very much while not so much.oxygen sensing material suitable for relative low temperature firing.

  • PDF

Tunneling Characteristics in $Pb/Bi_2Sr_2CaCu_2O_{8+\delta}$ Junctions as an Evidence for a d-wave Order Parameter Symmetry in $Bi_2Sr_2CaCu_2O_{8+\delta}$ Superconductors ($Bi_2Sr_2CaCu_2O_{8+\delta}$ 고온초전도체의 d-파 대칭성 증거로서의 $Pb/Bi_2Sr_2CaCu_2O_{8+\delta}$접합 투과전도특성)

  • Chang, Hyun-Sik;Lee, Hu-Jong
    • Progress in Superconductivity
    • /
    • v.2 no.2
    • /
    • pp.65-70
    • /
    • 2001
  • $Pb/Bi_2Sr_2CaCu_2O_{8+\delta}$-single-crystal junctions with the tunneling direction along the c axis of the crystal were fabricated to obtain an s-wave-superconductor/d-wave-superconductor Josephson junctions. The tunneling R (T) curves and current-voltage characteristics show distinct features which can be explained only under the assumption that the order parameter of high-$T_c/Bi_2Sr_2CaCu_2O_{8+{\delta}}$ superconductors has a pure d-wave symmetry, which is in contrast to the case of $YBa_2Cu_3O_{7+{\delta$}}$erconductors where a minor s-wave component is also present..

  • PDF

DATA and FT-IR absorption spectra of PbO-Bi2O3-B2O3-SiO2 glasses (PbO-Bi2O3-B2O3-SiO2 유리계 열시차분석과 FT-IR 흡수 스펙트럼)

  • Lee, Chan-Ku;Lee, Su-Dae
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.8 no.1
    • /
    • pp.17-22
    • /
    • 2003
  • The experimental FT-IR spectra and DTA curves of the $PbO-Bi_2O_3-B_2O_3-SiO_2$ glasses have been investigated. The composition ratio dependence of glass transition temperature showed that the structure of this glass system changes at 60 mol% $Bi_2O_3$. We have observed that the FT-IR spectra of the investigated samples with high bismuth content are dominated by bands associated to the structural units of the heaviest cation, $Bi^{3+}$ and the boron atoms in the treated samples are three and four coordinated even for very high $Bi_2O_3$ content. The low intensity of these non-bridging oxygen bands, for high PbO content glasses, can be attributed to the strong network-forming roles of PbO. The glasses absorption bands exhibited a greater change in intensities on crystallization.

  • PDF

Electrical Characteristics and Microstructure Control of Zinc Oxide Viaristors (ZnO 바리스터의 미세구조제어와 전기적 특성)

  • Kim, Gyeong-Nam;Han, Sang-Mok
    • Korean Journal of Materials Research
    • /
    • v.1 no.2
    • /
    • pp.65-70
    • /
    • 1991
  • The effect of inclusion particles on the microstructure development and electrical characteristics in the systems $ZnO-Bi_2O_3-CoO-Sb_2O_3\;and\;ZnO-Bi_2O_3-CoO-Sb_2O_3-Cr_2O_3 were investigated. The growth of ZnO grains, which was controlled by the spinel particles during sintering, decreased with increasing amount of spinel particles. Addition of $Cr_2O_3(0.5mol\%) increased the breakdown voltage without affecting the non-linear characteristics. The calculated barrier voltage of the $ZnO-Bi_2O_3-CoO-Sb_2O_3\;-and\;ZnO-Bi_2O_3-CoO-Sb_2O_3-Cr_2O_3$ systems were about 3.1V and 2.9V, respectively.

  • PDF

Investigation of low temperature sintering property and fabrication in $Bi_2(Zn_{1/3}Nb_{2/3})_2O_7\;and\;(Bi_{1.5}Zn_{0.5})(Zn_{0.5}Nb_{1.5})O_7$ pyrochlore ($Bi_2(Zn_{1/3}Nb_{2/3})_2O_7\;and\;(Bi_{1.5}Zn_{0.5})(Zn_{0.5}Nb_{1.5})O_7$ pyrochlore의 제조 및 저온 소결 특성 고찰)

  • Kim, Kwan-Soo;Yoon, Sang-Ok;Kim, Shin;Kim, Yun-Han;Kwan, Oh-Young;Park, Jong-Guk;Shim, Sang-Heung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.245-245
    • /
    • 2007
  • 본 연구는 $Bi_2O_3$, ZnO 및 $Nb_2O_5$로 이루어진 두 가지의 $Bi_2(Zn_{1/3}Nb_{2/3})_2O_7$$(Bi_{1.5}Zn_{0.5})(Zn_{0.5}Nb_{1.5})O_7$ pyrochlore를 제조한 후, ZBS 및 BZBS 유리를 각각 첨가하여 저온 소결 및 마이크로파 유전 특성을 고찰하였다. 두 가지의 pyrochlore에 대하여 하소 온도에 따른 상 합성 유무를 고찰한 결과 $900^{\circ}C$에서 단일 상을 갖는 pyrochlore를 제조할 수 있었다. 두 가지의 pyrochlore에 ZnO-rich ZBS 유리와 $Bi_2O_3$-rich BZBS 유리를 3, 5 wt%로 첨가한 후 $800{\sim}950^{\circ}C$에서 소결한 결과 ZBS 및 BZBS 유리를 5wt%를 첨가하였을 때 $900^{\circ}C$에서 소결이 가능하였다. 또한 마이크로파 유전 특성을 고찰한 결과, $(Bi_{1.5}Zn_{0.5})(Zn_{0.5}Nb_{1.5})O_7$의 pyrochlore는 고주파에서 유전 특성 측정이 되지 않았다. $Bi_2(Zn_{1/3}Nb_{2/3})_2O_7$의 pyrochlore의 경우 5 wt% ZBS 및 BZBS 유리를 첨가하여 $900^{\circ}C$에서 소결한 시편의 마이크로파 유전 특성은 ${\varepsilon}_r$= 62.8~68.3, $Q{\times}f$ value= 3,500~2,700 GHz을 나타내었다.

  • PDF

Growth of Bi:YIG Thick Films by Change of PO/Bi2O3 Molar Ratio (PO/Bi2O3 변화에 따른 Bi:YIC 단결정 후박의 성장)

  • 윤석규;김근영;김용탁;정현민;임영민;윤대호
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.6
    • /
    • pp.589-593
    • /
    • 2002
  • The single crystalline thick fi1ms of Bi:Y$_3$Fe$_{5}$ $O_{12}$(Bi:YIG) were grown on (GdCa)$_3$(GaMgZr)$_{5}$ $O_{12}$(SGGG) by Liquid Phase Epitaxy (LPE). The changes of lattice mismatch and Bi concentration were investigated in the thick film growth as a function of PO/Bi$_2$ $O_3$ molar ratio, with keeping constant of substrate rotation speed, supercooling and growth time. It was grown that the lattice constant of the garnet single crystalline thick films and Bi content increased with decreasing of PO/Bi$_2$ $O_3$ molar ratio. Bi concentration decreased with increasing of the film thickness.

Photocatalytic Decomposition of Rhodamin B over Bi2MoO6 Prepared Using Hydrothermal Process (수열합성법으로 제조된 Bi2MoO6에서 로다민 B의 광촉매 분해 반응)

  • Hong, Seong-Soo
    • Clean Technology
    • /
    • v.25 no.2
    • /
    • pp.123-128
    • /
    • 2019
  • $Bi_2MoO_6$ catalysts were successfully synthesized using ethylene glycol monomethyl ether (EGME), glycerol (GL), ethylene glycol (EG), and water as solvents by a conventional hydrothermal method. The synthesized catalysts were characterized by XRD, DRS, BET, SEM, and PL, and we also investigated the photocatalytic activity of these materials for the decomposition of Rhodamin B under visible light irradiation. The XRD results revealed the successful synthesis of 12-18 nm, well-crystallized ${\gamma}-Bi_2MoO_6$ crystals with an Aurivillius structure regardless of solvent. In addition, the $Bi_2MoO_6$ catalysts prepared below $140^{\circ}C$ showed an amorphous phase; however, those prepared above $160^{\circ}C$ showed well-crystallized ${\gamma}-Bi_2MoO_6$ crystals. All the catalysts have a similar absorption spectrum from the ultraviolet region up to the visible region less than 470 nm. This result suggests that all the $Bi_2MoO_6$ catalysts are potential visible-light-driven photocatalysts. The $Bi_2MoO_6$ catalysts prepared using EGME as a solvent showed the highest photocatalytic activity. In addition, the $Bi_2MoO_6$ catalysts prepared at $180^{\circ}C$ showed the highest photocatalytic activity. The PL peaks appeared at about 560 nm at all catalysts and the excitonic PL signal was proportional to the photocatalytic activity for the decomposition of Rhodamin B. This suggests that the stronger the PL intensity, the larger the amount of oxygen vacancies and defects, and the higher the photocatalytic activity.